At least 379 records · Page 21

Salt-Assisted Solution Combustion Synthesis of Ni and Ni/NiO Powders

In this work, Ni and Ni/NiO composite powders were synthesized by one-pot solution combustion method using different fuel to oxidant (φ) ratios (φ = 1, 1.25, 1.5, and 1.75). Phase evolution studied by X-ray diffraction (XRD) method showed that single phase Ni powders were formed at high fuel contents, while the low fuel contents led to the formation of Ni/NiO composite powders. The high combustion temperature resulted in the sintered and large Ni particles (1.1 μm). The particle size decreased up to 50 nm by adding KCl as diluent. However, the amount of NiO phase increased by addition of KCl. The saturation magnetization (Ms) of Ni powders decreased from 51 to 42 emu/g with the increase of φ values from 1.25 to 1.75. The Ms decreased up to 18.5 emu/g, due to the formation of a large amount of NiO phase by addition of KCl. The coercivity of the synthesized powders was in the range of 78 to 111 Oe, as a function of particle size.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

High fidelity model of directed energy deposition: Laser-powder-melt pool interaction and effect of laser beam profile on solidification microstructure

Metal additive manufacturing technologies keep receiving a great deal of interest as well as strong requests to develop methods to link the process science to printed parts performance and understand how to overcome inherent limitations. Here, a high-fidelity model based on the multiphysics ALE3D code was developed to reproduce the directed energy deposition process down to the powder scale. This includes resolving the laser-powder-melt pool interactions (powder impingement and incorporation into melt pool, hydrodynamics flow condition and laser absorption inefficiencies) as well as the resulting solidification microstructure. This micrometer scale digital twin captured the effect of powder incorporation process and powder flow rate on porosity. Furthermore, it was used to explore how a ring laser beam profile instead of the standard Gaussian laser profile could decrease the thermal gradient along the solidification front in the melt pool, which in turn can increase propensity for more desirable equiaxed grains.

36 MATERIALS SCIENCE↗

Ultrasmall-angle x-ray scattering (USAXS) studies of morphological trends in high energy milled NaA1H(sub 4) powders.

Transition metal dopants added to complex metal hydrides, specifically to sodium aluminum hydride (NaAlH{sub 4}), by high energy ball milling enhances dehydrogenation kinetics and induces dehydrogenation reaction reversibility. This study uses the power-law scattering parameter, p, gained from ultrasmall-angle X-ray scattering (USAXS) data to elucidate differences in NaAlH{sub 4} particle morphology as dopant type and mill time is varied. Four dopant types were used. Two dopant types were used to represent the best kinetic enhancements having high desorption rates (e.g. TiCl{sub 2}, TiCl{sub 3}) and were compared with two dopant types which do not perform as well (e.g. ZrCl{sub 3} and VCl{sub 3}). USAXS data for the doped hydrides were compared with undoped and milled NaAlH{sub 4} powders. Mill times used were 0 min (blended), 1, 5, and 25 min. As indicated by the USAXS power-law scattering data, the undoped NaAlH{sub 4} powders are comprised of primary particles each having a high surface area. The high particle surface area in the undoped NaAlH{sub 4} particle system persists as mill time increases - with only the 25 min sample undergoing a marked a decrease in primary particle surface area. Alternatively, the doped powders milled for 1, 5, and 25 min show uniformly decreasing hydride particle surface area. These decreases in particle surface area may be explained by either the colloidal particles increasing in surface smoothness or decreasing internal void space. TiCl{sub 3}-doped NaAlH{sub 4} powders show the trend of maintaining particles having a morphology comprised of higher particle surface area during the high energy milling stage of powder processing compared with other dopants.

36 MATERIALS SCIENCE↗

Hybrid additive manufacturing of AISI 316L via asynchronous powder and hot-wire laser directed energy deposition

Hybrid Additive Manufacturing (AM) offers a way to leverage the advantages of different AM technologies, enabling the efficient production of sizeable parts without compromising material properties or geometric complexity capabilities. This study presents an asynchronous hybrid Directed Energy Deposition (DED) strategy employing laser powder DED and laser hot-wire DED. AISI 316L parts comprising multiple powder and wire segments were fabricated with optional machining on AISI 316L substrates to investigate how quality is impacted by (i) alternative process sequences (laser powder DED followed by laser hot-wire DED and vice versa), (ii) machined vs. as-printed interfacial conditions, and (iii) material deposition on top vs. alongside previously built segments. Optical microscopy, X-ray computed tomography, and Vickers hardness were used to characterize the morphology and microstructure of the parts, localized porosity and lack of fusion defects, bulk density, and mechanical properties. Interfacial machining was necessary for dimensional control but promoted lack of fusion voids, resulting in a 99.71 ± 0.01% dense part. As-printed interfaces resulted in a denser part (99.82 ± 0.02%) at the expense of dimensional accuracy. The hardness of the parts with as-printed and machined interfaces was 196 ± 0.37 HV and 192 ± 0.40 HV, respectively, compared to 156 ± 1.4 HV for the substrate. Depositing powder alongside or on top of wire sections resulted in interfaces with a hardness of 217 ± 2.2 HV, compared to 185 ± 3.4 HV for the wire-powder interfaces.

36 MATERIALS SCIENCE↗

Removal of deuterium retained in boron powder by oxygen or high-temperature bakeout

Fuel retention in dust accumulated in fusion devices is a potential operational hazard. Boronization is one of the leading wall-conditioning candidates for future fusion devices. Fuel retention characteristics of boron dust must be studied to accurately understand the potential hazards of boron dust in fusion devices. We evaluated the retention of deuterium (D) in commercially available boron powder as a proxy for tritium retention in boron dust. Diffuse reflectance infrared Fourier transform spectroscopy revealed that boron powder between 300 and 500 K exposed to neutral hydrogen (H 2 ) gas retains H via B-H bonding. We utilized D 2 exposures of 17,400 L on the boron powder, which led to retention on the order of 0.5 g D per 100 kg B or 1.2 g D per m 2 B, as estimated from temperature programmed desorption measurements. We evaluated how powder bakeouts under ultra-high vacuum (UHV), or in an oxygen (O 2 ) or H 2 gas backfilled environment can remove the retained fuel. Bakeouts below 523 K under UHV exhibited poor D removal, promoting recapture of D 2 present as background gas in the chamber. Higher temperature bakeouts led to the removal of over 80% of the retained D within 3 days (623 K) or 1 h (723 K). Bakeouts at 423 K under an O 2 gas environment removed ∼150% more retained D from the boron powder, when compared to bakeouts conducted under UHV. These results suggest that efficient fuel removal from boron dust can be achieved by high-temperature bakeout (>623 K) or by bakeouts at lower temperature (423 K) under an O 2 environment.

Bakeout↗

Isothermal nitridation kinetics of TiSi{sub 2} powders

The aim of the present work is to determine the kinetics of reaction between TiSi{sub 2} powder and gaseous nitrogen. Isothermal nitridation of TiSi{sub 2} powders with fine (1.4 µm) and medium (4.5 µm) particle size has been studied in pure nitrogen atmosphere from 1000 to 1200 °C for duration up to 50 h. The isothermal nitridation kinetics of TiSi{sub 2} powders were investigated by thermogravimetry. The nitridation rate strongly depends on the particle size and temperature. Smaller size particle exhibits higher nitridation rate due to its larger surface area. The conversion process is complex with nucleation and growth of TiN at the surface of the grain and Si{sub 3}N{sub 4} inside the grain promoted by the Kirkendall effect with an influence of the volume increase. - Graphical abstract: Backscattered electrons image of a transverse TiSi{sub 2} grain nitrurated at 1100 °C for 50 h. - Highlights: • Influence of grain size on TiSi{sub 2} powder nitridation. • Influence of temperature on TiSi{sub 2} powder nitridation. • Experimental measurements of the nitridation kinetics. • An explanation of the nitridation mechanism.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructure and nanoindentation analysis of Mg-SiC nanocomposite powders synthesized by mechanical milling

Highlights: • Mechanical milling as an effective solution to reach a homogeneous distribution of SiC nanoparticles up to 10 vol% in Mg matrix • No deformation twinning in the nanostructured Mg matrix even after the severe plastic deformation and hard SiC nanoparticles up to 10 vol%. • Significant enhancement of nanohardness and reduced elastic modulus in the milled nanocomposite powders - Abstract: Mixtures of magnesium powder and SiC nanoparticles at various volume fractions were mechanically milled to produce nanocrystalline Mg-SiC nanocomposites. X-ray diffraction (XRD), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were utilized to characterize the microstructure of the milled powders. The microstructural evidences revealed that mechanical milling is a proper method to achieve a uniform distribution of the SiC nanoparticles, even up to 10% in the Mg matrix. Based on the results, higher volume fraction of the SiC nanoparticles raise the value of measured microstrain and reduce the crystallite size of the Mg matrix. The TEM results pointed to the fact that no deformation twinning takes place in the nanostructured Mg matrix even after severe plastic deformation through mechanical milling and the presence of hard SiC nanoparticles up to 10 vol%. The effects of nanoparticle volume fraction on mechanical properties of the milled Mg-SiC nanocomposites were evaluated using nanoindentation tests. The results clearly showed a significant enhancement of nanohardness and reduced elastic modulus in the milled powders compared to that of the reference material namely as-received pure magnesium. It was found that the SiC nanoparticles (even up to 10 vol%), well distributed in the magnesium matrix, remarkably improve the reduced elastic modulus and nanohardness of the nanocomposite powders.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Preparation and dielectric properties of B-doped SiC powders by combustion synthesis

The SiC(B) solid solution powders were synthesized via combustion reaction of Si/C system in Ar atmosphere, using boron powder as the dopant and polytetrafluoroethylene as the chemical activator, which were investigated by X-ray diffraction (XRD), scanning electronic microscope (SEM) and Raman spectra. Results show that the prepared powders are C-enriched SiC with C antisites and sp{sup 2} carbon defects in which the sp{sup 2} carbon is transformed to the sp{sup 3} carbon due to boron doping. The electric permittivities of the prepared powders were determined in the frequency range of 8.2-12.4 GHz. The dielectric real part {epsilon}' and dielectric loss tan {delta} of undoped powder have maximum values ({epsilon}' = 5.5-5.3, tan {delta} = 0.23-0.20), and decrease with increasing boron content. The mechanism of dielectric loss by doping has been discussed.

36 MATERIALS SCIENCE↗

Process and feedstock driven microstructure for laser powder bed fusion of 316L stainless steel

Here in the pursuit of improving additively manufactured (AM) component quality and reliability, fine-tuning critical process parameters such as laser power and scan speed is a great first step toward limiting defect formation and optimizing the microstructure. However, the synergistic effects between these process parameters, layer thickness, and feedstock attributes (e.g. powder size distribution) on part characteristics such as microstructure, density, hardness, and surface roughness are not as well-studied. In this work, we investigate 316L stainless steel density cubes built via laser powder bed fusion (L-PBF), emphasizing the significant microstructural changes that occur due to altering the volumetric energy density (VED) via laser power, scan speed, and layer thickness changes, coupled with different starting powder size distributions. This study demonstrates that there is not one ideal process set and powder size distribution for each machine. Instead, there are several combinations or feedstock/process parameter ‘recipes’ to achieve similar goals. This study also establishes that for equivalent VEDs, changing powder size can significantly alter part density, GND density, and hardness. Through proper parameter and feedstock control, part attributes such as density, grain size, texture, dislocation density, hardness, and surface roughness can be customized, thereby creating multiple high-performance regions in the AM process space.

316L stainless steel↗

Heisenberg model analysis on inelastic powder neutron scattering data using parent and K doped BaMn 2 As 2 samples

Low temperature powder inelastic neutron scattering measurements were performed on three different powder samples; parent BaMn 2 As 2 ,12.5% K-doped Ba 0.875 K 0.125 Mn 2 As 2 and 25% K-doped Ba (0.75) K 0.25 Mn 2 As 2 . The Heisenberg Model involving J 1 -J 2 -J z coupling constants were compared to the data by a powder integration routine using Monte Carlo integration methods. The best magnetic parameters were selected using a chi-square test where model intensities were compared to the full (q,E) dependence of magnetic scattering. A key step to this analysis is the characterization of the background which is formed mostly by phonon scattering intensities along with other sources including the magnetic impurity scattering events. The calculated powder magnetic intensities added to the estimated background obtained from the non-magnetic high momentum transfer region. The agreement between the simulated and the raw data enabled us to perform quantitative analysis of the unreacted MnO impurities. Overall, this is another confirmation along with earlier studies using this technique, that magnetic exchange constants can be calculated within an acceptable range with a very quick inelastic neutron powder experiment without need for a single crystal sample.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Cold compaction study of Armstrong Process Ti-6Al-4V powders

This work investigates the cold compaction behavior of Ti-6Al-4V powders produced by Armstrong Process . As-received as well as milled powders were characterized and these powders were uniaxially die-pressed at designated pressures up to 690 MPa to form disk samples with different aspect ratios. Samples with high aspect ratio exhibited non-uniform density along the pressing axis and the density distribution is in consistent with the result predicted by finite element analysis. The linear regression analysis on the experimental density data can be used to predict density of compacts with different aspect ratios. In the studied pressure range, an empirical powder compaction equation represents the green density pressure relationship very well for both the as-received and 1-hr milled Armstrong Ti-6Al-4V powders.

99 GENERAL AND MISCELLANEOUS↗

Commercial aluminum powders, Part I: Particle size characterization and slow heating rate thermal analysis.

We characterized nine commercial aluminum (Al) powders using several methods to measure particle characteristics and thermal analysis, with the goal to understand how these parameters influence energy release. Although it is well-known that lot-to-lot variations in commercial nanoparticles are common, the Al powders were more heterogeneous than anticipated – both with regards to particle size distributions and impurities. Manufacturer specifications – often quoted in the literature without confirmation – were not always accurate for the specific sample lots we investigated. In several cases, different conclusions could be drawn from individual particle size techniques; a combination of multiple techniques provides a clearer picture of the powder properties. Thorough characterization of Al powders is required prior to interpretation of experimental results from a variety of applications. In particular, previous studies have shown contradictory results on the influence of Al on detonation performance, perhaps partially due to insufficient characterization of the Al powders themselves.

36 MATERIALS SCIENCE↗

Recovery of yttrium from fluorescent powder of cathode ray tube, CRT: Zn removal by sulphide precipitation

Highlights: • Treatment of fluorescent powder of CRT waste. • Factorial experimental designs to study acid leaching of fluorescent powder and the purification of leach liquors. • Recover of yttrium by precipitation using oxalic acid. • Suitable flowsheet to recover yttrium from fluorescent powder. - Abstract: This work is focused on the recovery of yttrium and zinc from fluorescent powder of cathode ray tube (CRT). Metals are extracted by sulphuric acid in the presence of hydrogen peroxide. Leaching tests are carried out according to a 2{sup 2} full factorial plan and the highest extraction yields for yttrium and zinc equal to 100% are observed under the following conditions: 3 M of sulphuric acid, 10% v/v of H{sub 2}O{sub 2} concentrated solution at 30% v/v, 10% w/w pulp density, 70 °C and 3 h of reaction. Two series of precipitation tests for zinc are carried out: a 2{sup 2} full factorial design and a completely randomized factorial design. In these series the factors investigated are pH of solution during the precipitation and the amount of sodium sulphide added to precipitate zinc sulphide. The data of these tests are used to describe two empirical mathematical models for zinc and yttrium precipitation yields by regression analysis. The highest precipitation yields for zinc are obtained under the following conditions: pH equal to 2–2.5% and 10–12% v/v of Na{sub 2}S concentrated solution at 10% w/v. In these conditions the coprecipitation of yttrium is of 15–20%. Finally further yttrium precipitation experiments by oxalic acid on the residual solutions, after removing of zinc, show that yttrium could be recovered and calcined to obtain the final product as yttrium oxide. The achieved results allow to propose a CRT recycling process based on leaching of fluorescent powder from cathode ray tube and recovery of yttrium oxide after removing of zinc by precipitation. The final recovery of yttrium is 75–80%.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Quantification of Thermal Oxidation in Metallic Glass Powder using Ultra-small Angle X-ray Scattering

In this paper, the composition, structure, morphology and kinetics of evolution during isothermal oxidation of Fe 48 Cr 15 Mo 14 Y 2 C 15 B 6 metallic glass powder in the supercooled region are investigated by an integrated ex-situ and in-situ characterization and modelling approach. Raman and X-ray diffraction spectra established that oxidation yielded a hierarchical structure across decreasing length scales. At larger scale, Fe 2 O 3 grows as a uniform shell over the powder core. This shell, at smaller scale, consists of multiple grains. Ultra-small angle X-ray scattering intensity acquired during isothermal oxidation of the powder over a wide Q-range delineated direct quantification of oxidation behavior. The hierarchical structure was employed to construct a scattering model that was fitted to the measured intensity distributions to estimate the thickness of the oxide shell. The relative gain in mass during oxidation, computed theoretically from this model, relatively underestimated that measured in practice by a thermogravimetric analyzer due to the distribution in sizes of the particles. As a whole, this paper introduces the first direct quantification of oxidation in metallic glass powder by ultra-small angle X-ray scattering. It establishes novel experimental environments that can potentially unfold new paradigms of research into a wide spectrum of interfacial reactions in powder materials at elevated temperatures.

42 ENGINEERING↗

Additive manufacturing of defect-free TiZrNbTa refractory high-entropy alloy with enhanced elastic isotropy via in-situ alloying of elemental powders

Laser powder-bed fusion (L-PBF) additive manufacturing presents ample opportunities to produce net-shape parts. The complex laser-powder interactions result in high cooling rates that often lead to unique microstructures and excellent mechanical properties. Refractory high-entropy alloys show great potential for high-temperature applications but are notoriously difficult to process by additive processes due to their sensitivity to cracking and defects, such as un-melted powders and keyholes. Here, we present a method based on a normalized model-based processing diagram to achieve a nearly defect-free TiZrNbTa alloy via in-situ alloying of elemental powders during L-PBF. Compared to its as-cast counterpart, the as-printed TiZrNbTa exhibits comparable mechanical properties but with enhanced elastic isotropy. This method has good potential for other refractory alloy systems based on in-situ alloying of elemental powders, thereby creating new opportunities to rapidly expand the collection of processable refractory materials via L-PBF.

36 MATERIALS SCIENCE↗

Powder diffraction

Powder diffraction is a non-destructive technique, which is experimentally simple in principle. Because the physics behind diffraction is well understood, an exceptionally large amount of information can be obtained from a single measurement. The positions and relative intensities of the peaks yield a fingerprint that can be used for qualitative phase analysis. Quantitative phase analysis can be obtained by detailed analysis of the intensities. Unit cells can be derived from the peak positions. Crystal structures can be solved using powder diffraction data and refined by the Rietveld method. The peak profiles contain information about crystallite size, strain and nanostructure. Non-idealities in the intensities give information on texture. Abandoning the crystallographic model provides information about local structure, by pair distribution function analysis. For powder diffraction, everything is a sample; the technique is commonly applied to characterize minerals, ceramics, metals and alloys, catalysts, polymers, pharmaceuticals, organic compounds, environmental and forensic samples, among others. The major features of contemporary laboratory powder diffractometers are described. Methods for obtaining suitable powder specimens are summarized. Major applications of qualitative and quantitative phase analysis, structure solution, size/strain/nanostructure analysis using peak profiles, texture analysis and pair distribution function analysis are introduced.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of photocatalytic TiO 2 powder under varied environments using near ambient pressure X-ray photoelectron spectroscopy

Consecutive eight study phases under the successive presence and absence of UV irradiation, water vapor, and oxygen were conducted to characterize surface changes in the photocatalytic TiO2 powder using near-ambient-pressure X-ray photoelectron spectroscopy (XPS). Both Ti 2p and O 1s spectra show hysteresis through the experimental course. Under all the study environments, the bridging hydroxyl (OH br ) and terminal hydroxyl (OH t ) are identified at 1.1–1.3 eV and 2.1–2.3 eV above lattice oxygen, respectively. This enables novel and complementary approach to characterize reactivity of TiO 2 powder. The dynamic behavior of surface-bound water molecules under each study environment is identified, while maintaining a constant distance of 1.3 eV from the position of water vapor. In the dark, the continual supply of both water vapor and oxygen is the key factor retaining the activated state of the TiO 2 powder for a time period. Two new surface peaks at 1.7–1.8 and 4.0–4.2 eV above lattice oxygen are designated as peroxides (OOH/H 2 O 2 ) and H 2 O 2 dissolved in water, respectively. The persistent peroxides on the powder further explain previously observed prolonged oxidation capability of TiO 2 powder without light irradiation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Pulsed Neutron Powder Diffraction for Materials Science

The accelerator-based neutron diffraction began in the end of 60's at Tohoku University which was succeeded by the four spallation neutron facilities with proton accelerators at the High Energy Accelerator Research Organization (Japan), Argonne National Laboratory and Los Alamos Laboratory (USA), and Rutherford Appleton Laboratory (UK). Since then, the next generation source has been pursued for 20 years, and 1MW-class spallation neutron sources will be appeared in about three years at the three parts of the world: Japan, UK and USA. The joint proton accelerator project (J-PARC), a collaborative project between KEK and JAEA, is one of them. The aim of the talk is to describe about J-PARC and the neutron diffractometers being installed at the materials and life science facility of J-PARC. The materials and life science facility of J-PARC has 23 neutron beam ports and will start delivering the first neutron beam of 25 Hz from 2008 May. Until now, more than 20 proposals have been reviewed by the review committee, and accepted proposal groups have started to get fund. Those proposals include five polycrystalline diffractometers: a super high resolution powder diffractometer (SHRPD), a 0.2%-resolution powder diffractometer of Ibaraki prefecture (IPD), an engineering diffractometers (Takumi), a high intensity S(Q) diffractometer (VSD), and a high-pressure dedicated diffractometer. SHRPD, Takumi and IPD are being designed and constructed by the joint team of KEK, JAEA and Ibaraki University, whose member are originally from the KEK powder group. These three instruments are expected to start in 2008. VSD is a super high intensity diffractometer with the highest resolution of {delta}d/d = 0.3%. VSD can measure rapid time-dependent phenomena of crystalline materials as well as glass, liquid and amorphous materials. The pair distribution function will be routinely obtained by the Fourier transiformation of S(Q) data. Q range of VSD will be as wide as 0.01 A{sup -1}<Q<100 A{sup -1}. IPD is fully funded by Ibaraki prefecture for the promotion of new industries based on advanced science and technologies. It is for the first time in neutron facilities in Japan that a prefecture owns neutron instruments as well as neutron beam will be provided widely to industrial users. To make it successful, the user system is quite important because those users are expected to use IPD like chemical analyzers in their materials development process. Based on questionnaire data to several hundreds industries, IPD is designed as a versatile diffractometer including texture measurement, small angle scattering and total scattering as well as usual powder diffraction. IPD covers d range 0.15<d(A)<4 with {delta}d/d 0.15%, and covers 4<d(A)<60 with gradually changing resolution. Q range of IPD will be as wide as 0.01 A{sup -1}<Q<50A{sup -1} to be utilized for varieties of structures: local structure, nano structure and crystal structure analyses. Typical measuring time for the typical 'Rietveld-quality' data is several minutes with the sample size of laboratory X-ray: 0.4 cc. SHRPD is designed to be the world highest resolution with {delta}d/d = 0.03% without sacrificing intensity. The combination of the high quality data from HRPD and their high-precision analysis gives us information on tiny structural changes which have been overlooked. After careful examination with the moderator group five years ago, we have decided to develop a high-resolution and good S/N moderator to achieve the 0.03% resolution within 100 m flight path. This development was almost successful up to now. Instrumental simulation and radiation analysis were almost completed. The d range 0.5<d(A)<4 with {delta}d/d = 0.03%, and covers 4<d(A)<45 with gradually changing resolution. Takumi is the first priority instrument in JAEA for stress mapping inside structure materials with the highest resolution of {delta}d/d = 0.2% (corresponding to 10{approx}5 to 10{approx}6 strain precision). The typical gauge volume will be 1 mm3. JED has transmission radiography detectors to support stress mapping. Software group is planning so that basic software to cover data acquisition and data treatment should be common. Since 1 Gbyte data are typically obtained for single experiment in an instrument, the basic software is quite important. International TV conference between ISIS, IPNS, SNS has been held every month to exchange information on each development. KEK developed manyo-lib to help basic analysis. Analysis software development including powder diffraction is strongly related with the activity of the software group. However, users of IPD will be from various field of science and their background is different. It should cover wide topics and help both beginners and well-trained users. We have started with neutron intensity database, peak-search software, peak-match software, pattern simulation, whole pattern fitting, PDF and RDF analysis, and now start coding Rietveld software.

36 MATERIALS SCIENCE↗