Search NASA⌕ Search

SEARCH · Search NASA

Results for “STRESS INTENSITY FACTORS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Stresses in bonded materials with a crack perpendicular to the interface.

The problem of two elastic bonded half planes containing a crack perpendicular to the interface is considered. First the solution for the semi-infinite crack under concentrated wedge loading is given. Then the problem of a finite crack fully imbedded in one of the half planes of terminating at the interface is considered. The Mellin transform in conjunction with the dislocations is used to formulate the problem and to derive the integral equation. The integral equation is solved; the stress intensity factors, the crack surface displacement, and the stresses around the crack tip terminating at the interface are obtained. Noting that the power of the singularity for the interface tip of the crack is not -1/2, a tentative fracture criterion dealing with the initiation of fracture propagation is proposed.

Cook, T. S.↗

A study of crack closure in fatigue

Crack closure phenomenon in fatigue was studied by using a Ti-6Al-4V titanium alloy. The occurrence of crack closure was directly measured by an electrical-potential method, and indirectly by load-strain measurement. The experimental results showed that the onset of crack closure depends on both the stress ratio, and the maximum stress intensity factor. No crack closure was observed for stress ratio, greater than 0.3 in this alloy. A two-dimensional elastic model was used to explain the behavior of the recorded load-strain curves. Closure force was estimated by using this model. Yield level stress was found near the crack tip. Based on this estimated closure force, the crack opening displacement was calculated. This result showed that onset of crack closure detected by electrical-potential measurement and crack-opening-displacement measurement is the same. The implications of crack closure on fatigue crack are considered. The experimental results show that crack closure cannot fully account for the effect of stress ratio, on crack growth, and that it cannot be regarded as the sole cause for delay.

Shih, T. T.↗

Fracture analysis of various cracked configurations in sheet and plate materials

A two-parameter fracture criterion was derived which relates the linear-elastic stress-intensity factor at failure, the elastic nominal failure stress, and two material parameters. The fracture criterion was used previously to analyze fracture data for surface- and through-cracked sheet and plate specimens under tensile loading. The fracture criterion was applied to center-crack tension, compact, and notch-band fracture specimens made of steel, titanium, or aluminum alloy materials tested at room temperature. The fracture data included a wide range of crack lengths, specimen widths, and thicknesses. The materials analyzed had a wide range of tensile properties. Failure stresses calculated using the criterion agreed well (plus or minus 10 percent) with experimental failure stresses. The criterion was also found to correlate fracture data from different specimen types (such as center-crack tension and compact specimens), within plus or minus 10 percent for the same material, thickness, and test temperature.

Newman, J. C., Jr.↗

Fracture analysis of various cracked configurations in sheet and plate materials

A two-parameter fracture criterion has been derived which relates the linear-elastic stress-intensity factor at failure, the elastic nominal failure stress, and two material parameters. The fracture criterion was applied to center-crack tension, compact, and notch-bend fracture specimens made of steel, titanium, or aluminum alloy materials tested at room temperature. The fracture data included a wide range of crack lengths, specimen widths, and thicknesses. The materials analyzed had a wide range of tensile properties. Failure stresses calculated using the criterion agreed well (plus or minus 10 percent) with experimental failure stresses. The criterion was also found to correlate fracture data from different specimen types (such as center-crack tension and compact specimens), within plus or minus 10 percent for the same material, thickness, and test temperature.

Newman, J. C., Jr.↗

The fracture of boron fibre-reinforced 6061 aluminium alloy

The fracture of 6061 aluminium alloy reinforced with unidirectional and cross-plied 0/90 deg, 0/90/+ or - 45 deg boron fibres has been investigated. The results have been described in terms of a critical stress intensity, K(Q). Critical stress intensity factors were obtained by substituting the failure stress and the initial crack length into the appropriate expression for K(Q). Values were obtained that depended on the dimensions of the specimens. It was therefore concluded that, for the size of specimen tested, the values of K(Q) did not reflect any basic materials property.

Wright, M. A.↗

Laser Welded Edge Seals for Glass/Glass Modules

Polymers used in module construction are often involved in degradation mechanisms and hamper recycling. This project explores femtosecond (fs) laser welding of glass/glass modules to enable polymer-free modules. We are utilizing the knowledge base of the industrial laser community to apply glass/glass fs laser welding technology to solar modules. Experimentally measured stress intensity factors for glass welds are input into a COMSOL model of a full-size module to test weld failure under static loading. If successful, fs laser welding could enable modules that are polymer-free that will extend module warrantees, allow hermetically sealed glass/glass modules for moisture-sensitive semiconductors, and improve module recyclability.

COMSOL finite element model↗

Reactor dosimetry and RPV life management

Reactor dosimetry (RD) is a tool that provides data for neutron fluence accumulated over the reactor pressure vessel (RPV) during the reactor operation. This information, however, is not sufficient for RPV lifetime assessment. The life management of RPV is a multidisciplinary task. To assess whether the RPV steel properties at the current stage (for actual accumulated neutron fluence) of reactor operation are still 'safe enough,' the dependence of material properties on the fluence must be known; this is a task for material science (MS). Moreover, the mechanical loading over the RPV during normal operation and accidence have to be known, as well, for evaluation, if the RPV material integrity in this loading condition and existing cracks is provided. The crack loading path in terms of stress intensity factor is carried out by structural analyses (SA). Pressure and temperature distribution over RPV used in these analyses are obtained from a thermal hydraulic (TH) calculation. The conjunction of RD and other disciplines in RPV integrity assessment is analyzed in accordance with the FFP (fitness for purpose) approach. It could help to improve the efficiency in multi-disciplinary tasks solutions. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Interfacial Strength Evaluation of Oxide Films on Carbon Steel by Using the Laser Shock Adhesion Test

We investigate the adhesion strength (interfacial strength) of the oxide film formed on a carbon steel substrate by using a laser shock adhesion test (LaSAT). A rolled carbon steel (SS400) plate is first heated at high temperature (700 °C) under the atmosphere (heat treatment) to cause the formation of oxide films about 20-50 μm thick on the steel surface. The film consisted of multiple layers, including wustite (FeO), magnetite (Fe{sub 3}O{sub 4}), and hematite (Fe{sub 2}O{sub 3}). Next, the x-ray diffraction method was used to measure the residual stress in the film. We find that compression stress develops in the film because of a mismatch of thermal strain in between the film and substrate after the heat treatment. With LaSAT, strong elastic wave generates by a pulsed laser ablation of the substrate backside, and results in interfacial fractures in the oxide films. To monitor the normal (out-of-plane) displacement of the top surface film, a laser ultrasonic interferometer is simultaneously utilized, such that we detect film delamination and determine the critical laser energy for interfacial fracture to obtain the critical stress (interfacial strength). Furthermore, additional pulsed laser irradiation is conducted against a pre-delaminated specimen in order to examine the growth of delamination area and evaluate the interfacial fracture toughness. Finally, elastic wave propagation in the sample is computed using the finite element method (FEM) in order to evaluate the interfacial stress field, accurately. For the FEM, multiple layers in the oxide film are modeled, and the residual stress due to thermal strain mismatch is introduced. The FEM computations reveal the stress distribution around the interface and evaluate the critical stress and critical stress intensity factor for delamination. We thus quantitatively evaluate the interfacial strength and interfacial fracture toughness of the oxide film formed on carbon steel. The mechanism of interfacial fracture is also discussed on the basis of microstructures in a film with multiple layers. This result may be useful for understanding the adhesion quality of oxide film during the hot-rolling process.

36 MATERIALS SCIENCE↗

Microstructural Characterization of Bonding Interfaces in Aluminum 3003 Blocks Fabricated by Ultrasonic Additive Manufacturing

Ultrasonic additive manufacturing (UAM) is a process by which hybrid and near-netshaped products can be manufactured from thin metallic tapes. One of the main concerns of UAM is the development of anisotropic mechanical properties. In this work, the microstructures in the bond regions are characterized with optical and electron microscopy. Recrystallization and grain growth across the interface are proposed as a mechanism for the bond formation. The presence of voids or unbonded areas, which reduce the load-bearing cross section and create a stress intensity factor, is attributed to the transfer of the sonotrode texture to the new foil layer. This results in large peaks and valleys that are not filled in during processing. Tensile testing revealed the weld interface strength was 15% of the bulk foil. Shear tests of the weld interfaces showed almost 50% of the bulk shear strength of the material. Finally, optical microscopy of the fracture surfaces from the tensile tests revealed 34% of the interface area was unbonded.

99 GENERAL AND MISCELLANEOUS↗

A study on the assessment criteria of DHC in PWR spent fuel

One of the major degradation mechanisms of PWR spent fuel cladding is delayed hydride cracking (DHC), which can activate within a relatively low temperature range. Its maximum crack growth rate is estimated to be within the range of 10{sup -7} m/s, at which the cladding can rupture in 1 to 2 years during dry storage. For this reason, it is essential to prevent DHC crack growth itself, but most of the existing DHC studies have been focused on the crack growth rate. In this regard, the values and characteristics of the threshold stress intensity factor (K{sub IH}) for PWR Zircaloy-4 cladding were described. Based on the limited existing test results and analysis, the experimentally measured K{sub IH} were compared with the predicted K{sub IH}. The comparison shows that the predicted values are much lower than the measured ones and both theoretical estimation and measured values of K{sub IH} increase as the temperature increases. The possibilities of degradation by DHC were also discussed during long-term dry storage. For a more reliable analysis, additional information on a pre-existing crack of spent fuel is needed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Laser 3D Printing of Fe-Based Bulk Metallic Glass: Microstructure Evolution and Crack Propagation

This work presents a comprehensive study of microstructure evolution, crack development and hardness performance of Fe-based bulk metallic glass parts processed by laser 3D printing. The combination of a low scan speed and high energy density generates a low temperature gradient, leading to supercooling and the formation of coarse dendrite and cellular crystal microstructure. Columnar dendrites grow in a single direction with large stress, and cracks are easily formed between the dendrites. The stress intensity factor (SIF) caused by the crack surface tension is small, the crack healing effect is weak, and it is difficult to prevent crack propagation. Cellular grain growth is uniform and more easily accommodates the strain, preventing crack initiation and propagation. In contrast, use of a high scan speed with low energy input produces a fine and uniform dendrite or even nanocrystalline, microstructure with microcracks. The SIF caused by the crack surface tension is large, and the crack healing effect is strong and prevents crack initiation and propagation. For low energy density, the hardness of the sample is similar to the hardness of the cast amorphous. This result indicates that the printing sample retained some amorphous characteristics.

36 MATERIALS SCIENCE↗

Effect of Compressive Mode I on the Mixed Mode I/II Fatigue Crack Growth Rate of 42CrMo4

Subsurface cracks in mechanical contact loading components are subjected to mixed mode I/II, so it is necessary to evaluate the fatigue behavior of materials under mixed mode loading. For this purpose, fatigue crack propagation tests are performed with compact tension shear specimens for several stress intensity factor (SIF) ratios of mode I and mode II. The effect of compressive mode I loading on mixed mode I/II crack growth rate and fracture surface is investigated. Tests are carried out for the pure mode I, pure mode II, and two different mixed mode loading angles. On the basis of the experimental results, mixed mode crack growth rate parameters are proposed according to Tanaka and Richard with Paris’ law. Results show neither Richard’s nor Tanaka’s equivalent SIFs are very useful because these SIFs depend strongly on the loading angle, but Richard’s equivalent SIF formula is more suitable than Tanaka’s formula. The compressive mode I causes the crack closure, and the friction force between the crack surfaces resists against the crack growth. In compressive loading with 45° angle, da/dN increases as K{sub eq} decreases.

36 MATERIALS SCIENCE↗

ADDITIONAL STRESS AND FRACTURE MECHANICS ANALYSES OF PRESSURIZED WATER REACTOR PRESSURE VESSEL NOZZLES

In past years, the authors have undertaken various studies of nozzles in both boiling water reactors (BWRs) and pressurized water reactors (PWRs) located in the reactor pressure vessel (RPV) adjacent to the core beltline region. Those studies described stress and fracture mechanics analyses performed to assess various RPV nozzle geometries, which were selected based on their proximity to the core beltline region, i.e., those nozzle configurations that are located close enough to the core region such that they may receive sufficient fluence prior to end-of-life (EOL) to require evaluation of embrittlement as part of the RPV analyses associated with pressure-temperature (P-T) limits. In this paper, additional stress and fracture analyses are summarized that were performed for additional PWR nozzles with the following objectives: To expand the population of PWR nozzle configurations evaluated, which was limited in the previous work to just two nozzles (one inlet and one outlet nozzle). To model and understand differences in stress results obtained for an internal pressure load case using a two-dimensional (2-D) axi-symmetric finite element model (FEM) vs. a three-dimensional (3-D) FEM for these PWR nozzles. In particular, the ovalization (stress concentration) effect of two intersecting cylinders, which is typical of RPV nozzle configurations, was investigated. To investigate the applicability of previously recommended linear elastic fracture mechanics (LEFM) hand solutions for calculating the Mode I stress intensity factor for a postulated nozzle corner crack for pressure loading for these PWR nozzles. These analyses were performed to further expand earlier work completed to support potential revision and refinement of Title 10 to the U.S. Code of Federal Regulations (CFR), Part 50, Appendix G, Fracture Toughness Requirements, and are intended to supplement similar evaluation of nozzles presented at the 2008, 2009, and 2011 Pressure Vessels and Piping (PVP) Conferences. This work is also relevant to the ongoing efforts of the American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel (B&PV) Code, Section XI, Working Group on Operating Plant Criteria (WGOPC) efforts to incorporate nozzle fracture mechanics solutions into a revision to ASME B&PV Code, Section XI, Nonmandatory Appendix G.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Symmetric-Galerkin boundary element transient analysis of the DSIFs for the interaction of a crack with a circular inclusion

A dynamic analysis of crack-inclusion interaction is described in this paper. The analysis employs a two-dimensional symmetric-Galerkin boundary integral formulation for multi-domain elastodynamic fracture analysis in the frequency domain. The multi-domain technique is based on the assumption of perfectly bonded inclusions. The numerical implementation of this boundary integral formulation is carried out with standard quadratic elements, allowing the use of an improved quarter-point element for accurately determining frequency responses of the dynamic stress intensity factors (DSIFs). To deal with singular and hypersingular integrals, the formulation is decomposed into two parts: the rst part is identical to that for elastostatics while the second part contains at most logarithmic singularities. The treatment of the elastostatic singular and hypersingular singular integrals employs an exterior limit to the boundary, while the weakly singular integrals in the second part are handled by Gauss quadrature. Time histories (transient responses) of the DSIFs are obtained in a post-processing step by applying the fast Fourier transform (FFT) and inverse FFT to the frequency responses of these DSIFs. Two numerical examples are presented for the computation of the DSIFs due to crack-inclusion interaction under two types of impact loading: Heaviside step loading and blast loading. The numerical results are consistent and con rm the well known crack tip shielding mechanism observed during the interaction between a crack and a much stiffer inclusion.

36 MATERIALS SCIENCE↗

Investigation of Mode I Notch Toughness of Zr{sub 41.2}Ti{sub 13.8}Cu{sub 10}Ni{sub 12.5}Be{sub 22.5} Metallic Glass under Dynamic Loading Conditions

Based on dynamic three-point bending tests, the dynamic notch toughness (K{sub Q}{sup d}) of Zr{sub 41.2}Ti{sub 13.8}Cu{sub 10}Ni{sub 12.5}Be{sub 22.5} (Vit 1) bulk metallic glass (BMG) was found to be sensitive to stress intensity factor rate ( K-dot {sub Q}{sup d}), which varied from 5.21 to 31.90 MPa m{sup 1/2}. The number of shear bands (N{sub s}) in the notch tip plastic zone was quantitatively analyzed. The phenomenon wherein N{sub s} decreased with increasing loading rate was explained based on the theory of the shear transformation zone and the softening mechanism. Then, power law relationships were established among N{sub s}, K{sub Q}{sup d} and K-dot {sub Q}{sup d}. The results showed that shear bands can affect K{sub Q}{sup d} and K-dot {sub Q}{sup d} and act as a bridge connecting K{sub Q}{sup d} and K-dot {sub Q}{sup d}. The sensitivity of K{sub Q}{sup d} to K-dot {sub Q}{sup d} in BMGs can be well explained by the variation of N{sub s} with loading rate.

36 MATERIALS SCIENCE↗

Intergranular Strain Evolution near Fatigue Crack Tips in Polycrystalline Metals

The deformation field near a steady fatigue crack includes a plastic zone in front of the crack tip and a plastic wake behind it, and the magnitude, distribution, and history of the residual strain along the crack path depend on the stress multiaxiality, material properties, and history of stress intensity factor and crack growth rate. An in situ, full-field, non-destructive measurement of lattice strain (which relies on the intergranular interactions of the inhomogeneous deformation fields in neighboring grains) by neutron diffraction techniques has been performed for the fatigue test of a Ni-based superalloy compact tension specimen. These microscopic grain level measurements provided unprecedented information on the fatigue growth mechanisms. A two-scale model is developed to predict the lattice strain evolution near fatigue crack tips in polycrystalline materials. An irreversible, hysteretic cohesive interface model is adopted to simulate a steady fatigue crack, which allows us to generate the stress/strain distribution and history near the fatigue crack tip. The continuum deformation history is used as inputs for the micromechanical analysis of lattice strain evolution using the slip-based crystal plasticity model, thus making a mechanistic connection between macro- and micro-strains. Predictions from perfect grain-boundary simulations exhibit the same lattice strain distributions as in neutron diffraction measurements, except for discrepancies near the crack tip within about one-tenth of the plastic zone size. By considering the intergranular damage, which leads to vanishing intergranular strains as damage proceeds, we find a significantly improved agreement between predicted and measured lattice strains inside the fatigue process zone. Consequently, the intergranular damage near fatigue crack tip is concluded to be responsible for fatigue crack growth.

36 MATERIALS SCIENCE↗

Initial Probabilistic Evaluation of Reactor Pressure Vessel Fracture with Grizzly and Raven

The Grizzly code is being developed with the goal of creating a general tool that can be applied to study a variety of degradation mechanisms in nuclear power plant components. The first application of Grizzly has been to study fracture in embrittled reactor pressure vessels (RPVs). Grizzly can be used to model the thermal/mechanical response of an RPV under transient conditions that would be observed in a pressurized thermal shock (PTS) scenario. The global response of the vessel provides boundary conditions for local models of the material in the vicinity of a flaw. Fracture domain integrals are computed to obtain stress intensity factors, which can in turn be used to assess whether a fracture would initiate at a pre-existing flaw. These capabilities have been demonstrated previously. A typical RPV is likely to contain a large population of pre-existing flaws introduced during the manufacturing process. This flaw population is characterized stastistically through probability density functions of the flaw distributions. The use of probabilistic techniques is necessary to assess the likelihood of crack initiation during a transient event. This report documents initial work to perform probabilistic analysis of RPV fracture during a PTS event using a combination of the RAVEN risk analysis code and Grizzly. This work is limited in scope, considering only a single flaw with deterministic geometry, but with uncertainty introduced in the parameters that influence fracture toughness. These results are benchmarked against equivalent models run in the FAVOR code. When fully developed, the RAVEN/Grizzly methodology for modeling probabilistic fracture in RPVs will provide a general capability that can be used to consider a wider variety of vessel and flaw conditions that are difficult to consider with current tools. In addition, this will provide access to advanced probabilistic techniques provided by RAVEN, including adaptive sampling and parallelism, which can dramatically decrease run times.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Non destructive technique for cracks detection by an eddy current in differential mode for steel frames

In this paper, a nondestructive technique is used as a tool to control cracks and microcracks in materials. A simulation by a numerical approach such as the finite element method is employed to detect cracks and eventually; to study their propagation using a crucial parameter such as the stress intensity factor. This approach has been used in the aircraft industry to control cracks. Besides, it makes it possible to highlight the defects of parts while preserving the integrity of the controlled products. On the other side, it is proven that the reliability of the control of defects gives convincing results for the improvement of the quality and the safety of the material. Eddy current testing (ECT) is a standard technique in industry for the detection of surface breaking flaws in magnetic materials such as steels. In this context, simulation tools can be used to improve the understanding of experimental signals, optimize the design of sensors or evaluate the performance of ECT procedures. CEA-LIST has developed for many years semi-analytical models embedded into the simulation platform CIVA dedicated to non-destructive testing. The developments presented herein address the case of flaws located inside a planar and magnetic medium. Simulation results are obtained through the application of the Volume Integral Method (VIM). When considering the ECT of a single flaw, a system of two differential equations is derived from Maxwell equations. The numerical resolution of the system is carried out using the classical Galerkin variant of the Method of Moments. Besides, a probe response is calculated by application of the Lorentz reciprocity theorem. Finally, the approach itself as well as comparisons between simulation results and measured data are presented.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗