Search NASA⌕ Search

SEARCH · Search NASA

Results for “Dislocation Lines”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

In situ strain relaxation comparison between GaAsBi and GaInAs grown by molecular-beam epitaxy

The strain relaxation of GaAsBi is studied in order to determine both the maximum thickness before dislocations form for various misfits and the potential of GaAsBi for usage in the compositionally graded buffer of lattice-mismatched devices. Low-misfit GaAsBi epilayers are grown and compared with GaInAs, a well-studied material currently used in compositional grades. Relaxation behavior and dislocation energetics are compared using in situ wafer curvature. Samples are grown using molecular-beam epitaxy under similar conditions with misfit up to -0.81%. GaAsBi begins to relax at a lower thickness than GaInAs of the same mismatch. This leads to the majority of GaAsBi strain relaxation occurring with less material growth than comparable GaInAs. However, GaAsBi has greater residual strain than GaInAs after 2 {mu}m of growth. These results indicate that GaAsBi requires less elastic energy to form dislocations and more elastic energy to either encourage glide or multiply dislocations than GaInAs. GaAsBi shows less surface roughness than GaInAs for all samples, ruling out roughness as a source of dislocations and hindered glide in these alloys.

36 MATERIALS SCIENCE↗

Spontaneous formation of highly regular superlattice structure in InGaN epilayers grown by molecular beam epitaxy

In this letter, we have investigated the structural properties of thick InGaN layers grown on GaN by plasma-assisted molecular beam epitaxy, using two growth rates of 1.0 and 3.6 A/s. A highly regular superlattice (SL) structure is found to be spontaneously formed in the film grown at 3.6 A/s but not in the film grown at 1.0 A/s. The faster grown film also exhibits superior structural quality, which could be due to the surface roughness suppression caused by kinetic limitation, and the inhibition of the Frank-Read dislocation generation mechanism within the spontaneously formed SL structure.

36 MATERIALS SCIENCE↗

High-resolution x-ray diffraction investigation of relaxation and dislocations in SiGe layers grown on (001), (011), and (111) Si substrates

This work presents a detailed characterization, using high-resolution x-ray diffraction, of multilayered Si{sub 1-x}Ge{sub x} heterostructures grown on (001), (011), and (111) Si substrates by reduced pressure chemical vapor deposition. Reciprocal space mapping has been used to determine both the strain and Ge concentration depth profiles within each layer of the heterostructures after initially determining the crystallographic tilt of all the layers. Both symmetric and asymmetric reciprocal space maps were measured on each sample, and the evaluation was performed simultaneously for the whole data set. The ratio of misfit to threading dislocation densities has been estimated for each individual layer based on an analysis of diffuse x-ray scattering from the defects.

36 MATERIALS SCIENCE↗

The Growth of GaN on Si by the Beam Flux Modulation

AlGaN/GaN HEMT structure was grown on Si (111) substrate by plasma-assisted molecular beam epitaxy (PA-MBE) using a beam flux modulation methods. In this result, it was verified that the propagation of treading dislocation (TD) due to N-rich GaN layer was effectively suppressed.

36 MATERIALS SCIENCE↗

Dislocation network at InN/GaN interface revealed by scanning tunneling microscopy

For heteroepitaxy of InN on GaN(0001) by molecular-beam epitaxy, the lattice misfit strain is relieved by misfit dislocations (MDs) formed at the interface between InN and GaN. Imaging by scanning tunneling microscopy (STM) of the surfaces of thin InN epifilms reveals line feature parallel to <1120>. Their contrast becomes less apparent for thicker epifilms. From the interline spacing as well as a comparison with transmission electron microscopy studies, it is suggested that they correspond to the MDs beneath the surface. The STM contrast originates from both the surface distortion caused by the local strain at MDs and the electronic states of the defects.

36 MATERIALS SCIENCE↗

Cathodoluminescence and transmission electron microscopy study of dark line defects in thick In(0.2)Ga(0.8)As/GaAs multiple quantum wells

TEM and cathodoluminescence (CL) imaging and spectroscopy have been performed on In(0.2)Ga(0.8)As/GaAs MQW structures. Cross-sectional and plan-view TEM demonstrates that misfit dislocations (MDs) are confined to the MQW-to-GaAs interfacial regions. The observed large variation in the exciton luminescence intensity is interpreted as due to the presence of nonradiative recombination centers spread homogeneously in the MQW region away from interface MDs. These nonradiative recombination centers compete with exciton and midgap radiative centers at wavelengths of 950 nm and 1000-1600 nm, respectively, resulting in spatiallty correlated dark line defects for all CL imaging wavelengths.

Rich, D. H.↗

Systematic study of polycrystalline flow during tension test of sheet 304 austenitic stainless steel at room temperature

By systematic study the mapping of polycrystalline flow of sheet 304 austenitic stainless steel (ASS) during tension test at constant crosshead velocity at room temperature was obtained. The main results establish that the trajectory of crystals in the polycrystalline spatially extended system (PCSES), during irreversible deformation process obey a hyperbolic motion. Where, the ratio between the expansion velocity of the field and the velocity of the field source is not constant and the field lines of such trajectory of crystals become curved, this accelerated motion is called a hyperbolic motion. Such behavior is assisted by dislocations dynamics and self-accommodation process between crystals in the PCSES. Furthermore, by applying the quantum mechanics and relativistic model proposed by Muñoz-Andrade, the activation energy for polycrystalline flow during the tension test of 304 ASS was calculated for each instant in a global form. In conclusion was established that the mapping of the polycrystalline flow is fundamental to describe in an integral way the phenomenology and mechanics of irreversible deformation processes.

36 MATERIALS SCIENCE↗

Orientation and temperature dependence of some mechanical properties of the single-crystal nickel-base superalloy Rene N4. I - Tensile behavior

Single crystal specimens of a nickel-base superalloy with axes near 001, 011, and -112 were tested in tension at room temperature, 760, and 980 C. The alloy Rene N-4, was developed for gas turbine engine blades and has the nominal composition 3.7 Al, 4.2 Ti, 4 Ta, 0.5 Nb, 6 W, 1.5 Mo, 9 Cr, 7.5 Co, balance Ni, (all in weight percent). Analysis of slip band traces, specimen axis rotation, and dislocation Burgers vectors showed that at 760 and 980 C primary cube slip supplanted normal octahedral slip for the -112 line-oriented specimens. The other two orientations, which have lower resolved shear stresses on the cube system, exhibited octahedral slip at all three temperatures. The critical resolved shear stress is considerably greater on the cube system than on the octahedral system at room temperature. However, at 760 and 980 C the critical resolved shear stresses on the two systems are about the same. While the room temperature and 980 C yield strengths for the two orientations exhibiting octahedral slip could be rationalized on the basis of resolved shear stress, those at 760 C could not. Such violations of Schmid's law have previously been observed in other superalloys and single phase gamma-prime.

Miner, R. V.↗

Dislocation engineering in SiGe on periodic and aperiodic Si(001) templates studied by fast scanning X-ray nanodiffraction

Fast-scanning X-ray nanodiffraction microscopy is used to directly visualize the misfit dislocation network in a SiGe film deposited on a pit-patterned Si substrate at the beginning of plastic relaxation. X-ray real-space diffracted intensity maps are compared to topographic atomic force microscopy images, in which crosshatch lines can be seen. The change in intensity distribution as a function of the incidence angle shows localized variations in strain within the SiGe film. These variations, which reflect the order imposed by the substrate pattern, are attributed to the presence of both bunches of misfit dislocations and defect-free regions.

36 MATERIALS SCIENCE↗

Multistep damage evolution process in cubic zirconia irradiated with MeV ions

This work reports the study, via the combination of Rutherford backscattering spectrometry and channeling, x-ray diffraction, and transmission electron microscopy experiments, of the damage formation in cubic yttria-stabilized zirconia single crystals irradiated with medium-energy (4 MeV) heavy (Au) ions. The damage buildup, which is accounted for in the framework of the multistep damage accumulation model, occurs in three steps. The first step at low fluences (up to 10{sup 15} cm{sup -2}), characterized by a regular increase in both the damage yield and the elastic strain, is related to the formation of small defect clusters. The second step in the intermediate fluence range (from 10{sup 15} to 5x10{sup 15} cm{sup -2}) leads to a sharp increase in the damage yield and to a large drop of the strain due to the formation of dislocation loops which collapse into a network of tangled dislocations. The third step at high fluences (above 5x10{sup 15} cm{sup -2}) exhibits a surprising decrease in the damage yield, which may be attributed to the reorganization of the dislocation network that leads to the formation of weakly damaged regions with a size of the order of 100 nm.

36 MATERIALS SCIENCE↗

Comparative electron spin resonance study of epi-Lu{sub 2}O{sub 3}/(111)Si and a-Lu{sub 2}O{sub 3}/(100)Si interfaces: Misfit point defects

An electron spin resonance study has been carried out on heteroepitaxial Si/insulator structures obtained through growth of epi-Lu{sub 2}O{sub 3} films on (111)Si ({approx}4.5% mismatch) by molecular-beam epitaxy, with special attention to the inherent quality as well as the thermal stability of interfaces, monitored through occurring paramagnetic point defects. This indicates the presence, in the as-grown state, of P{sub b} defects ({approx}5x10{sup 11} cm{sup -2}) with the unpaired sp{sup 3} Si dangling bond along the [111] interface normal, the archetypical defect (trap) of the standard thermal (111)Si/SiO{sub 2} interface, directly revealing, and identified as the result of, imperfect epitaxy. The occurrence of P{sub b} defects, a major system of electrically detrimental interface traps, is ascribed to lattice mismatch with related introduction of misfit dislocations. This interface nature appears to persist for annealing in vacuum up to a temperature T{sub an{approx}}420 deg. C. Yet, in the range T{sub an{approx}}420-550 deg. C, the interface starts to ''degrade'' to standard Si/SiO{sub 2} properties, as indicated by the gradually increasing P{sub b} density and attendant appearance of the EX center, an SiO{sub 2}-associated defect. At T{sub an{approx}}700 deg. C, [P{sub b}] has increased to about 1.3 times the value for standard thermal (111)Si/SiO{sub 2}, to remain constant up to T{sub an{approx}}1000 deg. C, indicative of an unaltered interface structure. Annealing at T{sub an}>1000 deg. C results in disintegration altogether of the Si/SiO{sub 2}-type interface. Passivation anneal in H{sub 2} (405 deg. C) alarmingly fails to deactivate the P{sub b} system to the device grade (sub) 10{sup 10} cm{sup -2} eV{sup -1} level, which would disfavor c-Lu{sub 2}O{sub 3} as a suitable future high-{kappa} replacement for the a-SiO{sub 2} gate dielectric. Comparison of the thermal stability of the c-Lu{sub 2}O{sub 3}/(111)Si interface with that of molecular-beam deposited amorphous-Lu{sub 2}O{sub 3}/(100)Si shows the former to be superior, yet unlikely to meet technological thermal budget requirements. No Lu{sub 2}O{sub 3}-specific point defects could be observed.

36 MATERIALS SCIENCE↗

Microstructure versus Size: Mechanical Properties of Electroplated Single Crystalline Cu Nanopillars

We report results of uniaxial compression experiments on single-crystalline Cu nanopillars with nonzero initial dislocation densities produced without focused ion beam (FIB). Remarkably, we find the same power-law size-driven strengthening as FIB-fabricated face-centered cubic micropillars. TEM analysis reveals that initial dislocation density in our FIB-less pillars and those produced by FIB are on the order of 10{sup 14} m{sup -2} suggesting that mechanical response of nanoscale crystals is a stronger function of initial microstructure than of size regardless of fabrication method.

36 MATERIALS SCIENCE↗

X-Ray Diffraction Line Broadening in Shock Modified Pyrite [Book Chapter]

Powder compacts of a commercially-available pyrite, FeS 2 , have been subjected to controlled, quantitative high pressure shock loading at peak pressures from 7.5-22 GPa. The profiles of the x-ray diffraction lines have been examined to determine the reduction of the crystallite (domain) size and the introduction of residual microstrain due to defects and dislocations resulting from the transmission and interaction of the shockwave. Pyrite experience a surprisingly smaller profile broadening than observed for all other materials under similar shock conditions, suggesting a much more refractory character. Such small changes are consistent with low defect densities and with the relative low reaction activity (oxidation of sulfide to sulfate by humid air) observed on this material in the complementary studies.

36 MATERIALS SCIENCE↗

Investigation of deformation micro-mechanisms in nickel consolidated from a bimodal powder by spark plasma sintering

Bulk polycrystalline nickel compact was processed by spark plasma sintering from heterogeneous powder consisting of a mixture of nanometer and micrometer sized particles. The consolidated samples inherited the bimodal structure of the starting powder and was composed of ~ 55 vol.% coarse-grained (with the grain size larger than 1 μm) and ~ 45 vol.% ultrafine-grained (with an average grain size of ~ 550 nm) components. The deformation mechanisms were established by EBSD, X-ray line profile analysis and in-situ TEM observations. In the ultrafine-grained volume, the deformation occurred mainly through the activation of dislocation sources emitting full or partial dislocation either from grain interior or grain boundaries. Besides dislocation activity, rolling and sliding of nanograins were also observed during deformation by in-situ transmission electron microscopy, which have a considerable contribution to the observed high strain rate sensitivity of the bimodal microstructure. The cracks formed during deformation easily propagated in the nanograin regions due to the weaker particle bonding caused by the relatively high fraction of native oxide layer on the surface of the initial nanoparticles. - Highlights: • Bulk bimodal polycrystalline Ni was processed by SPS from a heterogeneous powder. • High SRS of the flow stress was observed which enhanced ductility and strength. • In-situ TEM revealed dislocation sources inside and at the boundaries of UFGs. • Twinning, partial dislocation and NG rolling were observed at crack tip vicinity. • The high SRS pertained to both dislocation activity in CG and NG rolling.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The crack-inclusion interaction problem

The general plane elastostatic problem of interaction between a crack and an inclusion is considered. The Green's functions for a pair of dislocations and a pair of concentrated body forces are used to generate the crack and the inclusion. Integral equations are obtained for a line crack and an elastic line inclusion having an arbitrary relative orientation and size. The nature of stress singularity around the end points of rigid and elastic inclusions is described and three special cases of this intersection problem are studied. The problem is solved for an arbitrary uniform stress state away from the crack-inclusion region. The nonintersecting crack-inclusion problem is considered for various relative size, orientation, and stiffness parameters, and the stress intensity factors at the ends of the inclusion and the crack are calculated. For the crack-inclusion intersection case, special stress intensity factors are defined and are calculated for various values of the parameters defining the relative size and orientation of the crack and the inclusion and the stiffness of the inclusion.

Xue-Hui, L.↗

The crack-inclusion interaction problem

The general plane elastostatic problem of interaction between a crack and an inclusion is considered. The Green's functions for a pair of dislocations and a pair of concentrated body forces are used to generate the crack and the inclusion. Integral equations are obtained for a line crack and an elastic line inclusion having an arbitrary relative orientation and size. The nature of stress singularity around the end points of rigid and elastic inclusions is described and three special cases of this intersection problem are studied. The problem is solved for an arbitrary uniform stress state away from the crack-inclusion region. The nonintersecting crack-inclusion problem is considered for various relative size, orientation, and stiffness parameters, and the stress intensity factors at the ends of the inclusion and the crack are calculated. For the crack-inclusion intersection case, special stress intensity factors are defined and are calculated for various values of the parameters defining the relative size and orientation of the crack and the inclusion and the stiffness of the inclusion.

Liu, X.-H.↗

In-Situ Optical Determination of Thermomechanical Properties of ZnSe and ZnTe Crystals

At temperatures above 1/2 T(sub m), the generation and movement of dislocations may result due to the load created by the weight of the crystal itself The deformation may be expected to increase the line defect density and may result in generation of low angle grain boundaries, especially in the regions of the crystal attached to the ampule. It has often been suspected that elimination of this effect in space can improve crystallinity of crystals grown under microgravity conditions, however, a direct experimental proof of such relation is still missing. In this work we have designed and built a system of in-situ optical detection and measurement of the mechanical deformations of a crystal wafer under its own weight, and studied the deformation effects as a function of temperature. The results of the measurements for ZnSe and ZnTe crystal wafers will be presented.

Burger, A.↗