Search NASA⌕ Search

SEARCH · Search NASA

Results for “CORROSIVE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

Iron-Based Amorphous-Metals: High-Performance Corrosion-Resistant Materials (HPCRM) Development Final Report

An overview of the High-Performance Corrosion-Resistant Materials (HPCRM) Program, which was co-sponsored by the Defense Advanced Research Projects Agency (DARPA) Defense Sciences Office (DSO) and the United States Department of Energy (DOE) Office of Civilian and Radioactive Waste Management (OCRWM), is discussed. Programmatic investigations have included a broad range of topics: alloy design and composition; materials synthesis; thermal stability; corrosion resistance; environmental cracking; mechanical properties; damage tolerance; radiation effects; and important potential applications. Amorphous alloys identified as SAM2X5 (Fe{sub 49.7}Cr{sub 17.7}Mn{sub 1.9}Mo{sub 7.4}W{sub 1.6}B{sub 15.2}C{sub 3.8}Si{sub 2.4}) and SAM1651 (Fe{sub 48}Mo{sub 14}Cr{sub 15}Y{sub 2}C{sub 15}B{sub 6}) have been produced as melt-spun ribbons, drop-cast ingots and thermal-spray coatings. Chromium (Cr), molybdenum (Mo) and tungsten (W) additions provided corrosion resistance, while boron (B) enabled glass formation. Earlier electrochemical studies of melt-spun ribbons and ingots of these amorphous alloys demonstrated outstanding passive film stability. More recently thermal-spray coatings of these amorphous alloys have been made and subjected to long-term salt-fog and immersion tests. Good corrosion resistance has been observed during salt-fog testing. Corrosion rates were measured in situ with linear polarization, while simultaneously monitoring the open-circuit corrosion potentials. Reasonably good performance was observed. The sensitivity of these measurements to electrolyte composition and temperature was determined. The high boron content of this particular amorphous metal make this amorphous alloy an effective neutron absorber, and suitable for criticality control applications. In general, the corrosion resistance of these iron-based amorphous metals is maintained at operating temperatures up to the glass transition temperature. These materials are much harder than conventional stainless steel and nickel-based materials, and are proving to have excellent wear properties, sufficient to warrant their use in earth excavation, drilling and tunnel boring applications. The observed corrosion resistance may enable applications of importance in industries such as: oil and gas production, refining, nuclear power generation, shipping, and others. Large areas have been successfully coated with these materials, with thicknesses of approximately one centimeter.

36 MATERIALS SCIENCE↗

ALTERNATIVE AND ENHANCED CHEMICAL CLEANING: CORROSION STUDIES RESULTS: FY2010

Due to the need to close High Level Waste storage tanks, chemical cleaning methods are needed for the removal of sludge heel materials remaining at the completion of mechanical tank cleaning efforts. Oxalic acid is considered the preferred cleaning reagent for heel dissolution of iron-based sludge. However, the large quantity of chemical reagents added to the tank farm from oxalic acid based cleaning has significant downstream impacts. Optimization of the oxalic acid cleaning process can potentially reduce the downstream impacts from chemical cleaning. To optimize oxalic acid usage, a detailed understanding of the chemistry of oxalic acid based sludge dissolution is required. Additionally, other acidic systems may be required for specific waste components that have low solubility in oxalic acid, and as a means to reduce oxalic acid usage in general. Electrochemical corrosion studies were conducted with 1 wt. % oxalic acid at mineral acid concentrations above and below the optimal conditions for this oxalic acid concentration. Testing environments included pure reagents, pure iron and aluminum phases, and sludge simulants. Mineral acid concentrations greater than 0.2 M and temperatures greater than 50 C result in unacceptably high corrosion rates. Results showed that manageable corrosion rates of carbon steel can be achieved at dilute mineral acid concentrations (i.e. less than 0.2 M) and low temperatures based on the contact times involved. Therefore, it is recommended that future dissolution and corrosion testing be performed with a dilute mineral acid and a less concentrated oxalic acid (e.g., 0.5 wt.%) that still promotes optimal dissolution. This recommendation requires the processing of greater water volumes than those for the baseline process during heel dissolution, but allows for minimization of oxalic acid additions. The following conclusions can be drawn from the test results: (1) In both nitric and sulfuric acid based reagents, the low temperature and dilute concentration environment resulted in carbon steel corrosion rates that were less than 150 mpy. These rates are manageable in that chemical cleaning processes could proceed for limited time without significant wall loss. Further optimization of the Alternative Enhance Chemical Cleaning (AECC) process should focus on testing in solutions of this dilute concentration and low temperature regime. (2) In general, for the nitric acid based reagent, the aluminum oxide phase environments resulted in higher corrosion rates than the iron oxide phase environments. (3) In general, for the sulfuric acid based reagent, the iron oxide phase environments resulted in higher corrosion rates than the aluminum oxide phase environments. (4) In general, for the nitric acid based reagent, the HM sludge simulant environments resulted in higher corrosion rates than the PUREX sludge simulant environments. This result agrees with the previous observation that the aluminum oxide phases are more aggressive than the iron oxide phase environments in the nitric acid reagent. (5) Pitting was more likely to occur in the sulfuric acid based reagents than in the nitric acid based reagents. (6) Pitting occurred only in the iron based pure oxide phases and the sludge simulants. No pitting was observed in the aluminum based pure oxide phases. (7) Pitting tended to occur more frequently in tests that involved the dilute mineral acid reagent. (8) Pitting was more severe at the higher temperature for a given mineral acid concentration. (9) Pitting was more severe at a higher mineral acid concentration for a given temperature. (10) Based on the combined results of the open circuit potential and cathodic polarization testing, there was a low propensity for hydrogen evolution in solutions where sludge has been dissolved.

08 HYDROGEN↗

Characterization of Encapsulated Corrosion Inhibitors for Environmentally Friendly Smart Coatings

The NASA Kennedy Space Center's Corrosion Technology Lab at the Kennedy Space Center in Florida, U.S.A. has been developing multifunctional smart coatings based on the microencapsulation of environmentally friendly corrosion indicators, inhibitors and self-healing agents. This allows the incorporation of autonomous corrosion control functionalities, such as corrosion detection and inhibition as well as the self-healing of mechanical damage, into coatings. This paper presents technical details on the characterization of inhibitor-containing particles and their corrosion inhibitive effects using electrochemical and mass loss methods. Three organic environmentally friendly corrosion inhibitors were encapsulated in organic microparticles that are compatible with desired coatings. The release of the inhibitors from the microparticles in basic solution was studied. Fast release, for immediate corrosion protection, as well as long-term release for continued protection, was observed. The inhibition efficacy of the inhibitors, incorporated directly and in microparticles, on carbon steel was evaluated. Polarization curves and mass loss measurements showed that, in the case of 2MBT, its corrosion inhibition effectiveness was greater when it was delivered from microparticles.

Corrosion↗

Release Properties and Electrochemical Characterization of Encapsulated Corrosion Inhibitors for Environmentally Friendly Smart Coatings

The NASA Kennedy Space Center's Corrosion Technology Lab at the Kennedy Space Center in Florida, U.S.A. has been developing multifunctional smart coatings based on the microencapsulation of environmentally friendly corrosion indicators, inhibitors and self-healing agents. This allows for the incorporation of autonomous corrosion control functionalities, such as corrosion detection and inhibition as well as the self-healing of mechanical damage, into coatings. This paper presents technical details on the characterization of inhibitor-containing particles and their corrosion inhibitive effects using electrochemical and mass loss methods. Three organic environmentally friendly corrosion inhibitors were encapsulated in organic microparticles that are compatible with desired coatings. The total inhibitor content and the release of one of the inhibitors from the microparticles in basic solution was measured. Particles with inhibitor contents of up 60 wt% were synthesized. Fast release, for immediate corrosion protection, as well as long-term release for continued protection, was observed. The inhibition efficacy of the inhibitors, both as the pure materials and in microparticles, on carbon steel was evaluated. Polarization curves and mass loss measurements showed that, in the case of 2MBT, its corrosion inhibition effectiveness was greater when it was delivered from microparticles.

Coatings↗

Long-Term Corrosivity at NASA Kennedy Space Center as a Function of Distance and Time from the Atlantic Ocean

Long-term data to record both seasonal and notional bounding values for corrosivity at multiple sites at NASA Kennedy Space Center was needed to make better materials choices for NASA-based ground and spaceflight programs. The data was valuable for two key reasons, 1) to measure corrosion rate and chloride concentration as a function of time and distance from the Atlantic Ocean, and 2) compare the corrosivity at launchpad and site-specific areas to the more accelerated conditions at the KSC Beachside Atmospheric Corrosion Test Site for coating and materials performance prediction. Sites were chosen from 45 meter (150 feet) to 8 kilometers (5 miles) from the Atlantic Ocean and corrosion variables at each site were measured throughout each year from June 2017 to April 2023, except the Beachside site, which includes data from November 2010. The summary includes corrosivity data and coating performance comparisons at select sites, which will be used as the updated NASA corrosivity standard for corrosion control requirements.

NASA↗

LOCALIZED CORROSION OF AUSTENITIC STAINLESS STEELEXPOSED TO MIXTURES OF PLUTONIUM OXIDE AND CHLORIDE SALTS

Laboratory corrosion tests were conducted to investigate the corrosivity of moist plutonium oxide/chloride (PuO{sub 2}/Cl-) salt mixtures on 304L and 316L stainless steel coupons. The tests exposed flat coupons for pitting evaluation and 'teardrop' stressed coupons for stress corrosion cracking (SCC) evaluation at room temperature to various mixtures of PuO{sub 2} and chloride-bearing salts for periods up to 500 days. The two flat coupons were placed so that the solid oxide/salt mixture contacted about one half of the coupon surface. One teardrop coupon was placed in contact with solid mixture; the second teardrop was in contact with the headspace gas only. The mixtures were loaded with nominally 0.5 wt % water under a helium atmosphere. Observations of corrosion ranged from superficial staining to pitting and SCC. The extent of corrosion depended on the total salt concentration and on the composition of the salt. The most significant corrosion was found in coupons that were exposed to 98 wt % PuO{sub 2}, 2 wt % chloride salt mixtures that contained calcium chloride. SCC was observed in two 304L stainless steel teardrop coupons exposed in solid contact to a mixture of 98 wt % PuO{sub 2}, 0.9 wt % NaCl, 0.9 wt % KCl, and 0.2 wt % CaCl{sub 2}. The cracking was associated with the heat-affected zone of an autogenous weld that ran across the center of the coupon. Cracking was not observed in coupons exposed to the headspace gas, nor in coupons exposed to other mixtures with either 0.92 wt% CaCl{sub 2} or no CaCl{sub 2}. The corrosion results point to the significance of the interaction between water loading and the concentration of the hydrating salt CaCl{sub 2} in the susceptibility of austenitic stainless steels to corrosion.

36 MATERIALS SCIENCE↗

POTENTIAL FOR STRESS CORROSION CRACKING OF A537 CARBON STEEL NUCLEAR WASTE TANKS CONTAINING HIGHLY CAUSTIC SOLUTIONS

The evaporator recycle streams of nuclear waste tanks may contain waste in a chemistry and temperature regime that exceeds the current corrosion control program, which imposes temperature limits to mitigate caustic stress corrosion cracking (CSCC). A review of the recent service history found that two of these A537 carbon steel tanks were operated in highly concentrated hydroxide solution at high temperature. Visual inspections, experimental testing, and a review of the tank service history have shown that CSCC has occurred in uncooled/un-stress relieved tanks of similar construction. Therefore, it appears that the efficacy of stress relief of welding residual stress is the primary corrosion-limiting mechanism. The objective of this experimental program is to test A537 carbon steel small scale welded U-bend specimens and large welded plates (30.48 x 30.38 x 2.54 cm) in a caustic solution with upper bound chemistry (12 M hydroxide and 1 M each of nitrate, nitrite, and aluminate) and temperature (125 C). These conditions simulate worst-case situations in these nuclear waste tanks. Both as-welded and stress-relieved specimens have been tested. No evidence of stress corrosion cracking was found in the U-bend specimens after 21 days of testing. The large plate test was completed after 12 weeks of immersion in a similar solution at 125 C except that the aluminate concentration was reduced to 0.3 M. Visual inspection of the plate revealed that stress corrosion cracking had not initiated from the machined crack tips in the weld or in the heat affected zone. NDE ultrasonic testing also confirmed subsurface cracking did not occur. Based on these results, it can be concluded that the environmental condition of these tests was unable to develop stress corrosion cracking within the test periods for the small welded U-bends and for the large plates, which were welded with an identical procedure as used in the construction of the actual nuclear waste tanks in the 1960s. The absence of evidence of stress corrosion cracking and general corrosion in the laboratory-scaled specimens indicate that this type of nuclear waste tank is not susceptible to highly caustic solutions up to 12 M hydroxide at 125 C when sufficient nitrite inhibitor is present.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrosion Inhibition of Cold-rolled Low Carbon Steel with Pulse Fiber Laser Ablation in Water

This study aims at the use of a fiber laser for modifying the surface properties of cold-rolled low carbon steel via a pulse laser ablation technique in water. The effect on the corrosion behavior of the fiber laser-treated metal surface was investigated in NaCl and HCl environments. Electrochemical tests showed significant improvement in the corrosion resistance of the laser-treated sample in NaCl, with an increase in open-circuit potential (OCP) from − 0.65 to − 0.60 V and an inhibition efficiency of 89.22% as obtained from the impedance study. Such improvement was less significant in an acidic environment. Lower corrosion rates of 20.9 mpy and 5.819 × 10{sup 3} mpy were obtained for the laser-treated samples in neutral and acidic electrolytes, respectively, than the corrosion rates obtained for the as-received samples (33.2 mpy and 11.98 × 10{sup 3} mpy). Morphological analysis indicated a passive film built by spherical grains of regular size on the metal surface after laser treatment. The corrosion inhibition effects in NaCl were evident by the nonexistence of the common corrosion products of lepidocrocite and crystalline structures that were seen on as-received samples; only polyhedral crystals with micrograins grown on them were seen covering the laser-treated surface. Therefore, the laser treatment using a fiber laser source improved the corrosion resistance of cold-rolled low carbon steel.

36 MATERIALS SCIENCE↗

Corrosion Performance of Fe-Based Alloys in Simulated Oxy-Fuel Environment

The long-term corrosion of Fe-based alloys in simulated oxy-fuel environment at 1023 K (750 A degrees C) was studied. Detailed results are presented on weight change, scale thickness, internal penetration, microstructural characteristics of the corrosion products, and the cracking of scales for the alloys after exposure at 1023 K (750 A degrees C) for up to 3600 hours. An incubation period during which the corrosion rate was low was observed for the alloys. After the incubation period, the corrosion accelerated, and the corrosion process followed linear kinetics. Effects of alloy, CaO-containing ash, and gas composition on the corrosion rate were also studied. In addition, synchrotron nanobeam X-ray analysis was employed to determine the phase and chemical composition of the oxide layers on the alloy surface. Results from these studies are being used to address the long-term corrosion performance of Fe-based alloys in various coal-ash combustion environments and to develop methods to mitigate high-temperature ash corrosion.

36 MATERIALS SCIENCE↗

Effect of Temper Condition on the Corrosion and Fatigue Performance of AA2219 Aluminum Alloy

The effect of temper condition and corrosion on the fatigue behavior of alloy AA2219 has been investigated in different temper conditions (T87 and T851). Corrosion testing was performed by exposing the tensile specimens to 3.5% NaCl solution for different time periods, and the corrosion damage was quantified using a 3D profilometer. The exposure-tested specimens were subjected for fatigue testing at different stress levels, and the reduction in fatigue life was measured along with detailed fracture morphology variations. The results indicated that the alloy in both tempers suffers localized corrosion damage and the measured corrosion depth was 120 and 1200 µm, respectively, for T87 and T851 conditions. The loss in fatigue strength was found to be high for T851 (67%) when compared to that of T87 temper condition (58%) for a pre-corrosion time of 15 days. In both cases, fatigue crack initiation is associated with corrosion pits, which act as stress raisers. However, the crack propagation was predominantly transgranular for T87 and a mixed transgranular and intergranular fracture in the case of T851 temper condition. This was shown to be due to the heterogeneous microstructure due to the thermomechanical working and the delay in quench time imposed on the alloy forging in T851 temper condition. The findings in this paper present useful information for the selection of appropriate heat treatment condition to facilitate control of the corrosion behavior which is of great significance for their fatigue performance.

36 MATERIALS SCIENCE↗

Effect of Nickel on the Adhesion and Corrosion Ability of Pseudomonas aeruginosa on Stainless Steel

Microbial colonization of metal surfaces or adhesion of bacteria on metal surfaces is a crucial step in initiating microbiologically influenced corrosion. As the substrate is essential in the development of a biofilm, an understanding of how substrate properties affect adhesion of bacterial cells, including the mechanism of bacterial adhesion, may assist in designing or modifying substrates to inhibit bacterial adhesion and prevent the corrosion of materials. A study was carried out to investigate the effect of nickel on the adhesion and corrosion ability of stainless steels with the same chromium content in nutrient-rich simulated seawater containing Pseudomonas aeruginosa. These stainless steels were 201, 316, 304 and 430 stainless steels. In addition, a carbon steel sample with fully nickel coated was included for comparison. The hydrophobicity of different materials was evaluated by measuring the contact angles made by the water, glycerol and formaldehyde. The number of bacteria adhering to the material surface after short-term immersion was counted by fluorescence microscopy. For corrosion study, the corrosion rates and pitting morphology were studied after 42 days of immersion. The corrosion behavior of the samples was also observed by scanning electron microscope (SEM) coupled with energy-dispersive x-ray spectroscopy (EDX) and inductively coupled plasma mass spectrometry (ICPMS). It was found that the nickel-coated sample had the highest level of bacteria attachment and offered poor corrosion resistance under artificial seawater with Pseudomonas aeruginosa strain. Higher nickel content in stainless steel resulted in a higher level of bacteria attachment. It was found that stainless steel with molybdenum exhibited better corrosion resistance in artificial seawater containing bacteria.

36 MATERIALS SCIENCE↗

Chloride-induced corrosion of steel in cracked concrete – Part I: Experimental studies under accelerated and natural marine environments

Parallel corrosion experiments were carried out for 2¼ years by exposing one half of 210 beam specimens (120 × 130 × 375 mm long) to accelerated laboratory corrosion (cyclic wetting and drying) while the other half underwent natural corrosion in a marine tidal zone. Experimental variables were crack width w{sub cr} (0, incipient crack, 0.4, 0.7 mm), cover c (20, 40 mm), binder type (PC, PC/GGBS, PC/FA) and w/b ratio (0.40, 0.55). Results show that corrosion rate (i{sub corr}) was affected by the experimental variables in the following manner: i{sub corr} increased with increase in crack width, and decreased with increase in concrete quality and cover depth. The results also show that the corrosion performance of concretes in the field under natural corrosion cannot be inferred from its performance in the laboratory under accelerated corrosion. Other factors such as corrosion process should be taken into account.

36 MATERIALS SCIENCE↗

Dynamic and static corrosion of chromium-alumina refractory in simulated nuclear waste glass

Monofrax® K-3, a chromium–alumina refractory, is widely used in nuclear waste glass melters due to its high durability. However, aggressive vitrification conditions still lead to corrosion that limits melter lifespan. Here, this study investigates two key corrosion modes, subsurface and melt-line corrosion, under static and dynamic conditions, using a custom setup enabling precise control of melt velocity and temperature. Experimental results, interpreted using diffusion-limited dissolution models, show that (i) subsurface corrosion increases by approximately 10% per mm/s increase in melt velocity, while melt-line corrosion remains virtually unaffected, (ii) corrosion rate dependence on temperature is inversely proportional to melt viscosity, and (iii) glass composition affects both corrosion modes similarly, based on Cr 2 O 3 , Al 2 O 3 , and alkali contents. The experimental data also allowed the determination of diffusion coefficients of major dissolving species, which were found to be consistent between the melt-line and subsurface corrosion models, indicating their suitability for future CFD studies.

12 - MGMT OF RADIOACTIVE AND NON-RADIOACTIVE WASTE↗

Corrosion characteristics of Mo and TZM alloy for plasma facing components in molten lithium at 623 K

Here, in this study, the corrosion behaviours of molybdenum (Mo) and a Mo-based alloy (TZM) were investigated using a static immersion corrosion technique. Weight loss, surface microstructure, and corrosion depth of Mo and the TZM alloy were correlated with elements. The compatibility of Mo and the TZM alloy in static liquid Li was suitable. Mo demonstrated uniform corrosion with a homogenous dissolution of free C and Mo, and TZM alloy exhibited a nonuniform corrosion behaviour with a preferential grain boundary attack caused by the selective dissolution of free C, Ti, and Zr. When the surface oxidation layer of the samples was consumed, free C from Mo and TZM diffused into molten Li to form Li 2 C 2 and then was captured by Zr, Ti, and Mo to form thermodynamically stable carbides, which resulted in the enrichment of the C layer near the sample surfaces. In addition, Ti and Zr acted as N-trappers in liquid Li; the formation of Zr and Ti nitrides resulted in the enrichment of N, Ti, and Zr elements on the surface and led to TZM corrosion increase. Thus, Zr and Ti depletion, pitting, and grain boundary corrosion were problematic for TZM under long-term exposure to liquid Li. Reducing the content of free C and nonmetallic N and increasing the amount of Ti and Zr carbides on the surface of and inside the raw TZM alloy helped improve the corrosion resistance of TZM in liquid Li.

36 MATERIALS SCIENCE↗

Hot corrosion behavior of 304 & P91 graded composite transition joint under molten sulfate salts

A novel graded composite transition joint (GCTJ) between AISI 304 stainless steel and ASTM A335 P91 steel, has been demonstrated remarkablely superior creep performance compared to the conventional dissimilar metal weldment (DMW) under equivalent conditions. However, this advance is challenged by hot corrosion under salt deposition at elevated temperatures. Here, this study investigates the hot corrosion behavior of 304&P91 GCTJ exposed to sulfate salts at 700°C. Compared to the 304 steel, corrosion attacks initiate in the P91 triangle, where the dual-phase microstructure of ferrite and tempered martensite significantly influences pitting initiation. Anodic dissolution mainly occurs within the tempered martensite due to more vulnerable sites within the tempered martensite. With prolonged exposure, corrosion propagates across both phases, and the corrosion depth within the P91 triangle is related to the exposed surface area ratio between 304 and P91. Electrochemical analysis reveals the occurrence of galvanic corrosion between the 304 and P91, with a positive linear relationship between anodic dissolution current density (I a ) and the exposed surface area ratio between 304 and P91 in molten salts, further emphasizing the critical impact of this ratio on the corrosion severity in the P91 triangle. These findings underscore the importance of transition zone design optimization in mitigating localized corrosion.

Galvanic corrosion↗

Study on the corrosion residual strength of the 1.0 wt.% Ce modified AZ91 magnesium alloy

The effect of corrosion on the tensile behaviour of the 1.0 wt.% Ce modified AZ91 magnesium alloy was investigated by the immersion of the test bar in 3.5 wt.% NaCl aqueous solution for 0, 12, 40, 108, 204, 372 and 468 h with the subsequent tensile tests in this paper. The fractography was analyzed by scanning electron microscopy. The results show that pitting corrosion should be responsible for the drop of the corrosion residual strength within the testing time. The depth of the corrosion pits was statistically and quantitatively obtained by an optical microscopy and the maximal value was recorded as the extreme depth of the corrosion pit. Furthermore, the corrosion residual strength is linearly dependent on the extreme depth of the corrosion pit, which can be attributed to the loss of cross-sectional area and the emergence of stress concentration caused by the initiation and development of corrosion pits.

36 MATERIALS SCIENCE↗

In situ corrosion analysis of Al-Zn-In-Mg-Ti-Ce sacrificial anode alloy

The corrosion behaviour of Al-5Zn-0.02In-1Mg-0.05Ti-0.5Ce (wt.%) alloy has been investigated by immersion test, scanning electron microscopy, energy dispersive X-ray detector, electrochemical impedance spectroscopy and electrochemical noise. The results show that there exist different corrosion types of the alloy in 3.5% NaCl solution with the immersion time. At the initial stage of immersion, pitting due to the precipitates predominates the corrosion with a typical inductive loop at low frequencies in electrochemical impedance spectroscopy. The major precipitates of the alloy are MgZn{sub 2} and Al{sub 2}CeZn{sub 2} particles. The corrosion potentials of the bulk MgZn{sub 2} and Al{sub 2}CeZn{sub 2} alloys are negative with respect to that of {alpha}-Al, so the MgZn{sub 2} and Al{sub 2}CeZn{sub 2} precipitates can act as activation centre and cause the pitting. In the late corrosion, a relative uniform corrosion predominates the corrosion process controlled by the dissolution/precipitation of the In ions and characterized by a capacitive loop at medium-high frequencies in electrochemical impedance spectroscopy. The potential noise of the pitting shows larger amplitude fluctuation and lower frequency, but the potential noise of the uniform corrosion occurs with smaller amplitude fluctuation and higher frequency.

36 MATERIALS SCIENCE↗

Synergistic Effects of Molten Salt Corrosion and Proton Irradiation on Grain Boundary Strength in Ni-20Cr

Nickel-based alloys are leading contenders for use as structural materials in molten salt reactors. While there have been extensive studies on the impact of fluoride/chloride-based molten salt corrosion on the microstructural evolution of various nickel-based alloys, the effects of simultaneous molten salt corrosion and radiation on the mechanical integrity of grain boundaries (GBs) remain underexplored. In this study, we use a Ni-20Cr model alloy to investigate this issue, subjecting it to simultaneous molten fluoride salt corrosion and proton irradiation. We performed cross-sectional and chemically-sensitive electron microscopy characterization of the microstructures of these materials, identifying the characteristic corrosion-induced microstructure and local chemical heterogeneity near GBs. After developing a sample preparation method for reliable characterization of GB strength, we assess the mechanical degradation of GBs using in situ push-to-pull micro tensile tests. Our findings reveal that voids induced by corrosion are the primary influence on the failure mode of GBs, regardless of whether proton irradiation is present. For materials that exhibit ductile fracture, those subjected to simultaneous corrosion and radiation exhibit lower yield strengths than those exposed to corrosion alone, which may be linked to the previously observed phenomenon of proton irradiation-decelerated intergranular corrosion in molten salt.

36 - MATERIALS SCIENCE↗