Search NASA⌕ Search

SEARCH · Search NASA

Results for “accelerated testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Nanoscale imaging of alteration layers of corroded international simple glass particles using ToF-SIMS

Glass particles with dimensions typically ranging from tens to hundreds of microns are often used in glass corrosion research in order to accelerate testing. Two-dimensional and three-dimensional nanoscale imaging techniques are badly needed to characterize the alteration layers at the surfaces of these corroded glass particles. Time-of-flight secondary ion mass spectrometry (ToF-SIMS) can provide a lateral resolution as low as ~100 nm, and, compared to other imaging techniques, is sensitive to elements lighter than carbon. In this work, we used ToF-SIMS to characterize the alteration layers of corroded international simple glass (ISG) particles. At most particle surfaces, inhomogeneous or no alteration layers were observed, indicating that the thickness of the alterations layers may be too thin to be observable by ToF-SIMS imaging. Relatively thick (e.g., 1-10 microns) alteration layers were inhomogeneously distributed at a small portion of surfaces. More interestingly, some large-size (tens of microns) glass particles were fully altered. Above observations suggest that weak attachment and the defects on ISG particle surfaces play an important role in ISG glass corrosion.

alteration layer↗

PV degradation curves: non‐linearities and failure modes

Abstract Photovoltaic (PV) reliability and durability have seen increased interest in recent years. Historically, and as a preliminarily reasonable approximation, linear degradation rates have been used to quantify long‐term module and system performance. The underlying assumption of linearity can be violated at the beginning of the life, as has been well documented, especially for thin‐film technology. Additionally, non‐linearities in the wear‐out phase can have significant economic impact and appear to be linked to different failure modes. In addition, associating specific degradation and failure modes with specific time series behavior will aid in duplicating these degradation modes in accelerated tests and, eventually, in service life prediction. In this paper, we discuss different degradation modes and how some of these may cause approximately linear degradation within the measurement uncertainty (e.g., modules that were mainly affected by encapsulant discoloration) while other degradation modes lead to distinctly non‐linear degradation (e.g., hot spots caused by cracked cells or solder bond failures and corrosion). The various behaviors are summarized with the goal of aiding in predictions of what may be seen in other systems. Published 2016. This article is a U.S. Government work and is in the public domain in the USA.

Jordan, Dirk C.↗

Initial Results of Transverse Beam Profile Measurements Using a LYSO:Ce Crystal

A prototype transverse beam profile monitor for eventual use at the Advanced Superconducting Test Accelerator (ASTA) has been tested at the Fermilab A0 Photoinjector. Results from low-charge (20 pC) studies indicate that a LYSO:Ce scintillator will be a viable alternative to a YAG:Ce scintillator when using intercepting radiation convertor screens for beam profiling. We will also describe the planned implementation of LYSO:Ce crystals to mitigate the coherent optical transition radiation due to the microbunching instability through the use of band-pass filters and specially timed cameras. Based upon tests conducted at the A0PI, we can conclude that the LYSO:Ce crystal will be a suitable alternative to the YAG:Ce crystal for beam imaging. The YAG:Ce and LYSO:Ce crystals both offer similar performance characteristics for low charge beam, but LYSO:Ce combined with a violet bandpass filter has the added benefit of mitigating the COTR due to themicrobunching instability in beam images. The OTR screen can also be used to avoid the scintillator saturation at high areal charge density and the thin foils generate less beam scattering. If the use of bandpass filters, CCD shutter timing and LYSO:Ce are not enough to reduce the COTR due to the microbunching instability, we could use a gated, intensified camera.

43 PARTICLE ACCELERATORS↗

Perovskite Photovoltaic Devices with Carbon-Based Electrodes Withstanding Reverse-Bias Voltages up to –9 V and Surpassing IEC 61215:2016 International Standard

One of the key challenges of perovskite photovoltaics (PV) is the long-term stability. Although efforts are made to improve the lifetime of perovskite PV devices, their degradation under reverse-bias conditions is barely addressed. Herein, perovskite solar cells with carbon-based electrodes are presented which demonstrate superior resilience against reverse-bias-induced degradation. Although their breakdown voltage is identified to be at approximately -3.6 V, cells do not degrade until the applied reverse-bias exceeds -9 V. Two main degradation mechanisms are identified: 1) iodine loss due to hole tunneling into perovskite, which takes place even at low reverse-bias but decomposes the perovskite only after long time durations; and 2) rapid heating at large reverse-bias leading to formation of PbI2, which starts at shunts and then follows the path of the least resistance for the cell current, which is primarily influenced by the electrode sheet resistances. Finally, perovskite solar modules with carbon-based electrodes are demonstrated, which are subjected to a "hotspot" test described in the IEC 61215:2016 international standard at an accredited module testing laboratory. Passing this accelerated test for the first time confirms the superior stability of perovskite PV devices with carbon-based electrodes and highlights their large industrialization potential.

14 SOLAR ENERGY↗

Initial tests of Accelerator Mass Spectrometry with the Argonne Gas-Filled Analyzer and the commissioning of the MONICA detector

As the scope of Accelerator Mass Spectrometry (AMS) expands, there is an increased need to extend the capability of isobaric separation to the medium-heavy mass region. Existing AMS facilities are limited in their ability to separate radioactive nuclei in the A = 100–200 range of interest from their neighboring stable isobars, as such measurements require higher energies than available in most facilities. ATLAS is one of the highest energy system used for AMS based experiments and has enabled isobaric discrimination for medium to heavy nuclides, notably via the Gas-Filled Magnet technique. Further, a preparatory experiment performed in November, 2019, successfully demonstrated isobaric separation of 92 Zr- 92 Mo using the Argonne Gas-Filled Analyzer (AGFA) with high magnetic rigidity. Since that time, MONICA, an eight-anode ionization chamber that measures both energy loss and position with two sets of split anodes, has been developed to aid in AMS experiments at AGFA and has undergone four commissioning runs at the Nuclear Science Laboratory at the University of Notre Dame utilizing Si, Fe/Ni, and Mn beams. This report presents the AGFA AMS run (November 2019) and the subsequent commissioning runs of the MONICA detector, including preliminary measurements on the long-lived isotopes 39 Ar (268 y) and for the first time on 42 Ar (33 y).

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

A Custom High-Throughput Optical Mapping Instrument for Accelerated Stress Testing of PV Module Materials

The performance and integrity of photovoltaic (PV) modules and materials may be assessed through optical characterizations. We have developed a custom optical mapping instrument (OMI) to improve measurement throughput time, facilitate automated measurements, allow for localized specimen examination, obtain spatial information relative to commercial benchtop spectrophotometer instruments, and provide automated data analysis. Both the key components and the methods used to improve the measurements are described. The measurement precision for the OMI is benchmarked for hemispherical transmittance relative to a previous round-robin study for commercial spectrophotometers. In addition to the unique instrument developed in this study, new insights have emerged from the examination of specimens from previous experiments, including: the depletion of the UV absorber is revealed for specimens beyond a certain size after artificial ultraviolet (UV) weathering; an optical degradation by internal haze formation is confirmed following Damp Heat (85 °C/85% relative humidity) testing; the better uniformity of the wear pattern for falling sand abrasion is used to select the DIN 52348 fixture over the ASTM D968 fixture; and the greater local (in the order of millimeters) heterogeneity of surface contamination in the soiling-prone location of Dubai relative to Kuwait. The results of the UV study have already been used to improve the standardized weathering of encapsulants. The example for Damp Heat testing is given to increase awareness of a degradation believed to be ubiquitously occurring in safety and design-type qualification testing of PV modules.

14 SOLAR ENERGY↗

Extended Accelerated Stress Testing of Lamination-Free Edge-Sealed Photovoltaic Minimodules

Lamination-free minimodules are constructed with silicon solar cells between glass sheets and an edge seal of polyisobutylene and silicone. These samples are stressed using a repeated sequential testing sequence including ultraviolet-containing simulated solar spectrum light exposure at elevated temperature, damp heat, humidity freeze, and thermal cycling adapted from the International Electrotechnical Commission (IEC) TS 63209-2:2022. The minimodule performance throughout the stressing is characterized by flash testing and electroluminescence imaging. Results are compared to conventional laminated minimodules using the same type of solar cells. The lamination-free minimodules experience up to 8% power loss compared to roughly 3% for the laminated versions. However, those losses, dominated by current and fill factor, are caused by glass soiling and busbar ribbon separation on the cells. When glass is replaced and the stressed cells are contacted with probes bypassing the delaminated ribbons, the initial performance is recovered, and overall losses of the lamination-free samples become negligible.

14 SOLAR ENERGY↗

Evaluating Non-Fluoropolymer-Based Co-Extruded Backsheets Using Combined-Accelerated Stress Testing and Materials Forensics

Co-extruded, non-fluoropolymer backsheet films for photovoltaic (PV) modules have gained popularity in recent years based on their cost competitiveness. However, their viability has been thrown into question as a result of widespread, early-life field-failures of some materials, particularly the polyamide (PA)-based “AAA” backsheet product. Failure to detect weaknesses in those earlier products could be due, in part, to insufficient quality testing practices. New testing protocols have recently been developed to better evaluate such materials. Here we show the testing results for a non-fluoropolymer, co-extruded PA-based backsheet film, which demonstrates greater durability than AAA and some commercial fluoropolymers. Using material characterization techniques including Fourier-transform infrared spectroscopy (FTIR), wide-angle x-ray scattering (WAXS), differential scanning calorimetry (DSC), X-ray photoelectron spectroscopy (XPS), elongation-to-break (ETB), and optical microscopy we perform a comprehensive failure analysis to better understand the materials weaknesses. This analysis can ultimately inform how best to improve the material and extend its lifetime. This work serves as a demonstration that some materials should not be discounted due to a single poorly designed product and that more appropriate qualification testing with subsequent materials analysis can be used to develop better materials.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Accelerated Leach Testing of GLASS (ALTGLASS): I. Informatics approach to high level waste glass gel formation and aging

Glass corrosion data from the ALTGLASS™ database were used to determine if gel compositions, which evolve as glass systems corrode, are correlated with the generation of zeolites and subsequent increase in the glass dissolution rate at long times. The gel compositions were estimated based on the difference between the elemental glass starting compositions and the measured elemental leachate concentrations from the long-term product consistency tests (ASTM C1285) at various stages of dissolution, ie, reaction progress. A well-characterized subset of high level waste glasses from the database was selected: these glasses had been leached for 15-20 years at reaction progresses up to ~80%. The gel composition data, at various reaction progresses, were subjected to a step-wise regression, which demonstrated that hydrogel compositions with Si*/Al* ratios of <1.0 did not generate zeolites and maintained low dissolution rates for the duration of the experiments. Glasses that formed hydrogel compositions with Si^*/Al^* ratios ≥1, generated zeolites accompanied by a resumption in the glass dissolution rate. Finally, the role of the gel Si/Al ratio, and the interactions with the leachate, provides the fundamental understanding needed to predict if and when the glass dissolution rate will increase due to zeolitization.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Accelerated Leach Testing of Glass (ALTGLASS): II. Mineralization of hydrogels by leachate strong bases

The durability of high level nuclear waste glasses must be predicted on geological time scales. Waste glass surfaces form hydrogels when in contact with water for varying test durations. As the glass hydrogels age, some exhibit an undesirable resumption of dissolution at long times while others exhibit near steady-state dissolution, that is, nonresumption of dissolution. Resumption of dissolution is associated with the formation of zeolitic phases while nonresumption of dissolution is associated with the formation of clay minerals. Hydrogels with a stoichiometry close to that of imogolite, (Al 2 O 3 ·Si(OH) 4 ), with ferrihydrite (Fe 2 O 3 ·0.5H 2 O), have been shown to be associated with waste glasses that resume dissolution. Aluminosilicate hydrogels with a stoichiometry of allophane-hisingerite ((Al,Fe) 2 O 3 ·1.3-2Si(OH) 4 ) have been shown to be associated with waste glasses that exhibit near steady-state dissolution at long times. These phases are all amorphous and poorly crystalline and are also found on natural weathered basalt glasses. Interaction of these hydrogels with excess alkali and OH – (strong base) in the leachates, causes the Al 2 O 3 · n SiO 2 (where n=1-2) hydrogels to mineralize to zeolites. Excess alkali in the leachate is generated by alkali in the glass. As a result, preliminary rate-determining leach layer forming exchange reactions are hypothesized based on these findings.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗