Search NASA⌕ Search

SEARCH · Search NASA

Results for “Polymer polymer interface”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Cohesive finite element modeling of the delamination of HTPB binder and HMX crystals under tensile loading

Accurately modeling the mechanical behavior of the polymer binders and the degradation of interfaces between binder and crystal is important to science-based understanding of the macro-scale response of polymer bonded explosives. The paper presents a description of relatively a simple bi-crystal HMX-HTPB specimen and associated tensile loading experiment including computed tomography imaging, the pertinent constitutive theory, and details of numerical simulations used to infer the behavior of the material during the delamination process. Within this work, mechanical testing and direct numerical simulation of this relatively simple bi-crystal system enabled reasonable isolation of binder-crystal interface delamination, in which the effects of the complicated thermomechanical response of explosive crystals were minimized. Cohesive finite element modeling of the degradation and delamination of the interface between a modified HTPB binder and HMX crystals was used to reproduce observed results from tensile loading experiments on bi-crystal specimens. Several comparisons are made with experimental measurements in order to identify appropriate constitutive behavior of the binder and appropriate parameters for the cohesive traction-separation behavior of the crystal-binder interface. This research demonstrates the utility of directly modeling the delamination between binder and crystal within crystal-binder-crystal tensile specimen towards characterizing the behavior of these interfaces in a manner amenable to larger scale simulation of polycrystalline PBX materials. One critical aspect of this approach is micro computed tomography imaging conducted during the experiments, which enabled comparison of delamination patterns between the direct numerical simulation and actual specimen. In addition to optimizing the cohesive interface parameters, one important finding from this investigation is that understanding and representing the strain-hardening plasticity of HTPB binder is important within the context of using a cohesive traction-separation model for the delamination of a crystal-binder system.

42 ENGINEERING↗

The effect of protein–precipitant interfaces and applied shear on the nucleation and growth of lysozyme crystals

The nucleation of lysozyme in microbatch experiments was linked to the formation of protein–precipitant interfaces. The use of oscillatory shear allowed decreasing the nucleation rate and extending the growth period for lysozyme crystals, presumably through the control of the number of interfaces and removal of impurities or defects. This paper is concerned with the effect of protein–precipitant interfaces and externally applied shear on the nucleation and growth kinetics of hen egg-white lysozyme crystals. The early stages of microbatch crystallization of lysozyme were explored using both optical and confocal fluorescence microscopy imaging. Initially, an antisolvent (precipitant) was added to a protein drop and the optical development of the protein–precipitant interface was followed with time. In the presence of the water-soluble polymer poly(ethylene glycol) (PEG) a sharp interface was observed to form immediately within the drop, giving an initial clear separation between the lighter protein solution and the heavier precipitant. This interface subsequently became unstable and quickly developed within a few seconds into several unstable ‘fingers’ that represented regions of high concentration-gradient interfaces. Confocal microscopy demonstrated that the subsequent nucleation of protein crystals occurred preferentially in the region of these interfaces. Additional experiments using an optical shearing system demonstrated that oscillatory shear significantly decreased nucleation rates whilst extending the growth period of the lysozyme crystals. The experimental observations relating to both nucleation and growth have relevance in developing efficient and reliable protocols for general crystallization procedures and the controlled crystallization of single large high-quality protein crystals for use in X-ray crystallography.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Understanding the Role of Interfaces for Water Management in Platinum Group Metal-Free Electrodes in Polymer Electrolyte Fuel Cells

For this study, a systematic analysis, both experimental and model-assisted, has been performed over three main configurations of platinum group metal-free (PGM-free) electrodes in polymer electrolyte fuel cells (PEFCs): Catalyst-coated membrane CCM technology is being compared to the gas-diffusion electrode (GDE) method of electrode fabrication and juxtaposed to a hybrid/combined GDE-CCM method of membrane-electrode assembly (MEA) fabrication. The corresponding electrodes were evaluated for their electrochemical performance, modeled, and studied with in situ and operando X-ray computed tomography (X-ray CT). The study establishes that through-thickness inhomogeneities play the most important role in water withdrawal/water management and affect most significantly PGM-free PEFC performance. The catalyst integration technique results in formation of interfacial regions with increased porosity and surface roughness. These regions form critical interfaces de facto responsible for flooding type behavior of the PEFC as shown for a first time by operando X-ray CT. The computational model shows that the PEFC performance critically depends on liquid water formation and transport at cold and wet conditions.

25 ENERGY STORAGE↗

The Impact of Device Polarity on the Performance of Polymer–Fullerene Solar Cells

Abstract Diketopyrrolopyrrole (DPP)‐conjugated polymers are a versatile class of semiconductors for application in organic solar cells because of their tunable optoelectronic properties. A record power conversion efficiency (PCE) of 9.4% was recently achieved for DPP polymers, but further improvements are required to reach true efficiency limits. Using five DPP polymers with different chemical structures and molecular weights, the device performance of polymer:fullerene solar cells is systematically optimized by considering device polarity, morphology, and light absorption. The polymer solubility is found to have a significant effect on the optimal device polarity. Soluble polymers show a 10–25% increase in PCE in inverted device configurations, while the device performance is independent of device polarity for less soluble DPP derivatives. The difference seems related to the polymer to fullerene weight ratio at the ZnO interface in inverted devices, which is higher for more soluble DPP polymers. Optimization of the nature of the cosolvent to narrow the fibril width of polymers in the blends toward the exciton diffusion length enhances charge generation. Additionally, the use of a retroreflective foil increases absorption of light. Combined, the effects afford a PCE of 9.6%, among the highest for DPP‐based polymer solar cells.

Li, Mengmeng↗

New Insights into Secondary Organic Aerosol Formation at the Air–Liquid Interface

Air-liquid interfacial processing of volatile organic compound oxidation has been suggested as an important source of secondary organic aerosols. However, owing to the lack of techniques for in situ air-liquid interface analysis, the detailed interfacial mechanism remains speculative. To obviate this, the analysis of air-liquid interfacial reactions and the dynamics of glyoxal oxidation as a model volatile organic compound using in situ liquid synchrotron-based vacuum ultraviolet single photon ionization mass spectrometry enabled by the system for analysis at the liquid vacuum interface microreactor is reported. This approach allows for determination of reaction intermediates and oxidation products including polymers and oligomers at the air-liquid interface by mass spectral analysis and appearance energy measurements. Furthermore, an expanded reaction mechanism of photooxidation free radical induced reactions as a source of aqueous secondary organic aerosol formation is proposed based on these new results, suggesting that single photon ionization could be applied to provide unique insights into interfacial chemistry changing the earth atmospheric composition.

aqueous secondary organic aerosol, glyoxal, photoo↗

Crystal Structure of the Nephila clavipes Major Ampullate Spidroin 1A N-terminal Domain Reveals Plasticity at the Dimer Interface

Spider dragline silk is a natural polymer harboring unique physical and biochemical properties that make it an ideal biomaterial. Artificial silk production requires an understanding of the in vivo mechanisms spiders use to convert soluble proteins, called spidroins, into insoluble fibers. Controlled dimerization of the spidroin N-terminal domain (NTD) is crucial to this process. In this paper, we report the crystal structure of the Nephila clavipes major ampullate spidroin NTD dimer. Comparison of our N. clavipes NTD structure with previously determined Euprosthenops australis NTD structures reveals subtle conformational alterations that lead to differences in how the subunits are arranged at the dimer interface. We observe a subset of contacts that are specific to each ortholog, as well as a substantial increase in asymmetry in the interactions observed at the N. clavipes NTD dimer interface. These asymmetric interactions include novel intermolecular salt bridges that provide new insights into the mechanism of NTD dimerization. We also observe a unique intramolecular “handshake” interaction between two conserved acidic residues that our data suggest adds an additional layer of complexity to the pH-sensitive relay mechanism for NTD dimerization. The results of a panel of tryptophan fluorescence dimerization assays probing the importance of these interactions support our structural observations. Based on our findings, we propose that conformational selectivity and plasticity at the NTD dimer interface play a role in the pH-dependent transition of the NTD from monomer to stably associated dimer as the spidroin progresses through the silk extrusion duct.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Aqueous-Based Polyimine Functionalization of Cellulose Nanofibrils for Effective Drying and Polymer Composite Reinforcement

Here a simple strategy was developed to synthesize polyimine-coated cellulose nanofibrils (CNF) for effective CNF drying and composite reinforcement. The polyimine was synthesized in an aqueous medium using a selective hydrophilic and hydrophobic component that forces the polyimine to precipitate, which prevents the reverse imine reaction. The polyimine coating allowed the CNF to be easily oven-dried while maintaining a fibrillar morphology to provide mechanical reinforcement in poly(ethylene terephthalate glycol) (PETG) composites. In comparison, poor mechanical performance and a heterogeneous fracture surface were observed when the coated CNF were incorporated into poly(l-lactide) (PLA) composites. It is hypothesized that intermolecular aromatic–aromatic interactions are formed at the interface between fibers and the polymer matrix in the PETG system, while no such phenomena occur in the PLA system. Overall, this facile strategy to produce modified, easily dried CNF can be adapted to produce polyimine-coated CNF with unique functionalities that are useful in a range of applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Bioadhesive polymer semiconductors and transistors for intimate biointerfaces

The use of bioelectronic devices relies on direct contact with soft biotissues. For transistor-type bioelectronic devices, the semiconductors that need to have direct interfacing with biotissues for effective signal transduction do not adhere well with wet tissues, thereby limiting the stability and conformability at the interface. Here we report a bioadhesive polymer semiconductor through a double-network structure formed by a bioadhesive brush polymer and a redox-active semiconducting polymer. The resulting semiconducting film can form rapid and strong adhesion with wet tissue surfaces together with high charge-carrier mobility of ~1 square centimeter per volt per second, high stretchability, and good biocompatibility. Further fabrication of a fully bioadhesive transistor sensor enabled us to produce high-quality and stable electrophysiological recordings on an isolated rat heart and in vivo rat muscles.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Stabilizing Liquids Using Interfacial Supramolecular Polymerization

The strong electrostatic interactions at the oil–water interface between a small molecule, 5,10,15,20-tetrakis(4-sulfonatophenyl)porphyrin, H 6 TPPS, dissolved in water, and an amine terminated hydrophobic polymer dissolved in oil are shown to produce a supramolecular polymer surfactant (SPS) of H 6 TPPS at the interface with a binding energy that is sufficiently strong to allow an intermolecular aggregation of the supramolecular polymers. SPSs at the oil–water interface are confirmed by in situ real-space atomic force microcopy imaging. The assemblies of these aggregates can jam at the interface, opening a novel route to kinetically trap the liquids in non-equilibrium shapes. The elastic film, comprised of SPSs, wrinkles upon compression, providing a strategy to stabilize liquids in non-equilibrium shapes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Interface conditions of two-shot molded parts

The focus of this work is on interfaces of two-shot molded parts. It is well known that e.g. material combination, process parameters and contact area structures show significant effects on the bond strength of multi-component injection molded parts. To get information about the bond strength at various process parameter settings and material combinations a test mold with core back technology was used to produce two-component injection molded tensile test specimens. At the core back process the different materials are injected consecutively, so each component runs through the whole injection molding cycle (two-shot process). Due to this consecutive injection molding processes, a cold interface is generated. This is defined as overmolding of a second melt to a solidified polymer preform. Strong interest lies in the way the interface conditions change during the adhesion formation between the individual components. Hence the interface conditions were investigated by computed tomography and Raman spectroscopy. By analyzing these conditions the understanding of the adhesion development during the multi-component injection molding was improved.

36 MATERIALS SCIENCE↗

A Test for Characterizing Delamination Migration in Carbon/Epoxy Tape Laminates

A new test method is presented for the purpose of investigating migration of a delamination between neighboring ply interfaces in fiber-reinforced, polymer matrix tape laminates. The test is a single cantilever beam configuration consisting of a cross-ply laminate with a polytetrafluoroethylene insert implanted at the mid-plane and spanning part way along the length of the specimen. The insert is located between a 0- degree ply (specimen length direction) and a stack of four 90-degree plies (specimen width direction). The specimen is clamped at both ends onto a rigid baseplate and is loaded on its upper surface via a piano hinge. Tests were conducted with the load-application point located on the intact portion of the specimen in order to initiate delamination growth onset followed by migration of the delamination to a neighboring 90/0 ply interface by kinking through the 90-degree ply stack. Varying this position was found to affect the distance relative to the load-application point at which migration initiated. In each specimen, migration initiated by a gradual transition of the delamination at the 0/90 interface into the 90-degree ply stack. In contrast, transition of the kinked crack into the 90/0 interface was sudden. Fractography of the specimens indicated that delamination prior to migration was generally mixed mode-I/II. Inspection of the kink surface revealed mode-I fracture. In general, use of this test allows for the observation of the growth of a delamination followed by migration of the delamination to another ply interface, and should thus provide a means for validating analyses aimed at simulating migration.

Ratcliffe, James G.↗

Characterizing Delamination Migration in Carbon/Epoxy Tape Laminates

A new test method is presented for the purpose of investigating migration of a delamination between neighboring ply interfaces in fiber-reinforced, polymer matrix tape laminates. The test is a single cantilever beam configuration consisting of a cross-ply laminate with a polytetrafluoroethylene (PTFE) insert implanted at the mid-plane and spanning part way along the length of the specimen. The insert is located between a 0-degree ply (specimen length direction) and a stack of four 90-degree plies (specimen width direction). The specimen is clamped at both ends onto a rigid baseplate and is loaded on its upper surface via a piano hinge. Tests were conducted with the load-application point located on the intact portion of the specimen in order to initiate delamination growth onset followed by migration of the delamination to a neighboring 90/0 ply interface by kinking through the 90- degree ply stack. Varying this position was found to affect the distance relative to the load-application point at which migration initiated. In each specimen, migration initiated by a gradual transition of the delamination at the 0/90 interface into the 90- degree ply stack. In contrast, transition of the kinked crack into the 90/0 interface was sudden. Fractography of the specimens indicated that delamination prior to migration was generally mixed mode-I/II. Inspection of the kink surface revealed mode-I fracture. In general, use of this test allows for the observation of the growth of a delamination followed by migration of the delamination to another ply interface, and should thus provide a means for validating analyses aimed at simulating migration.

Ratcliffe, James G.↗

Polymer Matrix Composites: A Perspective for a Special Issue of Polymer Reviews

Polymer matrix composites, with their high specific strength and stiffness, are used in a wide range of applications from large wind turbine blades to microelectronics. This perspective article provides a brief primer on polymer matrix composites, discusses some of their advantages and limitations, and describes a number of emerging trends in the field. In addition, it introduces four review articles on the topics of recent developments in carbon fibers, natural fiber reinforced composites, evaluation of the interface between the fiber reinforcement and polymer matrix, and carbon nanotube reinforced polymers.

36 MATERIALS SCIENCE↗

Higher Molecular Weight Leads to Improved Photoresponsivity Charge Transport and Interfacial Ordering in a Narrow Bandgap Semiconducting Polymer

Increasing the molecular weight of the low-bandgap semiconducting copolymer, poly[(4,4-didoecyldithieno[3,2-b:2',3'-d]silole)-2,6-diyl-alt-(2,1,3-benzothiadiazole)-4,7-diyl], Si-PDTBT, from 9 kDa to 38 kDa improves both photoresponsivity and charge transport properties dramatically. The photocurrent measured under steady state conditions is 20 times larger in the higher molecular weight polymer (HM{sub n} Si-PDTBT). Different decays of polarization memory in transient photoinduced spectroscopy measurements are consistent with more mobile photoexcitations in HM{sub n} Si-PDTBT relative to the lower molecular weight counterpart (LM{sub n} Si-PDTBT). Analysis of the current-voltage characteristics of field effect transistors reveals an increase in the mobility by a factor of 700 for HM{sub n} Si-PDTBT. Near edge X-ray absorption fine structure (NEXAFS) spectroscopy and grazing incidence small angle X-ray scattering (GISAXS) measurements demonstrate that LM{sub n} Si-PDTBT forms a disordered morphology throughout the depth of the film, whereas HM{sub n} Si-PDTBT exhibits pronounced {pi}-{pi} stacking in an edge-on configuration near the substrate interface. Increased interchain overlap between polymers in the edge-on configuration in HM{sub n} Si-PDTBT results in the higher carrier mobility. The improved optical response, transport mobility, and interfacial ordering highlight the subtle role that the degree of polymerization plays on the optoelectronic properties of conjugated polymer based organic semiconductors.

36 MATERIALS SCIENCE↗

Measuring the structure of thin soft matter films under confinement: A surface-force type apparatus for neutron reflection, based on a flexible membrane approach

A unique surface force type apparatus that allows the investigation of a confined thin film using neutron reflection is described. The central feature of the setup consists of a solid substrate (silicon) and a flexible polymer membrane (Melinex{sup Registered-Sign }). We show that inflation of the membrane against the solid surface provides close and even contact between the interfaces over a large surface area. Both heavy water and air can be completely squeezed out from between the flexible film and the solid substrate, leaving them in molecular contact. The strength of confinement is controlled by the pressure used to inflate the membrane. Dust provides a small problem for this approach as it can get trapped between membrane and substrate to prevent a small part of the membrane from making good contact with the substrate. This results in the measured neutron reflectivity containing a small component of an unwanted reflection, between 10% and 20% at low confining pressures (1 bar) and between 1% and 5% at high confining pressures (5 bar). However, we show that this extra signal does not prevent good and clear information on the structure of thin films being extracted from the neutron reflectivity. The effects of confinement are illustrated with data from a poly(vinyl pyrollidone) gel layer in water, a polyelectrolyte multilayer in water, and with data from a stack of supported lipid-bilayers swollen with D{sub 2}O vapor. The data demonstrates the potential of this apparatus to provide information on the structure of thin films under confinement for a known confining pressure.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Sliding of poly(vinyl chloride) on metals studied by Auger electron spectroscopy

The sliding of polyvinyl chloride on nickel, iron and S-Monel has been studied by Auger electron spectroscopy. Polymer was not transferred to the metals, rather shear appeared to take place at the interface. The metal was progressively chlorinated as the polymer made multiple passes on the surface. The thickness of this chlorine film was the order of one atomic layer. Electron-induced desorption studies indicate that the chlorine is chemisorbed to the metal. These results are interpreted as evidence for mechanically induced and/or thermal degradation of the polymer during sliding. Degradation products of HCl and Cl2 which chemisorb to the metal are evolved near the interface.

Pepper, S. V.↗

Understanding Interfacial Alignment in Solution Coated Conjugated Polymer Thin Films

Domain alignment in conjugated polymer thin films can significantly enhance charge carrier mobility. However, the alignment mechanism during meniscus-guided solution coating remains unclear. Furthermore, interfacial alignment has been rarely studied despite its direct relevance and critical importance to charge transport. In this study, we uncover a significantly higher degree of alignment at the top interface of solution coated thin films, using a donor–acceptor conjugated polymer, poly(diketopyrrolopyrrole-co-thiopheneco- thieno[3,2- b ]thiophene-co-thiophene) (DPP2T-TT), as the model system. At the molecular level, we observe in-plane π–π stacking anisotropy of up to 4.8 near the top interface with the polymer backbone aligned parallel to the coating direction. The bulk of the film is only weakly aligned with the backbone oriented transverse to coating. At the mesoscale, we observe a well-defined fibril-like morphology at the top interface with the fibril long axis pointing toward the coating direction. Significantly smaller fibrils with poor orientational order are found on the bottom interface, weakly aligned orthogonal to the fibrils on the top interface. The high degree of alignment at the top interface leads to a charge transport anisotropy of up to 5.4 compared to an anisotropy close to 1 on the bottom interface. We attribute the formation of distinct interfacial morphology to the skin-layer formation associated with high Peclet number, which promotes crystallization on the top interface while suppressing it in the bulk. As a result, we further infer that the interfacial fibril alignment is driven by the extensional flow on the top interface arisen from increasing solvent evaporation rate closer to the meniscus front.

36 MATERIALS SCIENCE↗