At least 361 records · Page 20

Heavy ion measurement on LDEF

A stack of CR-39 and Kodak CN track detectors was exposed on the NASA satellite LDEF and recovered after almost six years in space. The quick look analysis yielded heavy ion tracks on a background of low energy secondaries from proton interaction. The detected heavy ions show a steep energy spectrum which indicates a radiation belt origin.

Beaujean, R.↗

Hypervelocity impact microfoil perforations in the LEO space environment (LDEF, MAP AO-023 experiment)

The Microabrasion Foil Experiment comprises arrays of frames, each supporting two layers of closely spaced metallic foils and a back-stop plate. The arrays, deploying aluminum and brass foil ranging from 1.5 to some 30 microns were exposed for 5.78 years on NASA's LDEF at a mean altitude of 458 km. They were deployed on the North, South, East, West, and Space pointing faces; results presented comprise the perforation rates for each location as a function of foil thickness. Initial results refer primarily to aluminum of 5 microns thickness or greater. This penetration distribution, comprising 2,342 perforations in total, shows significantly differing characteristics for each detector face. The anisotropy confirms, incorporating the dynamics of particulate orbital mechanics, the dominance of incorporating extraterrestrial particulates penetrating thicknesses greater than 20 microns in Al foil, yielding fluxes compatible with hyperbolic geocentric velocities. For thinner foils, a disproportionate increase in flux of particles on the East, North, and South faces shows the presence of orbital particulates which exceed the extraterrestrial component perforation rate at 5 micron foil thickness by a factor of approx. 4.

Mcdonnell, J. A. M.↗

LDEF impact craters formed by carbon-rich impactors: A preliminary report

Two impact craters found in Al from the Long Duration Exposure Facility (LDEF) experiment tray have residues concentrated in the bottoms, along the walls, and on top of overturned rims. Analyses indicate a 'chondritic' compositional signature (Si, S, Ca, Fe, Mg, and Ni) for the bulk residue. In one crater (number 74), round to irregular silicate grains are overlain by carbon. In addition, carbon also partially covers the crater walls, the top of the raised overturned rim, and extends outward from the crater. The second crater (number 31) also contains carbon with similar distribution in and about the crater, although the silicate residue appears to be glassy. Silver, I, K, and F (possibly some of the Ca, S, and Cl) appear to be contaminants as well as analyzed aromatic carbonaceous species associated with the raised rim and the area surrounding the crater. The origin of the impactors is assumed to be extraterrestrial. The existence of impactor residue in two craters implies impact velocities less than or equal to 6 km, based on experimental hypervelocity studies.

Bunch, T. E.↗

Dynamic (computer) modelling of the particulate environment: Transformations from the LDEF reference frame to decode geocentric and interplanetary populations

The Long Duration Exposure Facility (LDEF) impact signature record and the size frequency distribution of craters and perforations offers a unique record of environmental data referenced conveniently to the geocentric reference frame. Chemical analysis of residues can offer only limited assistance. Hence, flux modeling has been developed to transform both geocentric orbital distributions and geocentrically unbounded interplanetary source distributions. This is applied to the foil and crater penetration records in the Ram (E), Trailing (W), and Space Pointing directions to offer the means of decoding the records. It shows that the mix of the components is size dependent. Parametric forms of the modeling transformations are presented for the orbital and unbounded populations.

Mcdonnell, J. A. M.↗

LDEF: 69 Months in Space. First Post-Retrieval Symposium, part 2

A compilation of papers from the symposium is presented. The preliminary data analysis is presented of the 57 experiments flown on the LDEF. The experiments include materials, coatings, thermal systems, power and propulsion, science (cosmic ray, interstellar gas, heavy ions, and micrometeoroid), electronics, optics, and life science.

Arlene S. Levine↗

Measurement of the O-18 to O-16 isotope ratio for characterizing oxide surface layers on LDEF samples

The ratio of the density of the oxygen 18 isotope (O-18) to the density of the oxygen 16 isotope (O-16) is a strong function of altitude in the atmosphere because of the stronger gravitational attraction on the heavier isotope. It is proposed that the measurement of this ratio for oxide surface layers on LDEF samples can easily distinguish oxides formed in orbit from contaminative oxides formed during retrieval procedures. Since the satellite altitude is known as a function of time, it may be possible to use the measured ratio to determine the time of formation of oxide layers, the accuracy depending upon the stability of the atmosphere.

Sagalyn, Paul L.↗

Long Duration Exposure Facility (LDEF) preliminary findings: LEO space effects on the space plasma-voltage drainage experiment

The Space Plasma-High Voltage Drainage Experiment (SP-HVDE) provided a unique opportunity to study long term space environmental effects on materials because it was comprised of two identical experimental trays; one tray located on the ram facing side (D-10), and the other on the wake facing side (B-4) of the LDEF. This configuration allows for the comparison of identical materials exposed to two distinctly different environments. The purpose of this work is to document an assessment of the effects of five and three quarters years of low Earth orbital space exposure on materials comprising the SP-HVDE (experiment no. A0054). The findings of the materials investigation reported focus on atomic oxygen effects, micrometeor and debris impact site documentation, thermal property measurements, and environmentally induced contamination.

Blakkolb, Brian K.↗

Effects on LDEF exposed copper film and bulk

Two forms of copper were exposed to the Long Duration Exposure Facility (LDEF) Mission 1 environment: a copper film initially 74.2 plus or minus 1.1 nm thick sputter coated on a fused silical flat and a bulk piece of oxygen free, high conductivity (OFHC) copper. The optical density of the copper film changed from 1.33 to 0.70 where exposed and the film thickness increased to 106.7 plus or minus 0.5 nm where exposed. The exposed area appears purple by reflection and green by transmission for the thin film and maroon color for the bulk copper piece. The exposed areas increased in thickness, but only increase in the thickness of thin film samples could be readily measured. The increase in film thickness is consistent with the density changes occurring during conversion of copper to an oxide. However, we have not been able to confirm appreciable conversion to an oxide by x ray diffraction studies. We have not yet subjected the sample to e-beams or more abusive conditions out of concern that the film might be modified.

Peters, Palmer N.↗

LDEF experiment A0034: Atomic oxygen stimulated outgassing

The passive Long Duration Exposure Facility (LDEF) Experiment A0034, 'Atomic Oxygen Stimulated Outgassing', consisted of two identical one-sixth tray modules, exposing selected thermal control coatings to atomic oxygen and the combined space environment on the leading edge, and for reference, to the relative 'wake' environment of the trailing edge. Optical mirrors were included adjacent to the thermal coatings for deposition of the outgassing products. Ultraviolet grade windows and metal covers were provided for additional assessment of the effects of various environmental factors. Preliminary results indicate that orbital atomic oxygen is both a degrading and optically restorative factor in the thermo-optical properties of selected thermal coatings. There is evidence of more severe optical degradation on collector mirrors adjacent to coatings that were exposed to RAM-impinging atomic oxygen. This evidence of atomic oxygen stimulated outgassing is discussed in relation to alternative factors that could affect degradation. The general effects of the space environment on the experiment hardware as well as the specimens are discussed.

Linton, Roger C.↗

Atomic oxygen interactions with FEP Teflon and silicones on LDEF

The Long Duration Exposure Facility (LDEF) spacecraft has enabled the measurement of the effects of fixed orientation exposure of high fluence atomic oxygen on fluorinated ethylene propylene (FEP Teflon) and silicones. The atomic oxygen erosion yield for the FEP Teflon was found to be 3.64 x 10(exp -25) cm(exp 3)/atom. This erosion yield is significantly higher than that measured from previous low fluence orbital data. The FEP Teflon erosion yield was found to have the same dependence on oxygen arrival angle as Kapton and Mylar. Atomic oxygen interaction with silicon polymers results in the crazing of silicon. Released silicone contaminants were found to darken upon further atomic oxygen exposure.

Bruce A. Banks↗

Silver Teflon blanket: LDEF tray C-08

A study of the Teflon blanket surface at the edge of tray C-08 illustrates the complexity of the microenvironments on the Long Duration Exposure Facility (LDEF). The distribution of particulate contaminants varied dramatically over a distance of half a centimeter (quarter of an inch) near the edge of the blanket. The geometry and optical effects of the atomic oxygen erosion varied significantly over the few centimeters where the blanket folded over the edge of the tray resulting in a variety of orientations to the atomic oxygen flux. A very complex region of combined mechanical and atomic oxygen damage occurred where the blanket contacted the edge of the tray. A brown film deposit apparently fixed by ultraviolet light traveling by reflection through the Teflon film was conspicuous beyond the tray contract zone. Chemical and structural analysis of the surface of the brown film and beyond toward the protected edge of the blanket indicated some penetration of energetic atomic oxygen at least five millimeters past the blanket-tray contact interface.

Crutcher, E. Russ↗

Ellipsometric study of oxide films formed on LDEF metal samples

The optical constants of samples of six different metals (Al, Cu, Ni, Ta, W, and Zr) exposed to space on the Long Duration Exposure Facility (LDEF) were studied by variable angle spectroscopic ellipsometry. Measurements were also carried out on portions of each sample which were shielded from direct exposure by a metal bar. A least-squares fit of the data using an effective medium approximation was then carried out, with thickness and composition of surface films formed on the metal substrates as variable parameters. The analysis revealed that exposed portions of the Cu, Ni, Ta, and Zr samples are covered with porous oxide films ranging in thickness from 500 to 1000 A. The 410 A thick film of Al2O3 on the exposed Al sample is practically free of voids. Except for Cu, the shielded portions of these metals are covered by thin non-porous oxide films characteristic of exposure to air. The shielded part of the Cu sample has a much thicker porous coating of Cu2O. The tungsten data could not be analyzed.

Franzen, W.↗

M0003-10: LDEF advanced composites experiment

The Advanced Composites Experiment includes nearly 500 samples of metal matrix, organic matrix, and glass matrix composites that were flown on the leading and trailing edges of the Long Duration Exposure Facility (LDEF). The experiment is a cooperative effort with participation by several aerospace companies. This paper is a review of the preliminary observations and test results. Estimated recession rates from atomic oxygen exposure for organic matrix composites are reported. Preliminary scanning electron microscopy observations for organic and metal matrix composites and microstructural analyses for metal matrix composites are presented.

Steckel, Gary L.↗

Survey of results from the Boeing modules on the M0003 experiment on LDEF

The Boeing Company provided specimens to be flown on the Long Duration Exposure Facility (LDEF) as part of the M0003 experiment. This hardware was for the M0003-8 and part of the M003-10 sub-experiments. These specimens were flown on the leading (tray D-9) and trailing (tray D-3) edges, and on trays D-8 (38 degrees from ram) and D-4. Some specimens were mounted in the Experiment Exposure Control Canisters.

Pippin, H. Gary↗

Results from analysis of Boeing composite specimens flown on LDEF experiment M0003

Specimens of three organic matrix/graphite fiber reinforced composites were flown at both the leading and trailing edge locations on the Long Duration Exposure Facility (LDEF). Selected specimens flown at the trailing edge position were held under tension, compression, and flexure loads for the duration of the flight. Also, two epoxy adhesives with composite and metallic adherends were flown at the trailing edge position. These specimens experienced 5.8 years of exposure to the low earth orbit (LEO) environment where they were subjected to atomic oxygen (AO), thermal cycling, ultraviolet (UV) light, and particulate radiation. Post flight mechanical, chemical, optical, and physical tests were performed and the results were compared to preflight and published values. AO erosion of the leading edge specimens resulted in a significant reduction of mechanical properties and a change in optical properties. Chemical changes occurred only on the surface.

George, Pete E.↗

Patterns of discoloration and oxidation by direct and scattered fluxes on LDEF, including oxygen on silicon

A number of interesting discoloration patterns are clearly evident on MOOO2-1 which resides on the three faces of the Long Duration Exposure Facility (LDEF). Most interesting is the pattern of blue oxidation on polished single crystal silicon apparently produced by scattered or direct ram oxygen atoms along the earth face. A complete explanation for the patterns has not yet been obtained. All honeycomb outgassing holes have a small discoloration ring around them that varies in color. The shadow cast by a suspended wire on the earth face surface is not easily explained by either solar photons or by ram flux. The shadows and the dark/light regions cannot be explained consistently by the process of solar ultraviolet paint-darkening modulated by ram flux oxygen bleaching of the paint.

Frederickson, A. R.↗

Atomic oxygen exposure of LDEF experiment trays

Atomic oxygen exposures were determined analytically for rows, longerons, and end bays of the Long Duration Exposure Facility (LDEF). The calculations are based on an analytical model that accounts for the effects of thermal molecular velocity, atmospheric temperature, number density, spacecraft velocity, incidence angle, and atmospheric rotation on atomic oxygen flux. Results incorporate variations in solar activity, geomagnetic index, and orbital parameters occurring over the 6-year flight of the spacecraft. To facilitate use of the data, both detailed tabulations and summary charts for atomic oxygen fluences are presented.

Bourassa, R. J.↗

Effects of the space environment on space-based radar phased-array antenna; status and preliminary observations (LDEF Experiment A0133)

The overall objective of the experiment was to evaluate the effect of the space environment on components considered for a Space-Based Radar (SBR) Phased-Array Antenna. Of primary interest was a study of the degradation of the polyimide film Kapton (DuPont trademark), the material considered for use in the antenna plane. The most striking result of the experiment was the overall good condition of the Kapton antenna planes and Kapton tensile specimens, despite nearly six years of exposure to the space environment. This was largely attributable to the orientation of the Kapton (parallel and flush on the space end) and the stability of the Long Duration Exposure Facility (LDEF) in orbit. However, weathering of exposed Kapton surfaces was not insignificant. Results on elongation and mechanical properties of the plain and the fiberglass-reinforced Kapton are presented. Reduction in strain to failure of flight-exposed Kapton is attributed to surface defects of these specimens. Physical property testing of the materials to date reveals no significant difference between flight-exposed and control material. The second objective was to investigate the interaction between high-voltage electrodes and typical spacecraft contaminants in simulation of discharge triggering across differentially charged dielectric surfaces (spacecraft charging conditions). Electronic data acquisition and memory systems appeared to operate correctly, but very few discharges were recorded. Induced radioactivity, contamination, impacts, and orientation features of atomic oxygen erosion were observed.

J B Whiteside↗