Search NASA⌕ Search

SEARCH · Search NASA

Results for “uranium carbide”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Resilience of uranium mononitride/zirconium carbide composites and uranium-zirconium carbonitride in hot hydrogen for nuclear thermal propulsion

Nuclear thermal rockets require fuels capable of withstanding flowing hydrogen propellant up to 3200 K. Presently, there has not been a fuel type that reliably operates at these conditions. A promising candidate anticipated to endure this demanding environment is a ceramic-ceramic composite comprising of uranium mononitride and zirconium carbide. Further, this investigation assesses the behavior and resilience of variations of this composite and its resultant homogenized form (uranium-zirconium carbonitride) under two hot hydrogen conditions (2273 K and 3000 K). The findings revealed that composites that homogenize into UZrCN exhibit superior structural integrity in hydrogen compared to heterogeneous counterparts. Consequently, this study underscores the potential of homogenized uranium-zirconium carbonitride for enhanced performance in nuclear thermal propulsion applications.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Quantitative Morphological Characterization of Carbide Inclusions in Uranium Metal

Uranium carbides (UCs) are prevalent inclusions in U metal that form during melting operations from interactions with crucible walls and the casting chamber atmosphere. Although UCs have been studied extensively since the beginning of U metal foundry operations, there are still unknowns regarding the effects of thermomechanical processing on their sizes and morphology. Here, we present the results of a series of controlled cooling experiments with molten uranium to elucidate the effect of cooling rate on inclusion morphology in a-U. Samples were melted using a vacuum induction melter and manually cooled at rates of 2.5, 1.7, 1.1, 0.8, 0.3 (± 1%) K/s from ~1600 K to <700 K in under 1 hour. Subsequent scanning electron microscopy (SEM) was performed on cross-sections of the samples, revealing a complex mixture of UC morphologies that are indicative of diffusion and growth influenced by the thermal processing of the U matrix. Image analysis using the Morphological Analysis of Materials (MAMA) software showed that UC sizes generally grew larger with slower cooling rates, and the two slowest cooling rates noticeably impacted the inclusion circularity and ellipse aspect ratio. These results indicate that UC morphology is sensitive to short cooling rates (<1 hour) and could therefore be controlled in the production of metallic nuclear fuels. Additionally, inclusion speciation and morphologies could potentially provide forensic clues about processing history of unknown metal samples. Understanding the driving forces involved in UC morphology evolution is beneficial for evaluating metal fuels for next generation nuclear reactors and for identifying signatures for nuclear forensics.

Athon, Matthew T.↗

Analysis and Design for Irradiation of High Power TRISO Fuel Compact Specimens in HFIR

Tristructural isotropic (TRISO) fuel is being proposed for use in several high-temperature advanced reactor concepts because of its structural integrity under high operating temperatures and burnup. One of these advanced reactor concepts is the Kairos Power fluoride salt-cooled high-temperature reactor (KP- FHR) under development by Kairos Power, LLC. Previous TRISO irradiation experiments were focused on qualification for high-temperature gas reactors (HTGRs), which have higher operating temperatures but lower particle powers than the KP-FHR design. To study the performance of TRISO fuel designed for HTGRs under prototypical FHR conditions, a set of experiments was designed using the MiniFuel irradiation vehicle at the Oak Ridge National Laboratory’s (ORNL) High Flux Isotope Reactor (HFIR). The experiments will irradiate 30 TRISO-containing carbon matrix compacts at inner small vertical experiment facilities in HFIR. Each compact will contain 20 TRISO particles (600 particles total) developed for HTGRs, consisting of either 14% enriched uranium dioxide uranium carbide, naturally enriched uranium dioxide, uranium carbide, or 9.6% enriched uranium dioxide fuel kernels with time- and volume-averaged silicon carbide layer temperatures between 500 and 900°C. This report summarizes the vehicle designs that have been developed, as well as the neutronic and thermal analyses completed for these irradiation experiments. These analyses show that MiniFuel compact irradiation is a versatile experiment that can be used to study a range of TRISO particle powers and fuel types while providing reasonable separation of burnup and temperature effects.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermodynamic Properties of Uranium-Zirconium Carbide Solid Solutions with Oxygen

Uranium-zirconium carbide solid solutions are potential candidates for fuel in space nuclear reactors. To support development of advanced robust fuels for space applications, (U y Zr 1-y )C x O z solid solutions were synthesized via carbothermic reduction with uranium, carbon, and oxygen contents raging from y=0.05 – 0.3, x=0.95 – 0.98, and z = 0.02 – 0.07. These solid solutions were subsequently characterized by X-ray diffraction and elemental combustion analysis. High-temperature oxidative drop solution calorimetry in molten sodium molybdate solvent at 1073 K was employed to determine the formation, oxidation, and mixing enthalpies of (U y Zr 1-y )C x O z solid solutions, and thereby for evaluating their thermodynamic stability. The solid solutions are enthalpically less stable than the UC and ZrC end members. They also become less stable and more reactive towards oxidation with increasing uranium content. Incorporation of oxygen into solid solutions increases their solid solution-stability and improves their oxidation resistance.

Calorimetry↗

Safety Testing and Destructive Examination of AGR-2 UO 2 Compact 3-1-1

Post-irradiation examination and elevated-temperature safety testing are being performed on compacts from the Advanced Gas Reactor (AGR) Fuel Development and Qualification Program’s second irradiation experiment (AGR-2). The compacts in the AGR-2 irradiation experiment held either tristructural isotropic (TRISO)-coated particles containing uranium oxide fuel kernels (UO 2 ) or TRISO-coated particles containing fuel kernels with both uranium carbide and uranium oxide phases (UCO). In UO 2 TRISO particles, oxygen released by uranium fission can react with the surrounding carbon in the buffer layer to form carbon monoxide (CO). Excess CO can lead to various irradiation performance issues under certain operating conditions, such as pressure-induced fracture, kernel migration, and silicon carbide (SiC) corrosion. In UCO TRISO particles, CO formation is reduced because the chemical potential for oxidation of uranium carbide is lower than for oxidation of carbon.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Irradiation of MiniFuel Targets Bearing TRISO Fuel Compacts (Status Report)

Irradiation testing of MiniFuel compacts bearing tristructural isotropic (TRISO) fuel particles was performed at Oak Ridge National Laboratory (ORNL) to support the development of Kairos Power’s (KP’s) fluoride salt–cooled high-temperature reactor concept. The fuel compacts were fabricated with TRISO fuel particles of different types—including low-enriched uranium oxide, uranium carbide (LEUCO), natural uranium oxide, uranium carbide (NUCO), and low-enriched uranium dioxide (LEUO 2 )—and inserted into MiniFuel irradiation targets. Five targets were assembled and inserted in the High Flux Isotope Reactor (HFIR) for four cycles. The data collected post-irradiation will provide experimental input to validate TRISO fuel performance models for high particle power operations. This report summarizes the completion of the HFIR irradiation, the as-irradiated numerical analysis, and the post-irradiation work performed to date. This work was performed under the Nuclear Science User Facility program.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Creep behavior of uranium carbide-based alloys

The present work gives the results of experiments on the influence of zirconium carbide and tungsten on the creep properties of uranium carbide. The creep behavior of high-density UC samples follows the classical time-dependence pattern of (1) an instantaneous deformation, (2) a primary creep region, and (3) a period of steady-state creep. Creep rates for unalloyed UC-1.01 and UC-1.05 are several orders of magnitude greater than those measured for carbide alloys containing a Zr-C and/or W dispersoid. The difference in creep strength between alloyed and unalloyed materials varies with temperature and applied stress.

Seltzer, M. S.↗

FY2020 Annual Report on Subcontract B631779 with UC Berkeley: Reactive Precursors Additive Manufacturing Report

This work succeeded in reaching each of the stated milestones for developing, printing, reacting, and characterizing the uranium carbide final products. Leveraging experience gained from creating magnesium oxide inks (milestone #1) and prior reactive precursor work with boron carbide (milestone #2) a uranium carbide reactive precursor ink was developed. The chosen composition of ink utilized a mixture of wax, petrolatum, and stearic acid as the binder. The reactive precursor portion of the ink was comprised of uranium oxide and nano particle activated carbon for production of uranium carbide via carbothermal reduction. Following an in-air burnout of the binder at 160C the printed samples were reacted and sintered at 1750C in an argon environment induction furnace. The resulting product has an open porosity dense, foam-like internal structure with a calculated density of 89% in the solid fraction.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Irradiation test of tungsten clad uranium carbide-zirconium carbide ((U,Zr)C) specimens for thermionic reactor application at conditions conductive to long-term performance

Uranium carbide fueled, thermionic emitter configurations were encapsulated and irradiated. One capsule contained a specimen clad with fluoride derived chemically vapor deposited (CVD) tungsten. The other capsule used a duplex clad specimen consisting of chloride derived on floride derived CVD tungsten. Both fuel pins were 16 millimeters in diameter and contained a 45.7-millimeter length of fuel.

Creagh, J. W. R.↗

Material development for thermionic fuel-cladding systems.

Fuel-cladding systems capable of maintaining stable dimension and electron emission characteristics at high temperatures under irradiation are essential to the successful operation of nuclear thermionic power sources. Studies regarding two possible systems, involving tungsten clad uranium carbide and uranium oxide, are considered. Out-of-pile developmental efforts and the in-pile evaluation results for the two systems are described. Prototypical emitters have been tested for 8000 hours for the carbide system and 4000 hours for the oxide system.

Yang, L.↗

ENDF/B-VIII.1: Thermal Neutron Scattering Sublibrary

The thermal neutron scattering law (TSL) sublibrary aims to describe the interaction of incident neutrons at thermal or sub-thermal energies with different compound materials such fuels, moderators and special-purpose materials. In ENDF/B-VIII.1 there was a large number of new and updated TSL evaluations, including traditional moderators (light water, Beryllium metal, Beryllium Oxide, Calcium Hydride, plastics (Polystyrene and Lucite), graphite (reactor-grade and crystalline), anhydrous Hydrogen Fluoride, and heavy paraffinic oil); exotic moderators (Beryllium Carbide, Zirconium Hydride, Yttrium Hydride, Lithium-7 Hydride and Deuteride), FLiBe molten salt, structural materials and cladding (Silicon Carbide, Silicon Dioxide, Zirconium Carbide), fuels (Plutonium Dioxide, Uranium Carbide, Uranium metal, Uranium Nitride, Uranium Dioxide, Uranium Hydride), and special purpose materials. In ENDF/B-VIII.1 we also distribute alongside the evaluated files, a comma-separated file (CSV), named TSL_MAT_numbers.csv, which lists all evaluated files in the current release and their corresponding unique MAT number.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Destructive PIE and Safety Testing of Six AGR-2 UO 2 Capsule 3 Compacts

The Advanced Gas Reactor (AGR) Fuel Development and Qualification Program’s second irradiation experiment (AGR-2) was irradiated in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) from June 2010 to October 2013 (Collin 2014). The fuel compacts in this experiment held either tristructural isotropic (TRISO)-coated spherical kernels of uranium oxide (UO2) or TRISO-coated kernels containing both uranium carbide and uranium oxide phases (UCO). There were six separately monitored and controlled capsules in the AGR-2 test train. Capsule 3 held twelve compacts containing UO2-TRISO particles fabricated by BWX Technologies Nuclear Operations Group. The AGR-2 TRISO particles were fabricated in a pilot-scale fluidized-bed chemical vapor deposition (FB-CVD) furnace with a coating chamber inner diameter of 150 mm (Phillips, Barnes, and Hunn 2010), which was a change from the first irradiation experiment (AGR-1) particles that had been coated in a lab-scale FB-CVD coating system with a chamber inner diameter of 50 mm (Lowden 2006). The TRISO particles were overcoated with resinated graphite flake at Oak Ridge National Laboratory (ORNL), and the overcoated particles were pressed into one-inch-long, half-inch-diameter cylinders (Hunn, Montgomery, and Pappano 2010). Each cylindrical compact held an average of 1,543 TRISO particles with 9.6% enriched UO2 kernels that had a nominal diameter of 500 μm (Hunn, Savage, and Silva 2012). Capsule 3 compacts were irradiated to average calculated burnups of 9.01–10.69% fissions per initial metal atom (FIMA), and the average calculated fluences of fast neutrons with energies E n > 0.18 MeV were 3.05–3.53×10 25 n/m 2 (Sterbentz 2014). The calculated time-average, volume-average Capsule 3 compact temperatures were 996–1,062°C. However, Capsule 3 compact temperatures varied several hundred degrees across each compact, and the timeaverage minimum (TA min ) and time-average maximum (TA max ) temperatures were between 889–999°C and 1,072–1,105°C, respectively (Hawkes 2014). After irradiation, the AGR-2 test train was transferred from ATR to the INL Materials and Fuels Complex for inspection and disassembly (Ploger, Demkowicz, and Harp 2015). The initial inspection included dimensional metrology of the compacts and graphite fuel holders. Like all the AGR-2 compacts, the compacts in Capsule 3 shrank slightly during irradiation, as expected, with an average length reduction of 1.07–1.24% and an average diameter reduction of 0.13–0.41%. Post-irradiation examination (PIE) of the capsule components was completed to measure select fission products ( 90 Sr, 110m Ag, 134 Cs, 137 Cs, 144 Ce, and 154 Eu) outside the compacts (Stempien and Demkowicz 2020). This involved gamma counting of the graphite and graphoil spacers at the top and bottom of each capsule, acid leaching for radiochemical analysis of fission products on the metallic capsule components, and burn-leach analysis of the graphite holders. The total amount of 110mAg measured on the Capsule 3 components was 13% of the calculated capsule inventory. This was significantly lower than the amount of 110m Ag measured on the three UCO capsule components, which ranged from 32–70%. The lower 110m Ag release in Capsule 3 was likely due to lower peak temperatures compared with the UCO fuel capsules (Hawkes 2014). Measured inventories of the other select fission products were also lower in Capsule 3.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Oxidation Testing and Examination of AGR-2 Particles

Post-irradiation examination (PIE) oxidation testing is being performed at Oak Ridge National Laboratory (ORNL) on fuel particles from the second Advanced Gas Reactor (AGR) irradiation experiment (AGR-2). Tristructural isotropic (TRISO)-coated particles containing mixed uranium carbide and uranium oxide (UCO) fuel kernels were taken from AGR-2 Compact 5-4-2 and heated in the Furnace for Irradiated TRISO Testing (FITT) under varying oxidizing conditions. Details on Compact 5-4-2 PIE can be found in a previous report (Hunn et al. 2018).

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Destructive PIE and Safety Testing of Six AGR-5/6/7 Capsule 2 Compacts

This study evaluates fission product retention and particle failure mechanisms in AGR-5/6/7 Capsule 2 uranium carbide and uranium oxide (UCO) tristructural isotropic (TRISO) fuel under high-temperature gas reactor accident-relevant conditions using high-temperature safety tests and destructive postirradiation examination. Three Capsule 2 compacts were held isothermally at 1600°C for approximately 300 hours and one compact at 1800°C for approximately 300 hours; two additional compacts were examined in the as-irradiated state. Post-test deconsolidation–leach–burn–leach (DLBL) quantified nuclide inventories in matrix and particles. Individual particles were surveyed for radioisotope inventories, and microanalytical approaches resolved microstructural evolution and fission product distributions within the coating layers. At 1600°C, no krypton was detected above the minimum detectable limit, and cesium releases were far below a single particle equivalent, indicating the absence of full TRISO failure or SiC failures. Silver releases were limited and primarily reflected depleted postirradiation inventories, consistent with prior compact-level exams indicating substantial in-pile 110mAg loss. At 1800°C, cumulative 134Cs release of approximately 2.5 particle equivalents and delayed 85Kr totaling approximately 0.53 particle equivalents were consistent with one full TRISO failure and two SiC failures. Europium and strontium releases were roughly one order of magnitude higher than at 1600°C and comparable to AGR-1/AGR-2 high-temperature tests, with sustained late-hold rates indicating diffusion through intact coatings coupled with matrix depletion. Overall, AGR-5/6/7 Capsule 2 UCO fuel demonstrated fission product retention during safety testing consistent with prior AGR campaigns, while distinctive in-pile 110mAg depletion and measurable 1600°C europium loss motivate targeted follow-on studies.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Destructive PIE and Safety Testing of Six AGR-5/6/7 Capsule 2 Compacts

This study evaluates fission product retention and particle failure mechanisms in AGR-5/6/7 Capsule 2 uranium carbide and uranium oxide (UCO) tristructural isotropic (TRISO) fuel under high-temperature gas reactor accident-relevant conditions using high-temperature safety tests and destructive post-irradiation examination. Three Capsule 2 compacts were held isothermally at 1600°C for approximately 300 hours and one compact at 1800°C for approximately 300 hours; two additional compacts were examined in the as-irradiated state. Post-test deconsolidation–leach–burn–leach (DLBL) quantified nuclide inventories in matrix and particles. Individual particles were surveyed for radioisotope inventories, and microanalytical approaches resolved microstructural evolution and fission product distributions within the coating layers. At 1600°C, no krypton was detected above the minimum detectable limit, and cesium releases were far below a single particle equivalent, indicating the absence of full TRISO failure or SiC failures. Silver releases were limited and primarily reflected depleted post-irradiation inventories, consistent with prior compact-level exams indicating substantial in-pile 110m Ag loss. At 1800°C, cumulative 134 Cs release of approximately 2.5 particle equivalents and delayed 85 Kr totaling approximately 0.53 particle equivalents were consistent with one full TRISO failure and two SiC failures. Europium and strontium releases were roughly one order of magnitude higher than at 1600°C and comparable to AGR-1/AGR-2 high-temperature tests, with sustained late-hold rates indicating diffusion through intact coatings coupled with matrix depletion. Overall, AGR-5/6/7 Capsule 2 UCO fuel demonstrated fission product retention during safety testing consistent with prior AGR campaigns, while distinctive in-pile 110m Ag depletion and measurable 1600°C europium loss motivate targeted follow-on studies.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗