Search NASA⌕ Search

SEARCH · Search NASA

Results for “PROTECTIVE COATING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Tuning Molecular Interactions between Peptoids and Substrates to Achieve Surface-Agnostic Coating

Achieving programmable and robust coatings that maintain functionality while adhering to various surface types with molecular-level tunability and programmable features remains challenging. In this study, we develop adaptable and stable surface-agnostic coatings (SACs) based on crystalline peptoid membranes by tuning interpeptoid and peptoid-substrate interactions. We utilize two complementary methods: (1) surfaceinduced assembly, where peptoid membranes form directly on substrates, and (2) depositing preformed peptoid crystalline membranes via an aqueous layer-by-layer (LbL) assembly technique. These strategies are applied to substrates with diverse surface chemistries and topographies, including mica, highly ordered pyrolytic graphite (HOPG), MoS 2 , sapphire, and porous membranes like porous alumina and polysulfide. Atomic force microscopy confirms the formation of peptoid coatings and reveals differences in assembly behavior across surfaces. Moisture vapor transport measurements serve as a proof-of-concept test for membrane continuity and tunable permeance. Together, these findings demonstrate the adaptability and programmability of peptoid-based SACs, enabling rational coating design on surfaces with diverse chemical and topographical features. Furthermore, this work opens pathways for using peptoid membranes as programmable surface modifiers in functional interfaces, protective coatings, and membrane platforms.

biomimetic polymers↗

Silicon nitride passivation of IC's

Feasibility study looks at effectiveness of silicon nitride passivation coating against moisture and mobile ions. Coating was tested on CMOS microcircuits. Tests included temperature cycling, high-temperature electrical stress, and temperature and humidity exposure. Report concludes plastic-encapsulated circuits with protective coating exhibit high survival rates; it includes tables summarizing test results and figures that show effects of flexing.

Erickson, J. J.↗

High Temperature Solid Particle Erosion of Environmental and Thermal Barrier Coatings

Solid particle erosion (SPE) is a common phenomenon observed in gas turbine engines. Particles entrained in the gas flow impact engine hardware resulting in micro-scale damage that leads to deleterious effects such as material removal. For protective coatings, damage due to SPE is a key concern since it can negatively affect the durability of the coating and subsequently the life of the underlying component. In this work, the high temperature SPE behavior of two state-of-the-art environmental barrier coatings (EBCs) deposited via air plasma spray (APS) is investigated using alumina erodent to understand the effect of particle kinetic energy, impingement angle and temperature. The SPE behavior of the EBCs is also compared to APS and electron beam – physical vapor deposition (EB-PVD) thermal barrier coatings (TBCs) to elucidate similarities and differences in the erosion response. The EBCs were more susceptible to SPE than the EB-PVD TBC but had greater SPE resistance compared to the APS TBC. Coating microstructure and porosity were shown to have a strong influence on the observed behavior.

Solid particle erosion↗

Detection of weldment lack of fusion using opaque additives

Problems in the production of aluminum weldments are caused by moisture absorbed by the aluminum oxide which forms on the surface before welding. Another problem is incomplete penetration of the weldment. The problems can be solved by coating the aluminum surfaces with an X-ray-opaque metal such as silver or copper. This will prevent the formation of moisture-absorbing aluminum oxide. Any protective coating remaining in an area of incomplete weld penetration can be seen in an inspection of the weldment conducted with the aid of an X-ray method. Details of copper deposition procedures are discussed along with a copper coating analysis and the testing of the weldments.

Cook, J. L.↗

MMOD Protection and Degradation Effects for Thermal Control Systems

Micrometeoroid and orbital debris (MMOD) environment overview Hypervelocity impact effects & MMOD shielding MMOD risk assessment process Requirements & protection techniques - ISS - Shuttle - Orion/Commercial Crew Vehicles MMOD effects on spacecraft systems & improving MMOD protection - Radiators Coatings - Thermal protection system (TPS) for atmospheric entry vehicles Coatings - Windows - Solar arrays - Solar array masts - EVA Handrails - Thermal Blankets Orbital Debris provided by JSC & is the predominate threat in low Earth orbit - ORDEM 3.0 is latest model (released December 2013) - http://orbitaldebris.jsc.nasa.gov/ - Man-made objects in orbit about Earth impacting up to 16 km/s average 9-10 km/s for ISS orbit - High-density debris (steel) is major issue Meteoroid model provided by MSFC - MEM-R2 is latest release - http://www.nasa.gov/offices/meo/home/index.html - Natural particles in orbit about sun Mg-silicates, Ni-Fe, others - Meteoroid environment (MEM): 11-72 km/s Average 22-23 km/s.

Christiansen, Eric↗

Ion beam deposited protective films

Single or dual ion beam sources were used to deposit thin films for different applications. Metal and metal oxide films were evaluated as protective coatings for the materials. Film adherence was measured and the most promising films were then tested under environments similar to operating conditions. It was shown that some materials do protect die material (H-13 steel) and do reduce thermal fatigue. Diamondlike films have many useful applications. A series of experiments were conducted to define and optimize new approaches to the manufacture of such films. A dual beam system using argon and methane gases was developed to generate these films.

Mirtich, M. J.↗

Diamondlike carbon applications in infrared optics and microelectronics

The use of diamondlike carbon (DLC) as a protective coating in harsh environments is addressed. There are three topics presented. The first is a description of the preparation of DLC on seven different infrared transmitting materials, and the possibility of using DLC as an antireflecting coating at commonly used wavelengths. DLC doesn't bond easily to all materials, and special techniques for bonding are presented. The second topic deals with how well DLC will protect a substrate from moisture penetration. This is an important aspect in numerous uses of DLC, including both infrared optics and integrated circuits. The third topic is the effect of particulate impact on film performance and integrity.

Woollam, John A.↗

Oxidation performance of platinum-clad Mo-47Re alloy

The alloy Mo-47Re has favorable mechanical properties at temperatures above 1400 C, but it undergoes severe oxidation when used in air with no protective coating. To shield the alloy from oxidation, platinum cladding has been evaluated. The unprotected alloy undergoes catastrophic oxidation under static and dynamic oxidation conditions. The platinum cladding provides good protection from static and dynamic oxidation for moderate times at 1260 C. Samples tested for longer times under static oxidation conditions experienced severe oxidation. The data suggest that oxidation results from the transport of oxygen through the grain boundaries and through the pinhole defects of the platinum cladding.

Clark, Ronald K.↗

Isotopic study of oxygen diffusion in oxide coatings

Diffusion of oxygen in thin films of silicon dioxide was studied using oxygen isotopically enriched in oxygen of atomic mass 18 (O-18). This subject is of interest because thin films of dielectrics such as SiO2 are proposed for use as a protective coatings for solar mirrors in low Earth orbit, which is a strongly oxidizing environment. Films of this material were prepared with a direct current magnetron using reactive sputtering techniques. To produce (O-18)- enriched SiO2, a standard 3.5-in.-diameter silicon wafer was reactively sputtered using (O-18)-enriched (95 percent) oxygen as the plasma feed gas. The films were characterized using Rutherford backscattering and Secondary Ion Mass Spectrometer (SIMS) to establish stoichiometry and purity. Subsequently, the films were exposed to an air-derived oxygen plasma in a standard laboratory plasma reactor for durations of up to 10 hr. The concentration ratio of O-16 as a function of depth was determined using SIMS profiling and compared to a baseline, nonplasma exposed sample. A value for the diffusivity of oxygen near the surface of these films was obtained and found to be about 10(-15)sq cm/sec.

Gulino, Daniel A.↗

Cyclic Oxidation and Hot Corrosion of NiCrY-Coated Disk Superalloy

Powder metallurgy disk superalloys have been designed for higher engine operating temperatures through improvement of their strength and creep resistance. Yet, increasing disk application temperatures to 704 C and higher could enhance oxidation and activate hot corrosion in harmful environments. Protective coatings could be necessary to mitigate such attack. Cylindrical coated specimens of disk superalloys LSHR and ME3 were subjected to thermal cycling to produce cyclic oxidation in air at a maximum temperature of 760 C. The effects of substrate roughness and coating thickness on coating integrity after cyclic oxidation were considered. Selected coated samples that had cyclic oxidation were then subjected to accelerated hot corrosion tests. The effects of this cyclic oxidation on resistance to subsequent hot corrosion attack were examined.

Hot corrosion↗

Diamond Coatings

Advances in materials technology have demonstrated that it is possible to get the advantages of diamond in a number of applications without the cost penalty, by coating and chemically bonding an inexpensive substrate with a thin film of diamond-like carbon (DLC). Diamond films offer tremendous technical and economic potential in such advances as chemically inert protective coatings; machine tools and parts capable of resisting wear 10 times longer; ball bearings and metal cutting tools; a broad variety of optical instruments and systems; and consumer products. Among the American companies engaged in DLC commercialization is Diamonex, Inc., a diamond coating spinoff of Air Products and Chemicals, Inc. Along with its own proprietary technology for both polycrystalline diamond and DLC coatings, Diamonex is using, under an exclusive license, NASA technology for depositing DLC on a substrate. Diamonex is developing, and offering commercially, under the trade name Diamond Aegis, a line of polycrystalline diamond-coated products that can be custom tailored for optical, electronic and engineering applications. Diamonex's initial focus is on optical products and the first commercial product is expected in late 1990. Other target applications include electronic heat sink substrates, x-ray lithography masks, metal cutting tools and bearings.

Source record↗

Development of a space stable thermal control coatings for use in large space vehicles

The preparation and evaluation of zinc orthotitanate and of several new pigments and the environmental testing and evaluation of these pigments and of coatings made from them constitute the bulk of the work accomplished. New pigments were prepared and EPR spectra of pigments and their precursor compounds studied. Results of extensive testing of commercially-available, strippable, protective coatings are reported; Owens-Illinois 650 glass resin has been stabilized against progressive mechanical failures; and definite improvements have been noted. A zinc oxide pigmented lithium silicate paint has demonstrated very good ultraviolet stability.

Gilligan, J. E.↗

Oxidation of Alumina-Forming MAX Phases in Turbine Environments

Protective coatings for high temperature turbine components are based on YSZ thermal barriers and oxidation resistant, alumina-forming NiAl or NiCoCrAlY bond coats. Ti2AlC and Cr2AlC MAX phases are thus of special interest because of good oxidation resistance and CTE that can match Al2O3 and YSZ. Their alumina scales grow according to cubic kinetics due to grain growth in the scale, with initial heating dominated by fast TiO2 growth. Protective cubic kinetics are also found in high pressure burner rig tests of MAXthal 211 Ti2AlC, but with reduced rates due to volatile TiO(OH)2 formation in water vapor. YSZ-coatings on bulk Ti2AlC exhibit remarkable durability up to 1300C in furnace tests and at least a 25x life advantage compared to superalloys. At another extreme, Cr2AlC is resistant to low temperature Na2SO4 hot corrosion and exhibits thermal cycling stability bonded to a superalloy disk material. Accordingly, sputtered Cr2AlC coatings on disk specimens prevented hot corrosion detriments on LCF. Breakaway oxidation (Ti2AlC), scale spallation (Cr2AlC), interdiffusion, and processing as coatings still present serious challenges. However the basic properties of MAX phases provide some unusual opportunities for use in high temperature turbines.

ceramics↗

Protection of solar array blankets from attack by low earth orbital atomic oxygen

The ram impact of low earth orbital atomic oxygen causes oxidation of spacecraft materials including polymers such as polyimides. The rate of oxidation is sufficiently high to potentially compromise the long term durability of Kapton solar array blankets. Ion beam sputter deposited atomic oxygen protective coatings of aluminum oxide, silicon dioxide, and codeposited silicon dioxide with small amounts of polytetrafluoroethylene were evaluated both in RF plasma asher tests and in low earth orbit. Deposition techniques, mechanical properties, and atomic oxygen protection performance are presented.

Banks, Bruce A.↗

Mast material test program (MAMATEP)

The Mast Material Test Program (MAMATEP) at NASA Lewis is discussed. Objectives include verifying the need for, and evaluating the performance of, various protection techniques for the Solar Array Assembly mast of the Space Station Photovoltaic Power Module. Mast material samples were evaluated in terms of mass and bending modulus, measured before and after environmental exposure. Test environments included atomic oxygen exposure (RF plasma asher), thermal cycling, and mechanical flexing. Protective coatings included CV-1144 silicon, a Ni/Au/InSn eutectic, and an open weave, Al braid. Results indicate that unprotected samples degrade in an atomic oxygen environment at a steady rate. Open weave, Al braid offers little protection for the fiberglass-epoxy sample in an asher environment. Ni/Au/InSn eutectic offers excellent protection in an asher environment prior to thermal cycling and mechanical flexing. Long duration asher results from unprotected samples indicate that, even though the fiberglass-epoxy degrades, a protection technique may not be necessary to ensure structural integrity. However, a protection technique may be desirable to limit or contain the amount of debris generated by the degradation of the fiberglass-epoxy.

Ciancone, Michael L.↗

Measuring Thicknesses of Coatings on Metals

Digital light sensor and eddy-current sensor measure thickness without contact. Surface of Coating reflects laser beam to optical sensor. Position of reflected spot on sensor used by microcomputer to calculate coating thickness. Eddy-current sensor maintains constant distance between optical sensor and metal substrate. When capabilities of available components fully exploited, instrument measures coatings from 0.001 to 6 in. (0.0025 to 15 cm) thick with accuracy of 1 part in 4,000. Instrument readily incorporated in automatic production and inspection systems. Used to inspect thermal-insulation layers, paint, and protective coatings. Also used to control application of coatings to preset thicknesses.

Cotty, Glenn M., Jr.↗

John F. Kennedy Space Center's Technology Development and Application 2006-2007 Report

Topics covered include: Reversible Chemochromic Hydrogen Detectors; Determining Trajectory of Triboelectrically Charged Particles, Using Discrete Element Modeling; Using Indium Tin Oxide To Mitigate Dust on Viewing Ports; High-Performance Polyimide Powder Coatings; Controlled-Release Microcapsules for Smart Coatings for Corrosion Applications; Aerocoat 7 Replacement Coatings; Photocatalytic Coatings for Exploration and Spaceport Design; New Materials for the Repair of Polyimide Electrical Wire Insulation; Commodity-Free Calibration; Novel Ice Mitigation Methods; Crack Offset Measurement With the Projected Laser Target Device; New Materials for Structural Composites and Protective Coatings; Fire Chemistry Testing of Spray-On Foam Insulation (SOFI); Using Aerogel-Based Insulation Material To Prevent Foam Loss on the Liquid-Hydrogen Intertank; Particle Ejection and Levitation Technology (PELT); Electrostatic Characterization of Lunar Dust; Numerical Analysis of Rocket Exhaust Cratering; RESOLVE Projects: Lunar Water Resource Demonstration and Regolith Volatile Characterization; Tribocharging Lunar Soil for Electrostatic Beneficiation; Numerically Modeling the Erosion of Lunar Soil by Rocket Exhaust Plumes; Trajectory Model of Lunar Dust Particles; Using Lunar Module Shadows To Scale the Effects of Rocket Exhaust Plumes; Predicting the Acoustic Environment Induced by the Launch of the Ares I Vehicle; Measuring Ultrasonic Acoustic Velocity in a Thin Sheet of Graphite Epoxy Composite; Hail Size Distribution Mapping; Launch Pad 39 Hail Monitor Array System; Autonomous Flight Safety System - Phase III; The Photogrammetry Cube; Bird Vision System; Automating Range Surveillance Through Radio Interferometry and Field Strength Mapping Techniques; Next-Generation Telemetry Workstation; GPS Metric Tracking Unit; and Space-Based Range.

Source record↗

Fretting of AISI 9310 and selected fretting resistant surface treatments

Fretting wear experiments were conducted with uncoated AISI 9310 mating surfaces, and with combinations incorporating a selected coating to one of the mating surfaces. Wear measurements and SEM observations indicated that surface fatigue, as made evident by spallation and surface crack formation, is an important mechanism in promoting fretting wear to uncoated 9310. Increasing humidity resulted in accelerated fretting, and a very noticeable difference in nature of the fretting debris. Of the coatings evaluated, aluminum bronze with a polyester additive was most effective at reducing wear and minimizing fretting damage to the mating uncoated surface, by means of a selflubricating film that developed on the fretting surfaces. Chromium plate performed as an effective protective coating, itself resisting fretting and not accelerating damage to the uncoated surface.

Bill, R. C.↗