Search NASA⌕ Search

SEARCH · Search NASA

Results for “Anode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

Flash Recycling of Graphite Anodes

The ever-increasing production of commercial lithium-ion batteries (LIBs) will result in a staggering accumulation of waste when they reach their end of life. A closed-loop solution, with effective recycling of spent LIBs, will lessen both the environmental impacts and economic cost of their use. Presently, <5% of spent LIBs are recycled and the regeneration of graphite anodes has, unfortunately, been mostly overlooked despite the considerable cost of battery-grade graphite. Here, in this work, an ultrafast flash recycling method to regenerate the graphite anode is developed and valuable battery metal resources are recovered. Selective Joule heating is applied for only seconds to efficiently decompose the resistive impurities. The generated inorganic salts, including lithium, cobalt, nickel, and manganese, can be easily recollected from the flashed anode waste using diluted acid, specifically 0.1 M HCl. The flash-recycled anode preserves the graphite structure and is coated with a solid-electrolyte-interphase-derived carbon shell, contributing to high initial specific capacity, superior rate performance, and cycling stability, when compared to anode materials recycled using a high-temperature-calcination method. Life-cycle-analysis relative to current graphite production and recycling methods indicate that flash recycling can significantly reduce the total energy consumption and greenhouse gas emission while turning anode recycling into an economically advantageous process.

36 MATERIALS SCIENCE↗

Impact of Anode to Cathode Crossover in Lithium‐metal Batteries With High‐Nickel Cathodes

The advancement of high-energy-density lithium-metal batteries (LMBs) is hindered by the chemical instability of both lithium-metal anode and high-nickel layered oxide cathodes. While cathode-to-anode crossover is well-documented, the reverse process of anode-to-cathode crossover remains underexplored. Here, we systematically investigate such crossovers and the degradation pathway in pouch cells with a localized high-concentration electrolyte, comparing NMC622, NMC811, and NMC90 cathodes paired with lithium-metal and graphite anodes. Despite delivering higher initial capacities, LMBs exhibit faster capacity fade under long-term cycling at 45 °C. To isolate cathode-side degradation, galvanostatic electrochemical impedance spectroscopy (GEIS) measurements of cycled cathodes paired with delithiated lithium iron phosphate (LFP) counter electrodes reveal significantly higher charge-transfer resistance in cathodes cycled with lithium-metal. Surface characterization via X-ray photoelectron spectroscopy (XPS) and time-of-flight secondary ion mass spectrometry (ToF-SIMS) reveals greater electrolyte decomposition on cathodes cycled with lithium metal, leading to thicker, more organic-rich cathode–electrolyte interphases (CEIs), consistent with the elevated charge-transfer resistance observed in GEIS measurements. Notably, NMC90 shows the most pronounced CEI thickening, linking higher cathode surface reactivity to greater susceptibility to anode-to-cathode crossover. This work presents compelling evidence of crosstalk degradation originating from lithium-metal anodes and underscores the importance of cross-interface stability for the design of durable LMBs.

25 ENERGY STORAGE↗

Silicon Anodes with Improved Calendar Life Enabled By Multivalent Additives

Silicon is widely recognized as the most promising upgrade for graphite anodes due to its much higher capacity, natural abundance, and ability to be directly applied in the slurry-based, roll-to-roll production lines. However, in addition to the fast capacity decay, silicon anodes also suffer from inferior calendar life in practical applications due to the unstable solid-electrode interface (SEI). Until now, strategies to effectively improve the calendar life by tailored SEIs remain largely unclear, especially in high-Si content, zero-graphite anodes. Here, silicon anodes with superior calendar life are developed by adding small concentrations of multivalent salts into the baseline electrolyte. The Ca additive reacts with the F ions in the electrolyte, forming a layer of nanocrystalline CaF 2 that is closely coated around the silicon particles. The CaF 2 -enabled new SEI is strong and dense, which effectively protects the silicon core from side reactions, leading to lower capacity decay after calendar aging at high voltage. More importantly, the Ca additive is effective universally for all available commercial silicon or SiO sources. This study provides a feasible and low-cost solution for developing silicon anodes with long calendar life, paving the way towards commercially viable silicon anodes.

25 ENERGY STORAGE↗

The electrolyte comprising more robust water and superhalides transforms Zn-metal anode reversibly and dendrite-free

A great challenge for all aqueous batteries, including Zn-metal batteries, is the parasitic hydrogen evolution reaction on the low-potential anode. Herein, we report the formula of a highly concentrated aqueous electrolyte that mitigates hydrogen evolution by transforming water molecules more inert. The electrolyte comprises primarily ZnCl 2 and LiCl as an additive, both of which are inexpensive salts. The O–H covalent bonds in water get strengthened in a chemical environment that has fewer hydrogen bonding interactions and a greater number of Zn–Cl superhalides, as suggested by integrated characterization and simulation. As a result, the average Coulombic efficiency of zinc-metal anode is raised to an unprecedented >99.7% at 1 mA cm –2 . In the new electrolyte, the plating/stripping processes leave the zinc-metal anode dendrite-free, and the zinc-metal anode delivers stable plating/stripping cycles for 4000 hours with an areal capacity of 4 mAh cm –2 at 2 mA cm –2 . Furthermore, the high Coulombic efficiency of zinc-metal anode in the ZnCl 2 -LiCl mixture electrolyte is demonstrated in full cells with a limited anode. The V 2 O 5 ·H 2 O| |Zn full cell with an N/P mass ratio of 1.2 delivers a stable life of more than 2500 cycles, and the LiMn 2 O 4 | |Zn hybrid cell with an N/P mass ratio of 0.6 exhibits 1500 cycles in its stable life.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fault Detection and Diagnosis In Hall–Héroult Cells Based on Individual Anode Current Measurements Using Dynamic Kernel PCA

Individual anode current signals in aluminum reduction cells provide localized cell conditions in the vicinity of each anode, which contain more information than the conventionally measured cell voltage and line current. One common use of this measurement is to identify process faults that can cause significant changes in the anode current signals. While this method is simple and direct, it ignores the interactions between anode currents and other important process variables. This paper presents an approach that applies multivariate statistical analysis techniques to individual anode currents and other process operating data, for the detection and diagnosis of local process abnormalities in aluminum reduction cells. Specifically, since the Hall–Héroult process is time-varying with its process variables dynamically and nonlinearly correlated, dynamic kernel principal component analysis with moving windows is used. The cell is discretized into a number of subsystems, with each subsystem representing one anode and cell conditions in its vicinity. The fault associated with each subsystem is identified based on multivariate statistical control charts. The results show that the proposed approach is able to not only effectively pinpoint the problematic areas in the cell, but also assess the effect of the fault on different parts of the cell.

36 MATERIALS SCIENCE↗

Electrochemical Investigations on AZ Series Magnesium Alloys as Anode Materials in a Sodium Chloride Solution

Electrochemical and discharge properties of Mg-air battery based on 3N5 Mg, AZ31, AZ61, AZ91 alloys were studied in a 0.6 M NaCl electrolyte, with the aim of selecting a common commercial Mg alloy to decrease passivation and self-corrosion of Mg anode for Mg-air battery. Results obtained indicate that self-corrosion and passivation decrease, and anodic utilization increases gradually with increasing Al content. This is associated with the double effect of Al on discharge performance of Mg anode. Al with high hydrogen overvoltage decreases self-corrosion of Mg anode and passivation of Mg anode by peeling off Mg(OH){sub 2} discharge products. Results of electrochemical impedance spectroscopy and discharge morphology relate well with the results of electrochemical and discharge performances. It is concluded that solution-treated AZ91 alloy has a better discharge performance as anode of Mg-air battery in 0.6 M NaCl electrolyte.

36 MATERIALS SCIENCE↗

NiMo-ceria-zirconia-based anode for solid oxide fuel cells operating on gasoline surrogate

A multi-functional NiMo-ceria-zirconia composite was developed as an anode for a solid oxide fuel cell (SOFC) running on isooctane that is a commonly used model fuel for gasoline. The anode layer was fabricated on an electrolyte-supported single cell using yttria-stabilized zirconia (YSZ) as the electrolyte and La0.6Sr0.4Co0.2Fe0.8O3-d as the cathode. Our results indicated that the single NiMo-ceria-zirconia layer possessed a dual-functionality: the first function was to internally convert complex hydrocarbons into a synthesis gas and the second function was to electrochemically oxidize the synthesis gas mixture for electric power generation. The addition of Mo to the Ni-ceria-zirconia allowed direct conversion of isooctane in SOFC. It significantly suppressed carbon deposition in the anode and improved the lifetime of a single cell. Additionally, the presence of Mo in the Ni-ceria-zirconia anode appeared to facilitate a higher degree of sintering, which increased the electrical conductivity and maximum power density of the single cell. When operating on isooctane at 800 °C, single cell with the 5 wt.% Mo in the Ni-ceria-zirconia-based anode displayed a maximum power density of 212 mW cm-2 at 0.48V which was higher than that of a single cell with the Ni-YSZ-based anode without the Mo promoter (49 mW cm-2 at 0.48 V).

NiMo-Ceria-Zirconia composite, Single layer multif↗

Degradation Mechanisms of Magnesium Metal Anodes in Electrolytes Based on (CF 3 SO 2 ) 2 N – at High Current Densities

The energy density of rechargeable batteries utilizing metals as anodes surpasses that of Li ion batteries, which employ carbon instead. Among possible metals, magnesium represents a potential alternative to the conventional choice, lithium, in terms of storage density, safety,stability, and cost. However, a major obstacle for metal-based batteries is the identification of electrolytes that show reversible deposition/dissolution of the metal anode and support reversible intercalation of ions into a cathode. Traditional Grignard-based Mg electrolytes are excellent with respect to the reversible deposition of Mg, but their limited anodic stability and compatibility with oxide cathodes hinder their applicability in Mg batteries with higher voltage. Non-Grignard electrolytes, which consist of ethereal solutions of magnesium(II) bis(trifluoromethanesulfonyl)imide (Mg(TFSI) 2 ), remain fairly stable near the potential of Mg deposition. The slight reactivity of these electrolytes toward Mg metal can be remedied by the addition of surface-protecting agents, such as MgCl 2 . Hence, ethereal solutions of Mg(TFSI) 2 salt with MgCl 2 as an additive have been suggested as a representative non-Grignard Mg electrolyte. In this work, the degradation mechanisms of a Mg metal anode in the TFSI-based electrolyte were studied using a current density of 1 mA cm -2 and an areal capacity of ~0.4 mAh cm -2 , which is close to those used in practical applications. The degradation mechanisms identified include the corrosion of Mg metal, which causes the loss of electronic pathways and mechanical integrity, the nonuniform deposition of Mg, and the decomposition of TFSI - anions. This study not only represents an assessment of the behavior of Mg metal anodes at practical current density and areal capacity but also details the outcomes of interfacial passivation, which was detected by simple cyclic voltammetry experiments. This study also points out the absolute absence of any passivation at the electrode-electrolyte interface for the premise of developing electrolytes compatible with a metal anode.

25 ENERGY STORAGE↗

Insights into Chemical Prelithiation of SiO x /Graphite Composite Anodes through Scanning Electron Microscope Imaging

Initial Coulombic efficiency (ICE) is critical for determining the energy density of lithium-ion batteries (LIBs) used for practical applications; however, it is typically disregarded in anode research. We used SiO x and graphite composite anodes for commercial lithium-ion batteries in our preliminary research to achieve a balance between ICE, capacity, and cycling life. ICE reached 88%; however, it needs further improvement for commercial applications. Prelithiation is a process that involves the introduction of extra lithium ions into LIBs during their manufacturing to enhance the overall performance of the LIBs. We applied a chemical prelithiation method on our SiO x /graphite composite anodes, which comprised 95 wt % of the active material mass loading on the electrode. The ICE increased from 88% to 98% using an aryllithium reagent impregnation method within 2 min of prelithiation. The anode’s specific capacity density, rate, and cycle performance also significantly improved. Scanning electron microscopy (SEM) imaging enhanced by an osmium tetroxide staining method indicated that the P-anode contained a stable solid electrolyte interface (SEI) layer after the prelithiation process and cycling electrochemical test. The P-anode’s stable charge differential peak over 500 cycles also showcases a robust artificial SEI layer that was generated by the prelithiation procedure. Here, this prelithiation process has significant potential for adoption in the LIB industry’s current electrode manufacturing process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Progress of 3D network binders in silicon anodes for lithium ion batteries

Prompted by its overwhelming benefits, silicon (Si) has evolved as one of the most promising anode materials for high-capacity lithium-ion batteries (LIBs). However, some of the intrinsic drawbacks such as low ionic conductivity and inevitable volume change during the alloying/dealloying process seriously hamper the commercialization of Si-based anodes in LIBs. Among the several strategies to overcome the challenges of the Si anode, the development of designed polymeric binders is imperative for enabling stable and satisfactory performance. The improved cell performance due to the designed binders is recognized as an economical and practical approach, especially from the industrial perspective. In addition to their conventional role in integrating electrode components, binders also play a significant role in alleviating the unfavorable phenomenon of volume expansion, and ultimately stabilizing the Si anode and Si-electrolyte interphase. The polymer architecture of the binders significantly influences the binder performance, and three-dimensional (3D) network binders are generally more effective at coping with the stress resulting from the huge volume change of the Si anode. To develop advanced 3D binders, substantial research efforts have been made including various crosslinking strategies in the past decade. In this review, we focus on diverse crosslinking methods including chemical-, physical-, and topological-crosslinking for rationally designing network binders for Si anodes and take a glance at dynamic interactions to construct healable binders for long-term stability.

25 ENERGY STORAGE↗

A chemical switch enabled autonomous two-stage crosslinking polymeric binder for high performance silicon anodes

Silicon (Si) is a promising high-capacity anode material for high-energy-density lithium-ion batteries. However, the drastic volumetric changes of Si upon lithiation/delithiation hinder the practical use of Si anodes. Although adhesive polymeric binders, such as poly(acrylic acid) (PAA), mitigate this issue, the cycling performance of the fabricated Si anodes is still far from meeting the criteria of practical applications. In this study, we present a novel polymeric binder system for Si anodes consisting of PAA, a chemical switch (ammonia, NH 3 ), and a crosslinker (branched polyethylenimine, PEI). The crosslinking between PAA and PEI is switched off in the slurry, which can then be turned on during electrode drying. Interestingly, the crosslinking reaction consists of two stages: ionic cross-linking (PAA-PEI-i) and covalent crosslinking (PAA-PEI-c) at a higher temperature (e.g., 130 °C). In half-cells, Si anodes fabricated using the PAA-PEI-c binder show a 67% increase in capacity retention compared to PAA anodes over 150 cycles at C/3 rate. The PAA-PEI-c binder also outperforms PAA in full cells. In addition, the chemical switch controlled crosslinking binder system also facilitates the slurry making process by avoiding early crosslinking. This system requires no additional steps compared to the conventional electrode lamination process, showing enormous potential for direct adoption in large-scale manufacturing.

25 ENERGY STORAGE↗

Top-emission Si-based phosphor organic light emitting diode with Au doped ultrathin n-Si film anode and bottom Al mirror

We report a highly efficient top-emission Si-based phosphor organic light emitting diode (PhOLED) with an ultrathin polycrystalline n-Si:Au film anode and a bottom Al mirror. This anode is formed by magnetron sputtering followed by Ni induced crystallization and then Au diffusion. By optimizing the thickness of the n-Si:Au film anode, the Au diffusion temperature, and the other parameters of the PhOLED, the highest current and power efficiencies of the n-Si:Au film anode PhOLED reached 85{+-}9 cd/A and 80{+-}8 lm/W, respectively, corresponding to an external quantum efficiency of 21{+-}2% and a power conversion efficiency of 15{+-}2%, respectively, which are about 60% and 110% higher than those of the indium tin oxide anode counterpart and 70% and 50% higher than those of the bulk n{sup +}-Si:Au anode counterpart, respectively.

36 MATERIALS SCIENCE↗

Improvement of four anode rods ion source

In this work, an improved form of a saddle field ion source has been designed and constructed. It consists of four anode rods made from copper and two copper cathode discs. The two cathode discs are placed symmetrically on both sides of the four anode rods. The electrical discharge and output ion beam characteristics were measured at different pressures using argon gas. The optimum distance between each two anode rods was determined. Also the optimum distance between the four anode rods and any cathode disc was obtained. It was found that the optimum distance between each two anode rods equal to 6 mm, while the optimum distance between the four anode rods and any cathode disc equal to 16 mm, where a stable discharge current and maximum output ion beam current can be obtained. The effect of negative extraction voltage applied to both the extractor electrode and Faraday cup on the output ion beam current was studied. The sputter yield of copper and aluminum targets using argon ions of different energies was determined.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Brightness enhancement of plasma ion source by utilizing anode spot for nano applications

Anode spots are known as additional discharges on positively biased electrode immersed in plasmas. The anode spot plasma ion source (ASPIS) has been investigated as a high brightness ion source for nano applications such as focused ion beam (FIB) and nano medium energy ion scattering (nano-MEIS). The generation of anode spot is found to enhance brightness of ion beam since the anode spot increases plasma density near the extraction aperture. Brightness of the ASPIS has been estimated from measurement of emittance for total ion beam extracted through sub-mm aperture. The ASPIS is installed to the FIB system. Currents and diameters of the focused beams with/without anode spot are measured and compared. As the anode spot is turned on, the enhancement of beam current is observed at fixed diameter of the focused ion beam. Consequently, the brightness of the focused ion beam is enhanced as well. For argon ion beam, the maximum normalized brightness of 12 300 A/m{sup 2} SrV is acquired. The ASPIS is applied to nano-MEIS as well. The ASPIS is found to increase the beam current density and the power efficiency of the ion source for nano-MEIS. From the present study, it is shown that the ASPIS can enhance the performance of devices for nano applications.

43 PARTICLE ACCELERATORS↗

Variation of anode grid surface morphology and its effect on operation of a triode virtual cathode oscillator

After repeatedly operation of a triode virtual cathode oscillator, the surface morphology of anode grid is studied by a scanning electron microscope. It is found that there are many quasi-periodic sawteeth formed on the anode grid, which are about 300-500 {mu}m in height, {approx}200 {mu}m in width, and 150-200 {mu}m in period. The formation of this sawteeth implies that there is possible Rayleigh-Taylor-like instability on the anode grid during the irradiation by high-current relativistic electron beam. These sawteeth enhance the electric field on anode grid, leading to more feasible of anode plasma generation, and more rapidly expansion of that plasma. As a result, the electron transmissivity of anode grid is decreased, the output microwave power of the virtual cathode oscillator is lowered and its operational performance is degraded.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Exciton quenching at PEDOT:PSS anode in polymer blue-light-emitting diodes

The quenching of excitons at the poly(3,4-ethylenedioxythiophene):poly(styrenesulfonic acid) (PEDOT:PSS) anode in blue polyalkoxyspirobifluorene-arylamine polymer light-emitting diodes is investigated. Due to the combination of a higher electron mobility and the presence of electron traps, the recombination zone shifts from the cathode to the anode with increasing voltage. The exciton quenching at the anode at higher voltages leads to an efficiency roll-off. The voltage dependence of the luminous efficiency is reproduced by a drift-diffusion model under the condition that quenching of excitons at the PEDOT:PSS anode and metallic cathode is of equal strength. Experimentally, the efficiency roll-off at high voltages due to anode quenching is eliminated by the use of an electron-blocking layer between the anode and the light-emitting polymer.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Anode current density distribution in a cusped field thruster

The cusped field thruster is a new electric propulsion device that is expected to have a non-uniform radial current density at the anode. To further study the anode current density distribution, a multi-annulus anode is designed to directly measure the anode current density for the first time. The anode current density decreases sharply at larger radii; the magnitude of collected current density at the center is far higher compared with the outer annuli. The anode current density non-uniformity does not demonstrate a significant change with varying working conditions.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Specific features of an electric discharge operating between an electrolytic anode and a metal cathode

Results are presented from experimental studies of a high-current electric discharge operating between an St45 steel cathode and a service water anode in a wide range of air pressures. Peculiarities of discharge ignition and specific features of cathode and anode spots were revealed. The behavior of the current density on a service water anode was investigated for the first time. Comparison of the current densities j on the steel cathode and service water anode shows that, in the parameter range under study, Hehl's law is not satisfied on the water anode. The two-dimensional distribution of the potential inside and on the surface of the service water anode was measured.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗