Optimization of Annealing for WZ-Phase Removal and Densification in Sb-Doped CdSexTe1-x Solar Cells
The impact of high temperature annealing (HTA) treatments on the performance of Sb-doped CdSeTe solar cells containing a CdSe0.25Te0.75/CdTe front stack and a vapor transport (VT) deposited CdTe:Sb absorber was studied. The HTA treatment of the thermally evaporated CdSe0.25Te0.75/CdTe front stack converts the mixed-phase film into a single zinc blende structure through recrystallization of the photo-inactive wurtzite phase. Subsequently, HTA treatment of the full device stack after vapor transport deposition of CdTe:Sb absorber promotes Se-Te intermixing, reduces voids, densifies the full stack and enhances CdTe:Sb grain growth. Comprehensive characterizations revealed that the combined HTA treatments significantly improved film crystallinity, removed the WZ phase in the front stack, enhanced full-stack densification, reduced defect densities, and enhanced carrier dynamics. With HTA treatments, the open-circuit voltage (VOC) of CdSeTe:Sb devices increased from ~ 400 mV to >= 600 mV, and when combined with optimized CdCl2 treatment, VOC reached 849 mV. The net carrier concentrations (NA-ND) of representative devices were NA-ND = 1.5 x 10^15, 1.1 x 10^15, and 3.5 x 10^14 cm-3 for the no-HTA, moderate-HTA, and optimized high-VOC conditions, respectively. Since the highest VOC corresponds to the lowest apparent NA-ND, , which is similar to a Cu-doped-only CdSeTe solar cell (NA-ND ~= 2 x 10^14 cm-3), the data indicate that improved device performance does not result from increased electrically active Sb; instead, it points to structural improvement as the dominant effect of HTA. The findings demonstrate the potential of HTA treatments to improve the structural and electrical properties of CdSeXTe1-X solar cells.