Search NASA⌕ Search

SEARCH · Search NASA

Results for “thermoelectric material skutterudite”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Thermal Expansion Studies of Selected High Temperature Thermoelectric Materials

Radioisotope thermoelectric generators (RTGs) generate electrical power by converting the heat released from the nuclear decay of radioactive isotopes (typically plutonium-238) into electricity using a thermoelectric converter. RTGs have been successfully used to power a number of space missions and have demonstrated their reliability over an extended period of time (tens of years) and are compact, rugged, radiation resistant, scalable, and produce no noise, vibration or torque during operation. System conversion efficiency for state-of-practice RTGs is about 6% and specific power less than or equal to 5.1 W/kg. Higher specific power would result in more on-board power for the same RTG mass, or less RTG mass for the same on-board power. The Jet Propulsion Laboratory has been leading, under the advanced thermoelectric converter (ATEC) project, the development of new high-temperature thermoelectric materials and components for integration into advanced, more efficient RTGs. Thermoelectric materials investigated to date include skutterudites, the Yb14MnSb11 compound, and SiGe alloys. The development of long-lived thermoelectric couples based on some of these materials has been initiated and is assisted by a thermo-mechanical stress analysis to ensure that all stresses under both fabrication and operation conditions will be within yield limits for those materials. Several physical parameters are needed as input to this analysis. Among those parameters, the coefficient of thermal expansion (CTE) is critically important. Thermal expansion coefficient measurements of several thermoelectric materials under consideration for ATEC are described in this paper. The stress response at the interfaces in material stacks subjected to changes in temperature is discussed, drawing on work from the literature and project-specific tools developed here. The degree of CTE mismatch and the associated effect on the formation of stress is highlighted.

silicon germanium↗

Advanced thermoelectric materials with enhanced crystal lattice structure and methods of preparation

New skutterudite phases including Ru.sub.0.5 Pd.sub.0.5 Sb.sub.3, RuSb.sub.2 Te, and FeSb.sub.2 Te, have been prepared having desirable thermoelectric properties. In addition, a novel thermoelectric device has been prepared using skutterudite phase Fe.sub.0.5 Ni.sub.0.5 Sb.sub.3. The skutterudite-type crystal lattice structure of these semiconductor compounds and their enhanced thermoelectric properties results in semiconductor materials which may be used in the fabrication of thermoelectric elements to substantially improve the efficiency of the resulting thermoelectric device. Semiconductor materials having the desired skutterudite-type crystal lattice structure may be prepared in accordance with the present invention by using powder metallurgy techniques. Measurements of electrical and thermal transport properties of selected semiconductor materials prepared in accordance with the present invention, demonstrated high Hall mobilities and good Seebeck coefficients. These materials have low thermal conductivity and relatively low electrical resistivity, and are good candidates for low temperature thermoelectric applications.

Fleurial, Jean-Pierre↗

Promising Thermoelectric Materials for Terrestrial-Space Applications

Since the discovery of state-of-the-art thermoelectric materials in the 1960s, little improvement has been made in the thermoelectric material efficiency. Although numerous materials have been investigated for their thermoelectric properties, ZT value of 1 has not been significantly exceeded. This paper presents a new family of materials with the skutterudite crystal structure which, based on initial results obtained on several compounds of this family, has a good potential for thermoelectric applications. This class of materials covers a wide range of decomposition temperatures and bandgaps, which could be used for low, intermediate to high temperature applications.

thermoelectric material skutterudite↗

Hierarchical microstructure of Yb-filled skutterudites through ultrasonically atomized spherical powders for enhanced thermoelectric performance

Hierarchical microstructures are widely explored as a strategy to reduce lattice thermal conductivity in thermoelectric materials while preserving favorable electronic transport. Here we demonstrate that ultrasonic atomization of precursor powders provides an intrinsic pathway to generate such architectures in n-type Yb0.3Co4Sb12 skutterudites. Materials were synthesized by both conventional sealed-ampoule and ultrasonic atomization routes, each yielding essentially single-phase skutterudite after densification. However, the atomized spherical powders undergo a distinct reaction-driven microstructural evolution during thermal treatment prior to densification. Electron microscopy reveals that the skutterudite phase within the particles induces swelling, cracking, and fragmentation of the droplets before consolidation. Multimodal structural and microstructural characterizations show that densification of these fragmented powders produces a hierarchical microstructure consisting of submicron grains, micrometer-scale faceted crystallites, and powder-derived domains separated by oxide-decorated boundaries. Comprehensive thermoelectric transport measurements evidence that this multiscale architecture lowers the lattice thermal conductivity while maintaining favorable electronic transport, leading to an average ~10% enhancement in the thermoelectric figure of merit. Complementary 121Sb Mössbauer spectroscopy further indicates lattice softening in the atomized material. These results demonstrate that ultrasonic atomization provides an effective route to engineer hierarchical microstructures in skutterudite thermoelectrics and offers a promising strategy for tailoring thermal transport in energy-conversion materials.

Bouteiller, Hugo [ORNL] (ORCID:0009000421322962)↗

Semiconductor apparatus utilizing gradient freeze and liquid-solid techniques

Transition metals of Group VIII (Co, Rh and Ir) have been prepared as semiconductor compounds with the general formula TSb.sub.3. The skutterudite-type crystal lattice structure of these semiconductor compounds and their enhanced thermoelectric properties results in semiconductor materials which may be used in the fabrication of thermoelectric elements to substantially improve the efficiency of the resulting thermoelectric device. Semiconductor materials having the desired skutterudite-type crystal lattice structure may be prepared in accordance with the present invention by using vertical gradient freezing techniques and/or liquid phase sintering techniques. Measurements of electrical and thermal transport properties of selected semiconductor materials prepared in accordance with the present invention, demonstrated high Hall mobilities (up to 1200 cm.sup.2.V.sup.-1.s.sup.-1) and good Seebeck coefficients (up to 150 .mu.VK.sup.-1 between 300.degree. C. and 700.degree. C.). Optimizing the transport properties of semiconductor materials prepared from elemental mixtures Co, Rh, Ir and Sb resulted in a substantial increase in the thermoelectric figure of merit (ZT) at temperatures as high as 400.degree. C. for thermoelectric elements fabricated from such semiconductor materials.

Fleurial, Jean-Pierre↗

High performance thermoelectric materials and methods of preparation

Transition metals (T) of Group VIII (Co, Rh and Ir) have been prepared as semiconductor alloys with Sb having the general formula TSb.sub.3. The skutterudite-type crystal lattice structure of these semiconductor alloys and their enhanced thermoelectric properties results in semiconductor materials which may be used in the fabrication of thermoelectric elements to substantially improve the efficiency of the resulting thermoelectric device. Semiconductor alloys having the desired skutterudite-type crystal lattice structure may be prepared in accordance with the present invention by using vertical gradient freeze techniques, liquid-solid phase sintering techniques, low temperature powder sintering and/or hot-pressing. Measurements of electrical and thermal transport properties of selected semiconductor materials prepared in accordance with the present invention, demonstrated high Hall mobilities (up to 8000 cm.sup.2.V.sup.-1.s.sup.-1), good Seebeck coefficients (up to 400 .mu.VK.sup.-1 between 300.degree. C. and 700.degree. C.), and low thermal conductivities (as low as 15 mW/cmK). Optimizing the transport properties of semiconductor materials prepared from elemental mixtures Co, Rh, Ir and Sb resulted in a two fold increase in the thermoelectric figure of merit (ZT) at temperatures as high as 400.degree. C. for thermoelectric elements fabricated from such semiconductor materials.

Fleurial, Jean-Pierre↗

Coating Thermoelectric Devices To Suppress Sublimation

A technique for suppressing sublimation of key elements from skutterudite compounds in advanced thermoelectric devices has been demonstrated. The essence of the technique is to cover what would otherwise be the exposed skutterudite surface of such a device with a thin, continuous film of a chemically and physically compatible metal. Although similar to other sublimation-suppression techniques, this technique has been specifically tailored for application to skutterudite antimonides. The primary cause of deterioration of most thermoelectric materials is thermal decomposition or sublimation - one or more elements sublime from the hot side of a thermoelectric couple, changing the stoichiometry of the device. Examples of elements that sublime from their respective thermoelectric materials are Ge from SiGe, Te from Pb/Te, and now Sb from skutterudite antimonides. The skutterudite antimonides of primary interest are CoSb3 [electron-donor (n) type] and CeFe(3-x)Co(x)Sb12 [electron-acceptor (p) type]. When these compounds are subjected to typical operating conditions [temperature of 700 C and pressure <10(exp -5) torr (0.0013 Pa)], Sb sublimes from their surfaces, with the result that Sb depletion layers form and advance toward their interiors. As the depletion layer advances in a given device, the change in stoichiometry diminishes the thermal-to-electric conversion efficiency of the device. The problem, then, is to prevent sublimation, or at least reduce it to an acceptably low level. In preparation for an experiment on suppression of sublimation, a specimen of CoSb3 was tightly wrapped in a foil of niobium, which was selected for its chemical stability. In the experiment, the wrapped specimen was heated to a temperature of 700 C in a vacuum of residual pressure <10(exp -5) torr (0.0013 Pa), then cooled and sectioned. Examination of the sectioned specimen revealed that no depletion layer had formed, indicating the niobium foil prevented sublimation of antimony at 700 C. This was a considerable improvement, considering that uncoated CoSb3 had been found to decompose to form the lowest antimonide at the surface at only 600 C. Evidently, because the mean free path of Sb at the given temperature and pressure was of the order of tens of centimeters, any barrier closer than tens of centimeters (as was the niobium foil) would have suppressed transport of Sb vapor, thereby suppressing sublimation of Sb

Sakamoto, Jeffrey↗

CoSb(sub 3)-IrSb(sub 3)Solid Solutions: Preparations and Characterization

The binary antimonide compounds of the skutterudite family have a good potential for thermoelectric applications as recent results at JPL have shown. However, the room temperature thermal conductivity of these materials is about 10 Wm(sup -1)K(sup -1) with an 80 % contribution from the lattice. To achieve maximum ZT values, the lattice thermal conductivity needs to be lowered. Because the lattice thermal conductivity of solid solutions can substantially decrease due to the addition of point defect phonon scattering (all state-of-the-art thermoelectric materials are solid solutions), a study of the formation of solid solutions between the antimonide skutterudite compounds is of interest. The preparation and characterization of both p-type and n-type CoSb(sub 3)-IrSb(sub 3) solid solutions by several techniques is reviewed in this paper. Experimental results showed that solid solutions were successfully formed in a wide range of compositions. The changes in the thermoelectric properties indicated the influence of a strong point defect scattering, resulting in large decreases in Hall mobility and thermal conductivity. The potential for high ZT values in CoSb(sub 3)-IrSb(sub 3) solid solutions is discussed.

mobility↗

Filled Co (sub X) Ni (sub 4-x) Sb (sub 12-y) Sn (sub Y) Skutterudites: Processing and Thermoelectric Properties

Skutterudites have proven to be a useful thermoelectric system as a result of their enhanced figure of merit (ZT1), cheap material cost, favorable mechanical properties, and good thermal stability. The majority of skutterudite interest in recent years has been focused on binary skutterudites like CoSb3 or CoAs3. Binary skutterudites are often double and triple filled, with a range of elements from the lanthanide series, in order to reduce the lattice component of thermal conductivity. Ternary and quaternary skutterudites, such as Co4Ge6Se6 or Ni4Sb8Sn4, provide additional paths to tune the electronic structure. The thermal conductivity can further be improved in these complex skutterudites by the introduction of fillers. The Co (sub X) Ni (sub 4-x) Sb (sub 12-y) Sn (sub Y) system has been investigated as both a p- and n-type thermoelectric material, and is stable up to 200 degrees Centigrade. Yb, Ce, and Dy fillers have been introduced into the skutterudite to study the influence of both the type and the quantity of fillers on processing conditions and thermoelectric properties. The system was processed through a multi-step technique that includes solidification, mechano-chemical alloying, and hot pressing which will be discussed along with thermoelectric transport properties.

Thermoelectricity↗

Fabrication of stable electrode/diffusion barrier layers for thermoelectric filled skutterudite devices

Disclosed are methods for the manufacture of n-type and p-type filled skutterudite thermoelectric legs of an electrical contact. A first material of CoSi2 and a dopant are ball-milled to form a first powder which is thermo-mechanically processed with a second powder of n-type skutterudite to form a n-type skutterudite layer disposed between a first layer and a third layer of the doped-CoSi2. In addition, a plurality of components such as iron, and nickel, and at least one of cobalt or chromium are ball-milled form a first powder that is thermo-mechanically processed with a p-type skutterudite layer to form a p-type skutterudite layer “second layer” disposed between a first and a third layer of the first powder. The specific contact resistance between the first layer and the skutterudite layer for both the n-type and the p-type skutterudites subsequent to hot-pressing is less than about 10.0 μΩ·cm2.

Jie, Qing↗

Preparation and Thermoelectric Properties of the Skutterudite-Related Phase Ru(0.5)Pd(0.5)Sb3

A new skutterudite phase Ru(0.5)Pd(0.5)Sb3 was prepared. This new phase adds to a large number of already known materials with the skutterudite structure which have shown good potential for thermoelectric applications. Single phase, polycrystalline samples were prepared and characterized by x-ray analysis, electron probe microanalysis, density, sound velocity, thermal-expansion coefficient, and differential thermal analysis measurements. Ru(0.5)Pd(0.5)Sb3 has a cubic lattice, space group Im3 (T(sup 5, sub h)), with a = 9.298 A and decomposes at about 920 K. The Seebeck coefficient, the electrical resistivity, the Hall effect, and the thermal conductivity were measured on hot-pressed samples over a wide range of temperatures. Preliminary results show that Ru(0.5)Pd(0.5)Sb3 behaves as a heavily doped semiconductor with an estimated band gap of about 0.6 eV. The lattice thermal conductivity of Ru(0.5)Pd(0.5)Sb3 is substantially lower than that of the binary isostructural compounds CoSb3 and IrSb3. The unusually low thermal conductivity might be explained by additional hole and charge transfer phonon scattering in this material. The potential of this material for thermoelectric applications is discussed.

Caillat, T.↗

A Novel High-Performance Mission-Enabling Multi-Purpose Radioisotope Heat Source

Recent studies indicate science mission concepts targeting access to the sub-surface oceans of icy moons require ice-penetrating cryobots powered by advanced Radioisotope Power Systems (RPS). These systems would deliver waste heat for ice-melting in the range of 10 kW. Minimizing the transit time through the kilometers-thick ice shells to just a few years requires these RPS to utilize heat sources having a higher thermal energy volumetric density than the existing flight-qualified General-Purpose Heat Source (GPHS). A Compact Heat Source (CPHS)has been conceptualized in which the graphite impact shells(GIS) of the existing GPHS are rearranged in a hexagonal aeroshell containing seven GIS per module, as opposed to the standard two per module; offering a thermal energy density of 0.57 W/cm3versus 0.29 W/cm3 offered by the GPHS simply from the repackaging of Technology Readiness Level (TRL)9 subassemblies. Preliminary thermal modeling of the CPHS integrated into a notional radioisotope thermoelectric generator(RTG) structure further suggests that centerline temperatures are well within allowable limits during nominal operation. Given the need for the CPHS for a subset of missions, it is worth exploring the applicability of the CPHS for more general RTG purposes. We discuss herein how the CPHS may be implemented with either heritage or in-development thermoelectric converter technologies into a Next-Generation RTG concept. Due to a higher energy density, the legacy heat rejection fin arrangement must be modified to permit a sufficiently low cold-side temperature. Preliminary finite element analysis suggests fin-root temperatures can be kept as low as 520 K while allowing the generator to fit within the usable dimensions of currently available United States Department of Energy shipping containers. Such temperatures would certainly be compatible with the use of high temperature thermoelectric converter technologies.. A prime candidate is the heritage silicon-germanium (SiGe) unicouple, whose design could be adapted by approximately halving the leg-length, but without changes in hot and cold junction interfaces, which are features critical to the proven performance and reliability of these devices. The estimated Beginning of Life power for a SiGe-based CPHS-RTG using 12 CPHS for a thermal inventory of 10.5 kW is greater than 600 W under deep space operating conditions. Using higher performance segmented couples currently in development that are based on skutterudite,La3−xTe4and 14-1-11 Zintl thermoelectric materials in lieu of the SiGe unicouples would increase the power level to more than1 kW. The high specific power (We/kg) attribute of CPHS-RTGs found in this study could potentially enable Radioisotope Electric Propulsion (REP) mission concepts. Past NASA REP mission concept studies identified specific power needs in excess of 6to 8 We/kg. Based on a GPHS-RTG-like system configuration, we show that at fin root temperatures between 530 K and 570K (deep space environment), specific powers exceeding 10 We/kg are achievable using high performance segmented thermoelectric converters. The compact sizing and power density of the CPHS-RTG would constitute a significant step upgrade in specific power when compared to heritage GPHS-RTG (approximately5.1 We/kg) and off-the-shelf Multi-Mission RTG (approximately 2.6 We/kg).

Nesmith, Bill J.↗

Filled Nd(z)Fe(x)Co(4-x)Sb(12-y)Ge(y) Skutterudites: Processing and Thermoelectric Properties

Skutterudites have proven to be a useful thermoelectric system as a result of their enhanced figure of merit (ZT1), cheap material cost, favorable mechanical properties, and good thermal stability. The majority of skutterudite interest in recent years has been focused on binary skutterudites like CoSb3. Binary skutterudites are often double and triple filled, with a range of elements from the lanthanide series, in order to reduce the lattice component of thermal conductivity. Ternary and quaternary skutterudites, such as Co4Ge6Se6 or Ni4Sb8Sn4, provide additional paths to tune the electronic structure. The thermal conductivity can further be improved in these complex skutterudites by the introduction of fillers. The Nd(z)Fe(x)Co(4-x)Sb(12-y)Ge(y) system has been investigated as a p-type thermoelectric material, and is stable up to 600 C. The influence of Fe and Ge content, along with filler Nd, was investigated on thermoelectric transport properties. In addition to the chemical influence on properties, some processing details of the system will also be addressed.

Thermoelectric↗

Filled Nd(sub z) Fe(sub x) Co(sub 4-x) Sb(sub 12-y) Ge(sub y) Skutterudites: Processing and Thermoelectric Properties

Skutterudites have proven to be a useful thermoelectric system as a result of their enhanced figure of merit (ZT1), cheap material cost, favorable mechanical properties, and good thermal stability. The majority of skutterudite interest in recent years has been focused on binary skutterudites like CoSb3. Binary skutterudites are often double and triple filled, with a range of elements from the lanthanide series, in order to reduce the lattice component of thermal conductivity. Ternary and quaternary skutterudites, such as Co4Ge6Se6 or Ni4Sb8Sn4, provide additional paths to tune the electronic structure. The thermal conductivity can further be improved in these complex skutterudites by the introduction of fillers. The Nd (sub z) Fe (sub x) Co (sub 4-x) Sb (sub 12-y)Ge (sub y) system has been investigated as a p-type thermoelectric material, and is stable up to 600 degrees Centigrade. The influence of Fe and Ge content, along with filler Nd, was investigated on thermoelectric transport properties. In addition to the chemical influence on properties, some processing details of the system will also be addressed.

Electical Conductivity↗

High-Performance Thermoelectric Semiconductors

Figures of merit almost double current state-of-art thermoelectric materials. IrSb3 is semiconductor found to exhibit exceptional thermoelectric properties. CoSb3 and RhSb3 have same skutterudite crystallographic structure as IrSb3, and exhibit exceptional transport properties expected to contribute to high thermoelectric performance. These three compounds form solid solutions. Combination of properties offers potential for development of new high-performance thermoelectric materials for more efficient thermoelectric power generators, coolers, and detectors.

Fleurial, Jean-Pierre↗

Boosting Thermoelectric Performance in Nanocrystalline Ternary Skutterudite Thin Films through Metallic CoTe 2 Integration

Metal–semiconductor nanocomposites have emerged as a viable strategy for concurrently tailoring both thermal and electronic transport properties of established thermoelectric materials, ultimately achieving synergistic performance. In this investigation, a series of nanocomposite thin films were synthesized, embedding metallic cobalt telluride (CoTe 2 ) nanophase within the nanocrystalline ternary skutterudite (Co(Ge 1.22 Sb 0.22 )Te 1.58 or CGST) matrix. Our approach harnessed composition fluctuation-induced phase separation and in situ growth during thermal annealing to seamlessly integrate the metallic phase. The distinctive band structures of both materials have developed an ohmic-type contact characteristic at the interface, which raised carrier density considerably yet negligibly affected the mobility counterpart, leading to a substantial improvement in electrical conductivity. The intricate balance in transport properties is further influenced by the metallic CoTe 2 phase’s role in diminishing lattice thermal conductivity. The presence of the metallic phase instigates enhanced phonon scattering at the interface boundaries. Consequently, a 2-fold enhancement in the thermoelectric figure of merit (zT ~ 1.30) is attained with CGST-7 wt. % CoTe 2 nanocomposite film at 655 K compared to that of pristine CGST.

36 MATERIALS SCIENCE↗

Skutterudites: An Update

Materials with the skutterudite crystal structure possess attractive transport properties and have a good potential for achieving ZT values substantially larger than for state-of-the-art thermoelectric materials.

properties ternary compounds heavily Doped n-type ↗