Search NASA⌕ Search

SEARCH · Search NASA

Results for “recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

EBSD characterization of boundary types after discontinuous precipitation in a grit-blasted nickel-based superalloy

Highlights: • During recrystallization, high-angle grain boundaries increased dramatically. • The reaction fronts are high-angle GBs, but are not always correspond to CSL type. • Σ3 twin boundaries have been confirmed to be positive on reducing residual stress. • No advancing reaction front corresponds to Σ3 twin boundary type. - Abstract: In the present work, direct and detailed insights with respect to the statistical information on boundary type of discontinuous precipitates and their advancing reaction fronts in a Re-containing single crystal superalloy DD6 have been obtained by EBSD. With the annealing time prolonging, the reaction fronts proceeded into the original matrix for gradual release of grit-blast induced stress. The average recrystallized grain diameter and the average depth of recrystallization were respective 0.83 μm and 3.98 μm for the specimen annealed at 1050 °C for 10 min, which, after 16 h, had grown to the average values of 3.22 μm and 31.17 μm. The reaction fronts of discontinuous precipitation have been confirmed to be high-angle grain boundaries, but do not always correspond to CSL type. Besides the role of strain energy dissipation for recrystallization, the formation of twin structure has no direct relationship with the proceeding of reaction fronts. The information of boundary type of discontinuous precipitation and its advancing reaction fronts would provide new insight into the cellular recrystallization behavior.

36 MATERIALS SCIENCE↗

Investigation of temperature dependent microstructure evolution of pure iron during friction stir welding using liquid CO2 rapid cooling

Highlights: • Microstructure evolution during the FSW of pure iron was investigated under low and high heat input conditions, respectively. • Rapid cooling, tool stop action, marker insert and short-time annealing were employed to clarify the microstructure evolution. • Continuous and discontinuous dynamic recrystallizations occur during the microstructure evolution under both the conditions. • Incomplete and complete recrystallized microstructures were developed severally under the low and high heat input conditions. • Grain growth occurs during the normal cooling stage but it is very limited under the low heat input condition. - Abstract: The microstructure evolution of pure iron during friction stir welding was reconstructed by an ingenious experimental design, in which the rapid cooling friction stir welding combined with the tool “stop action” technique and the subsequent short-time annealing were adopted to “freeze” the transient microstructure during the stirring and reproduce the normal cooling during conventional friction stir welding, respectively. The microstructure evolution during the stirring and normal cooling was investigated along the material flow path and in the annealed “frozen” weld zone by high-resolution electron-backscatter-diffraction technique. The results show that the continuous and discontinuous dynamic recrystallizations occur simultaneously at the severe deformation stage in front of the tool both under low and high heat input conditions. However, during the material flow, the microstructure evolution involves the plastic deformation, recrystallization, high angle boundaries migration and dynamic recovery under the low heat input condition, while in a dynamic balance of deformation, recrystallization and grain growth under the high heat input conditions. At the cooling stage, normal grain growth occurs both for the low and high heat input welding conditions, while it is very limited for the low heat input condition.

36 MATERIALS SCIENCE↗

Isothermal deformation and spheroidization mechanism of (TiB + La2O3)/Ti composites with different initial structures

Highlights: • Different initial microstructures were obtained through designed heat treatment. • Refined lamellar microstructures promoted dynamic recrystallization. • The spheroidization mechanism was attributed to dynamic recrystallization. • The micron TiB and submicron La{sub 2}O{sub 3} impeded dislocation movement. (TiB + La{sub 2}O{sub 3})/Ti composites with different initial structures were obtained through designed heat treatment. The isothermal deformation and spheroidization mechanisms of (TiB + La{sub 2}O{sub 3})/Ti composites with different initial structures were investigated. Initial structures were refined as the heat treatment temperature decreased. Simultaneously, the quenching and reheating resulted in finer α lamella colonies and α interlamellar spacing compared to the furnace cooling. The flow resistance of furnace cooled samples was lower than the quenched and reheated samples in terms of flow stress data. Following the deformation at 920 °C, the furnace cooled samples demonstrated lamellar α phase and partial spheroidized structure. Moreover, the spheroidization mechanism was similar to the boundary splitting model. Recrystallized grains of approximately 1 μm in diameter were obtained in the quenched and reheated sample following deformation at 920 °C. The spheroidization mechanism was attributed to the development of finer needles through quenching and reheating, as well as to subsequent dynamic recrystallization during the hot deformation. Additionally, the dislocation movement was blocked by the reinforcements on account of the composites with micron TiB and submicron La{sub 2}O{sub 3} during the hot deformation. Furthermore, the reinforcements could facilitate the dynamic recrystallization (DRX) of the α phase.

36 MATERIALS SCIENCE↗

The clumped-isotope geochemistry of exhumed marbles from Naxos, Greece

Exhumation and accompanying retrograde metamorphism alter the compositions and textures of metamorphic rocks through deformation, mineral–mineral reactions, water–rock reactions, and diffusion-controlled intra- and inter-mineral atomic mobility. Here, we demonstrate that these processes are recorded in the clumped- and single-isotope (δ 13 C and δ 18 O) compositions of marbles, which can be used to constrain retrograde metamorphic histories. We collected 27 calcite and dolomite marbles along a transect from the rim to the center of the metamorphic core-complex of Naxos (Greece), and analyzed their carbonate single- and clumped-isotope compositions. The majority of Δ 47 values of whole-rock samples are consistent with exhumation- controlled cooling of the metamorphic complex. However, the data also reveal that water–rock interaction, deformation driven recrystallization and thermal shock associated with hydrothermal alteration may considerably impact the overall distribution of Δ 47 values. We analyzed specific carbonate fabrics influenced by deformation and fluid–rock reaction to study how these processes register in the carbonate clumped-isotope system. Δ 47 values of domains drilled from a calcite marble show a bimodal distribution. Low Δ 47 values correspond to an apparent temperature of 260 °C and are common in static fabrics; high Δ 47 values correspond to an apparent temperature of 200 °C and are common in dynamically recrystallized fabrics. We suggest that the low Δ 47 values reflect diffusion-controlled isotopic reordering during cooling, whereas high Δ 47 values reflect isotopic reordering driven by dynamic recrystallization. We further studied the mechanism by which dynamic recrystallization may alter Δ 47 values by controlled heating experiments. Results show no significant difference between laboratory reactions rates in the static and dynamic fabrics, consistent with a mineral-extrinsic mechanism, in which slip along crystal planes was associated with atomic-scale isotopic reordering in the calcite lattice. An intrinsic mechanism (enhanced isotopic reordering rate in deformed minerals) is contraindicated by these experiments. We suggest that Δ 47 values of dynamically recrystallized fabrics that form below the diffusion-controlled blocking-temperature for calcite constrain the temperature of deformation. We find that Δ 47 -based temperatures of static fabrics from Naxos marbles are ~60–80 °C higher than commonly observed in slowly cooled metamorphic rocks, and would suggest cooling rates of ~10 5 °CMyr -1 . A similar thermal history is inferred for dolomite marbles from the core vicinity, which preserve apparent temperatures up to 200 °C higher than a typical blocking temperature (~300 °C). This finding could be explained by a hydrothermal event driving a brief thermal pulse and locally resetting Δ 47 values. Rapid cooling of the core-complex region is consistent with a compilation of published cooling ages and a new apatite U–Th/He age, associating the thermal event with the emplacement of a granodiorite pluton at ~12 Ma.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Defect cluster and nonequilibrium gas bubble associated growth in irradiated UMo fuels – a cluster dynamics and phase field model

Irradiation examination shows that gas bubble swelling kinetics is much faster after irradiation-induced recrystallization than that prior recrystallization in UMo fuels. It implies that gas bubbles in coarse grains and small recrystallized grains have different growth behavior. In this work, a phase-field model of gas bubble evolution integrating microstructure dependent cluster dynamics has been developed, for the first time, to study the gas bubble swelling behavior in the recrystallization zone of UMo fuels. Generation, diffusion, reaction, sink, emission and clustering of vacancies and interstitials are described by the cluster dynamics model while a phase-field model is used to describe the evolution of non-equilibrium gas bubbles including nucleation and growth. With the coupled model, the effect of defect generation rate, clustering rate, interstitial emission and sink rates on grain boundaries on the gas bubble evolution are systematically simulated. A set of model parameters (defect generation rate, clustering rate, interstitial emission and sink rates) is determined by comparing measured and simulated gas bubble swelling kinetics. The results demonstrate that interstitial clustering is one of the important physical mechanisms which results in a fast gas bubble swelling kinetics in the recrystallization zone. The developed model can also be extended to study the associated growth of defect and second phase precipitates often observed in irradiated materials.

Hu, Shenyang↗

Boundary migration in a 3D deformed microstructure inside an opaque sample

How boundaries surrounding recrystallization grains migrate through the 3D network of dislocation boundaries in deformed crystalline materials is unknown and critical for the resulting recrystallized crystalline materials. Furthermore, by using X-ray Laue diffraction microscopy, we show for the first time the migration pattern of a typical recrystallization boundary through a well-characterized deformation matrix. The data provide a unique possibility to investigate effects of both boundary misorientation and plane normal on the migration, information which cannot be accessed with any other techniques. Our results show that neither of these two parameters can explain the observed migration behavior. Instead we suggest that the subdivision of the deformed microstructure ahead of the boundary plays the dominant role. Our experimental observations challenge the assumptions of existing recrystallization theories, and set the stage for determination of mobilities of recrystallization boundaries.

36 MATERIALS SCIENCE↗

Thin, High Lifetime Silicon Wafers with No Sawing; Re-crystallization in a Thin Film Capsule

The project fits within the area of renewable energy called photovoltaics (PV), or the generation of electricity directly from sunlight using semiconductor devices. PV has the greatest potential of any renewable energy technology. The vast majority of photovoltaic modules are made on crystalline silicon wafers and these wafers accounts for the largest fraction of the cost of a photovoltaic module. Thus, a method of making high quality, low cost wafers would be extremely beneficial to the PV industry. The industry standard technology creates wafers by casting an ingot and then sawing wafers from the ingot. Sawing rendered half of the highly refined silicon feedstock as un-reclaimable dust. Being a brittle material, the sawing is actually a type of grinding operation which is costly both in terms of capital equipment and in terms of consumables costs. The consumables costs associated with the wire sawing technology are particularly burdensome and include the cost of the wire itself (continuously fed, one time use), the abrasive particles, and, waste disposal. The goal of this project was to make wafers directly from molten silicon with no sawing required. The fundamental concept was to create a very low cost (but low quality) wafer of the desired shape and size and then to improve the quality of the wafer by a specialized thermal treatment (called re-crystallization). Others have attempted to create silicon sheet by recrystallization with varying degrees of success. Key among the difficulties encountered by others were: a) difficulty in maintaining the physical shape of the sheet during the recrystallization process and b) difficulty in maintaining the cleanliness of the sheet during recrystallization. Our method solved both of these challenges by encapsulating the preform wafer in a protective capsule prior to recrystallization (see below). The recrystallization method developed in this work was extremely effective at maintaining the shape and the cleanliness of the wafer. In addition, it was found to be suitable for growing very large crystals. The equipment used was simple and inexpensive to operate. Reasonable solar cells were fabricated on re-crystallized material.

14 SOLAR ENERGY↗

Low-Temperature Friction-Stir Welding of 2024 Aluminum

Solid state friction-stir welding (FSW) has been demonstrated to involve dynamic recrystallization producing ultra-fine, equiaxed grain structures to facilitate superplastic deformation as the welding or joining mechanism. However, the average residual, equiaxed, grain size in the weld zone has ranged from roughly 0.5 micron to slightly more than 10 micron, and the larger weld zone grain sizes have been characterized as residual or static grain growth as a consequence of the temperatures in the weld zone (where center-line temperatures in the FSW of 6061 Al have been shown to be as high as 480C or -0.8 T(sub M) where T(sub M) is the absolute melting temperature)). In addition, the average residual weld zone grain size has been observed to increase near the top of the weld, and to decrease with distance on either side of the weld-zone centerline, an d this corresponds roughly to temperature variations within the weld zone. The residual grain size also generally decreases with decreasing FSW tool rotation speed. These observations are consistent with the general rules for recrystallization where the recrystallized grain size decreases with increasing strain (or deformation) at constant strain rate, or with increasing strain-rate, or with increasing strain rate at constant strain; especially at lower ambient temperatures, (or annealing temperatures). Since the recrystallization temperature also decreases with increasing strain rate, the FSW process is somewhat complicated because the ambient temperature, the frictional heating fraction, and the adiabatic heating fraction )proportional to the product of strain and strain-rate) will all influence both the recrystallization and growth within the FSW zone. Significantly reducing the ambient temperature of the base metal or work pieces to be welded would be expected to reduce the residual weld-zone grain size. The practical consequences of this temperature reduction would be the achievement of low temperature welding. This study compares the residual grain sizes and microstructures in 2024 Al friction-stir welded at room temperature (about 30C and low temperature (-30C).

Benavides, S.↗

Constraining the Texture and Composition of Pore-Filling Cements at Gale Crater, Mars

The Mars Science Laboratory (MSL) rover Curiosity has encountered a wide variety of sedimentary rocks deposited in fluvio-lacuestrine sequences at the base of Gale Crater. The presence of sedimentary rocks requires that initial sediments underwent diagenesis and were lithified. Lithification involves sediment compaction, cementation, and re-crystallization (or authigenic) processes. Analysis of the texture and composition of the cement can reveal the environmental conditions when the cements were deposited, enabling better understanding of early environments present within Gale Crater. The first step in lithification is sediment compaction. The Gale crater sediments do not show evidence for extensive compaction prior to cementation; the Sheepbed mudstone in Yellowknife Bay (YKB) has preserved void spaces ("hollow nodules"), indicating that sediments were cemented around the hollow prior to compaction, and conglomerates show imbrication, indicating minimal grain reorganization prior to lithification. Furthermore, assuming the maximum burial depth of these sediments is equivalent to the depth of Gale Crater, the sediments were never under more than 1 kb of pressure, and assuming a 15 C/km thermal gradient in the late Noachian, the maximum temperature of diagenesis would have been approximately 75 C. This is comparable to shallow burial diagenetic conditions on Earth. The cementation and recrystallization components of lithification are closely intertwined. Cementation describes the precipitation of minerals between grains from pore fluids, and recrystallization (or authigenesis) is when the original sedimentary mineral grains are altered into secondary minerals. The presence of authigenic smectites and magnetite in the YKB formation suggests that some recrystallization has taken place. The relatively high percentage of XRD-amorphous material (25-40%) detected by CheMin suggests that this recrystallization may be limited in scope, and therefore may not contribute significantly to the cementing material. However, relatively persistent amorphous components could exist in the Martian environment (e.g. amorphous MgSO4), so recrystallization, including loss of crystallinity, cannot yet be excluded as a method of cementation. In order to describe the rock cementation, both the rock textures and their composition must be considered. Here, we attempt to summarize the current understanding of the textural and compositional aspects of the cement across the rocks analyzed by Curiosity to this point.

Siebach, K. L.↗

Mineralogical Analysis of Calcium-Aluminum-Rich Inclusions Provides Insight Into Post-Formation Processes

Introduction: Calcium-aluminum inclusions (CAIs) are cm- to mm-sized intergrowths of refractory phases found in chondritic meteorites [1]. Their mineral compositions closely match the compositions of the solids thought to condense from an extremely hot (>1500K) gas with a bulk solar composition [2-4], suggesting that CAIs were the earliest solids within the Solar System [2-4]. These inclusions provide invaluable insights into the conditions and dynamics of the early Solar System. CAIs must be transported from their formation region near the protosun to the chondrite parent-body accretion region. The nature of their journey could affect how, when, and where the secondary processes recorded in these CAIs occurred [4]. Did these secondary processes occur in the solar nebula or during accretion with the parent body, or both? How were the CAIs affected by varying thermochemical processes? To better answer these questions, we have undertaken an in-depth, textural study of the secondary alteration of select CAI samples. Methods: We chose three CAIs that experienced a range of post-formation processing to gain better understanding of secondary alteration based on previous preliminary examination [5]. Representative CAIs were chosen from NWA 5508 (CV3), NWA 12772 (CV3), and Coolidge (CL4) carbonaceous chondrites. We used scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD) techniques for detailed chemical, mineralogical, and textural analysis of the CAIs. Backscattered electron (BSE) images and X-ray elemental maps were taken of Coolidge and NWA 5508 using the Lunar and Planetary Institute (LPI) Phenom SEM. The JEOL 7900F SEM at NASA Johnson Space Center (JSC) was used to obtain energy dispersive spectroscopy (EDS) chemical maps of all samples. High resolution EBSD analysis identified the mineral phases and textures, providing key information on their nature. Based on the SEM and EBSD data, minerals of interest were selected for quantitative chemical electron probe micro-analysis (EPMA) using the JEOL JXA-8530F at NASA JSC. Results and Discussion: The EDS maps show that the NWA 5508 and NWA 12772 CAIs designated “Saguaro” and “Hoopoe” respectively [5] are enriched in calcium while the Coolidge CAI designated “Cottonwood” is aluminum and magnesium rich. Saguaro. A ~1.5cm diameter igneous Type B CAI with a rounded shape. The dominant phases are melilite, spinel, and Al-Ti pyroxene with minor anorthite. Spinel is subhedral and occurs in clusters. Some of these clusters have a circular geometry which encloses other minerals, known as a palisade structure [6] (Fig. 1). Some palisades form near perfect circles while others are more irregular in shape. Melilite in Saguaro ranges in size from coarse (>250m) to fine-grained (5-7m) and forms intergrown laths. A third of the melilite grains exhibit simple twinning about their <001> axis. The spinel palisades and twinned melilite in Saguaro suggest an igneous history, and the lack of secondary minerals suggests minimal aqueous alteration. At some point in time after the initial condensation of the minerals and formation of the inclusion, the sample was remelted and quickly solidified. The formation of the palisades is still heavily debated. One hypothesis is that the palisades are the rims of smaller CAIs that accreted early on, essentially acting as xenoliths within the larger CAIs [7]. Another hypothesis suggests an igneous origin for palisade structures [6-8] wherein the melt traps gas bubbles, and the spinel nucleates on the surface of this bubble. Based on the WDS spot analyses of 41 melilite grains using EPMA, the data suggest that the composition inside and outside the palisades is nearly identical. This finding indicates that these palisades are likely not exogenous but rather formed from melt-vapor reactions. Our results are consistent with studies by Simon and Grossman,1997 [6] and Zhang et al. (2019) [8]. Hoopoe. A ~0.5cm compact Type A CAI with an irregular shape. The dominant mineral phases are melilite, spinel, and hibonite with minor amounts of anorthite, augite, and perovskite. The melilite ranges in size from ~500 to 50µm. The larger melilite grains have simple twinning along the <001> axis like melilite in Saguaro. Melilite in Hoopoe exhibits crystal-plastic strain with misorientation dominantly about the <010> and <110> axes. Spinel shows subhedral to euhedral morphology and appears in clusters. Hibonite grains are similar to spinel in habit and size but show more plastic strain. The two minerals are often found together with one appearing to replace the other. Perovskite appears in fine grained recrystallized regions alongside fine augite and spinel. The abundant strain and deformation features in the melilite and hibonite suggest that Hoopoe experienced shock. This shock could have occurred in the nebula [9] or from an impact of another body on the parent body asteroid. The appearance of fine-grained (<10m) areas of augite, perovskite, and spinel in the dominantly coarse-grained inclusion suggest recrystallization, possibly due to the sudden increase in pressure and temperature. Cottonwood. This ~0.5cm CAI exhibits distinct mineralogy and textures suggesting a high degree of alteration. It is irregular in shape. The dominant mineral phases are spinel and anorthite with minor amounts of augite and rutile. The two main texture types can be seen in Fig. 2. The first type consists of coarse euhedral to subhedral spinel and anorthite. The second includes fine grained spinel, anorthite, rutile, and iron sulfides. Within these fine-grained regions, the anorthite grains are clustered into domains exhibiting the same crystallographic orientation. Rutile exclusively occurs with fine anorthite indicating a potential relationship between the two. Cottonwood has a clear and unbroken Wark-Lovering [10] rim (Fig. 2) on one side that consists of a sequence of spinel followed by anorthite and an outer layer of augite. The abundance of the fine-grained regions containing iron oxides and iron sulfides, secondary phases such as rutile, and oriented anorthite grains is evidence for recrystallization associated with a high degree of thermal metamorphism. The EPMA analyses on both coarse- and fine-grained spinel show that the fine spinel grains are more enriched in Cr (1-2 wt. %) than their coarse counterparts (0.1-0.5 wt. %). The data suggest thermal metamorphism drove chemical exchange of the previously refractory inclusion, introducing chromium and iron as well as sulfur, which is moderately volatile. Conclusions: The three CAIs analyzed record distinct secondary nebular and parent body processes. Saguaro melted in the nebula as seen by the twinned melilite and spinel palisades. Hoopoe experienced intense shock which deformed its melilite and recrystallized perovskite, augite, and spinel in fine-grained regions. Cottonwood shows evidence of recrystallization and chemical changes consistent with thermal metamorphism occurring after accretion into the parent-body.

V E Burnette↗

Z4B, AREVA NP's most recent material for structural fuel assembly components

Z4B is AREVA NP's advanced material for fuel channels and BWR fuel assembly structural components such as water channels, which are made of zirconium base material. As such, Z4B is envisaged to replace Zircaloy-2 and Zircaloy-4 as a fuel channel and water channel material. The chemical composition of Z4B is similar to that of Zircaloy-4 with the exception of an increased iron and chromium content slightly above the ASTM specification. The manufacturing processes applied to produce Z4B components are the same as those that have been applied for Zircaloy-2 and Zircaloy-4 materials. AREVA NP has irradiated a total of 74 lead fuel channels made of Z4B either in beta-quenched condition or in fully recrystallized condition in eight BWRs worldwide. Sixty-six of these are still in service with 26 of these lead fuel channels on fuel assemblies of various ATRIUM 10 designs and 40 on ATRIUM 11 lead fuel assemblies. In addition to Z4B fuel channels, the ATRIUM 11 design also features fully recrystallized water channels. The first ATRIUM 11 lead fuel assemblies were inserted in-core in 2012. The first Z4B beta-quenched lead fuel channels were inserted in 2009 and will reach an estimated burnup of 60 MWd/kgHM in 2016 after seven annual cycles of irradiation. The first Z4B fully recrystallized lead fuel channels were also inserted in 2009 and have been discharged with EOL burnups of about 47 MWd/kgHM after three biennial cycles of irradiation. Pool-side inspections of these leads have confirmed the superior uniform and shadow corrosion behavior of Z4B fuel channels relative to Zircaloy-4 fuel channels. This increased corrosion resistance combined with a similar hydrogen pickup fraction to Zircaloy-4 will lead to an overall decrease in total hydrogen content and minimize the potential of hydrogen assisted irradiation growth and abnormal bow of fuel channels in the recrystallized condition. The use of Z4B fuel channels in the beta-quenched condition decreases bow even further due to the resulting quasi-isotropic microstructure. Additionally, fuel channels made of Z4B tend to exhibit reduced bulge, which is valid in both conditions, beta-quenched and recrystallized.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Physical and mechanical metallurgy of high purity Nb for accelerator cavities

In the past decade, high Q values have been achieved in high purity Nb superconducting radio frequency (SRF) cavities. Fundamental understanding of the physical metallurgy of Nb that enables these achievements is beginning to reveal what challenges remain to establish reproducible and cost-effective production of high performance SRF cavities. Recent studies of dislocation substructure development and effects of recrystallization arising from welding and heat treatments and their correlations with cavity performance are considered. With better fundamental understanding of the effects of dislocation substructure evolution and recrystallization on electron and phonon conduction, as well as the interior and surface states, it will be possible to design optimal processing paths for cost-effective performance using approaches such as hydroforming, which minimizes or eliminates welds in a cavity.

43 PARTICLE ACCELERATORS↗

Influence of Temperature on the Texture Distribution in Two-Phase Region Hot Deformation of Grain-Oriented Silicon Steel

Hot deformation simulation test of 3% Si grain-oriented silicon (CGO) steel was carried out at different temperatures, and evolution of microstructures and recrystallized textures in two-phase region was analyzed by electron backscatter diffraction and optical microscopy. The “δ → γ” and “γ → α” phase transformation points of the two-phase region measured by differential scanning calorimetry method are 1272 and 819 °C, respectively, which are within the ranges of 1300-1350 and 800-850 °C, measured by water quenching. The hot deformation temperature has a large effect on the microstructure and texture in the steel. A higher hot deformation temperature leads to higher degree of recrystallization and larger average grain size, more γ-fiber textures and cube {100} <001> texture, but the rotated cube {100} <011> texture is stable. The recrystallized microstructure was also affected by the phase compositions. While the cube {100} <001> texture results in typical austenite recrystallization texture, {111} textures lead to typical ferrite rolling textures.

36 MATERIALS SCIENCE↗

Effect of Post-deformation Annealing Treatment on the Microstructural Evolution of a Cold-Worked Corrosion-Resistant Superalloy (CRSA) Steel

The post-deformation annealing treatments of a commercial cold-worked corrosion-resistant superalloy steel (Sanicro 28 steel) were carried out at different temperatures in the range of 900-1100 °C for different holding durations of 5, 10, and 15 min. The effects of post-deformation annealing time and temperature on the microstructural evolution and subsequent mechanical properties of the processed Sanicro 28 steel were investigated. The observations indicated that twin–twin hardening in cold deformation condition mainly correlates with abundant nucleation of mechanical twins in multiple directions resulting in considerable strain hardening behavior. Microstructural investigations showed that the static recrystallization takes place after isothermal holding at 900 °C for 5 min. Increasing the annealing temperature from 900 to 1050 °C leads to recrystallization development and grain refinement in the as-recrystallized state. In addition, an increase in annealing duration from 5 to 15 min leads to subgrain coarsening and subsequently larger recrystallized grains size. The occurrence of large proportion of the grain refinement, which is achieved in the first annealing stage at 1050 °C after 5 min, is considered as the main factor for the maximum elongation at this stage.

36 MATERIALS SCIENCE↗

Hot Deformation Behavior and Microstructural Evolution of Antibacterial Austenitic Stainless Steel Containing 3.60% Cu

Hot deformation behavior of as-cast antibacterial austenitic stainless steel containing 3.60% copper was investigated in a temperature range of 900-1150 °C and strain rate range of 0.01-20 s{sup −1}. At strain rates higher than 1 s {sup −1}, the flow stress curves were corrected considering adiabatic heating. Kinetic analysis indicated that the hot deformation activation energy of steel was 376.02 kJ mol{sup −1}. The microstructural evolution under different temperatures was observed by optical microscopy. The nucleation sites for recrystallization and different orientations and twin ratios under different strain rates were analyzed by electron backscatter diffraction. The results showed that hot deformation was dominated by continuous dynamic recrystallization in the high-temperature and high-strain-rate region (1050-1150 °C, 1-20 s{sup −1}). On increasing the temperature and strain rate, the degree of recrystallization and twinning increased simultaneously. These phenomena promoted one another. Thus, the volume fraction of the recrystallized and twinned grains increased with the addition of Cu.

36 MATERIALS SCIENCE↗

Mechanical Alloying and Powder Forging of 18%Cr Oxide Dispersion-Strengthened Steel Produced Using Elemental Powders

Oxide dispersion-strengthened (ODS) ferritic steels are potential materials for cladding tubes in fast breeder fission reactors. These are mostly prepared by mechanical alloying of yttria powder with pre-alloyed powders. Using elemental powders offers flexibility in the choice of alloy compositions. Here we report mechanical alloying of Fe-18Cr-2W-0.2Ti-0.35Y{sub 2}O{sub 3} (compositions in wt.%) ODS steel using elemental powders of Fe, Cr, W and Ti with yttria powder. After 5 h of milling, no significant changes in particle size and crystallite size were observed. Powders milled for 5 and 7 h were consolidated through powder forging route. The optimum milling time for mechanical alloying could be determined only after evaluating the forgings. It is difficult to achieve recrystallization in ODS alloys. The forging process parameters were optimized to achieve a dense alloy with a fine recrystallized microstructure. Factors leading to recrystallization are discussed. It is shown that recrystallization in ODS steels is more likely to occur during forging as compared to extrusion/rolling. The powder forging route offers several advantages over the conventional extrusion or HIP routes.

36 MATERIALS SCIENCE↗

Experiments and modeling to characterize microstructure and hardness in 304L

Drawn 304L stainless steel tubing was subjected to 42 different annealing heat treatments with the goal of initializing a microstructural model to select a heat treatment to soften the tubing from a hardness of 305 Knoop to 225–275 Knoop. The amount of recrystallization and grain size caused by 18 heat treatments were analyzed via optical microscopy and image analysis, revealing the full range of recrystallization from 0 to 100%. The formation of carbides during the longer duration and higher-temperature heat treatments was monitored via transmission electron microscope evaluation. The experimental results informed a model which includes recovery, recrystallization, and grain growth to predict microstructure and hardness. After initialization of the model, it was able to predict hardness with a R 2 value of 0.95 and recrystallization with an R 2 value of 0.99. As a result, the model was then utilized in the design and testing of a heat treatment to soften the tubing.

36 MATERIALS SCIENCE↗

Microstructure-process relationships in monolithic U-10Mo fuel foil single-pass rolling: A parametric simulation study

In this work, a previously validated coupling of Kinetic Monte Carlo (KMC) Potts Model and finite element method (FEM) simulations was implemented to investigate the effects of microstructural features in as-cast and homogenized monolithic U-10Mo foils on the emergent microstructure after rolling and reheating. Parameters that could potentially affect recrystallization behavior of the rolled U-10Mo foils were considered: grain size distribution, uranium carbide (UC) size distribution, UC volume fraction, spatial distribution of UC, and rolling reduction magnitude. Grain structure and the magnitude of rolling reduction have the strongest influence on recrystallization kinetics and the fabricated grain size distribution. The UC distribution had only a weak effect on the recrystallization kinetics and final microstructures. While particle-stimulated nucleation (PSN) occurred in simulation more frequently as grain size increased, its incidence did not appear to considerably affect the recrystallization kinetics or grain size distribution.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗