Search NASA⌕ Search

SEARCH · Search NASA

Results for “Capacity Loss”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

Corrosion of lithium metal anodes during calendar ageing and its microscopic origins

Rechargeable lithium (Li) metal batteries must have long cycle life and calendar life (retention of capacity during storage at open circuit). Particular emphasis has been placed on prolonging the cycle life of Li metal anodes, but calendar ageing is less understood. Here, we show that Li metal loses at least 2–3% of its capacity after only 24 hours of ageing, regardless of the electrolyte chemistry. These losses of capacity during calendar ageing also shorten the cycle life of Li metal batteries. Cryogenic transmission electron microscopy shows that chemical corrosion of Li and the continuous growth of the solid electrolyte interphase—a passivation film on Li—cause the loss of capacity. Electrolytes with long cycle life do not necessarily form a solid electrolyte interphase with more resistance to chemical corrosion, so functional electrolytes must simultaneously minimize the rate of solid electrolyte interphase growth and the surface area of electrodeposited Li metal.

36 MATERIALS SCIENCE↗

Selected test results from the neosonic polymer Li-ion battery.

The performance of the Neosonic polymer Li-ion battery was measured using a number of tests including capacity, capacity as a function of temperature, ohmic resistance, spectral impedance, hybrid pulsed power test, utility partial state of charge (PSOC) pulsed cycle test, and an over-charge/voltage abuse test. The goal of this work was to evaluate the performance of the polymer Li-ion battery technology for utility applications requiring frequent charges and discharges, such as voltage support, frequency regulation, wind farm energy smoothing, and solar photovoltaic energy smoothing. Test results have indicated that the Neosonic polymer Li-ion battery technology can provide power levels up to the 10C{sub 1} discharge rate with minimal energy loss compared to the 1 h (1C) discharge rate. Two of the three cells used in the utility PSOC pulsed cycle test completed about 12,000 cycles with only a gradual loss in capacity of 10 and 13%. The third cell experienced a 40% loss in capacity at about 11,000 cycles. The DC ohmic resistance and AC spectral impedance measurements also indicate that there were increases in impedance after cycling, especially for the third cell. Cell No.3 impedance Rs increased significantly along with extensive ballooning of the foil pouch. Finally, at a 1C (10 A) charge rate, the over charge/voltage abuse test with cell confinement similar to a multi cell string resulted in the cell venting hot gases at about 45 C 45 minutes into the test. At 104 minutes into the test the cell voltage spiked to the 12 volt limit and continued out to the end of the test at 151 minutes. In summary, the Neosonic cells performed as expected with good cycle-life and safety.

17 WIND ENERGY↗

Low Latency and High Data Rate (LLHD) Scheduler: A Multipath TCP Scheduler for Dynamic and Heterogeneous Networks

The scheduler is a crucial component of the multipath transmission control protocol (MPTCP) that dictates the path that a data packet takes. Schedulers are in charge of delivering data packets in the right order to prevent delays caused by head-of-line blocking. The modern Internet is a complicated network whose characteristics change in real-time. MPTCP schedulers are supposed to understand the real-time properties of the underlying network, such as latency, path loss, and capacity, in order to make appropriate scheduling decisions. However, the present scheduler does not take into account all of these characteristics together, resulting in lower performance. We present the low latency and high data rate (LLHD) scheduler, which successfully makes scheduling decisions based on real-time information on latency, path loss, and capacity, and achieves around 25% higher throughput and 45% lower data transmission delay than Linux’s default MPTCP scheduler.

97 MATHEMATICS AND COMPUTING↗

Effect of Gaseous Impurities on Long-Term Thermal Cycling and Aging Properties of Complex Hydrides for Hydrogen Storage

This program was dedicated to understanding the effect of impurities on Long-Term Thermal Cycling and aging properties of Complex Hydrides for Hydrogen Storage. At the start of the program we found reversibility between Li2NH+LiH LiH+LiNH2 (yielding ~5.8 wt.%H capacity). Then we tested the effect of impurity in H2 gas by pressure cycling at 255°C; first with industrial gas containing ppm levels of O2 and H2O as major impurities. Both these impurities had a significant impact on the reversibility and decreased the capacity by 2.65 wt.%H. Further increase in number of cycles from 500 to 1100 showed only a 0.2 wt%H more weight loss, showing some capacity is still maintained after a significant number of cycles. The loss of capacity is attributed to the formation of ~55 wt% LiH and ~30% Li2O, as major contaminant phases, along with the hydride Li2NH phase; suggesting loss of nitrogen during cycling. The effect of 100 ppm H2O in H2 also showed a decrease of ~2.5 wt.%H (after 560 cycles), and 100ppm O2 in H2; a loss of ~4.1 wt.%. Methane impurity (100 ppm, 100cycles), showed a very small capacity loss of 0.9 wt.%H under similar conditions. However, when Li3N was pressure cycled with 100ppmN2-H2 there were beneficial effects were observed (255oC); the reversible capacity increased to 8.4wt.%H after 853 cycles. Furthermore, with 20 mol.%N2-H2 capacity increased to ~10 wt.%H after 516 cycles. We attribute this enhancement to the reaction of nitrogen with liquid lithium during cycling as the Gibbs free energy of formation of Li3N (Go = -98.7 kJ/mol) is more negative than that of LiH (Go = -50.3 kJ/mol). We propose that the mitigation of hydrogen capacity losses is due to the destabilization of the LiH phase that tends to accumulate during cycling. Also more Li2NH phase was found in the cycled product. Mixed Alanates (3LiNH2:Li3AlH6) showed that 7 wt% hydrogen desorbed under dynamic vacuum. Equilibrium experiments (maximum 12 bar H2) showed up to 4wt% hydrogen reversibly stored in the material after the first desorption. The activation energy was found to be 51 kJ/mol, as compared to 81 kJ/mol for pure lithium alanate. It is proposed that based on the data obtained and CALPHAD modeling that the improvement in cycling is due to the formation of pure lithium (liquid at 255°C), which is able to react with nitrogen specifically forming Li3N. The presence of nitrogen in the 80/20 molar mixtures in a hydride bed along with hydrogen causes Li to form Li3N rather than LiH, and subsequently regenerates the Li2NH phase and yields a ~10 wt.%H reversibly.

08 HYDROGEN↗

First-Principles Analysis of Defect Thermodynamics and Ion Transport in Inorganic SEI Compounds: LiF and NaF

The formation mechanism and composition of the solid electrolyte interphase (SEI) in lithium ion batteries has been widely explored. However, relatively little is known about the function of the SEI as a transport medium. Such critical information is directly relevant to battery rate performance, power loss, and capacity fading. To partially bridge this gap in the case of inorganic SEI compounds, we report herein the results of first-principles calculations on the defect thermodynamics, the dominant diffusion carriers, and the diffusion pathways associated with crystalline LiF and NaF, which are stable components of the SEI in Li-ion and Na-ion batteries, respectively. The thermodynamics of common point defects are computed, and the dominant diffusion carriers are determined over a voltage range of 0-4 V, corresponding to conditions relevant to both anode and cathode SEI's. Our analyses reveal that for both compounds, vacancy defects are energetically more favorable, therefore form more readily than interstitials, due to the close-packed nature of the crystal structures. However, the vacancy concentrations are very small for the diffusion processes facilitated by defects. Ionic conductivities are calculated as a function of voltage, considering the diffusion carrier concentration and the diffusion barriers as determined by nudged elastic band calculations. These conductivities are more than ten orders of magnitude smaller in NaF than in LiF. As compared to the diffusivity of Li in other common inorganic SEI compounds, such as Li2CO3 and Li2O,the cation diffusivity in LiF and NaF is quite low, with at least three orders of magnitude lower ionic conductivities. The results quantify the extent to which fluorides pose rate limitations in Li and Na batteries.

Yildirim, Handan↗

In-situ observation of inhomogeneous degradation in large format Li-ion cells by neutron diffraction

This work presents a non-destructive in-situ method for probing degradation mechanisms in large format, operating, commercial lithium-ion batteries by neutron diffraction. A fresh battery (15 Ah capacity) was shown to have a uniform (homogeneous) local state of charge (SOC) at 4.0 V (9 Ah SOC) and 4.2 V (15 Ah SOC), with 1.33 C and 2.67 C charging rates, respectively. This battery was then aggressively cycled until it retained only a 9 Ah capacity, 60% of its original value. Inhomogeneous deterioration in the battery was observed: near the edges, both the graphite anode and the spinel-based cathode showed a significant loss of capacity, while near the central area, both electrodes functioned properly. An SOC mapping measurement of the degraded battery in the fully charged state (4.2 V) indicated that the loss of local capacity of the anode and cathode is coupled.

25 ENERGY STORAGE↗

Capacity retention in hydrogen storage alloys

Results of our examination of the properties of several candidate materials for hydrogen storage electrodes and their relation to the decrease in H-storage capacity upon open-circuit storage over time are reported. In some of the alloy samples examined to date, only about 10 percent of the hydrogen capacity was lost upon storage for 20 days, while in others, this number was as high as 30 percent for the same period of time. This loss in capacity is attributed to two separate mechanisms: (1) hydrogen desorbed from the electrode due to pressure differences between the cell and the electrode sample; and (2) chemical and/or electrochemical degradation of the alloy electrode upon exposure to the cell environment. The former process is a direct consequence of the equilibrium dissociation pressure of the hydride alloy phase and the partial pressure of hydrogen in the hydride phase in equilibrium with that in the electrolyte environment, while the latter is related to the stability of the alloy phase in the cell environment. Comparison of the equilibrium gas-phase dissociation pressures of these alloys indicate that reversible loss of hydrogen capacity is higher in alloys with P(eqm) greater than 1 atm than in those with P(eqm) less than 1 atm.

Anani, A.↗

Performance and Achievable Rates of the Gottesman-Kitaev-Preskill Code for Pure-Loss and Amplification Channels

Quantum error-correction codes protect information from realistic noisy channels and lie at the heart of quantum computation and communication tasks. Understanding the optimal performance and other information-theoretic properties, such as the achievable rates, of a given code is crucial, as these factors determine the fundamental limits imposed by the encoding in conjunction with the noise channel. Here, we use the transpose channel to analytically obtain the near-optimal performance of any Gottesman-Kitaev-Preskill (GKP) code under pure loss and pure amplification. We present rigorous connections between GKP code’s near-optimal performance and its dual lattice geometry and average input energy. With no energy constraint, we show that when |𝜏/(1−𝜏)| is an integer, specific families of GKP codes simultaneously achieve the loss and amplification capacity. 𝜏 is the transmissivity (gain) for loss (amplification). Our results establish GKP code as the first structured bosonic code family that achieves the capacity of loss and amplification.

Zheng, Guo [Univ. of Chicago, IL (United States)] ↗

Beneficial Effect of Li 5 FeO 4 Lithium Source for Li-Ion Batteries with a Layered NMC Cathode and Si Anode

The energy density of lithium-ion batteries can be increased by replacing the traditional graphite anode with a high capacity silicon anode. However, volume changes and interfacial instabilities cause a large irreversible capacity and a continual loss of lithium during cycling, which lead to rapid capacity loss. In this work, we add Li 5 FeO 4 (LFO) to a LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC) cathode as a pre-lithiation additive, which increases the lithium inventory and extends the cycle life of Si-graphite/NMC full cells, and decreases the NMC particle degradation. LFO delivers a large 764 mAh g –1 LFO capacity below 4.7 V vs Li/Li + . By tuning the LFO content in Si-graphite/LFO-NMC full cells, we show higher capacity, improved retention, lower impedance, and superior rate performance compared to full cells without LFO. Post-test characterizations demonstrate that LFO inclusion in the cathode matrix leads to less NMC secondary particle segregation/cracking and a thinner surface reduced layer on the NMC particles. The beneficial effects of LFO endure after the lithium reserve has been exhausted, highlighting a lasting synergy between the lithium source and electrode active materials. This study introduces a new approach to simultaneously increase lithium inventory and reduce cathode degradation, and makes critical advances toward enabling Si anodes for lithium-ion batteries.

25 ENERGY STORAGE↗

Long Duration Sorbent Testbed

The Long Duration Sorbent Testbed (LDST) is a flight experiment demonstration designed to expose current and future candidate carbon dioxide removal system sorbents to an actual crewed space cabin environment to assess and compare sorption working capacity degradation resulting from long term operation. An analysis of sorbent materials returned to Earth after approximately one year of operation in the International Space Station's (ISS) Carbon Dioxide Removal Assembly (CDRA) indicated as much as a 70% loss of working capacity of the silica gel desiccant material at the extreme system inlet location, with a gradient of capacity loss down the bed. The primary science objective is to assess the degradation of potential sorbents for exploration class missions and ISS upgrades when operated in a true crewed space cabin environment. A secondary objective is to compare degradation of flight test to a ground test unit with contaminant dosing to determine applicability of ground testing.

Howard, David F.↗

Long Duration Sorbent Testbed

The LDST is a flight experiment demonstration designed to expose current and future candidate carbon dioxide removal system sorbents to an actual crewed space cabin environment to assess and compare sorption working capacity degradation resulting from long term operation. An analysis of sorbent materials returned to earth after approximately one year of operation in the International Space Station's (ISS) Carbon Dioxide Removal Assembly (CDRA) indicated as much as a 70% loss of working capacity of the silica gel desiccant material at the extreme system inlet location, with a gradient of capacity loss down the bed. The primary science objective is to assess the degradation of potential sorbents for exploration class missions and ISS upgrades when operated in a true crewed space cabin environment. A secondary objective is to compare degradation of flight test to a ground test unit with contaminant dosing to determine applicability of ground testing.

Knox, James↗

Impacts of Varying Penetration of Distributed Resources with & without Volt/Var Control: Case Study of Varying Load Types

This paper provides a follow-up to an earlier one on impacts of distributed energy resources (DR) on distribution feeders. As DR penetration level on the feeder increases, there can be impacts to distribution system/feeder capacity, line losses, and voltage regulation. These can vary as the penetration level reaches the capacity of the distribution feeder/system or loading. The question is how high of a DR level can be accommodated without any major changes to system operation, system design and protection. Our objective for this work was to address the question of how the DR impacts vary in regards to both DR voltage regulation capability and load mix. A dynamic analysis was used to focus on the impacts of DR with and without volt/var control with different load composition on the distribution feeder. The study considered an example 10MVA distribution feeder in which two inverter-based DRs were used to provide voltage regulation. The results due to DR without voltage regulation capability are compared with DR capable of providing local (at its bus) voltage regulation. The analysis was repeated for four different feeder load compositions consisting of (1) constant power, (2) constant impedance, (3) constant current and (4) ZIP (equal combination of previous three).

24 POWER TRANSMISSION AND DISTRIBUTION↗

Enhanced CO2/N2 Selectivity in Amidoxime-Modified Porous Carbon

In this work, we examine the use of the amidoxime functional group grafted onto a hierarchical porous carbon framework for the selective capture and removal of carbon dioxide from combustion streams. Measured CO2/N2 ideal selectivity values for the amidoxime-grafted carbon were significantly higher than the pristine porous carbon with improvements of 65%. Though the overall CO2 capacity decreased slightly for the activated carbon from 4.97 mmol g-1 to 4.24 mmol g-1 after surface modification due to a reduction in the total surface area, the isosteric heats of adsorption increased after amidoxime incorporation indicating an increased interaction of CO2 with the sorbent. Total capacity was reproducible and stable after multiple adsorption/desorption cycles with no loss of capacity suggesting that modification with the amidoxime group is a potential method to enhance carbon capture.

Mahurin, Shannon Mark↗

Physical Properties of Hilti HIT-RE 500 V3 After Irradiation: Slant Shear, Tensile, Flexural, and Compressive

There are various applications in which epoxy adhesives may be used within hot-cell environments. These epoxies currently see limited use within hot cells since it is known that organics see degradation after small doses even as low as 50 kilogray (kGy). These losses in physical property strengths limit the use of these epoxies to non-structural applications. In modern construction, however, the use of epoxies to bond structural components such as rebar or threaded anchors is becoming increasingly prevalent. To employ these types of materials the Idaho National Laboratory (INL) has begun investigating the specific degradation properties of epoxies for use in structural applications in environments where radiation is present. Hilti HIT-RE 500 V3 is used extensively in new construction and renovation projects across the world. The INL has conducted various tests on this epoxy for low dose environments. These tests include tensile, flexural, compression, and slant shear tests following the American Society for Testing Material International (ASTM) standards D638, D790, D695, and C882/882M respectively. Two sample sets for each test were created where the baseline specimens were not irradiated, and another set was irradiated to an accumulated dose of approximately 50-60 kGy. All the samples were destructively tested and analyzed focusing on the change in physical properties, examples of these tests are shown in Figures 1-4. Tensile testing results indicate a 0.9% loss in maximum load capacity, a 0.5% loss in tensile stress at maximum load, a 1.4% loss in tensile strain at break, and a 15% decrease in modulus of elasticity. Flexural testing results display an increase in all the following: 12% in strain at maximum load, 10% in maximum load capacity, 5% in stress at maximum load, and 3% in young’s modulus. The compressive physical properties after irradiation display a 1% increase in maximum load, a 3% decrease in stress at yield, and a 5% decrease in modulus of elasticity. The maximum compressive stress saw no measurable change after irradiation. The slant shear specimens after irradiation displayed a 2% increase in maximum load capacity and maximum compressive stress. Though a structural analysis would have to be completed as is normal for building design the increases and decreases in the measured physical properties indicate that this material may be used for structural applications in low dose hot-cell environments without adhesive failure.

36 MATERIALS SCIENCE↗

NO2 Aging and Iodine Loading of Silver-Functionalized Aerogels

Off-gas treatment systems in used fuel reprocessing which use fixed-bed adsorbers are typically designed to operate for an extended period of time before replacement or regeneration of the adsorbent. During this time, the sorbent material will be exposed to the off-gas stream. Exposure could last for months, depending on the replacement cycle time. The gas stream will be at elevated temperature and will possibly contain a mixture of water vapor, NOx, nitric acid vapors, and a variety of other constituents in addition to the radionuclides of capture interest. A series of studies were undertaken to evaluate the effects of long-term exposure, or aging, on proposed iodine sorbent materials under increasingly harsh off-gas conditions. Previous studies have evaluated the effects of up to 6 months of aging under dry air and under humid air conditions on the iodine loading behavior of Ag0-functionalized aerogels. This study examines the effects of extended exposure (up to 6 months) to NO2 on the iodine loading capacity of Ag0- functionalized aerogels. Material aged for 1 and 2 months appeared to have a similar total loading capacity to fresh material. Over an aging period of 4 months, a loss of approximately 15% of the total iodine capacity was seen. The iodine capacity loss on silver-functionalized aerogels due to NO2 was smaller than the iodine capacity loss due to humid or dry air aging.

Patton, K K↗

Pulsed Laser Deposition and Characterization of Heteroepitaxial LiMn 2 O 4 /La 0.5 Sr 0.5 CoO 3 Bilayer Thin Films as Model Lithium Ion Battery Cathodes

Epitaxial LiMn 2 O 4 (LMO)/La 0.5 Sr 0.5 CoO 3 (LSCO) bilayer thin films were grown on single crystalline SrTiO 3 (STO) (111) substrates as model lithium ion battery cathodes. The LSCO layer was used as an electrically conducting buffer layer for electrochemical testing. The LMO and LSCO layers were both epitaxial, with sub-nano flat LMO/LSCO interfaces as seen by X-ray diffraction, synchrotron X-ray scattering, and high-resolution transmission electron microscopy (HRTEM), but with a large LMO surface roughness due to the relatively large lattice mismatch with LSCO. Three-dimensional islands and depressions were formed on the strain-relaxed LMO layer, and misfit dislocations at the LMO/LSCO interface were discerned through HRTEM imaging, suggesting a Stranski–Krastanov (SK) mode thin-film growth. A crystalline structural change from cubic spinel at the LMO surface and interior to tetragonal oxygen-deficient LMO at the LMO/LSCO interface was examined. Furthermore, electrochemical tests along with in situ synchrotron X-ray scattering measurements on the epitaxial LMO/LSCO bilayers showed a significant loss of capacity after the first cycle, which was attributed to an electrical conductivity loss of the LSCO buffer layer due to irreversible lattice oxygen loss.

25 ENERGY STORAGE↗

Supine Treadmill Exercise in Lower Body Negative Pressure Combined with Resistive Exercise Counteracts Bone Loss, Reduced Aerobic Upright Exercise Capacity and Reduced Muscle Strength

Long-term exposure to weightlessness leads to cardiovascular and musculoskeletal deconditioning. In this report, the effectiveness of combined supine treadmill exercise in a lower body negative pressure chamber (LBNPex) and flywheel resistive exercise (Rex) countermeasures was determined to prevent bone loss, reduced aerobic upright exercise capacity and reduced muscle strength. We hypothesized that exercise subjects would show less decrease in bone mineral density (BMD), peak oxygen consumption (VO2pk) and knee extensor strength (KES) than control subjects. Sixteen healthy female subjects participated in a 60-d 6(sup 0) head-down tilt bed rest (BR) study after providing written informed consent. Subjects were assigned to one of two groups: a non-exercising control group CON or an exercise group EX performing LBNPex 2-4 d/wk and Rex every 3rd-d. VO2pk was measured with a maximal, graded, upright treadmill test performed pre-BR and on 3-d after BR. BMD was assessed before and 3-d after BR. Isokinetic KES was measured before and 5-d after BR. Two-way repeated measures ANOVA were performed. Statistical significance was set at p less than 0.05. CON experienced a significant decrease in BMD in the trochanter (PRE: 0.670 plus or minus 0.045; POST: 0.646 plus or minus 0.352 g (raised dot) per square centimeter) and in the whole hip (PRE=0.894 plus or minus 0.059; POST: 0.858 plus or minus 0.057 g (raised dot) per square centimeter). BMD also decreased significantly in EX in the trochanter (PRE: 0.753 plus or minus 0.0617; POST: 0.741 plus or minus 0.061 g (raised dot) per square centimeter) and whole hip (PRE: 0.954 plus or minus 0.067; POST: 0.935 plus or minus 0.069 g (raised dot) per square centimeter). BMD losses were significantly less in EX than in CON subjects. VO2pk was significantly decreased in the CON after BR (PRE: 38.0 plus or minus 4.8; POST: 29.9 plus or minus 4.2 ml (raised dot) per kilogram per minute), but not in the EX (PRE: 39.0 plus or minus 2.0; POST: 37.8 plus or minus 1.9 ml (raised dot) per kilogram per minute). KES was significantly reduced by 30% in Con (PRE: 113 plus or minus 12; POST: 78 plus or minus 8 N-m), but was not different in EX (PRE: 126 plus or minus 25; POST: 115 plus or minus 25 N-m). The combination LBNPex and Rex during 60-d BR protects against cardiovascular and musculoskeletal deconditioning and may be efficacious countermeasure for prolonged space flight.

Meuche, Sabine↗

Performance and Safety Testing of Cylindrical Moli Lithium-Ion Cells

The Moli lithium-ion cells were tested under normal and abuse conditions. The cells exhibit only 50% of their original capacity at about -10 C. The optimum charge/discharge rate with the least percentage loss in capacity is C/2 charge and C/4 discharge. The cells did not explode or go into a thermal runaway during venting at very high temperatures. They exhibited good tolerance under the vibration conditions tested and could potentially be used in the build up of large batteries that have high current pulse (up to 3C) applications.

Jeevarajan, Judith A.↗