Search NASA⌕ Search

SEARCH · Search NASA

Results for “stainless steel corrosion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Understanding the efficacy of concentrated interstitial carbon in enhancing the pitting corrosion resistance of stainless steel

By introducing a high fraction of interstitial carbon through low temperature carburization, the pitting corrosion resistance of austenitic stainless steel can be significantly improved. Previous work attributed this to strengthening of the passive film by carbon. Here, however, we present a paradigm shift by showing that carbon actually weakens the passive film but strengthens the bonding within the alloy by forming localized (covalent) bonds with the metal atoms (Fe, Cr, Ni). Accordingly, the enhancement in pitting resistance is a result of carbon reducing the metal dissolution rate in a local pit environment by many orders of magnitude, which extremely decreases the growth stability of a pit and prevents it from transitioning into stable growth. Electronic structure calculations confirm that carbon bonds to the metal atoms and that the metal–carbon bonds are 1.4 to 2.0 times stronger than the metal–metal bonds. These results suggest a new strategy for the design of corrosion resistant alloys, namely surface engineering by infusion of concentrated interstitials that form strong bonds with the matrix atoms.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of Microstructural Bands on the Localized Corrosion of Laser Surface-melted 316L Stainless Steel

The localized corrosion of laser surface melted (LSM) 316L stainless steel is investigated by a combination of potentiodynamic anodic polarization in 0.1M HCl and microscopic investigation of the initiation and propagation of localized corrosion. The pitting potential of LSM 316L is significantly lower than the pitting potential of wrought 316L. The LSM microstructure is highly banded as a consequence of the high laser power density and high linear energy density. The bands are composed of zones of changing modes of solidification, cycling between very narrow regions of primary austenite solidification and very wide regions of primary ferrite solidification. Pits initiate in the outer edge of each band where the mode of solidification is primary austenite plane front solidification and primary austenite cellular solidification. The primary austenite regions have low chromium concentration (and possibly low molybdenum concentration), which explains their susceptibility to pitting corrosion. The ferrite is enriched in chromium, which explains the absence of pitting in the primary ferrite regions. The presence of the low chromium regions of primary austenite solidification explains the lower pitting resistance of LSM 316L relative to wrought 316L. The influence of banding on localized corrosion is applicable to other rapidly solidified processes such as additive manufacturing.

36 MATERIALS SCIENCE↗

Corrosion of 316L & 316H stainless steel in molten LiF-NaF-KF (FLiNaK)

The corrosion behavior of 316L and 316H stainless steels (low and high carbon, respectively) in molten LiF-NaF-KF (FLiNaK) salt at 700 °C for 500 h has been investigated. Tests were performed in 316L stainless steel, pyrolytic boron nitride, and glassy carbon capsule materials. The capsule material had a notable effect on the corrosion behavior of the two stainless steels. Further, the modes of corrosion for the two types of stainless steel in various capsule materials were classified into three categories, namely, uniform surface recession, selective grain boundary Cr dissolution, and the dissolution of Cr in the bulk grains. By most metrics, the 316H stainless steel exhibited slightly superior corrosion resistance, while by others the two stainless steels were comparable. These differences in corrosion behavior are attributed to the differences in grain size and the degree of sensitization.

36 MATERIALS SCIENCE↗

Effect of thermal aging on corrosion behavior of duplex stainless steels

Abstract Despite their exceptional mechanical and corrosion properties, duplex stainless steels (DSS) have not found widespread use in high-temperature applications due to concerns over thermal aging and embrittlement at elevated operational temperatures (> 300 °C). The present study investigated the effect of thermal aging time on the electrochemical properties of lean and standard grade DSS that are exposed to a range of pressurized water reactors containing LiOH and H 3 BO 3 . The results indicated that the electrolyte chemistry plays a significant role in the corrosion behavior of the DSS alloys. Corrosion resistance decreased with thermal aging time for all DSS alloys; however, standard grade DSS (2205 and 2209-w) alloys showed better corrosion resistance than lean grades (2003, 2101, 2101-w). The presence of dissolved oxygen in the electrolytes resulted in a significant increase in corrosion rate for the DSS alloys, but it did not affect the general trend of corrosion rates with aging time. All DSS alloys became vulnerable to pitting corrosion due to chloride addition, but the pitting resistance decreased with increasing thermal aging time. Increased boron B content resulted in degradation of corrosion resistance of the DSS alloys, while minor changes in pH did not show a significant change in corrosion resistance. Mechanical and metallurgical characterization coupled with electrochemical characterization of the DSS alloys gave a comprehensive insight into the effects of thermal aging on the electrochemical response of the DSS. Graphical abstract

Murkute, Pratik (ORCID:0000000278636346)↗

Corrosion of 304 stainless steel in static liquid lithium under high vacuum

To study the compatibility especially the corrosion characteristic of structural material stainless steel (SS) with liquid lithium (Li) is an important factor for the simultaneous application of liquid Li and SS as a blanket material or potential plasma facing material (PFM) in future fusion devices. Here, the corrosion behaviors of 304SS exposed to liquid Li at 700 K for 1320 hr under high vacuum were investigated. After exposure to liquid Li, 304SS produces non-uniform corrosion which includes corrosion products and grain boundary corrosion. Compared with the corrosion behaviors at 600 K and 640 K, temperature plays an important role in the corrosion behaviors of 304SS in static liquid Li. The weight loss, corrosion depth and corrosion products of 304SS specimens increase with the corrosion temperature. In general, the compatibility between 304SS and static liquid Li is relatively good under the experimental conditions. And besides, it is unexpectedly found that the compatibility of copper with Li is not good.

304SS↗

Corrosion interactions between stainless steel and lead vanado-iodoapatite nuclear waste form part II

This paper studied the release of iodine from lead vanado-iodoapatite (I-APT, Pb 9.85 (VO 4 ) 6 I 1.7 ), a potential nuclear waste form for the radioactive waste element of I-129, which can be enhanced when crevice corrosion of stainless steel (SS) occurring nearby. Reference corrosion studies of I-APT were performed in different bulk solutions including DI water, 0.6 M and 6 M NaCl, and 0.1 M HNO 3 without metal crevice corrosion interactions. The localized enrichment of Cl – , one of the major consequences of SS crevice corrosion, was found to be the decisive factor that led to the enhanced release of iodine. A surface alteration layer consisting of a mixture of nanocrystalline I-APT and Cl-rich apatite (Cl-APT) formed on I-APT surface. Meanwhile, large Cl-APT crystals formed at the crevice mouth on the I-APT surface. This study reveals a new near-field corrosion mechanism for ceramic waste forms when they are exposed to aggressive local corrosive conditions created by the electrochemical reactions of nearby metals. The insight gained in this study could be beneficial for a more accurate prediction of waste form degradation.

36 MATERIALS SCIENCE↗

Corrosion interactions between stainless steel and lead vanado-iodoapatite nuclear waste form part I

This study explores the corrosion interactions between a metallic canister material, stainless steel (SS) 316, and an I-bearing ceramic waste form, lead vanado-iodoapatite (I-APT, Pb 9.85 (VO 4 ) 6 I 1.7 ), in a chloride solution. Crevice corrosion of the SS in close proximity to the I-APT resulted in the development of an aggressive environment at the interface of the two materials, which was acidic and enriched in Cl – anions. I-APT also corroded in the crevice region, primarily through ion-exchange between the I – ions from the I-APT matrix and anions from the environment. The enrichment of Cl – anions within the occluded crevice space as the result of SS crevice corrosion enhanced the corrosion of I-APT. The release of iodine from this apatite waste form could be accelerated owing to this mechanism. This is evidenced by a depletion of iodine from the I-APT matrix and a large amount of Cl-bearing precipitates on the surfaces of both SS and I-APT. On the other hand, the corrosion of I-APT leads to the precipitation of a V- and Pb-rich layer, which inhibits the localized corrosion of SS to an extent. This study advances the understanding of the near-field corrosion interactions between metallic canisters and ceramic waste forms.

36 MATERIALS SCIENCE↗

Stainless and carbon steel corrosion in aqueous piperazine at absorber and water wash conditions

Corrosion of carbon steel (C1010) and stainless steels (304, 316L, 430) was measured at absorber and water wash conditions at the bench scale. Corrosion rate decreases with increasing concentration of piperazine (PZ). With more than 0.003 m PZ in solution, carbon steel has acceptable corrosion performance. Corrosion of carbon steel increases with increasing partial pressure of CO2, suggesting loading is another dominant parameter. The effect is more significant for dilute PZ; therefore, untreated flue gas with high CO2 content should be avoided in the water wash. Temperature has a less significant effect than PZ concentration and loading. Carbon steel corrosion increases with increasing flow velocity at both absorber and water wash conditions

Liu, Ching-Ting↗

Data Package of Results from Salt Spill Testing

This document provides or identifies the full suite of data that was measured in laboratory salt spill tests on molten salt spreading and heat transfer, molten salt flowing and freezing in tubing, stainless steel corrosion kinetics in molten salt, and molten salt splashing and aerosol generation. The background, motivation, and methods for the work are explained in detail in an accompanying report (Thomas and Jackson, 2021), which includes representative results for all measurements. Quantitative data are tabulated to facilitate use in follow-on calculations and qualitative data in the form of visual and infrared video files are indexed for reference.

36 MATERIALS SCIENCE↗

Testing to Evaluate Processes Expected to Occur during MSR Salt Spill Accidents

Obtaining a license for a new nuclear reactor requires the identification and assessment of the potential consequences of specified accident scenarios, which are achieved using accident progression models. Those models need to be parameterized and validated using experimental data, but existing experimental data addressing processes relevant to molten salt reactor accidents are sparse. Specifically, experimental data that quantify the sensitives of important processes to the initial conditions of the spill, the ambient environment, and the containment features are needed to parameterize individual process models. Integrated experiments that simulate accident scenarios are also needed to provide data for model validation, but these experiments will require the use of proven methods to quantify the processes under evaluation. The overarching objectives of this work are to develop the methods for simulating the targeted processes, to determine the effectiveness of the methods in producing the data required for model development, to generate data that can be used to parameterize individual process models, and to provide key insights into the behavior of spilled molten salt that should be considered in models. Experimental methods were designed to quantify aspects of individual processes expected to occur during or after a molten salt spill accident that will affect the fate of spilled molten salt and the radionuclides within. These processes include 1) molten salt spreading and heat transfer, 2) molten salt flowing and freezing in tubing, 3) stainless steel corrosion kinetics in molten salt, and 4) molten salt splashing and aerosol generation. The initial tests described in this report were conducted using eutectic FLiNaK to demonstrate the test methods, the data that are generated, and the analyses of the data to derive values needed for modeling. The primary variables that were tested include initial salt temperature and the presence of volatile surrogate fission products (e.g., cesium and iodine). The developed methods are shown to be effective in quantifying the desired processes and can be applied to study more complex salt compositions of interest to molten salt reactor developers, a wide range of environmental conditions of interest to modelers, and additional variables relevant to salt spill accidents. The developed methods and insights gained from laboratory tests can also be incorporated in future large-scale integrated tests used to simulate molten salt spill accidents.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Critical role of slags in pitting corrosion of additively manufactured stainless steel in simulated seawater

Abstract Pitting corrosion in seawater is one of the most difficult forms of corrosion to identify and control. A workhorse material for marine applications, 316L stainless steel (316L SS) is known to balance resistance to pitting with good mechanical properties. The advent of additive manufacturing (AM), particularly laser powder bed fusion (LPBF), has prompted numerous microstructural and mechanical investigations of LPBF 316L SS; however, the origins of pitting corrosion on as-built surfaces is unknown, despite their utmost importance for certification of LPBF 316L SS prior to fielding. Here, we show that Mn-rich silicate slags are responsible for pitting of the as-built LPBF material in sodium chloride due to their introduction of deleterious defects such as cracks or surface oxide heterogeneities. In addition, we explain how slags are formed in the liquid metal and deposited at the as-built surfaces using high-fidelity melt pool simulations. Our work uncovers how LPBF changes surface oxides due to rapid solidification and high-temperature oxidation, leading to fundamentally different pitting corrosion mechanisms.

36 MATERIALS SCIENCE↗

Corrosion of 316 L stainless steel under the natural circulation of molten NaCl-MgCl 2 salt

The corrosion behavior of 316 L stainless steel (SS) was studied via the natural circulation of molten eutectic NaCl-MgCl 2 salt through a microloop. The post-corrosion tested 316 L SS microloop sections were characterized with microscopy techniques to determine the microstructural and microchemical changes that occurred at the alloy/salt interface. It was found that 316 L SS showed heterogeneous dissolution at the hot-leg, whereas deposition of corrosion products occurred at the cold-leg. For the first time, experimentally obtained molten salt flow-induced corrosion of 316 L SS results were combined with computational thermodynamic-kinetic models to validate the dissolution and deposition in terms of elemental compositional changes at the alloy/salt interface. The thermodynamic-kinetic modeling predicted that the heterogeneous dissolution of Cr and Fe from the hot-leg section of 316 L SS persisted throughout the salt circulation. The model also estimated that, despite Cr deposition starting earlier than Fe, the total redeposition of Fe is expected to be significantly greater than that of Cr over the circulation of salt. Furthermore, the modeling accurately predicted the subsurface enrichment of Mo which is attributed to the reduced Cr activity and the relatively higher diffusion rate of Mo within the alloy matrix. Here, the agreement between modeling and experimental results confirms that Fe chlorides dissolve at the hot-leg and subsequently deposit at the cold-leg due to activity changes driven by the thermal gradient. By contrast, Cr was not detected in the cold-leg deposits, which is attributed to its weaker temperature dependence on activity, limiting its redeposition under these conditions.

36 - MATERIALS SCIENCE↗

Galvanic Corrosion of Carbon Steel and Stainless Steel Couples: Effects of γ-Radiation and Solution Environment - 20348

Galvanic corrosion between carbon steel (CS) and stainless steel (SS) in different aqueous environments was investigated using a combination of electrochemical measurements and surface characterizations. In a basic environment (pH 10.6), the galvanic effect is negligible due to the high corrosion resistance of both alloys. In an acidic to near neutral environment (pH 6.0), the galvanic effect is more significant. Coupling to SS, increasing temperature, and irradiation at this pH have a synergistic effect on the corrosion progression of CS, and their effects vary with time. Initially, the oxidation rate of CS increases after galvanic coupling to SS. Increasing temperature or applying γ-radiation accelerates this oxidation process. However, at a longer time when the saturation limits of metal cations are reached, they also lead to the formation and growth of oxides on CS at a much faster rate, resulting in the suppression of the subsequent Fe dissolution. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Electrochemical corrosion of multiphase stainless steel-based alloy nuclear waste forms

Abstract The electrochemical corrosion behaviors of two multiphase alloys representing waste forms made with 316 L stainless steel and different amounts of surrogate metallic fuel wastes were measured and related to the microstructures. Potentiodynamic (PD) scans were performed in an acid brine solution and the corroded surfaces were characterized with scanning electron microscopy (SEM) to compare the electrochemical responses to the corrosion of specific phases. PD scans for the two multiphase alloys, 316 L stainless steel, and pure palladium were compared to understand the complex corrosion behavior of these multiphase alloys also recently classified as multi principle element alloys (MPEAs) and to determine the effects of alloying elements and noble metals present in constituent phases on the corrosion behavior.

Gattu, Vineeth Kumar (ORCID:0000000307265813)↗

Analysis of Microbial Communities as Indicators of Microbially Induced Corrosion Potential in Stainless Steel Piping

The 200 West Area Pump-and-Treat (200W P&T) facility is part of the final remedy decision for the 200 ZP-1 Operable Unit (OU) and is the interim remedial action for 200-UP-1 OU at the Hanford Site. The facility also treats water from other sources across the site, including 200-DV-1 OU perched water, groundwater from the 200-BP-5 OU, and leachate from the Environmental Restoration Disposal Facility. The facility originally operated a biological treatment process for nitrate that resulted in systemic biofouling and loss of injection well capacity, requiring frequent and costly well rehabilitation. Biofouling has also contributed to corrosion of welds and pitting of stainless-steel piping at the facility. The biological treatment for nitrate was suspended at the end of 2019 calendar year to eliminate negative impacts from biological treatments which improve facility operations and treatment of carbon tetrachloride. Evaluation of the 200W P&T facility’s response to operational improvements, specifically the suspension of the biological treatment, provides information on the potential for continued microbially induced corrosion (MIC). To this end, historical data sets (2015-2017) were compared with molecular biological analyses of 200W P&T water samples from 2018-2020 to quantify trends in total microbial biomass and specific microbial indicator species (iron, sulfate, nitrate, and manganese reducing bacteria) known to cause and enhance metal corrosion. Results showed unequivocal reductions (in excess of 90%) in all microbiological indicators measured following the suspension of the biological treatment. Although abundance measurements for all corrosive MIC populations initially declined after removal of the treatment system, nitrate-reducing bacteria (nirK) and sulfate-reducing bacteria remain highly abundant in the system, an order of magnitude higher than the number of cells present prior to the removal of the biological treatment system [5.14e (1.4) cells/L, vs. 1.14e (0.07) cells/L, reported as average (±SD) for n=3]. In addition, there was an unexpected inflection point in 2019 where all microbial indicators increased unexpectedly in abundance in 2020 by as much as two orders of magnitude compared to 2019 samples. Given the limited number of water samples available for this analysis, the cause of the increase in microbial indicators post-biological treatment has not yet been determined. Systematic sampling of the facility for continued monitoring is recommended so that the responses of MIC populations can be evaluated to ensure that further corrosion is avoided, allowing the 200W P&T facility to operate safely and efficiently at design capacity.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Machine-to-machine variability of roughness and corrosion in additively manufactured 316L stainless steel

Numerous studies on the corrosion response of metal AM have been conducted. Nonetheless, the specimens being tested are commonly ground or polished to remove the outer as-built surface. If metal AM is truly going to be employed as a transformative technology that can produce complex shapes that do not require traditional machining, then the material needs to be evaluated in the as-built state. The reality is that AM alloys have shown significant inconsistencies regarding as-built surface texture, topology, and residual stress. One metric that has shown significant unpredictability in the literature is the susceptibility to localized corrosion of typically passive alloys, such as stainless steel (SS). There are a large number of studies that have attempted to understand the corrosion response of metal AM materials, but these studies are typically performed on materials that have been printed on a single machine and often mechanically polished to a smooth finish. This study compares the corrosion response of as-built AM, laser-beam powder bed fusion (LB-PBF), 316L SS parts that have been fabricated on five different machines. The majority of this work focused on understanding the susceptibility to localized corrosion of AM metals with respect to machine-dependent variables, namely surface roughness, and build angle. Surface roughness data was collected using scanning white light triangulation, laser scanning confocal microscopy, and coherence scanning interferometry. The results show that there is significant variability (p two-tail < 0.05) in the susceptibility to local corrosion initiation of LB-PBF 316L SS samples built on different machines. Surface oxides were probed with electron dispersive spectroscopy and revealed that variations in local corrosion susceptibility likely arise from differences in the stability of the passive film caused by chemical segregation, unique microstructure, and tortuous roughness features at the as-built surfaces. The variability of roughness and corrosion properties from test samples printed on different machines was corroborated by property measurements performed at five different testing sites, proving reproducibility of the data. Most importantly, this study shows that if the as-built surface layer is removed through grinding or electropolishing the machine-to-machine variation observed in the corrosion susceptibility is reduced.

36 MATERIALS SCIENCE↗

Applied Research and Development to Support Open Water Testing at PacWave – Task 5: Development of additively manufactured, functionally graded, corrosion resistant clads for wave energy applications

In this task, we focused on developing corrosion-resistant claddings for wave energy applications. Wave energy systems are exposed to saline conditions, which are corrosive to many metallic structural materials (e.g., carbon steel). Corrosion-resistant (stainless) steels are typically alloyed with >18% chromium (Cr) and >8% nickel (Ni), which dramatically raises material costs and can hinder the development of wave energy systems; thus, coatings are a necessary corrosion protection method for most. Non-metallic coatings (paint, epoxy) have shorter service lives, limited resistance to mechanical stress and wear, plus additional costs of inspection and eventual replacement. Therefore, overlay stainless steel (SS) claddings have a cost-effective use case for protecting components from corrosion, particularly for those that may be subject to mechanical stress / wear and with long service lives.

16 TIDAL AND WAVE POWER↗

Corrosion Resistance of 309L Stainless Steel Claddings on Carbon Steel Produced with Wire-Fed Directed Energy Deposition

Additive manufacturing (AM) tools are capable of applying overlay austenitic stainless steel (SS) claddings to carbon steel components. The benefits of this approach over arc welding include a smaller heat-affected zone, residual stress reduction, and material savings. In particular, wire-directed energy deposition is a suitable technique because of its low material cost and high rate of production compared to other AM methods. However, metallurgical variations in composition, phase fraction, and microsegregation can potentially influence the corrosion behavior of such claddings. In this work, 309L SS is clad on carbon steel substrates and electrochemical methods are used to measure their general and pitting corrosion resistance in simulated marine environments (3.5 wt% NaCl solutions). Two-layer claddings are fabricated with four laser powers to understand the effects of bulk chemical composition, austenite/δ-ferrite phase fractions, and individual phase compositions on corrosion behavior. The two-layer claddings are compared to a single-layer cladding, wrought 304 SS, and the carbon steel substrate for a comprehensive assessment of corrosion performance. The two-layer claddings are remarkably resistant to general corrosion in the 3.5 wt% NaCl environment because of their high Cr content (21.6 wt% to 23.3 wt% Cr). The single-layer cladding exhibits localized corrosion at unmixed Fe-rich peninsulas that originate at the dissimilar metal boundary and protrude into the first cladding layer. All two-layer claddings possess higher pitting corrosion resistance than wrought 304 SS, demonstrating their effectiveness as a corrosion-resistant barrier. Here, the pitting corrosion resistance is superior for claddings made with lower laser powers, due to low dilution and greater δ-ferrite contents.

36 MATERIALS SCIENCE↗