Thermal Aging Degradation of Cast Stainless Steels in LWR Systems

Cast austenitic stainless steels (CASSs) have been extensively used for the large components of light water reactor (LWR) power plants such as primary coolant piping and pump casing. Since a large number of massive CASS components are installed in every modern nuclear power plant, any significant degradation of CASS components will raise serious concerns on the integrity of the entire power plant. Upon the presumption that the replacement cost of such massive components is prohibitive, therefore, thorough scientific understanding and systematic monitoring the thermal aging degradation of CASS components should be essential requirements for assessing the plant safety. In the past few decades many researches have concluded that the formation of Cr-rich α-phase by Spinoidal decomposition of δ-ferrite phase, which is formed in high temperature region during cooling, is the primary mechanism for the thermal embrittlement. Cracking mechanism in the thermally-embrittled duplex stainless steels consists of cleavage initiation at ferrite and crack propagation via separation of ferrite-austenite interphase. It has been known, however, that such thermal aging embrittlement is observed only in accelerated aging conditions and the cast stainless steel grades used in nuclear plants have performed well without experiencing real embrittlement. It has been speculated that long-term thermal aging for ≥ 60 years could lead to further decomposition of designed phases and increase of precipitation. This will result in significantly increased susceptibility to embrittlement or other degradation due to thermal aging-radiation synergistic effect, irradiation-induced degradation, stress-corrosion cracking, and general corrosion. Currently, therefore, the thermal embrittlement of CASS components is one of the most serious concerns for extended operation of nuclear power plants. A scientific research is underway to address the issues related to the thermal aging degradation of CASS components. The research aims to provide knowledge-based conclusive prediction for the integrity of the CASS components of LWR power plants during extended operation up to and beyond 60 years. This presentation intends to provide an introductory overview on the thermal aging phenomena in LWR relevant conditions and discussion on the measurements of mechanical property degradation after accelerated and LWR relevant thermal aging treatments. First, the thermal aging effect on toughness is discussed in terms of the causes of embrittlement and influential parameters. Second, the talk will include a comprehensive discussion on the thermal aging effects in different CASS grades (i.e., CF3, CF3M, CF8, and CF8M), which will focus on the influence of alloying elements such as molybdenum and carbon. Third, approximate analysis on thermal reaction in CASS was carried out using Arrhenius equation to decide the effective temperature range for accelerated aging experiments to simulate 60 and 80 years of services in limited time frame. The results will provide valuable insights in the degree of thermal aging. Fourth, calculation on equilibrium precipitation was performed for model CASS alloys using the CALPHAD program, and the results will be used to describe the precipitation behaviors in association with the degradation in mechanical properties. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Determining the Crosslinking and Degradation Reaction Kinetics in Photovoltaic Encapsulants Using Accelerated Aging: Preprint

Degradation of photovoltaic (PV) module encapsulant mechanical characteristics that lead to embrittlement and delamination remains a cause of failure in solar installations. A multiscale reliability model based on detailed molecular degradation reaction kinetics was previously published, connecting the encapsulant mechanical properties (elastic modulus, yield strength, and adhesion energy) to the degraded molecular structure and interfacial bond density to adjacent solar cell and glass substrates. The model, developed primarily for poly(ethylene-co-vinyl acetate) (EVA) encapsulants, remains to be experimentally validated. Determining the degradation and crosslinking kinetics of alternative encapsulants, such as polyolefin elastomer (POE) and EVA/POE/EVA composites (EPE), can further generalize the model. Importantly, the activation energy for crosslinking of fully cured PV encapsulant products from temperature or UV is presently unknown or unavailable. In this work, we subject EVA, POE, and EPE encapsulants to a set of accelerated aging conditions, varying the temperature, UV intensity, and relative humidity. We use DSC, FTIR, and Soxhlet extraction (gel content) to characterize the encapsulants' changing molecular structure. This allows for determination of the photochemical degradation and crosslinking kinetics of the encapsulants. Preliminary results show an increase in gel content (crosslinking) and a decrease in crystallinity of EVA, POE, and EPE encapsulants under hot-aerobic (90 deg C, 22% RH) and hot-anaerobic (90oC, sealed in N2 air) accelerated aging, even in the absence of UV and crosslinking initiating agents. For a least squares regression with an assumed first-order crosslinking kinetics, the crosslinking rate parameters were computed for the three encapsulants under hot-aerobic and hot-anaerobic aging conditions. FTIR analysis showed insignificant encapsulant degradation for hot-aerobic and hot-anaerobic aging, demonstrating the critical role of UV and moisture in accelerating degradation. Aging conditions with UV exposure and elevated humidity are presently in progress.

adhesion↗

From Femtoseconds to Gigaseconds: The SolDeg Project to Analyze and Mitigate the Performance Degradation of a-Si:H/c-Si Heterojunction Solar Cells

We pursued two major projects. In the first, we studied the degradation of a-Si/c-Si Heterojunction cells. We substantially expanded our previously developed SolDeg platform, and incorporated hydrogen into it. We also expanded the capabilities of SolDeg by developing a three channel model for a very efficient way to determine long term junction dynamics. The first main result was that we identified hydrogen drifting away from the interface as a key degradation channel. The second was that we developed and proposed the concept of a “reverse silicon density gradient” in the a-Si layer that had the promise of reducing degradation by up to 80%. In the second project, we studied the degradation of TOPCon solar cells. We again identified a key degradation channel, which in these cells was the formation of pinholes across the oxide layer. We then again were able to develop and to propose a way to dramatically reduce degradation by discovering that tuning the hydrogen concentration forms a sharp and deep minimum of the recombination current.

14 SOLAR ENERGY↗

Evidence of Polarization‐Type Potential‐Induced Degradation (PID‐p) in the Field and Investigation of the Recovery Mechanism on Bifacial p ‐PERC Modules

This study investigates the polarization-type potential-induced degradation (PID-p) of bifacial glass/glass p-type passivated emitter rear contact (p-PERC) modules in the field and their recovery behavior. Modules were installed with three mounting configurations providing different albedo conditions. System voltage (–600, –1500, and +1500 V) was applied to the cell circuits, with respect to the grounded module frames. No degradation was observed for positively biased modules, but PID-p was identified on the rear side when cells are negatively biased, with maximum power dropping during the first days and stabilizing at values up to 8% loss. Electroluminescence images revealed a variation of the cells' PID-p susceptibility within a module. Three parameters were shown to impact the degradation rate: rear albedo light, voltage, and wetness conditions. Degraded modules were recovered either by (1) a positive bias (+1500 V), (2) outdoor illumination with the front side facing sun, (3) outdoor illumination with the rear side facing sun, or (4) dark storage. A recovery pattern was identified with I–V parameters decreasing to a local minimum before increasing to full recovery. The proposed mechanism is based on the band bending at the rear p-type Si/AlO x/SiN x interface, going from inversion to depletion and accumulation states. Full recovery was achieved in 2–7 h for the modules recovered with the rear side facing sun, four to eight nights for the modules positively biased at night, and 10–20 days for the modules with the front side facing sun. Dark storage showed slower recovery rates as I–V parameters were not improving even after 1 month. Here, the recovery rates were correlated with the net Coulombs transferred during the preceding PID stress: When more Coulombs are transferred during the degradation, the extent of degradation is greater, leading to slower recovery rates.

14 SOLAR ENERGY↗

Degradation and Accelerated Recovery of Surface Passivation in n+, p+, and Intrinsic Poly-Si/SiOx Passivating Contacts for Silicon Solar Cells

We report on the degradation and recovery of surface passivation of fired poly-Si/SiOx passivating contacts with hydrogen containing Al2O3 during annealing in the dark and under illumination. Upon firing to a peak temperature of 670 degrees C, the iVoc for symmetric test structures with n+, p+, and intrinsic poly-Si/SiOx contacts decreases due to a loss of surface passivation. Upon further annealing over the temperature range of 200-350 degrees C in the dark, depending on the type of doping, the surface passivation either shows further degradation followed by recovery, or direct recovery to the initial iVoc. Annealing at higher temperatures and/or higher illumination intensities accelerates the kinetics for both degradation and recovery processes. We show that the degradation and recovery processes are thermally activated and proceed identically in subsequent firing and annealing steps showing their cyclic nature. We present a series reaction model to explain the kinetics of degradation and recovery processes for n+ and intrinsic poly-Si/SiOx contacts. By fitting the model's rate expressions to the data, the determined effective activation energy barriers for degradation and recovery for n+ poly-Si/SiOx contacts in the dark are 1.24 and 1.51 eV, which are lowered under 7.5 Suns illumination to 0.76 and 1.15 eV, respectively.

14 SOLAR ENERGY↗

Chemical and Mechanical Degradation of Sulfonated Poly(sulfone) Membranes in Vanadium Redox Flow Batteries

A sulfonated poly(sulfone) (S-Radel{reg_sign}) membrane with high proton conductivity and low vanadium ion diffusion showed high initial performance in a vanadium redox flow battery (VRFB) but suffered damage during charge/discharge cycling. The S-Radel membrane had different degradation behaviors in flow cell cycling and ex-situ vanadium ion immersion tests. The S-Radel membrane immersed in V5+ solution cracked into small pieces, but in the VRFB cell, the membrane underwent internal delamination preferentially on the side of the membrane that faced the positive electrode. A vanadium-rich interface was observed near the membrane surface that experienced delamination and Raman spectroscopic analysis of the surfaces of the membrane indicated a slightly depressed 1026 cm-1 band corresponding to the sulfonate SO2 stretch for the degraded surface. Even though the S-Radel membrane underwent severe mechanical damage during the flow cell cycling, significant chemical degradation was not obvious from the spectroscopic analyses. For the VRFB containing an S-Radel membrane, an increase in membrane resistance caused an abnormal voltage depression during the discharge cycle. The reversible increase in membrane resistance and severe mechanical degradation of the membrane during cycling may be attributed repeated formation and dissolution of particles inside the membrane. The mechanical stresses imposed by the particles coupled with a small amount of chemical degradation of the polymer by V5+, are likely degradation mechanisms of the S-Radel membrane in VRFBs under high state-of-charge conditions.

25 ENERGY STORAGE↗

Polysaccharide degradation systems of the saprophytic bacterium Cellvibrio japonicus

Study of recalcitrant polysaccharide degradation by bacterial systems is critical for understanding biological processes such as global carbon cycling, nutritional contributions of the human gut microbiome, and the production of renewable fuels and chemicals. One bacterium that has a robust ability to degrade polysaccharides is the Gram-negative saprophyte Cellvibrio japonicus . A bacterium with a circuitous history, C. japonicus underwent several taxonomy changes from an initially described Pseudomonas sp. Most of the enzymes described in the pre-genomics era have also been renamed. Furthermore, this review aims to consolidate the biochemical, structural, and genetic data published on C. japonicus and its remarkable ability to degrade cellulose, xylan, and pectin substrates. Initially, C. japonicus carbohydrate-active enzymes were studied biochemically and structurally for their novel polysaccharide binding and degradation characteristics, while more recent systems biology approaches have begun to unravel the complex regulation required for lignocellulose degradation in an environmental context. Also included is a discussion for the future of C. japonicus as a model system, with emphasis on current areas unexplored in terms of polysaccharide degradation and emerging directions for C. japonicus in both environmental and biotechnological applications.

59 BASIC BIOLOGICAL SCIENCES↗

Performance degradation in proton-conducting ceramic fuel cell and electrolyzer stacks

Proton-conducting ceramics are emerging as enabling materials for efficient electrochemical electricity generation, energy storage, and fuels synthesis. In this work, we present longer-term degradation results for protonic-ceramic fuel cells and electrolyzers based on a BaCe 0.4 Zr 0.4 Y 0.1 Yb 0.1 O 3-δ (BCZYYb) electrolyte. The cells are packaged within unit-cell stacks, including metallic interconnects, current collectors, sealing glasses and gaskets. Durability is found to be superior in protonic-ceramic electrolyzers in comparison to fuel cells. Operating conditions have a large impact on degradation rates; better stability is found at fuel-cell operating temperatures above 600 °C, and electrolyzer steam feeds below 20%. Here, we find that both fuel-cell and electrolyzer degradation is greatly reduced via the introduction of a gadolinium-doped ceria interlayer between the electrolyte and the air–steam electrode. Fuel-cell degradation falls to 1.2% khr –1 under methane fuel at 600 °C; electrolyzer degradation is reduced to 1% khr –1 at 550 °C and 50% steam. Further analyses of electrochemical impedance spectroscopy and distribution of relaxation times provide insight to root processes and degradation phenomena in protonic electroceramics.

25 ENERGY STORAGE↗

Differential degradation patterns of photovoltaic backsheets at the array level

There are relatively few field studies on the degradation of non-fluoropolymer-based backsheets, and understanding their in-field behavior is critical for further development of such products. In this paper, backsheet degradation of modules with one of these new types of backsheets (polyethylene naphthalate (PEN)-based) was documented at a four-year old utility-scale array located in Maryland (USA). Visual inspection, colorimetry, glossimetry, and Fourier-transform infrared spectroscopy (FTIR) revealed highly varied properties depending on module position within the array. Specifically, modules near the edge of the array and with higher mounting elevations underwent greater amounts of backsheet degradation, as indicated by yellowing and gloss-loss. The reason for these unique degradation patterns were differential backside exposure conditions, especially of ultraviolet light. This was strongly influenced by the array design, including array structural and environmental factors, such as module spacing and ground cover, respectively. Within the array, no clear link between backsheet degradation and module output or safety has been identified. However, such a relationship may be expected to become more pronounced with time, affecting system lifetime and ultimately the levelized cost of electricity (LCOE). Finally, the observed phenomena have implications for both backsheet product development and array design, especially for modules that utilize newer classes of non-fluoropolymer-based backsheets which are typically more susceptible to environmental degradation.

14 SOLAR ENERGY↗

Evaluation of clear-sky and satellite-derived irradiance data for determining the degradation of photovoltaic system performance

Knowing the degradation in performance of a photovoltaic (PV) system over time is important for estimating the lifetime energy produced and the financial return. A key parameter for normalizing performance and determining degradation is the plane-of-array (POA) irradiance. Because accurate long-term POA measurements are not always readily available, three methods of providing irradiance data for determining the degradation rate of PV systems were evaluated—a method using irradiance data modeled with the Ineichen clear-sky model and monthly Linke turbidity coefficients, a method using the supplemental clear-sky irradiance data from the National Solar Radiation Data Base (NSRDB), and a method using the NSRDB solar irradiance data for both cloudy and clear-sky conditions (all-sky). The irradiance data from the three methods were evaluated using measured irradiance data from 1998 through 2018 for the seven-station SURFRAD network and for 3-, 5-, and 10-year periods that might be used for evaluating PV system performance. Only the two clear-sky methods for the 10-year periods had less uncertainty with respect to determining PV system degradation than the expected median degradation rate for PV systems of -0.5%/year to -0.6%/year. Shorter periods and the all-sky method had larger uncertainties, making their use questionable for determining the degradation rates of PV systems.

14 SOLAR ENERGY↗

Degradation mechanisms and partial shading of glass-backsheet and double-glass photovoltaic modules in three climate zones determined by remote monitoring of time-series current–voltage and power datastreams

Degradation and partial shading impact the long-term reliability and power production of photovoltaic (PV) modules and power plants. Time-series power (P mp ) and current–voltage (I-V) curve datastreams from PV modules enable a remote diagnostic approach to quantify active degradation mechanisms and identify partial shading. We study three to nine years of these datastreams, including 3.6 million P mp I-V curves and 36 million values, from eight PV modules, four each of double-glass and glass-backsheet module architectures, located in three distinctly different Köppen-Geiger climate zones, to determine the module’s performance loss rates (PLR), identify active degradation mechanisms and power loss modes, along with partial shading by local objects. Considering both module architectures, PLR results indicate that the BSh climate zone is the most aggressive for module degradation, while the Alpine ET zone is the mildest climate. PLR of double-glass modules located in BWh and BSh climate zones are different due to the significantly greater uniform current loss (ΔP Isc ) for double-glass modules in BSh, at a 5% significance level. Power loss for four out of five modules located in the BWh and BSh climates are dominated by uniform current degradation. Statistical analysis of multistep I-V curves detects partial shading experienced by three studied modules with details of the shading profile, the shading Poynting vector diagram for the obstacle’s relative position, shading scenarios, and duration. Lastly, this work demonstrates how remote monitoring and diagnosis of P mp & I-V time-series of modules can provide quantitative operations and maintenance insights into system performance, degradation mechanisms, and shading.

14 SOLAR ENERGY↗

Dependence of adhesion on degradation mechanisms of ethylene co-vinyl acetate encapsulants over the lifetime of photovoltaic modules

The long-term reliability of encapsulation has a critical impact on the overall cost and effectiveness of photovoltaic modules. An often overlooked but important element of this reliability concerns adhesive degradation of the encapsulant, which results in delamination. This work critically examines the degradation mechanisms – deacetylation, β-scission, and hydrolytic depolymerization – primarily responsible for adhesion loss in ethylene co-vinyl acetate (EVA) encapsulants to provide evidence and clarity regarding the contribution of these mechanisms to the adhesive degradation over the lifetime of a module. EVA samples obtained from mini-modules exposed in two sets of controlled, accelerated conditions – with and without ultraviolet (UV) radiation – are characterized to find specific evidence for the proposed degradation mechanisms. The mini-modules were exposed up to 10,000 h, which represents up to 15–20 years in the field. Results affirm that initially, deacetylation dominates the degradation before scission takes over, followed by hydrolytic depolymerization. Additional analysis highlights the climacteric interdependency between deacetylation and hydrolytic depolymerization as it relates to eventual delamination, where deacetylation products catalyze interfacial hydrolysis reactions. Furthermore, effects occurring at a given interface are isolated, explicitly providing evidence for how these mechanisms are nonuniform throughout the thickness of the EVA. Results demonstrate that the EVA that interfaces with the glass as opposed to the cell experiences increased levels of degradation, explaining why this initially stronger interface becomes the preferential interface for delamination after longer periods of exposure. Additionally, elevated temperatures alone are shown to induce limited migration of sodium ions across the glass/EVA interface.

36 MATERIALS SCIENCE↗

Composition and Structure of Fluorescent Graphene Quantum Dots Generated by Enzymatic Degradation of Graphene Oxide

The broad applications of carbon nanomaterials (CNMs) in both materials and life sciences necessitate investigation of their metabolites due to the inevitable contact of CNMs and biological systems. Graphene oxide (GO), along with other types of CNMs, can be enzymatically degraded by myeloperoxidase (MPO), an enzyme released during the innate immune response. However, the enzymatic degradation products are neither well-defined nor well-understood. Some products generated during MPO-catalyzed degradation of GO could emit blue photoluminescence (PL) and were simply dubbed graphene quantum dots (GQDs) without further elucidating their structures. In this work, we use liquid chromatography-mass spectrometry (LC-MS) to isolate and elucidate chemical structures of the MPO-catalyzed degradation products. A general chemical formula screening workflow was developed for the GQDs, which are in the form of polyaromatic hydrocarbons (PAHs), obtained in the degradation products. Structures of the PAHs responsible for the blue PL were further proposed using density functional theory (DFT) calculations. Our results indicated that structures with several conjugated benzene rings are likely to generate the observed PL. This work provides insights into the mechanism of enzymatic degradation and open opportunities for fluorescence imaging of GO in biological systems.

composition and structure screening↗

From Femtoseconds to Gigaseconds: The SolDeg Platform for the Performance Degradation Analysis of Silicon Heterojunction Solar Cells

Heterojunction Si solar cells exhibit notable performance degradation. Here, we modeled this degradation by electronic defects getting generated by thermal activation across energy barriers over time. To analyze the physics of this degradation, we developed the SolDeg platform to simulate the dynamics of electronic defect generation. First, femtosecond molecular dynamics simulations were performed to create a-Si/c-Si stacks, using the machine learning-based Gaussian approximation potential. Second, we created shocked clusters by a cluster blaster method. Third, the shocked clusters were analyzed to identify which of them supported electronic defects. Fourth, the distribution of energy barriers that control the generation of these electronic defects was determined. Fifth, an accelerated Monte Carlo method was developed to simulate the thermally activated time-dependent defect generation across the barriers. Our main conclusions are as follows. (1) The degradation of a-Si/c-Si heterojunction solar cells via defect generation is controlled by a broad distribution of energy barriers. (2) We developed the SolDeg platform to track the microscopic dynamics of defect generation across this wide barrier distribution and determined the time-dependent defect density N(t) from femtoseconds to gigaseconds, over 24 orders of magnitude in time. (3) We have shown that a stretched exponential analytical form can successfully describe the defect generation N(t) over at least 10 orders of magnitude in time. (4) We found that in relative terms, Voc degrades at a rate of 0.2%/year over the first year, slowing with advancing time. (5) We developed the time correspondence curve to calibrate and validate the accelerated testing of solar cells. We found a compellingly simple scaling relationship between accelerated and normal times t normal ∝ t accel T(accel)/T(normal) . (6) We also carried out experimental studies of defect generation in a-Si:H/c-Si stacks. We found a relatively high degradation rate at early times that slowed considerably at longer time scales.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemical Characterization of Degradation Modes of High-Voltage Li x Ni 0.33 Mn 0.33 Co 0.33 O 2 Electrodes

While deeply charged high-voltage cathodes can improve battery energy density, understanding and preventing any accelerated cell degradation is crucial to practical success. Here, to analyze the degradation of LiNi x Mn y Co 1–x–y O 2 (NMC) type material charged to 4.3 and 4.5 V, a physics-based model is applied to cycling data to obtain parameter estimates indicative of degradation modes, which are validated by simple electrochemical measurements and further interpreted by materials characterization. Growth rates of interfacial impedance and active material loss are greater at 4.5 V, as might be expected. However, when charged to 4.5 V, degradation rates are initially lower at a cycling C-rate of 1.0 C than at 0.5 C. Once degradation mode changes are quantified, simulations evaluate the contribution of individual degradation mode to performance losses and provide estimates of the energy-power correlation (Ragone plots) of cells after cycling.

25 ENERGY STORAGE↗

Degradation Dynamics of Perovskite Solar Cells Under Fixed Reverse-Current Injection

Previous studies of reverse-bias stability in perovskite solar cells have focused primarily on voltage-controlled tests. Here we instead investigate perovskite solar cell degradation under well-defined, constant reverse-current stress. We show that the choice of hole-transport layer dictates the dominant degradation pathway: cells using thick poly(triphenylamine) (PTAA) layers can tolerate high reverse bias but quickly undergo catastrophic breakdown under fixed reverse current near their one-sun maximum power-point. In contrast, cells modified with phosphonic-acid interface layer MeO-2PACz, with poorer indium-doped tin oxide (ITO) coverage compared to PTAA, exhibit gradual and recoverable degradation under certain stress and recovery conditions. For MeO-2PACz devices, degradation increases with both current magnitude and duration. Importantly, when normalized by injected charge (current times duration), lower currents applied over longer times cause more degradation than higher currents over shorter periods. Here, combining electrical measurements with spatially resolved photoluminescence imaging, our observations support an ion- and charge-mediated interfacial electrochemical degradation mode.

Degradation↗

Cell degradation of a Na–NiCl 2 (ZEBRA) battery

In this work, the parameters influencing the degradation of a Na-NiCl 2 (ZEBRA) battery were investigated. Planar Na-NiCl 2 cells using β”-alumina solid electrolyte (BASE) were tested with different C-rates, Ni/NaCl ratios, and capacity windows, in order to identify the key parameters for the degradation of Na-NiCl 2 battery. The morphology of NaCl and Ni particles were extensively investigated after 60 cycles under various test conditions using a scanning electron microscope. A strong correlation between the particle size (NaCl and Ni) and battery degradation was observed in this work. Even though the growth of both Ni and NaCl can influence the cell degradation, our results indicate that the growth of NaCl is a dominant factor in cell degradation. The use of excess Ni seems to play a role in tolerating the negative effects of particle growth on degradation since the available active surface area of Ni particles can be still sufficient even after particle growth. For NaCl, a large cycling window was the most significant factor, of which effects were amplified with decrease in Ni/NaCl ratio.

25 ENERGY STORAGE↗

Reducing Interanalyst Variability in Photovoltaic Degradation Rate Assessments

The economic return on investment of a commercial photovoltaic system depends greatly on its performance over the long term and, hence, its degradation rate. Many methods have been proposed for assessing system degradation rates from outdoor performance data. However, comparing reported values from one analyst and research group to another requires a common baseline of performance; consistency between methods and analysts can be a challenge. An interlaboratory study was conducted involving different volunteer analysts reporting on the same photovoltaic performance data using different methodologies. Initial variability of the reported degradation rates was so high that analysts could not come to a consensus whether a system degraded or not. More consistent values are received when written guidance is provided to each analyst. Further improvements in analyst variance was accomplished by using the free open-source software RdTools, allowing a reduction in variance between analysts by more than two orders of magnitude over the first round, where multiple analysis methods are allowed. This article highlights many pitfalls in conducting 'routine' degradation analysis, and it addresses some of the factors that must be considered when comparing degradation results reported by different analysts or methods.

14 SOLAR ENERGY↗