Search NASA⌕ Search

SEARCH · Search NASA

Results for “alloy layers”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Rapid assessment of structural and compositional changes during early stages of zirconium alloy oxidation

A multimodal chemical imaging approach has been developed and applied to detail the dynamic, atomic-scale changes associated with oxidation of a zirconium alloy (Zircaloy-4). Scanning transmission electron microscopy, a gas-phase reactor chamber attached to an atom probe tomography instrument, and synchrotron-based X-ray absorption near-edge spectroscopy were employed to reveal morphology, composition, crystal, and electronic structure changes that occur during initial stages of oxidation at 300 °C. Oxidation was carried out in 10 mbar O 2 gas for short exposure times of 1 and 5 min. A multilayered oxide film with a cubic ZrO adjacent to the oxide/metal interface, a nanoscopic transition region with a graded composition of ZrO 2-x (where 0 < x < 1), and tetragonal ZrO 2 in the outermost oxide were formed. Partitioning of the major alloying element (tin) to the oxide/metal interface and heterogeneously within the oxide accompanied the development of the layered oxide. Our work provides a rapid, high-throughput approach for detailed characterisation of initial stages of zirconium alloy oxidation at an accelerated time scale, with implications for several other alloy systems.

36 MATERIALS SCIENCE↗

Formulation and testing of a high-tin borosilicate nuclear waste glass for in-can melting

Here, borosilicate waste glasses were successfully developed to immobilize two high-level waste raffinate streams via an in-can melter process with an Inconel 601 canister at 1050 °C. Measured viscosity and crystallinity thermal profiles were within the targeted processing constraints for the in-can melter process. Measured chemical durability of the glass by ASTM C1285–21 (Method A), ranged from normalized loss of boron, NL(B) = 1.44 – 2.65 g•m -2 , and NL(B) decreased with increased waste loading, accompanied by increased SnO 2 crystallinity. Measured corrosion of the in-can melter canister by a glass melt showed that Inconel 601 performed well at 1100 °C for up to 500 hr. Resistance polarization measurements versus time revealed that Inconel 601 corrosion rates in (and by) glass melts decreased from an initial rate of 63 mm•y -1 down to 10.2 mm•y -1 after 137 h with increased duration, which was attributed to formation of an oxide passivation layer (mainly Cr 2 O 3 ) at the alloy-glass interface.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Minority carrier lifetime and photoluminescence of mid-wave infrared InAsSbBi

Time-resolved photoluminescence measurements are reported for InAsSbBi alloys grown by molecular beam epitaxy with Bi mole fractions ranging from 0 to 0.8%, yielding minority carrier lifetimes on the order of hundreds of nanoseconds. The minority carrier lifetimes extracted from the time-resolved photoluminescence measurements are comparable to those of lattice-matched InAsSb grown at the same respective temperatures. Nomarski imaging shows that smooth, droplet-free surface morphologies are obtained in 1 μm thick InAsSbBi epilayers grown at temperatures between 360 and 380 °C. The alloy composition-dependent bandgap energies for the InAsSbBi samples are determined from temperature-dependent steady-state photoluminescence measurements and compared with the tetragonal distortion measured by x-ray diffraction to determine the Sb and Bi mole fractions of each sample. The minority carrier lifetime and the achievable extension of the InAsSb(Bi) cut-off wavelength are analyzed as functions of alloy composition and compared with the performance of InAsSb layers with similar growth parameters.

Petluru, Priyanka (ORCID:0000000257154284)↗

A Critical Review on the History of Fabricating Monolithic U-Mo Fuel Plates

Fabrication of uranium-molybdenum alloy fuels has been occurring since the early 2000s in support of the development of a high-uranium-density low-enrichment fuel for use in high-performance research and test reactors which operate at relatively low temperatures. The primary fuel form—a thin foil of uranium, alloyed with 10wt% molybdenum, which is coated in a layer of zirconium and then encapsulated with aluminum 6061 as a cladding material—was developed over a number of years.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High-temperature oxidation/corrosion of iron-based superalloys

The oxidation and sulfidation of several novel iron-base superalloys were evaluated in high-temperature cyclic tests. The experimental austenitic alloys examined were modifications of NASAUT-4GA which were developed for Stirling-engine application. The weight gains and resulting surface scales were measured and analyzed. Mixed oxide scales were found to form on all specimens exposed above 871 C. The build-up of these scales led to a depletion of Mn and Cr in a zone adjacent to the oxides. In addition, the initial oxidation of the Fe-rich alloy was inhibited by a thin but tenacious Si layer which formed at the interface between oxides and the parent layer. Sulfidation tests using Na2SO4 coatings resulted in the formation of a protective spinel and alpha-Fe2O3 phases. Preferential attack of the carbide phase by hydrogen was not observed after 350 h at 871 C.

Lemkey, F. D.↗

Vacuum Plasma Spray (VPS) Material Applications for Thruster Components

A variety of vacuum plasma spray (VPS) material systems have been successfully applied to injector and thrust chamber components. VPS offers a versatile fabrication process with relatively low costs to produce near net shape parts. The materials available with VPS increase operating margins and improve component life by providing superior thermal and oxidation protection in specific engine environments. Functional gradient materials (FGM) formed with VPS allow thrust chamber liners to be fabricated with GRCop-84 (an alloy of copper, chrome, and niobium) and a protective layer of NiCrAlY on the hot wall. A variety of thrust chamber liner designs have been fabricated to demonstrate the versatility of the process. Hot-fire test results have confirmed the improved durability and high temperature performance of the material systems for thrust chamber liners. Similar FGM s have been applied to provide superior thermal protection on injector faceplates with NiCrAlY and zirconia coatings. The durability of the applied materials has been demonstrated with hot-fire cycle testing on injector faceplates in high temperature environments. The material systems can benefit the components used in booster and main engine propulsion systems. More recent VPS efforts are focused on producing rhenium based material systems for high temperature applications to benefit in-space engines like reaction control system (RCS) thrusters.

Elam, Sandra↗

Vacuum Plasma Spray (VPS) Material Applications for Thruster Components

A variety of vacuum plasma spray (VPS) material systems have been successfully applied to injector and thrust chamber components. VPS offers a versatile fabrication process with relatively low costs to produce near net shape parts. The materials available with VPS increase operating margins and improve component life by providing superior thermal and oxidation protection in specific engine environments. Functional gradient materials (FGM) formed with VPS allow thrust chamber liners to be fabricated with GRCop-84 (an alloy of copper, chrome, and niobium) and a protective layer of NiCrAlY on the hot wall. A variety of thrust chamber liner designs have been fabricated to demonstrate the versatility of the process. Hot-fire test results have confined the improved durability and high temperature performance of the material systems for thrust chamber liners. Similar FGM s have been applied to provide superior thermal protection on injector faceplates with NiCrAlY and zirconia coatings. The durability of the applied materials has been demonstrated with hot-fire cycle testing on injector faceplates in high temperature environments. The material systems can benefit the components used in booster and main engine propulsion systems. More recent VPS efforts are focused on producing rhenium based material systems for high temperature applications to benefit in-space engines like reaction control system (RCS) thrusters.

Elam, Sandra↗

Burnishing Techniques Strengthen Hip Implants

In the late 1990s, Lambda Research Inc., of Cincinnati, Ohio, received Small Business Innovation Research (SBIR) awards from Glenn Research Center to demonstrate low plasticity burnishing (LPB) on metal engine components. By producing a thermally stable deep layer of compressive residual stress, LPB significantly strengthened turbine alloys. After Lambda patented the process, the Federal Aviation Administration accepted LPB for repair and alteration of commercial aircraft components, the U.S. Department of Energy found LPB suitable for treating nuclear waste containers at Yucca Mountain. Data from the U.S. Food and Drug Administration confirmed LPB to completely eliminate the occurrence of fretting fatigue failures in modular hip implants.

Source record↗

Impacts on the Hubble Space Telescope Wide Field and Planetary Camera 2: Microanalysis and Recognition of Micrometeoroid Compositions

Postflight surveys of the Wide Field and Planetary Camera 2 (WFPC2) on the Hubble Space Telescope have located hundreds of features on the 2.2 by 0.8 m curved plate, evidence of hypervelocity impact by small particles during 16 years of exposure to space in low Earth orbit (LEO). The radiator has a 100 - 200 micron surface layer of white paint, overlying 4 mm thick Al alloy, which was not fully penetrated by any impact. Over 460 WFPC2 samples were extracted by coring at JSC. About half were sent to NHM in a collaborative program with NASA, ESA and IBC. The structural and compositional heterogeneity at micrometer scale required microanalysis by electron and ion beam microscopes to determine the nature of the impactors (artificial orbital debris, or natural micrometeoroids, MM). Examples of MM impacts are described elsewhere. Here we describe the development of novel electron beam analysis protocols, required to recognize the subtle traces of MM residues.

Kearsley, A. T.↗

Thermal Inspection for the Assessment of Adhesively Bonded Metal Adherends

Certification of adhesively bonded structures is currently a challenge for aircraft manufacturers. The ability to certify bonds in primary structure can reduce dependence on fasteners and this will enable more efficient manufacturing. For example, drilling holes and installing fasteners in bonded joints can be a potentially significant bottleneck in airframe manufacturing. In addition, fasteners increase the airframe weight and can add stress concentration areas. Reducing fastener count can accelerate manufacturing and improve aircraft performance. NASA is currently investigating nondestructive evaluation (NDE) techniques to assess bond integrity. For example, bond thickness influences bond strength and therefore NDE techniques are being investigated to determine bond thickness. For bonded metal structures, there is a large difference in the thermal diffusivity between the 7075 aluminum alloy metal adherends and aircraft grade adhesive. Multi-layered thermal models show a large variation in the thermal response for bondline adhesive thicknesses that vary from 100 to 300 microns for adherend thicknesses of 0.163 cm. Experimental through-transmission thermal measurements reveal promise to quantitatively characterize the bondline thickness. Results were validated with X-ray computed tomography and optical microscopy measurements, and influence of porosity on the thermal model and measurements are investigated.

X-ray computed tomography↗

Thermal Inspection for the Assessment of Adhesively Bonded Metal Adherents

Certification of adhesively bonded structures is currently a challenge for aircraft manufacturers. The ability to certify bonds in primary structure can reduce dependence on fasteners and this will enable more efficient manufacturing. For example, drilling holes and installing fasteners in bonded joints can be a potentially significant bottleneck in airframe manufacturing. In addition, fasteners increase the airframe weight and can add stress concentration areas. Reducing fastener count can accelerate manufacturing and improve aircraft performance. NASA is currently investigating nondestructive evaluation (NDE) techniques to assess bond integrity. For example, bond thickness influences bond strength and therefore NDE techniques are being investigated to determine bond thickness. For bonded metal structures, there is a large difference in the thermal diffusivity between the 7075 aluminum alloy metal adherends and aircraft grade adhesive. Multi-layered thermal models show a large variation in the thermal response for bondline adhesive thicknesses that vary from 100 to 300 microns for adherend thicknesses of 0.163 cm. Experimental through-transmission thermal measurements reveal promise to quantitatively characterize the bondline thickness. Results were validated with X-ray computed tomography and optical microscopy measurements, and influence of porosity on the thermal model and measurements are investigated.

bondline thickness↗

Minimizing Cr-Evaporation from Balance Of Plant Components By Utilizing Cost-Effective Alumina-Forming Austenitic Steels

A solid oxide fuel cell (SOFC) is a clean and efficient energy conversion device. The development of intermediate-temperature SOFCs has made it preferable to use metallic interconnects (MICs) to greatly reduce the cost and significantly increase the efficiency compared to ceramic interconnect materials. However, gaseous chromium species will evaporate from the chromium-containing layer formed on the surface of commonly used MICs and balance of plant (BoP) components. Volatile chromium species have been shown to form solid deposits which poison the cathodes of SOFCs, causing drastic cell performance degradation and thereby limiting commercialization. In order to alleviate the Cr poisoning and achieve long-term high performance of SOFC stacks, various Al 2 O 3 -forming austenitic (AFA) stainless steels applied at different temperatures are evaluated in this project. Based on our Phase I results (500 h operation), it is shown that on the AFAs, an alumina-based protective layer forms under high temperature that is invulnerable to water vapor effects and suppresses the diffusion of chromium and manganese which can prevent the generation of spinels on the alloy surface. Therefore, 310S, OC4 and OC5 at 800 °C and 625, OC11 and OC11LZ at 900 °C are selected to be tested in the Phase II long-term operation. From the results, we find that besides the lower Cr evaporation rates and better oxidation resistance of AFAs than benchmark alloys after short-term (500 h) operation, AFAs also possess the sturdy and compact alumina layer after a long-term operation (5000 h). A protective oxide layer is of great importance for the long-term high-temperature operation of structural materials. The high-temperature oxidation behavior of AFAs and commercial 310S and 625 alloys in Air + 10% H 2 O at 800 °C and 900 °C is systematically investigated. Severe breakaway oxidation and minor spallation are observed for the 310S and 625 after the long-term operation, while the AFAs show high oxidation resistance. It is found that the formation of a continuous alumina layer could greatly prevent the volatilization of chromium vapors. In addition, the corresponding evolving models are discussed. Chromium evaporation from BoP components in high-temperature environment could severely deteriorate the electrochemical performance of SOFC. Several methods were applied to evaluate the Cr evaporation rates of BoP after 500 h exposure at 800 °C to 900 °C in air with 10% H 2 O. An optimal method was designed to exclude the effect of silicon (Si) deposits from quartz tube and sodium (Na) deposits from the sodium carbonate on the oxidation process and the chemical interaction between Cr gaseous species and alumina tube which could provide further quantitative correlation of the evaporated Cr species quantities and degradation rates of SOFC. Based on the great performance of AFAs after long-term operation, AFAs are assembled with Anode-supported cells (ASC) to investigate the the Cr deposition of anode-supported cell under a constant current density of 0.5 A cm -2 at 800 °C with AFA alloys compared with commercial alloys. In addition, the anodic and cathodic processes are deconvoluted by distribution of relaxation times (DRT) method which are comprehensively discussed. It is found out that the voltage exhibited a slight decrease of 5.09 % and 1.54 % in the presence of OC11 and OC11LZA alloy, respectively. However, a considerable decrease of 22.14 % and 12.06 % was determined in the presence of 310S and 625 alloy, respectively. AFAs possessing the low-cost, low Cr evaporation rates and the high oxidation resistance will make it of great potential to replace the existing BoP components.

01 COAL, LIGNITE, AND PEAT↗

Minimizing Cr-Evaporation from Balance of Plant Components by Utilizing Cost-Effective Alumina-Forming Austenitic Steels

A solid oxide fuel cell (SOFC) is a clean and efficient energy conversion device. The development of intermediate-temperature SOFCs has made it preferable to use metallic interconnects (MICs) to greatly reduce the cost and significantly increase the efficiency compared to ceramic interconnect materials. However, gaseous chromium species will evaporate from the chromium-containing layer formed on the surface of commonly used MICs and balance of plant (BoP) components. Volatile chromium species have been shown to form solid deposits which poison the cathodes of SOFCs, causing drastic cell performance degradation and thereby limiting commercialization. In order to alleviate the Cr poisoning and achieve long-term high performance of SOFC stacks, various Al2O3-forming austenitic (AFA) stainless steels applied at different temperatures are evaluated in this project. Based on our Phase I results (500 h operation), it is shown that on the AFAs, an alumina-based protective layer forms under high temperature that is invulnerable to water vapor effects and suppresses the diffusion of chromium and manganese which can prevent the generation of spinels on the alloy surface. Therefore, 310S, OC4 and OC5 at 800 °C and 625, OC11 and OC11LZ at 900 °C are selected to be tested in the Phase II long-term operation. From the results, we find that besides the lower Cr evaporation rates and better oxidation resistance of AFAs than benchmark alloys after short-term (500 h) operation, AFAs also possess the sturdy and compact alumina layer after a long-term operation (5000 h). A protective oxide layer is of great importance for the long-term high-temperature operation of structural materials. The high-temperature oxidation behavior of AFAs and commercial 310S and 625 alloys in Air + 10% H 2 O at 800 °C and 900 °C is systematically investigated. Severe breakaway oxidation and minor spallation are observed for the 310S and 625 after the long-term operation, while the AFAs show high oxidation resistance. It is found that the formation of a continuous alumina layer could greatly prevent the volatilization of chromium vapors. In addition, the corresponding evolving models are discussed. Chromium evaporation from BoP components in high-temperature environment could severely deteriorate the electrochemical performance of SOFC. Several methods were applied to evaluate the Cr evaporation rates of BoP after 500 h exposure at 800 °C to 900 °C in air with 10% H 2 O. An optimal method was designed to exclude the effect of silicon (Si) deposits from quartz tube and sodium (Na) deposits from the sodium carbonate on the oxidation process and the chemical interaction between Cr gaseous species and alumina tube which could provide further quantitative correlation of the evaporated Cr species quantities and degradation rates of SOFC. Based on the great performance of AFAs after long-term operation, AFAs are assembled with Anode-supported cells (ASC) to investigate the the Cr deposition of anode-supported cell under a constant current density of 0.5 A cm -2 at 800 °C with AFA alloys compared with commercial alloys. In addition, the anodic and cathodic processes are deconvoluted by distribution of relaxation times (DRT) method which are comprehensively discussed. It is found out that the voltage exhibited a slight decrease of 5.09 % and 1.54 % in the presence of OC11 and OC11LZA alloy, respectively. However, a considerable decrease of 22.14 % and 12.06 % was determined in the presence of 310S and 625 alloy, respectively. AFAs possessing the low-cost, low Cr evaporation rates and the high oxidation resistance will make it of great potential to replace the existing BoP components.

36 MATERIALS SCIENCE↗

Low-Pressure Diffusion Bonding of Vanadium to Commercially Pure Titanium and Ti-6Al-4V

Modern technology increasingly requires components to be made from specific high-performance materials. To support complex multi-metal structures, a variety of techniques are required to join dissimilar metal parts with precise shapes. This study evaluates vacuum diffusion bonding as a method for joining titanium and vanadium, focusing on both pure titanium and the common alloy Ti-6Al-4V. We employ modest pressure provided by a weight and simple surface preparation to simulate the most commercially applicable process. Here, we show that Ti-6Al-4V alloy bonds readily to V, forming a continuous, clearly defined interdiffusion layer with predictable kinetics. Conversely, commercially pure Ti forms a crack-prone bond with V that fails to improve at higher bonding temperatures or longer times. We attribute this failure to the concentration of stress caused by the ß-to-α phase transformation in Ti. The contrasting bonding efficacy between pure Ti and the alloy provides insight into the crystallographic interactions that occur at the interface during bonding and cooling. These results provide surprising insight into a new method for bonding Ti alloys to V and possibly other metals that share the body-centered cubic crystal structure.

36 MATERIALS SCIENCE↗

Bonding of vanadium- and Iron-based alloys as interlayers for plasma-facing and structural materials in fusion systems

Vanadium alloys and FeCrAl were investigated as interlayers between tungsten and reduced activation ferritic martensitic steel for fusion system components to avoid formation of intermetallic phase at operating temperatures between 550 and 1100 °C, while maintaining a body centered cubic phase throughout the interface. Physical and mechanical properties need to be graded between tungsten and steel, but recent results showed a significant hardness increase at the FeCrAl to vanadium alloy interface. Here, a sintered sample of these alloys was annealed for extended time, and the microstructure was investigated to provide a better understanding of the phenomena. A comparison with an additively manufactured interface of the same material is provided. An unexpected L2 1 intermetallic phase formation has been revealed using microscopy and synchrotron techniques and will inform future additive manufacturing approaches of the interface. A Cr layer interface as a preliminary solution was proposed between the Vanadium alloy and FeCrAl alloy interface.

Additive manufacturing↗

Oxide Scales Formed on NiTi and NiPtTi Shape Memory Alloys

Ni-49Ti and Ni-30Pt-50Ti (at.%) shape memory alloys were oxidized isothermally in air over the temperature range of 500 to 900 C. The microstructure, composition, and phase content of the scales were studied by SEM, EDS, XRD, and metallography. Extensive plan view SEM/EDS identified various features of intact or spalled scale surfaces. The outer surface of the scale was a relatively pure TiO2 rutile structure, typified by a distinct highly striated and faceted crystal morphology. Crystal size increased significantly with temperature. Spalled regions exhibited some porosity and less distinct features. More detailed information was obtained by correlation of SEM/EDS studies of 700 C/100 hr cross-sections with XRD analyses of serial or taper-polishing of plan surfaces. Overall, multiple layers exhibited graded mixtures of NiO, TiO2, NiTiO3, Ni(Ti) or Pt(Ni,Ti) metal dispersoids, Ni3Ti or Pt3Ti depletion zones, and substrate, in that order. The NiTi alloy contained a 3 at.% Fe impurity that appeared in embedded localized Fe-Ti-rich oxides, while the NiPtTi alloy contained a 2 v/o dispersion of TiC that appeared in lower layers. The oxidation kinetics of both alloys (in a previous report) indicated parabolic growth and an activation energy (250 kJ/mole) near those reported in other Ti and NiTi studies. This is generally consistent with TiO2 existing as the primary scale constituent, as described here.

Smialek, James L.↗

Degradation of a two-layer thermal barrier coating under thermal cycling

A two-layer plasma-sprayed thermal barrier coating on a directionally solidified nickel-base eutectic alloy substrate was characterized prior to and after thermal cycling to 1095 C in an accelerated furnace test. The coating was comprised of an inner layer of Ni-16.4Cr-5.1Al-0.15Y (wt%) bond coat and an outer layer of ZrO2-7.9Y2O3 (wt%) thermal barrier. Characterization of the bond coat revealed that substantial amounts of yttrium and aluminum were oxidized during plasma-spraying in air. The oxidation of these elements reduced the protective capacity of the bond coat so that, on thermal exposure, severe degradation of the bond coat resulted and large amounts of nickel oxide formed. This nickel oxide was demonstrated to grow outward into the thermal barrier, which appears to have increased the stresses in the thermal barrier and contributed to its failure near the thermal barrier-bond coat interface.

Maier, R. D.↗

High Temperature Oxidation Behavior of Ni-based High Entropy Superalloys

A new class of polycrystalline gamma-prime strengthened superalloys with alloy compositions of (wt%) Ni-20Co-13Cr-6Fe-4Al-3W-2Mo-(4-x)Nb-(x)Ti (x = 0,1,2) were subjected to cyclic oxidation exposures in dry air at 800 °C for 3600 h. The alloys were borderline chromia/alumina formers, showing good oxidation resistance relative to commercially available materials of similar composition. While all alloys formed alumina scales initially, only the alloy with the lowest Ti/Nb ratio retained an alumina scale for the duration of the exposure. Formation of a continuous layer of rutile TiO 2 at the alumina/alloy interface is proposed to cause eventual alumina failure for the alloys containing Ti.

36 MATERIALS SCIENCE↗