Search NASA⌕ Search

SEARCH · Search NASA

Results for “cathode electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

Design of a multi-functional gel polymer electrolyte with a 3D compact stacked polymer micro-sphere matrix for high-performance lithium metal batteries

We report lithium metal batteries (LMBs) are considered as promising high energy density batteries. However, they still suffer from poor cyclability due to the instability of solid electrolyte interphases (SEIs) and Li dendrite issues. Herein, a novel 3D densely packed multifunctional crosslinked gel polymer electrolyte (PHGPE) has been synthesized by in situ copolymerization of pentaerythritol tetraacrylate and 2-hydroxyethyl acrylate in a liquid electrolyte via a thermal initiation method. Due to intermolecular hydrogen bonding in the frameworks, the PHGPE exhibits a 3D compact-stacked and crosslinked micro-sphere structure, which benefits the construction of homogeneous Li + flux, enabling uniform Li plating/stripping and formation of robust SEIs onto the lithium electrode. Benefiting from the above advantages, symmetric Li cells in the PHGPE deliver excellent cyclabilities of 6000 h at a current density of 1 mA cm -2 (1 mA h cm -2 ) and 7700 h at 0.5 mA cm -2 (2 mA h cm -2 ). Moreover, the PHGPE has such a wide electrochemical window that it is compatible with both high-voltage LiNi 0.8 Co 0.1 Mn 0.1 O 2 and sulfur cathodes to realize long cycle life. Additionally, a LiFePO 4 based pouch size LMB also presents promising performance. Therefore, this study of the PHGPE has opened a new avenue for high-performance LMBs with excellent versatility and practicality.

25 ENERGY STORAGE↗

Constructing a multi-functional polymer network for ultra-stable and safe Li-metal batteries

We report the practical application of lithium (Li) metal electrodes is impeded by Li dendrite growth and unstable solid electrolyte interphase (SEI). Herein, a multi-grafting polymer network, poly(dimethyl siloxane)-g-[poly(poly(ethylene glycol) methyl ether methacrylate)-r-sodium poly(p-styrene sulfonate)] (PPS), is chemically synthesized from reversible addition-fragmentation chain transfer (RAFT) polymerization. With integrated stretchability, ionic conductivity, and mechanical robustness, it serves a dual role to stabilize the Li electrode. As artificial SEI layer, the PPS enables superior electrochemical performance in half cells, symmetric cells, and full cells (PPS@Li/LiFePO 4 , capacity retention of >70% after 600 cycles). Utilized as solid polymer electrolyte (SPE), the all-solid-state Li/SPE/LiFePO 4 full cell delivers excellent cycling performance with an unprecedented capacity retention of 90% over 1,700 cycles at 0.5 C and 81% over 1,000 cycles at 1.0 C. With high-voltage LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) as cathode, the Li/SPE/NMC811 cell exhibits an initial discharge capacity of 162.2 mAh g -1 with a capacity retention of 72% after 200 cycles. The assembled solid-state Li/SPE/LiFePO4 pouch cell with SPE exhibits stable cycling performance over 200 cycles with a capacity retention of 75% and still operates well even after curling, folding, and cutting, demonstrating great potential for achieving ultra-safe and high energy density batteries.

25 ENERGY STORAGE↗

Multimodal quantification of degradation pathways during extreme fast charging of lithium-ion batteries

Enabling fast charging of Li-ion batteries will be a key step towards realizing the technology's full potential in electric vehicles. Currently, fast charging is limited by a variety of processes that reduce cell capacity upon extended cycling. Using a multimodal approach combining incremental capacity analysis (dQ/dV), high energy X-ray diffraction (HEXRD), and mass spectrometry titration (MST), we identify specific degradation mechanisms—including Li plating, dead Li x C 6 formation, Li 2 C 2 formation, solid carbonate solid-electrolyte interphase (SEI) deposition, and loss of positive electrode active material (LAM PE )—that occur during extended fast charge cycling. We find that Li plating is the major source of capacity loss in cells cycled at 6C, while non-carbonate SEI species deposition on the graphite anode is the main source of capacity loss when cycled at 4C. We also study local degradative phenomena by examining specific ~1–5 cm 2 regions of the cells using HEXRD and MST. Here, we find that plated Li is often collocated with dead Li x C 6 , Li 2 C 2 , and solid carbonate SEI species, and these additional species cumulatively account for ~20% of the capacity lost during 6C cycling. Finally, in a cell with an anomalously high amount of LAM PE (quantified via dQ/dV), we find that regions of cathode degradation were accompanied by non-carbonate SEI products on the adjacent region of the anode. We postulate that this phenomenon arises due to crosstalk between the electrodes, wherein soluble electrolyte oxidation products formed at the delithiated cathode migrate to the graphite anode and are ultimately deposited on the graphite surface. This work demonstrates the utility of combining multiple characterization techniques to reveal a more holistic understanding of degradative phenomena that occur across multiple length scales during fast charge.

25 ENERGY STORAGE↗

Synergy of Epoxy Chemical Tethers and Defect‐Free Graphene in Enabling Stable Lithium Cycling of Silicon Nanoparticles

Abstract We report a new approach for nanosilicon–graphene hybrids with uniquely stable solid electrolyte interphase. Expanded graphite is gently exfoliated creating “defect‐free” graphene that is non‐catalytic towards electrolyte decomposition, simultaneously introducing high mass loading (48 wt. %) Si nanoparticles. Silane surface treatment creates epoxy chemical tethers, mechanically binding nano‐Si to CMC binder through epoxy ring‐opening reaction while stabilizing the Si surface chemistry. Epoxy‐tethered silicon pristine–graphene hybrid “E‐Si‐pG” exhibits state‐of‐the‐art performance in full battery opposing commercial mass loading (12 mg cm −2 ) LiCoO 2 (LCO) cathode. At 0.4 C, with areal capacity of 1.62 mAh cm −2 and energy of 437 Wh kg −1 , achieving 1.32 mAh cm −2 , 340.4 Wh kg −1 at 1 C. After 150 cycles, it retains 1.25 mAh cm −2 , 306.5 Wh kg −1 . Sputter‐down XPS demonstrates survival of surface C‐Si‐O‐Si groups in E‐Si‐pG after repeated cycling. The discovered synergy between support defects, chemical‐mechanical stabilization of Si surfaces, and SEI‐related failure may become key LIB anode design rule.

Liu, Wei↗

Localized High‐Concentration Electrolytes Boost Potassium Storage in High‐Loading Graphite

Abstract Reversible intercalation of potassium‐ion (K + ) into graphite makes it a promising anode material for rechargeable potassium‐ion batteries (PIBs). However, the current graphite anodes in PIBs often suffer from poor cyclic stability with low coulombic efficiency. A stable solid electrolyte interphase (SEI) is necessary for stabilizing the large interlayer expansion during K + insertion. Herein, a localized high‐concentration electrolyte (LHCE) is designed by adding a highly fluorinated ether into the concentrated potassium bis(fluorosulfonyl)imide/dimethoxyethane, which forms a durable SEI on the graphite surface and enables highly reversible K + intercalation/deintercalation without solvent cointercalation. Furthermore, this LHCE shows a high ionic conductivity (13.6 mS cm −1 ) and excellent oxidation stability up to 5.3 V (vs K + /K), which enables compatibility with high‐voltage cathodes. The kinetics study reveals that K + intercalation/deintercalation does not follow the same pathway. The potassiated graphite exhibits excellent depotassiation rate capability, while the formation of a low stage intercalation compound is the rate‐limiting step during potassiation.

Qin, Lei↗

Monolithic solid–electrolyte interphases formed in fluorinated orthoformate-based electrolytes minimize Li depletion and pulverization

Lithium (Li) pulverization and associated large volume expansion during cycling is one of the most critical barriers for the safe operation of Li-metal batteries. Here, we report an approach to minimize the Li pulverization using an electrolyte based on a fluorinated orthoformate solvent. The solid–electrolyte interphase (SEI) formed in this electrolyte clearly exhibits a monolithic feature, which is in sharp contrast with the widely reported mosaic- or multilayer-type SEIs that are not homogeneous and could lead to uneven Li stripping/plating and fast Li and electrolyte depletion over cycling. The highly homogeneous and amorphous SEI not only prevents dendritic Li formation, but also minimizes Li loss and volumetric expansion. Furthermore, this new electrolyte strongly suppresses the phase transformation of the LiNi 0.8 Co 0.1 Mn 0.1 O 2 cathode (from layered structure to rock salt) and stabilizes its structure. In conclusion, tests of high-voltage Li||NMC811 cells show long-term cycling stability and high rate capability, as well as reduced safety concerns.

25 ENERGY STORAGE↗

Stable Anode–Free All–Solid–State Lithium Battery through Tuned Metal Wetting on the Copper Current Collector

A stable anode-free all-solid-state battery (AF-ASSB) with sulfide-based solid-electrolyte (SE) (argyrodite Li 6 PS 5 Cl) is achieved by tuning wetting of lithium metal on “empty” copper current-collector. Lithiophilic 1 µm Li 2 Te is synthesized by exposing the collector to tellurium vapor, followed by in situ Li activation during the first charge. The Li 2 Te significantly reduces the electrodeposition/electrodissolution overpotentials and improves Coulombic efficiency (CE). During continuous electrodeposition experiments using half-cells (1 mA cm –2 ), the accumulated thickness of electrodeposited Li on Li 2 Te–Cu is more than 70 µm, which is the thickness of the Li foil counter-electrode. Full AF-ASSB with NMC811 cathode delivers an initial CE of 83% at 0.2C, with a cycling CE above 99%. Additionally, cryogenic focused ion beam (Cryo-FIB) sectioning demonstrates uniform electrodeposited metal microstructure, with no signs of voids or dendrites at the collector-SE interface. Electrodissolution is uniform and complete, with Li 2 Te remaining structurally stable and adherent. By contrast, an unmodified Cu current-collector promotes inhomogeneous Li electrodeposition/electrodissolution, electrochemically inactive “dead metal,” dendrites that extend into SE, and thick non-uniform solid electrolyte interphase (SEI) interspersed with pores. Density functional theory (DFT) and mesoscale calculations provide complementary insight regarding nucleation-growth behavior. Unlike conventional liquid-electrolyte metal batteries, the role of current collector/support lithiophilicity has not been explored for emerging AF-ASSBs.

36 MATERIALS SCIENCE↗

Electrolyte design for LiF-rich solid–electrolyte interfaces to enable high-performance microsized alloy anodes for batteries

Lithium batteries with Si, Al or Bi microsized (>10 µm) particle anodes promise a high capacity, ease of production, low cost and low environmental impact, yet they suffer from fast degradation and a low Coulombic efficiency. In this paper, we demonstrate that a rationally designed electrolyte (2.0 M LiPF 6 in 1:1 v/v mixture of tetrahydrofuran and 2-methyltetrahydrofuran) enables 100 cycles of full cells that contain microsized Si, Al and Bi anodes with commercial LiFePO 4 and LiNi 0.8 Co 0.15 Al 0.05 O 2 cathodes. Alloy anodes with areal capacities of more than 2.5 mAh cm -2 achieved >300 cycles with a high initial Coulombic efficiency of >90% and average Coulombic efficiency of >99.9%. These improvements are facilitated by the formation of a high-modulus LiF–organic bilayer interphase, in which LiF possesses a high interfacial energy with the alloy anode to accommodate plastic deformation of the lithiated alloy during cycling. Lastly, this work provides a simple yet practical solution to current battery technology without any binder modification or special fabrication methods.

25 ENERGY STORAGE↗

Intermetallics Based on Sodium Chalcogenides Promote Stable Electrodeposition–Electrodissolution of Sodium Metal Anodes

Sodiophilic micro-composite films of sodium-chalcogenide intermetallics (Na 2 Te and Na 2 S) and Cu particles are fabricated onto commercial copper foam current collectors (Na 2 Te@CF and Na 2 S@CF). For the first time a controllable capacity thermal infusion process is demonstrated. Enhanced wetting by the metal electrodeposition leads to state-of-the-art electrochemical performance. For example, Na 2 Te@CF-based half-cells demonstrate stable cycling at 6 mA cm -2 and 6 mAh cm -2 , corresponding to 54 µm of Na electrodeposited/electrodissolved by geometric area. Sodium metal batteries with Na 3 V 2 (PO 4 ) 3 cathodes are stable at 30C (7 mA cm -2 ) and for 10 000 cycles at 5C and 10C. Cross-sectional cryogenic focused ion beam (cryo-FIB) microscopy details deposited and remnant dissolved microstructures. Sodium metal electrodeposition onto Na 2 Te@CF is dense, smooth, and free of dendrites or pores. On unmodified copper foam, sodium grows in a filament-like manner, not requiring cycling to achieve this geometry. Substrate–metal interaction critically affects the metal–electrolyte interface, namely the thickness and morphology of the solid electrolyte interphase. Density functional theory and mesoscale simulations provide insight into support-adatom energetics, nucleation response, and early-stage morphological evolution. On Na 2 Te sodium atomic dispersion is thermodynamically more stable than isolated clusters, leading to conformal adatom coverage of the surface.

36 MATERIALS SCIENCE↗

A Universal Design of Lithium Anode via Dynamic Stability Strategy for Practical All‐Solid‐State Batteries

Abstract All‐solid‐state Li‐metal battery (ASSLB) chemistry with thin solid‐state electrolyte (SSE) membranes features high energy density and intrinsic safety but suffers from severe dendrite formation and poor interface contact during cycling, which hampers the practical application of rechargeable ASSLB. Here, we propose a universal design of thin Li‐metal anode (LMA) via a dynamic stability strategy to address these issues. The ultra‐thin LMA (20 μm) is in situ constructed with uniform highly Li‐ion conductive solid‐electrolyte interphase and composite‐polymer interphase (CPI) via electroplating process. As a result, the passivation layer with poor Li‐ion conduction on Li anode can be dissolved and small surface resistance can be achieved due to the good compatibility of CPI to SSEs. The cycling of Li symmetric cell with Li 6 PS 5 Cl thin film electrolyte (<100 μm) shows a high critical current density of >2.0 mA cm −2 with excellent cycling stability at 1.0 mA cm −2 . The ASSLBs paring with Ni‐rich LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathode demonstrated the feasibility of engineered LMA design by presenting good rate capability from 0.1 C to 1.0 C at room temperature, as well as long‐term cycling stability (81 % retention after 100 cycles). This work represents a general pathway to make thin dendrite‐free LMA available for high‐energy‐density ASSLBs.

Deng, Tao [Department of Chemical and Biomolecular↗

A Universal Design of Lithium Anode via Dynamic Stability Strategy for Practical All‐Solid‐State Batteries

Abstract All‐solid‐state Li‐metal battery (ASSLB) chemistry with thin solid‐state electrolyte (SSE) membranes features high energy density and intrinsic safety but suffers from severe dendrite formation and poor interface contact during cycling, which hampers the practical application of rechargeable ASSLB. Here, we propose a universal design of thin Li‐metal anode (LMA) via a dynamic stability strategy to address these issues. The ultra‐thin LMA (20 μm) is in situ constructed with uniform highly Li‐ion conductive solid‐electrolyte interphase and composite‐polymer interphase (CPI) via electroplating process. As a result, the passivation layer with poor Li‐ion conduction on Li anode can be dissolved and small surface resistance can be achieved due to the good compatibility of CPI to SSEs. The cycling of Li symmetric cell with Li 6 PS 5 Cl thin film electrolyte (<100 μm) shows a high critical current density of >2.0 mA cm −2 with excellent cycling stability at 1.0 mA cm −2 . The ASSLBs paring with Ni‐rich LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathode demonstrated the feasibility of engineered LMA design by presenting good rate capability from 0.1 C to 1.0 C at room temperature, as well as long‐term cycling stability (81 % retention after 100 cycles). This work represents a general pathway to make thin dendrite‐free LMA available for high‐energy‐density ASSLBs.

Deng, Tao [Department of Chemical and Biomolecular↗

Highly reversible Zn metal anode enabled by sustainable hydroxyl chemistry

Rechargeable Zn metal batteries (RZMBs) may provide a more sustainable and lower-cost alternative to established battery technologies in meeting energy storage applications of the future. However, the most promising electrolytes for RZMBs are generally aqueous and require high concentrations of salt(s) to bring efficiencies toward commercially viable levels and mitigate water-originated parasitic reactions including hydrogen evolution and corrosion. Electrolytes based on nonaqueous solvents are promising for avoiding these issues, although full cell performance demonstrations with solvents other than water have been very limited. To address these challenges, we investigated MeOH as an alternative electrolyte solvent. These MeOH-based electrolytes exhibited exceptional Zn reversibility over a wide temperature range, with a Coulombic efficiency > 99.5% at 50% Zn utilization without cell short-circuit behavior for > 1,800 h. More important, this remarkable performance translates well to Zn || metal-free organic cathode full cells, supporting < 6% capacity decay after > 800 cycles at –40°C.

25 ENERGY STORAGE↗

The effect of water-containing electrolyte on lithium-sulfur batteries

Dissolved polysulfides, formed during Li-S battery operation, freely migrate and react with both the Li anode and the sulfur cathode. These soluble polysulfides shuttle between the anode and cathode – the so-called shuttle effect – resulting in an infinite recharge process and poor Columbic efficiency. We present that water present as an additive in the Li-S battery electrolyte is found to reduce the shuttle effect in Li-S batteries. Batteries where water content was below 50 ppm exhibited a substantial shuttle effect and low charge capacity. Alternatively, addition of 250 ppm water led to stable charge/discharge behavior with high Coulombic efficiency. XPS results show that H 2 O addition results in the formation of solid electrolyte interphase (SEI) film with more LiOH on Li anode which protects the Li anode from the polysulfides. Batteries cycled without water result in a SEI film with more Li 2 CO 3 likely formed by direct contact between the Li metal and the solvent. Intermediate quantities of H 2 O in the electrolyte result in high cycle efficiency for the first few cycles which then rapidly decays. Lastly, this suggests that H 2 O is consumed during battery cycling, likely by interaction with freshly exposed Li metal formed during Li deposition.

25 ENERGY STORAGE↗

Fast Charging of Li-Ion Cells: Part I. Using Li/Cu Reference Electrodes to Probe Individual Electrode Potentials

Increasing the charge rate of Li-ion cells over 1–2C (full charge in 30–60 min) would be highly desirable, but high currents flowing through the active materials push these cells to their endurance limits. In this article, we aim to understand how such high-current regimes affect electrochemical properties of the cells. Formation of Li metal deposits is a recognized hazard of high-rate charging, as Li plating can overtake lithium intercalation in the negative electrode. Here we demonstrate how microprobe Li/Cu reference electrodes can be used to characterize the graphite anode and layered oxide (NCM523) cathode during constant-current (≤ 6C) voltage-limited (4.39 V) charging of Li-ion cells. These reference electrodes are used to monitor the onset of Li plating conditions in situ during cell charging. As the current increases over 3C, the anode potentials decrease below -40 mV causing lithium nucleation. Surprisingly, this nucleation (at least, initially) does not result in capacity fade or a higher anode impedance even in strongly polarized cells, so it appears that the nascent Li nuclei are isolated from electrolyte by the pre-existing solid electrolyte interphase. Our study shows that microprobe reference electrodes are an important diagnostic tool to characterize full-cell behavior in the high-current regimes.

25 ENERGY STORAGE↗

A new cyclic carbonate enables high power/ low temperature lithium-ion batteries

The modern lithium-ion battery (LIB) configuration was enabled by the "magic chemistry" between ethylene carbonate (EC) and graphitic carbon anode. Despite the constant changes of cathode chemistries with improved energy densities, EC-graphite combination remained static during the last three decades. While the interphase generated by EC protects the fragile graphitic structure, the intrinsic disadvantages of EC (high viscosity, high melting point, excessive interphase growth) lead to mediocre power density and poor performances of LIB at sub-zero temperatures, where lithium depositions form upon charging. Such performance compromises arise from the fundamental dilemma between requiring effective interphase protection and high impedance from excessive growth of interphase. In this work, we designed and synthesized a "double EC" molecule as electrolyte additive to resolve the above dilemma. Erythritol bis(carbonate) (EBC) possesses lower LUMO energy level than EC and hence tends to decompose prior to EC reduction, but its weak solvation toward Li + restricts the extent of its reduction, thus minimizing the interphase thickness and the corresponding impedances. Electrolytes containing EBC enables both the charging and discharging of ampere-size LIB pouch cells at sub-zero temperatures from 0 to -20°C, demonstrating that the key approach to improve low temperature performances lies in how to tailor interphasial chemistry rather than the bulk electrolyte composition.

25 ENERGY STORAGE↗

Factors Limiting Li+ Charge Transfer Kinetics in Li-ion Batteries

Understanding the factors limiting Li+ charge transfer kinetics in Li-ion batteries is essential in improving the rate performance, especially at lower temperatures. The Li+ charge transfer process involved in the lithium intercalation of graphite anode includes the step of de-solvation of the solvated Li+ in the liquid electrolyte and the step of transport of Li+ in the preformed solid electrolyte interphase (SEI) on electrodes until the Li+ accepts an electron at the electrode and becomes a Li in the electrode. Whether the de-solvation process or the Li+ transport through the SEI is a limiting step depends on the nature of the interphases at the electrode and electrolyte interfaces. Several examples involving the electrode materials such as graphite, lithium titanate (LTO), lithium iron phosphate (LFP), lithium nickel cobalt aluminum oxide (NCA) and solid Li+ conductor such as lithium lanthanum titanate or Li-Al-Ti-phosphate are reviewed and discussed to clarify the conditions at which either the de-solvation or the transport of Li+ in SEI is dominating and how the electrolyte components affect the activation energy of Li+ charge transfer kinetics. How the electrolyte additives impact the Li+ charge transfer kinetics at both the anode and the cathode has been examined at the same time in 3-electrode full cells. The resulting impact on Li+ charge transfer resistance, Rct, and activation energy, Ea, at both electrodes are reported and discussed.