Search NASA⌕ Search

SEARCH · Search NASA

Results for “CATALYSTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Catalytic Activity of an Ensemble of Sites for CO 2 Hydrogenation to Methanol on a ZrO 2 -on-Cu Inverse Catalyst

The significant increase in CO 2 emissions from heavy fossil fuel utilization has raised serious concerns, highlighting the need for effective methods to convert CO 2 into value-added chemicals. Here, in this work, we report a computational investigation on the catalytic activity of ZrO 2 -on-Cu inverse catalysts for CO 2 hydrogenation to methanol, considering highly dispersed ZrO 2 trimers on Cu (111). Such clusters present a large ensemble of formate-containing configurations, Zr 3 O n (OH) m (OCHO) l , making the evaluation of the catalytic activity very challenging. We found that the sites on the various catalyst configurations exhibit markedly different activities for formate hydrogenation, despite their similar free energy and composition. To understand these differences in reactivity, we examined the structural and electronic nature of the low free-energy catalyst configurations and identified that the energy of the lowest unoccupied orbital of the reacting formate, modified by its binding with the catalytic site, is a descriptor for the reaction energy of the formate hydrogenation step. From there, we screened an ensemble of catalyst structures using this descriptor to predict highly active metastable catalyst configurations and computed the reaction pathways and transition states for formate hydrogenation. From this investigation, we distinguished reactive from nonreactive sites and formate species on the ZrO 2 /Cu inverse catalyst based on structural and electronic features. We showed that rare metastable configurations control the activity. Additionally, an efficient method for examining the reactivity of a large number of coexisting catalyst structures was developed.

catalysts↗

Silver-decorated palladium on carbon catalyst for enhanced ammonium formate dehydrogenation

Palladium (Pd)-based catalysts efficiently convert ammonium formate solution to hydrogen at low temperatures (<100 °C), but they tend to deactivate quickly during stability testing. This manuscript presents a systematic investigation into the catalytic properties of Pd–Ag bimetallic catalysts, focusing on their surface compositions and exploring the mechanisms behind the deactivation of Pd/Ag-based catalysts. Here this study reports a carbon-supported Pd–Ag bimetallic nanoparticle (NP) catalyst obtained through a galvanic replacement method, which showed enhanced formate dehydrogenation performance. The best catalyst, Pd 3 Ag 10 /ACA-G (Pd–Ag bimetallic NPs with a 3 : 10 mass ratio loaded on acid-washed activated carbon, prepared by the galvanic replacement method), presents the highest activity with a TOF of 5202 h -1 (~2.6-fold of commercial Pd/C). The enhanced electron density of Pd–Ag bimetallic nanoparticles, coupled with the advantages of a smaller nanoparticle size, and the modulation of hydrogen adsorption energy through the Ag/Pd surface alloy on the Ag/Pd(111) facet, collectively resulted in experimentally higher turnover rates of hydrogen production. The changes on the catalyst surface, including surface Ag fraction decrease, NP size growth, and O-containing species (carboxylate, etc.) adsorption, gradually resulted in catalyst deactivation.

08 HYDROGEN↗

Revealing the structure of a catalytic combustion active-site ensemble combining uniform nanocrystal catalysts and theory insights

Supported metal catalysts are extensively used in industrial and environmental applications. To improve their performance, it is crucial to identify the most active sites. This identification is, however, made challenging by the presence of a large number of potential surface structures that complicate such an assignment. Often, the active site is formed by an ensemble of atoms, thus introducing further complications in its identification. Being able to produce uniform structures and identify the ones that are responsible for the catalyst performance is a crucial goal. Here, we utilize a combination of uniform Pd/Pt nanocrystal catalysts and theory to reveal the catalytic active-site ensemble in highly active propene combustion materials. Using colloidal chemistry to exquisitely control nanoparticle size, we find that intrinsic rates for propene combustion in the presence of water increase monotonically with particle size on Pt-rich catalysts, suggesting that the reaction is structure dependent. We also reveal that water has a near-zero or mildly positive reaction rate order over Pd/Pt catalysts. Theory insights allow us to determine that the interaction of water with extended terraces present in large particles leads to the formation of step sites on metallic surfaces. These specific step-edge sites are responsible for the efficient combustion of propene at low temperature. This work reveals an elusive geometric ensemble, thus clearly identifying the active site in alkene combustion catalysts. These insights demonstrate how the combination of uniform catalysts and theory can provide a much deeper understanding of active-site geometry for many applications

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Developing novel electrodes with ultralow catalyst loading for high-efficiency hydrogen production in proton exchange membrane electrolyzer cells

Hydrogen plays more crucial roles for decarbonizing the planets and meeting the climate challenges because of its high energy density and zero-emission. It can be produced with proton exchange membrane electrolyzer cells (PEMECs) driven by sustainable and renewable energy resources. Although PEMECs have a number of advantages, including high purity production, quick response, and the ability to operate at high pressure facilitating the gas delivering, their performance and cost greatly hinder their commercial-scale applications. To achieve high-efficiency and cost-reduced hydrogen production in PEMECs, we proposed thin engineered liquid/gas diffusion layers (LGDLs) and associated electrodes, i.e., catalyst-coated LGDLs (CCLGDLs), over conventional porous transport layers (PTLs) and catalyst-coated membranes (CCMs). The research approaches in this project are based on material synthesis, in-situ and ex-situ characterizations, component design and treatment, numerical modeling, and cost analysis. The thin and tunable LGDLs (TT-LGDLs) and CCLGDLs were successfully developed with great performance improvement as demonstrated in lab-scale, bench-scale, and system-scale electrolyzer tests. The electrode thickness was reduced from 370 µm to less than 100 µm with simplified fabrication processes. With the catalytically enhanced Ir-based catalyst coating, the as-developed CCLGDLs with a catalyst loading of 0.34 mg Ir /cm 2 achieved a cell performance of 1.77 V at 2 A cm -2 , exhibiting the catalyst mass activity enhanced by >20 times with significant catalyst saving over conventional catalyst cell design. In-situ PEMEC characterizations, including the current distribution mapping and high-speed and multiscale visualizations, were conducted for a deeper understanding of mass transport and electrochemical reactions within an electrolyzer with LGDLs and CCLGDLs. A 2D cell model was developed and validated for the enhanced performance on TT-LGDL through reducing ohmic losses due to nonuniform hydration and water transport. Further, the cost analysis results have shown a path to move beyond equivalency and surpass costs associated with the project baseline. In this project, the design and fabrication of TT-LGDLs and CCLGDLs will contribute to the performance enhancement, manufacturing simplification, and cost reduction for PEMECs and other energy conversion devices, thus shortening their pathways towards commercialization. This project also provides a good foundation for furthering the in-situ reaction interface research.

08 HYDROGEN↗

An In-Depth Exploration of the Electrochemical Oxygen Reduction Reaction (ORR) Phenomenon on Carbon-Based Catalysts in Alkaline and Acidic Mediums

Detailed studies of the electrochemical oxygen reduction reaction (ORR) on catalyst materials are crucial to improving the performance of different electrochemical energy conversion and storage systems (e.g., fuel cells and batteries), as well as numerous chemical synthesis processes. In the effort to reduce the loading of expensive platinum group metal (PGM)-based catalysts for ORR in the electrochemical systems, many carbon-based catalysts have already shown promising results and numerous investigations on those catalysts are in progress. Most of these studies show the catalyst materials’ ORR performance as current density data obtained through the rotating disk electrode (RDE), rotating ring-disk electrode (RRDE) experiments taking cyclic voltammograms (CV) or linear sweep voltammograms (LSV) approaches. However, the provided descriptions or interpretations of those data curves are often ambiguous and recondite which can lead to an erroneous understanding of the ORR phenomenon in those specific systems and inaccurate characterization of the catalyst materials. In this paper, we presented a study of ORR on a newly developed carbon-based catalyst, the nitrogen-doped graphene/metal-organic framework (N-G/MOF), through RDE and RRDE experiments in both alkaline and acidic mediums, taking the LSV approach. The functions and crucial considerations for the different parts of the RDE/RRDE experiment such as the working electrode, reference electrode, counter electrode, electrolyte, and overall RDE/RRDE process are delineated which can serve as guidelines for the new researchers in this field. Experimentally obtained LSV curves’ shapes and their correlations with the possible ORR reaction pathways within the applied potential range are discussed in depth. We also demonstrated how the presence of hydrogen peroxide (H2O2), a possible intermediate of ORR, in the alkaline electrolyte and the concentration of acid in the acidic electrolyte can maneuver the ORR current density output in compliance with the possible ORR pathways.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mapping of Heterogeneous Catalyst Degradation in Polymer Electrolyte Fuel Cells

Pt catalysts in polymer electrolyte fuel cells degrade heterogeneously as the catalyst particles are exposed to local variations throughout the catalyst layer during operation. State-of-the-art analytical techniques for studying degradation of Pt catalysts do not possess fine spatial resolution to elucidate such non-uniform degradation behavior at a large electrode level. A new methodology is developed to spatially resolve and quantify the heterogeneous Pt catalyst degradation over a large area (several cm ) of aged MEAs based on synchrotron X-ray microdiffraction. PEFC single cells are aged using voltage cycling as an accelerated stress test and the degradation heterogeneity at a micrometer length scale is visualized by mapping Pt catalyst particle size after voltage cycling. It is demonstrated in detail that the Pt catalyst particle size growth is non-uniform and follows the flow field geometry. The Pt particle size growth is greater in the area under the flow field land, while it is minimal in the area under the flow field channel. Additional non-uniformity is observed with the Pt particle size increasing more rapidly at the air outlet area than the Pt particle size at the inlet area.

36 MATERIALS SCIENCE↗

Synergistic Electrocatalytic Syngas Production from Carbon Dioxide by Bi‐Metallic Atomically Dispersed Catalysts

Abstract The production of syngas by traditional processes such as steam methane reforming is energetically intensive and produces a large amount of CO 2 emissions. In contrast, the electrochemical CO 2 reduction reaction (CO 2 RR) enables the carbon neutral production of syngas at ambient conditions. Among non‐precious metal catalysts, metal‐nitrogen‐carbon electrocatalysts are inexpensive and highly selective towards syngas production. This study examined the selectivity of mono‐ and bi‐metallic (M−N−C, M=Fe, Mo or FeMo) electrocatalysts towards syngas production. The ratio of the CO : H 2 in the syngas was tuned by modifying the ratio of the metallic precursors in the bi‐metallic FeMo−N−C catalysts, tailoring the catalysts’ selectivity towards the CO 2 RR or the hydrogen evolution reaction (HER). The catalyst synthesis temperature(s) were considered as they influence the catalyst morphology and activity. Further, the dependence of the ratio of CO : H 2 in the syngas as a function of the potential was explored for the different bi‐metallic catalysts. This work showed that by tailoring both the ratio of Fe : Mo in the bi‐metallic catalyst and optimizing the reductive potential, a CO : H 2 ratio between 0.25 to 5 was achievable. This study demonstrated a novel approach in which the ratio of the product syngas composition could be tailored in a single reaction, without the need for further downstream processing to reach a desired composition.

Delafontaine, Laurent↗

Single vs double atom catalyst for N 2 activation in nitrogen reduction reaction: A DFT perspective

Abstract Ammonia synthesis through electrochemical reduction of nitrogen molecules is a promising strategy to significantly reduce the energy consumption in traditional industrial process. Detailed mechanism study of multistep complex nitrogen reduction reaction is prerequisite for the design of highly efficient catalyst. Stable atomically dispersed catalyst with unique geometric and electronic structure is suitable for the mechanism clarification of such a complex reaction. In this study, d ‐block transition‐metal (TM) anchored C 2 N single layer catalyst is investigated by the density functional theory (DFT) calculation. Both single TM‐anchored single atom catalyst (SAC) and double TM‐anchored double atom catalyst (DAC) exhibit good thermodynamic stability in atomically dispersed catalyst. In the case of SACs, IVB metals (Ti, Zr, Hf) exhibit the highest reactivity and lowest overpotential. While in the case of DACs, Cr─Cr system leads to the NH 3 formation, but V─V system leads to the N 2 H 4 formation. The SACs show much lower overpotential and stronger activation of N 2 molecule than the DACs due to the different activation mechanisms: traditional σ ‐donation/ π ‐backdonation N 2 activation mechanism is found in SACs, while a new π ‐donation/π‐backdonation N 2 activation mechanism is found in the DACs. The present work demonstrates that the different catalytic effect for NRR between SAC and DAC and their corresponding electronic structure origin, which gives more insight into the single atom catalyst. image

Qian, Yumin↗

Grafted nickel-promoter catalysts for dry reforming of methane identified through high-throughput experimentation

High-throughput synthesis of a series of monometallic and bimetallic catalysts (45 bimetallic and 50 monometallic samples) consisting of nickel and one of nine different metal promoters (B, Co, Cu, Fe, Mg, Mn, Sn, V and Zn) supported on one of six different metal oxides alumina, ceria, magnesia, silica and titania) is carried out via organometallic grafting using a robotic platform. The catalysts are evaluated for their activity and selectivity for the dry reforming of methane at a feed ratio of CH 4 :CO 2 of 1 at 650–800 °C in a parallel flow reactor system. The type of oxide support prevails over the type of additive for both catalyst activity and stability. On Al 2 O 3 and MgO, Fe was found to be the best promoter; on SiO 2 , Cu is the best promoter at 700 °C and higher, while on TiO 2 , Mn is found to enhance the conversion at 800 °C. On CeO 2 , all additives except Fe have beneficial effects. Twenty-five catalysts show > 90% methane conversion with ten catalysts showing > 95% conversion at 800 °C with the H 2 :CO ratios ranging from 0.8 to 1.2. Amongst the ten highest performers, NiFe/Al 2 O 3 and NiFe/MgO are more active than Ni/Al 2 O 3 and Ni/MgO, respectively and were stable over a period of 25 h at 800 °C. Characterization on the as-prepared samples reveals highly dispersed phase, while after reduction in H 2 , highly dispersed and reduced nickel particles up to 10 nm are formed. The particles do not increase in size under dry reforming reaction conditions at 800 °C. An increased hydrogen consumption observed during H 2 -TPR of the nickel particles is positively correlated with methane conversion for Al 2 O 3 -based catalysts. The resistance to deactivation by coking and variation in coke structure are investigated by spectroscopic and microscopic methods to identify the relationship between metal promoters, alloy formation, and type of surface carbon deposits. Carbon whiskers were observed on the ten selected spent samples and are preferentially deposited on Ni rather than on the promoters. Carbon nanotube formation and metal particle removal from support were not observed to cause deactivation while amorphous carbon formation was clearly linked to catalyst deactivation, as amorphous carbon could encapsulate nickel, either on the support or at the end of the carbon nanotube. Furthermore, the organometallic grafting technique is an efficient and suitable technique for synthesizing highly dispersed and homogeneous phases which lead to high conversion and high durability for dry reforming of methane.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Transient kinetic insights into selective propene oxidation over industrial bismuth molybdate catalysts

Selective oxidation of propene to acrolein over industrial multicomponent bismuth molybdate (BMO) catalysts significantly depends on reaction conditions that include operating parameters and catalyst state. Here, this work investigates selective propene oxidation in the intrinsic kinetic paradigm of Temporal Analysis of Products (TAP) reactor by systematically varying catalyst redox state, temperature, and oxygen-to-propene feed ratio. A 93 % propene conversion with an acrolein yield of 80 % is achieved at elevated temperatures (450 °C) on oxidized catalysts under oxygen-rich conditions (O 2 :C 3 H 6 = 10). However, these conditions diminish acrolein-to-CO 2 selectivity due to enhanced total oxidation to CO 2 . In contrast, a reduced catalyst state, moderate temperature (350 °C), and lower oxygen feed (O 2 :C 3 H 6 = 1) nearly doubles the acrolein to-CO 2 selectivity, albeit at a lower acrolein yield (33 %). Transient kinetic studies together with a kinetic model that simplify the major product formation pathways in lumped non-elementary forms reveal that the availability of surface oxygen species plays a pivotal role in governing reaction pathways. Additionally, density functional theory (DFT) calculations on pure BMO catalysts inform the role of surface redox states on propene and oxygen activation barriers. Lattice oxygen at acrolein-selective sites drives both acrolein and CO 2 formation, while adsorbed oxygen at activation sites favors unselective CO 2 generation. This work establishes a critical relationship between transient product selectivity and surface oxygen availability, which is strongly influenced by catalyst redox state, feed ratio, and reaction temperature. These insights underscore the importance of dynamic reactor operation strategies and offer a foundation for designing next-generation propene oxidation processes with tunable acrolein selectivity.

42 - ENGINEERING↗

Structural dependence of hydrogen evolution reaction on transition metal catalysts sputtered at different temperatures in alkaline media

In the present article, we studied the catalytic activity of magnetron sputtered Mo, V, Ni, and Co thin films for hydrogen evolution reaction (HER) in the alkaline electrolyte. Here, we find that the HER potentials (η 10 ) of the Mo and V thin film catalysts sputtered at 800 °C shift positive with respect to those of the film catalysts sputtered at 25°C. For Mo metal the observed shift of η 10 was 280 mV and for V metal observed shift of η 10 was 390 mV. On the other hand, minimal effect of sputtering temperature on both Ni and Co thin film catalyst activity for HER was observed. Structural analysis reveals that Mo and V prepared at 800 °C have uncommon face centered cubic (fcc, 0.74 packing density) structure as opposed to room-temperature sputtered Mo and V thin films which have common body centered cubic (bcc, 0.68 packing density) structure, resulting in significant increases of the packing densities when they are prepared at 800 °C. On the other hand, the high-temperature prepared thin films of Ni and Co retained fcc structures, resulting in no density changes compared to the room-temperature prepared fcc Ni and hexagonal close packed (hcp, 0.74 packing density) Co. Impedance spectroscopy shows that fcc Mo is a better catalyst than fcc Ni, which is considered an industry standard for non-noble pure metal-based catalysts in alkaline media. Stability tests also suggest that fcc Mo thin film catalysts prepared at 800 °C are more durable than fcc Ni thin films. Our study points out that structure phases of catalysts can be a key factor governing the activities of transition metals for HER in alkaline media.

08 HYDROGEN↗

Pairing Ga/Al-Zeolites with tailored acidity as tandem catalysts for the conversion of alcohols to olefins

Zeolites are versatile catalysts owing to their tunable acidity where the active site(s) can be placed within the crystal framework or as extra-framework species in confined pores. A common approach to tailor Brønsted acidity is heteroatom exchange involving the replacement of framework aluminum with alternative elements. Introduction of heteroatoms often results in less acidic catalysts that can be used in tandem reactions for targeted reactive intermediates. Here, in this study, we prepare a series of three different zeolites with MWW, CHA, and MFI frameworks as aluminosilicates and gallosilicates to demonstrate their performance in alcohol dehydration reactions. The two reactions examined in this study are methanol conversion to dimethyl ether and ethanol conversion to ethylene. Our findings reveal that Ga-zeolites exhibit superior performance with Ga-MCM-22 (MWW) achieving nearly 100% alcohol conversion and selectivity to desired products at contact times that are significantly less than most dehydration catalysts reported in literature. The unique properties of Ga-zeolites are attributed to their reduced acid site strength via a direct (one-pot) synthesis that avoids conventional time-intensive, multi-step post-synthesis modifications of Al-zeolites. Here we demonstrate the use of Ga-zeolites as tandem catalysts when paired with a downstream Al-zeolite in a dual-bed reactor configuration to convert cheaper reagents (alcohols) upstream to more desired intermediates as feeds for downstream catalysts to produce light olefins. We demonstrate that dual beds using Ga-zeolite – Al-ZSM-5 (upstream–downstream) pairings outperform single bed configurations with Al-ZSM-5 or a physical mixture (Ga-/Al-zeolite) for methanol to hydrocarbons reactions, with notable improvements in catalyst lifetime and increased light olefins selectivity. Similarly, dual beds using Ga-zeolite – Al-SSZ-13 (upstream–downstream) pairings result in improved performance for ethanol to propylene reactions with significant increases in propylene selectivity (>20 %) compared to a conventional single bed configuration of Al-SSZ-13. Overall, this study offers a new perspective on the use of heteroatom-exchanged zeolite catalysts in tandem reactions as a means of capitalizing on their reduced acid site strength and suggests differences in the intrinsic acidity of zeolite crystal structures.

42 ENGINEERING↗

Laser-engraved defects in TiO 2 support: Enhancing reducibility and redox capability of Pt/TiO 2 catalyst for reactive and selective hydrogenation

Titanium dioxide (TiO 2 ) has been studied as catalyst or catalyst support in catalysis. Its synthesis or modification approach controls the structural, optical, and electronic properties. Here, in this work, we applied laser engraving to the anatase TiO 2 and studied the consequent changes in its structure and property as well as the properties of TiO 2 supported platinum (i.e., Pt/TiO 2 ) catalyst. The laser engraving enlarged the particle size, formed rutile phase and created defects (i.e., oxygen vacancy (O v ) and Ti 3+ ) in anatase TiO 2 . This induced band gap change and enhanced visible light absorption. The defects created by laser engraving are stable and more reducible than those existed in the pristine TiO 2 . The defective TiO 2 is structurally stable and has great redox properties. The metal-support interaction in the Pt/defective TiO 2 catalyst is stronger than that of the pristine Pt/TiO 2 catalyst, which enabled higher reactivity and selectivity in hydrogenation of 3-nitrostyrene and furfuryl alcohol. Laser-engraved TiO 2 has been rarely studied for thermal catalysis. This work provides basic understanding of material properties and catalysis application of laser-engraved catalyst supports and catalysts in field of thermal catalysis.

25 ENERGY STORAGE↗

Operando S/TEM Reactions of Pt/TiO 2 Catalysts for Catalytic Fast Pyrolysis

Conversion of lignocellulosic biomass into the transportation fuel is an attractive concept. Using ex situ Catalytic Fast Pyrolysis (CFP) improves to upgrade bio-oils via catalytic deoxygenation of the biomass pyrolysis vapors. Zeolites are often used in this technique as the catalyst; however, in order to reduce minimum fuel selling price and improve carbon yields, ongoing research emphasizes catalyst optimization. By using bifunctional metal-acid catalysts and utilizing hydrogen, it is possible to improve carbon yields by minimizing the carbon-containing light gasses (since oxygen is removed aswater) and by reducing coke formation. Current research and development activities focuses on Pt/TiO 2 catalysts as the most promising catalyst candidates for the hydrodeoxygenation process. Here, our aim is to determine the structure-function relationships of the Pt/TiO 2 catalyst and the role of Pt dispersions within the catalyst on performance, using operando scanning transmission electron microscopy (S/TEM).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Cross-Scale Catalyst Modeling Applied to H 2 Storage and Release via Formic Acid

Here, we propose the Systems-to-Atoms (S2A) modeling framework that integrates the kinetics of reaction chemistry and structural configurations across various length scales with the aim of establishing a versatile template for multiscale modeling of reactive flow problems and to predict the operando activity of catalyst materials. The approach encompasses a microkinetic model to analyze surface reactions on individual facets of catalyst nanoparticles coupled with the computation of average surface reaction rates for catalyst nanoparticles of specific size distributions. Macro-homogeneous surface reaction kinetics are derived as a function of catalyst loading and used as input parameters for the continuum-scale reactor model. The cross-scale framework enables the optimization of catalyst utilization through reactor design and operating strategy. To demonstrate the framework, we studied the storage and release of hydrogen from formic acid, a promising liquid organic hydrogen carrier (LOHC), over Pd, Pt, and Cu catalysts. The framework predicts observed trends in formic acid dehydrogenation activity for catalysts with comparable weight loadings and metal particle diameters, demonstrating satisfactory quantitative alignment. Finally, the seamless transmission of parameter uncertainties between scales is also discussed.

08 HYDROGEN↗

Development of Ternary Transition Metal Oxide Catalysts for Oxygen Evolution Reaction

Electrochemical water splitting, a promising method for green hydrogen production, is currently hindered by the high cost of precious-group metal (PGM)-based catalysts for the oxygen evolution reaction (OER). This study addresses this challenge by advancing the development of catalysts for OER, focusing on the development of high-performance PGM-free catalysts using nickel-iron-cobalt (NiFeCo)-based aerogels. The catalysts were synthesized via a sol-gel method and critical point drying to achieve a highly porous structure with an exceptionally high surface area. The designed catalyst structure provides an ideal platform for maximizing catalytic active sites and enhancing mass transport kinetics. Co has been systematically incorporated into the current PGM-free state-of-the-art, NiFeOx catalyst, and the metal ratios have been optimized. In addition to the experimental studies, density functional theory calculations were performed to study the material’s properties of this ternary catalyst and the effect of Co addition on enhancing OER catalysis.

Mizrahi, Michal [Bar-Ilan University, Ramat Gan, I↗

Recreating Fuel Cell Catalyst Degradation in Aqueous Environments for Identical-Location Scanning Transmission Electron Microscopy Studies

The recent surge in interest of proton exchange membrane fuel cells (PEMFCs) for heavy-duty vehicles increases the demand on the durability of oxygen reduction reaction electrocatalysts used in the fuel cell cathode. This prioritizes efforts aimed at understanding and subsequently controlling catalyst degradation. Identical-location scanning transmission electron microscopy (IL-STEM) is a powerful method that enables precise characterization of degradation processes in individual catalyst nanoparticles across various stages of cycling. Recreating the degradation processes that occur in PEMFC membrane electrode assemblies (MEAs) within the aqueous cell used for IL-STEM experiments is vital for generating an accurate understanding of these processes. In this work, we investigate the type and degree of catalyst degradation achieved by cycling in an aqueous cell compared to a PEMFC MEA. While significant degradation is observed in IL-STEM experiments performed on a traditional Pt catalyst using the standard accelerated stress test potential window (0.6-0.95 VRHE), degradation of a PtCo catalyst designed for heavy-duty vehicle use is very limited compared to that observed in MEAs. We therefore explore various experimental parameters such as temperature, acid type, acid concentration, ionomer content, and potential window to identify conditions that reproduce the degradation observed in MEAs. We find that by extending the cycling potential window to 0.4-1.0 V RHE in an electrolyte containing Pt ions, the degraded particle size distribution and alloy composition better match that observed in MEAs. In particular, these conditions increase the relative contribution of Ostwald ripening, which appears to play a more significant role in the degradation of larger alloy particles supported on high-surface-area carbons than coalescence. Results from this work highlight the potential for discrepancies between ex situ aqueous experiments and MEA tests. While different catalysts may require a unique modification to the AST protocol, strategies provided in this work enable future in situ and identical-location experiments that will play an important role in the development of robust catalysts for heavy-duty vehicle applications.

30 DIRECT ENERGY CONVERSION↗