Spall and re-compaction in OFHC copper under high velocity impact
Copper spall and re-compaction experiments were performed with a single stage large bore (76.2 mm) light gas gun capable of planar impacts at low impact velocity. The experiments used PDV to capture the velocity history of the back surface of the target and the projectile velocity (collimating probes). The tilts for these experiments typically range from 1–2 mrad. A re-compaction wave was clearly observed using Photon Doppler Velocimetry (PDV) on the back surface of the copper target as well as identified using Electron Backscatter Diffraction (EBSD) in the recovered samples. The spall and re-compaction data are similar until re-compaction occurs; the time-resolved data show clear evidence for spall damage in the first case and spall followed by re-compaction in the second case. For the initial spall signature, ringing consistent with half the thickness of the target is observed in all cases; after re-compaction, ringing is observed that is consistent with the full sample thickness. Samples recovered using the soft catch system were analyzed, and the cross-sectional view from the spalled target clearly showed a spall plane with voids, whereas the re-compaction target showed an area of plastic deformation. It is hypothesized that the voids formed by spall close during re-compaction and leave behind a deformed area.