Search NASA⌕ Search

SEARCH · Search NASA

Results for “deposition”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

The Influence of Ozone: Superstoichiometric Oxygen in Atomic Layer Deposition of Fe 2 O 3 Using tert -Butylferrocene and O 3

Understanding the chemical mechanisms at play in atomic layer deposition (ALD) is critical for effective process development and expansion of ALD into more complex classes of materials. In this work, a mechanistic study of iron oxide deposited by ALD using tert-butylferrocene and ozone as reactants is performed. Iron oxide ALD using ozone is a useful model system for mechanistic studies due to the prevalence of ozone-based ALD processes and the uses of iron oxide in ternary and quaternary metal oxides. Results show that saturation conditions require significantly greater exposures of both reactants than is typically reported in the literature, and growths per cycle of greater than one monolayer of Fe 2 O 3 per cycle are observed and explained. A growth mechanism is proposed whereby increased ozone exposure results in uptake of superstoichiometric oxygen into the film. X-ray characterizations reveal the presence of excess oxygen stored near the surface of films deposited with larger ozone exposures and show that increased ozone exposures cause crystalline domain rearrangement and conversion of the film from the γ-maghemite phase to the α-hematite phase. The mechanism described here has implications for the wider class of ozone-based ALD processes, and potential applications of this growth phenomenon are discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Pristine Interface between Lithium Lanthanum Zirconate and Lithium Manganese Oxide by Pulsed Laser Deposition

Solid state lithium-ion batteries have garnered increasing interest in recent years due to several potential advantages over liquid-electrolyte based systems. The possibility of integrating the lithium garnet oxide, Li 6.75 La 3 Zr 1.75 Ta 0.25 O 12 (LLZTO), with the high voltage cathode, spinel Li x Mn 2 O 4 (LMO), is evaluated here. Thin film bilayer structures are prepared by pulsed laser deposition on MgO (001) substrates and characterized by x-ray diffraction and transmission electron microscopy. The LLZTO is grown by an alternating layer-by-layer deposition of LLZTO and Li 3 N and subsequently annealed for several hours at 575 °C to promote crystallinity. Growth of crystalline LMO with a pristine interface to LLZTO is achieved by gentle heat treatment (500 °C) to remove surface carbonate from the electrolyte and by cathode growth at a low temperature of 250 °C. Higher temperature depositions (330 – 450 °C) result in reaction between the two materials and the appearance of Li 2 MnO 3 , which may be in part due to the presence of excess lithium in the electrolyte layer. Because fully lithiated LiMn 2 O 4 has a voltage of ≈3.7 V versus Li+/Li, the observation of a well-defined interface, free of impurity phases and with no interdiffusion of elements, indicates LLZTO is stable to at least 3.7 V.

Garnet LLZO↗

Localized Heterogeneous Nucleation for Vapor‐Assisted Sequential Deposition of Metal Halide Perovskites

Vapor-assisted hybrid two-step deposition, which combines thermally evaporated inorganic layers with solution-processed organic halides to form halide perovskites, has emerged as a scalable and industry-compatible route for textured tandem photovoltaics. However, this process is often hindered by reaction-limited phase formation, particularly when compact, non-porous, and highly crystalline inorganic layers formed by thermal evaporation restrict subsequent conversion, resulting in incomplete reaction and pronounced depth-dependent heterogeneity. In this study, we introduce a strategy to regulate the inorganic precursor layer by incorporating localized heterogeneous nucleation sites. Sparsely distributed hydrophilic metal oxide species serve as effective nucleation centers during vapor deposition, enabling effective control over film morphology and crystal orientation from the early stages of growth. This tailored inorganic framework facilitates the subsequent incorporation of organic halides, alleviating reaction limitations and suppressing residual unreacted precursors. Consequently, the perovskite films exhibit improved stoichiometric uniformity and enhanced optoelectronic quality, enabling wide-bandgap perovskite solar cells with markedly improved performance and operational stability. This work provides important mechanistic insight into crystal growth engineering of vapor-deposited perovskite thin films.

nucleation↗

The Effect of Surface Terminations on the Initial Stages of TiO 2 Deposition on Functionalized Silicon

As atomic layer deposition (ALD) emerges as a method to fabricate architectures with atomic precision, emphasis is placed on understanding surface reactions and nucleation mechanisms. ALD of titanium dioxide with TiCl 4 and water has been used to investigate deposition processes in general, but the effect of surface termination on the initial TiO 2 nucleation lacks needed mechanistic insights. Here, this work examines the adsorption of TiCl 4 on Cl–, H–, and HO– terminated Si(100) and Si(111) surfaces to elucidate the general role of different surface structures and defect types in manipulating surface reactivity of growth and non-growth substrates. The surface sites and their role in the initial stages of deposition are examined by X-ray photoelectron spectroscopy (XPS) and atomic force microscopy (AFM). Density functional theory (DFT) computations of the local functionalized silicon surfaces suggest oxygen-containing defects are primary drivers of selectivity loss on these surfaces.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Time-Resolved Grazing Incidence X-Ray Absorption Spectroscopy for the In Situ Investigation of the Initial Stages of Sputter-Deposited Copper Thin Films

The sputter deposition and the growth of thin copper films on float glass substrates are in situ studied using grazing incidence, reflection mode X-ray absorption fine structure spectroscopy with subsecond time resolution. The experimental data are compared with model calculations, assuming the presence of crystalline, face-centered cubic metallic Cu nanostructures. From a detailed analysis of the measured spectra, the film thickness as well as the surface roughness is determined, leading to a detailed understanding of the films growth as a function of the sputter deposition time. In particular, different stages of film growth can clearly be distinguished from the fits of the experimental data. The results suggest the formation of isolated, approximately nm-sized copper clusters in the initial phase of the film deposition for the first few seconds, a coalescence phase with a nominal thickness of ≈1.5–2.8 nm, constant roughness of about 1.4 nm for the subsequent ≈5 s, and finally 3D growth of the Cu crystallites in the film for later stages of film growth. Further prospects of the methodology are given.

36 MATERIALS SCIENCE↗

Effects of lead and lean in multi-axis directed energy deposition

Here, the present study examines the effect of varying laser incidence angles on textural, microstructural, and geometric characteristics of directed energy deposition (DED) processed materials, providing a more comprehensive outlook on participating laser-matter interaction phenomena and ultimately devising strategies to ameliorate print performance. In this study, single-layer, single-/multi-track specimens were processed to examine the effect of non-orthogonal angular configurations on bead morphology, microstructure, phase composition, and textural representation of DED-processed 316L stainless steel materials. It was observed that bead size decreased at increasing lead and lean angles. Asymmetry in the distribution of the bead morphology as a function of lead angle indicates better catchment for acute lead angle configurations over obtuse configurations. No significant differences in phase composition, texture, and microstructure were observed in moderate off-axis configurations. When the penetration depth for the deposits was below 20 μm, columnar structures dominated the microstructure of the deposited material. At deeper penetration depths, columnar and equiaxed structures were observed at the bead-substrate interface and center of the bead, respectively. Compared to powder-blown DED, wire-DED dilution profiles were found to be asymmetric in both orthogonal and non-orthogonal wire DED samples.

36 MATERIALS SCIENCE↗

Microstructure and Properties of Inconel 718 Fabricated by Directed Energy Deposition with In-Situ Ultrasonic Impact Peening

Many inherent issues, such as the detrimental residual stress, columnar grains with anisotropy, and weak mechanical properties, have severely impeded the adoption of metal additive manufacturing (AM) techniques including powder bed fusion and directed energy deposition (DED) processes. In this study, a hybrid AM process that consists of layer-wise laser metal deposition (i.e., a DED process) and in-situ ultrasonic impact peening (UIP) was applied to obtain Inconel 718 superalloy workpieces. Also, for further property enhancement, a post-heat treatment was applied to the deposited material obtained by the hybrid AM process. Scanning electron microscopy and transmission electron microscope were used to investigate the microstructure morphology and reveal the underlying strengthening mechanism. Electron backscatter diffraction was employed to quantitatively study the microstructure resulted from the hybrid AM process and the post-heat treatment. The profile of residual stress along the depth direction was obtained through X-ray diffraction. The results demonstrate that this hybrid AM process is capable of producing high-quality metal parts with significantly refined microstructure, and beneficial compressive residual stress along the depth into surface. Severe plastic strains are introduced by UIP, and the resulted mechanical twinning and dynamic recrystallization play an important role in refining microstructure. The material microstructure is further refined down to 100 µm, and the texture anisotropy is significantly diminished after solution treatment at 980 °C for 1 hour. Under the as-built condition, in-situ ultrasonic peening alters the residual stress component from a tensile state to an overall compressive state with a maximum value of − 190 MPa within the range of measurement depth.

36 MATERIALS SCIENCE↗

Coaxial color channel focus evaluation to estimate standoff height in directed energy deposition additive manufacturing

Directed energy deposition (DED) is an additive manufacturing process that is being rapidly adopted by industry and is well suited for the fabrication of complex components in a variety of metal alloys. In laser cladding systems such as DED, powder is blown in a stream to a metal substrate coincident with a laser necessary to deposit molten metal with 3D spatial control. The focus of both the laser and the powder stream are crucial, and best deposition occurs at a predetermined standoff height between the build surface and the print head. Generally, no monitoring of this distance is implemented in commercial DED systems. Due to potential over or under building, the standoff height often changes over time but tends to self-correct. However, inexpensive and minimally intrusive methods to identify optimal standoff are required to provide real-time control to maintain the optimal distance. The present work explores the quantification of the focus of the three-color channels of a coaxial camera to determine the standoff height. An experiment was performed in which a 254 mm wall is built and the standoff height, initially 5.0 mm below the optimal position, was then intentionally increased every 25.4 mm of wall length by an amount of 1.0 mm to a final position 7.0 mm above optimal. Computer vision is demonstrated to monitor the amount of focus in each color band and estimate standoff distance. Finally, a response can be calculated in under 40 ms using simple hardware and can work in most laser-based DED systems.

36 MATERIALS SCIENCE↗

Review of Computer-Aided Manufacturing (CAM) strategies for hybrid directed energy deposition

Hybrid additive manufacturing intertwines both additive and subtractive manufacturing layer by layer to digitally fabricate parts with complex geometries, improved surface finish and tight dimensional accuracies, the sum of which is difficult to obtain with any single process. Computer-Aided Manufacturing (CAM) software is required to orchestrate the machine toolpathing for both the deposition as well as the machining processes and is crucial for the successful fabrication of high quality structures. Additionally, CAM requires substantial operator input to account for challenging aspects of each fabricated structure. For example, deciding at which layer of deposition will the machining process continue to maintain access to complex cavities for finishing - internal features that would otherwise be unfinishable due to reach limitations or obstructions. Moreover, of the many commercially-available hybrid systems, each has a unique kinematic environment which can benefit from specific optimization of toolpath planning and substantial research has directly correlated toolpathing with the microstructure evolution, mechanical properties, porosity and residual stress state of the final fabricated part. This review explores the available strategies for CAM in the context of hybrid direct energy deposition, discusses the advantages and disadvantages of each and considers future CAM trends for this transformational digital manufacturing technology.

36 MATERIALS SCIENCE↗

Investigation of irradiation damage and heat deposition: a comparative analysis for HEU-to-LEU conversion in HFIR

The planned conversion of the High Flux Isotope Reactor (HFIR) at Oak Ridge National Laboratory from highly enriched uranium (HEU) to low-enriched uranium (LEU) fuel requires detailed evaluation of experiment-relevant parameters to ensure continued performance for materials testing and isotope production. Here, this study presents the first comprehensive assessment of displacements per atom (dpa) and heat deposition rates in target materials within the HFIR flux trap with both HEU and candidate LEU core configurations. Seven analyses were conducted to evaluate key performance metrics, including fast neutron flux distribution, cross section response functions, cross section data, and local dpa and heat deposition rates using mesh- and cell-based tallies. Simulations employed Shift, Monte Carlo N-Particle (MCNP), and the HIFR Controller (HFIRCON) tool suite for high-fidelity transport and depletion modeling. The LEU designs—using U 3 Si 2 -Al dispersion fuel and operating at 95 MW—were compared to the current 85 MW HEU configuration. Results show that while the candidate LEU cores exhibit higher dpa rates due to a harder spectrum and extended cycle lengths, they also demonstrate reduced heat deposition rates in irradiation experiments, primarily due to increased gamma self-shielding from higher 238 U content in the core. These findings confirm that LEU conversion can maintain HFIR’s materials irradiation capabilities but may require redesigning existing experimental hardware.

HEU↗

A New One-Pot Sequential Reduction-Deposition Method for the synthesis of Silica-supported NiPt and CuPt Bimetallic Catalysts

A one-pot redox deposition method is described to prepare silica-supported bimetallic NiPt and CuPt catalysts using differences in standard reduction potentials. The synthesis involved the initial reduction of non-noble metal ions (Ni 2+ and Cu 2+ ) by NaBH 4 , followed by reduction of Pt ions by these reduced metals. Alloy formation and phase purity were established by X-ray diffraction (XRD), bulk composition by X-ray fluorescence (XRF), and surface composition by X-ray photoelectron spectroscopy (XPS). Alloy formation was enhanced by increase in the amount of base metals available to reduce Pt, or through the use of excess NaBH 4 after redox deposition. The catalysts were evaluated for methane oxidation at 300-400 °C and atmospheric pressure. Reference samples prepared using the incipient wetness impregnation (IW) method had inferior performance and characteristics. The redox deposition method provides a simple and versatile protocol for the preparation of bimetallic alloys between noble metals and base metals.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding non-stochiometric deposition of multi-principal elemental NiCoCr thin films

Multi-principal elemental NiCoCr thin films with compositional flexibility have potential applications as a thermal barrier, corrosion-resistant coatings, and functional energy materials. In this study, the non-stochiometric multi-principal element alloy thin film formation behavior from an equiatomic ablation target of NiCoCr using pulsed laser deposition has been reported. Here, the effect of varying laser fluence on compositions of constituent elements in the NiCoCr thin films is systematically investigated. The increase in laser fluence typically increases the likelihood of acquiring undesirable particulates in thin films. Therefore, to maintain the film quality the laser fluences are adjusted within the range of 1.3–3.3 J·cm -2 , while the film thicknesses are kept constant at ~30 nm. Results show that the constituent elements are well-distributed in the formed NiCoCr thin films, however, having average atomic percentages of Ni and Cr twice as high as Co irrespective of the equiatomic composition of individual elements in the ablation target. This stochiometric alteration in the as-deposited thin films is governed by the rate of ablation and subsequent evaporation of each element, which is facilitated by the optical properties and vapor pressure of individual constituent elements. Additionally, electron energy-loss spectroscopy and x-ray absorption spectroscopy analysis reveal that the thin films have partially oxidized, with the Cr oxidation contributing the most to the O-K edge in comparison to Ni and Co. Finally, this study presents a laser-assisted pathway for fabricating compositionally flexible NiCoCr thin films and develops an understanding of the non-equilibrium laser-material interactions and how the intrinsic properties of constituent elements affect the stoichiometric flow of materials from the target to the final film deposition.

36 MATERIALS SCIENCE↗

Au assisted smooth ultrathin epitaxial ZnO film grown by pulsed laser deposition on sapphire(0001)

High quality ZnO has applications in photonics and electronics. Literature has shown that continuous, but rough ZnO film can be grown on sapphire substrate by pulsed laser deposition (PLD). In this work, ZnO and Au were co-deposited by PLD on sapphire(0001) substrates from a single ZnO target overlaid with an Au strip that serves as a catalyst. The reflection high-energy electron diffraction (RHEED) patterns show paired double stripes from sample of ZnO-Au where the difference of in-plane lattice parameters between ZnO and Au is 11.4 %. The two-dimensional (2D) reciprocal space maps constructed from azimuthal RHEED (ARHEED) patterns reveal parallel epitaxial relationship between ZnO and Au in the continuous ZnO-Au film on sapphire substrate. Transmission electron microscopy (TEM) cross section images and energy dispersive spectroscopy maps show a minute amount of Au nanocrystals distributed in the entire ultrathin ZnO film. Atomic force microscopy shows the root-mean-square roughness of the surface of ultrathin ZnO film with Au is in the sub-nm range. The ARHEED and TEM results show that a couple of atomic percentages of Au co-deposited with ZnO catalyzes the growth of smooth ultrathin epitaxial ZnO film.

36 MATERIALS SCIENCE↗

Laser diagnostics to characterize the in-flame growth of platinum nanoparticles manufactured by the reactive spray deposition technology

Reactive Spray Deposition Technology (RSDT) is an atmospheric pressure, flame-based advanced manufacturing method used to fabricate Membrane Electrode Assemblies (MEAs) for proton exchange fuel cells and water electrolyzers. RSDT combines the flame synthesis of catalyst nanoparticles and their deposition onto the membrane in one step. The properties of the synthesized nanoparticles, such as their Size Distribution Function (SDF), determine the manufactured electrodes’ performance, which can be evaluated when the deposition is complete via ex-situ characterization of the products. Efforts to improve RSDT for manufacturing state-of-the-art MEAs can be significantly enhanced with integrated laser diagnostics that enable in situ measurement of the synthesized catalyst nanoparticles. This paper reports the implementation of laser diagnostics in an RSDT facility and evaluates their potential to assist the manufacturing process. Laser Light Scattering (LS) and Laser-Induced Incandescence (LII) measurements are performed in the oxygen-rich zone of the flame at various distances from the flame fuel jet nozzle downstream of its luminous region. The measurements quantitatively track the evolution in size and volume fraction of platinum-based nanoparticles in two flames that yield different catalytic properties in the manufactured electrodes. The profiles of the measured nanoparticles’ volume fraction along the flame axis can be estimated a priori so that the average nanoparticle sizes can be measured in quasi-real time via LS. Nanoparticles experience an extremely slow growth rate while being convected at distances from 150 nm to 300 nm from the fuel nozzle. Complementary characterizations of the synthesized nanoparticles are performed ex-situ via High-Angle Annular Darkfield Scanning Transmission Electron Microscopy (HAADF-STEM) image analyses of samples collected on grids at a fixed distance from the fuel jet nozzle. Comparing the results from laser and microscopy techniques not only cross-validates the findings but also provides the parameters to infer the bimodal SDF in-situ and yields evidence that the coagulation efficiency of the synthesized nanoparticles has extremely low values in the investigated zone of the flames.

Rayleigh Light Scattering (LS)↗

Recent progress on the mesoscale modeling of architected thin-films via phase-field formulations of physical vapor deposition

Thin-film coatings can be found everywhere in modern technological applications due to desirable electrical, mechanical, chemical, and optical properties. These properties directly depend upon the thin-film’s microstructural features, which are themselves influenced by the materials and vapor-deposition processing conditions used for fabrication. As such, understanding processing-microstructure relationships is essential to designing thin-films with optimized properties, and discovering new processing conditions that allow for novel thin-films with multifunctional microstructures. Here, a short review is presented on recent developments that utilize the phase-field method to simultaneously model the vapor-deposition process and corresponding microstructure formation at the mesoscale. Also phase-field-based vapor-deposition models that simulate thin-film growth of immiscible alloy and polycrystalline systems are highlighted in addition to machine-learning-based surrogate models that can facilitate accelerated high-fidelity simulations along with materials design and exploration studies.

36 MATERIALS SCIENCE↗

Gas hydrate deposit formation in transient flowloop tests and mitigation with a surface treatment

Thermodynamic and thermal mitigation strategies are traditionally utilized to prevent gas hydrate formation but may be rendered ineffective for certain unplanned, extended shut-in scenarios. Unfortunately, the current knowledge regarding transient gas hydrate formation has been extremely limited to only a few studies and unable to address this complex issue adequately. This work, conducted in a lab-scale flowloop, aims to add to the understanding of this area by delving into the implications of transient conditions on gas hydrate formation mechanisms, while also exploring a possible mitigation strategy of a surface treatment. Specifically, the effects of phase separation on gas hydrate formation locations, transportability, and plugging are presented for an oil-dominated system. An omniphobic surface treatment is shown to affect initial gas hydrate deposition and its wall adherence strength, as well as the overall plugging outcome. Overall, this work combines observational information with process data measurements to provide a better understanding of phase separated gas hydrate systems and passive deposition mitigation strategies. This can further aid advanced gas hydrate modeling efforts, which currently do not adequately address transient flow effects on phase separation/dispersion. Here, it offers representative gas hydrate testing for coatings, which have exclusively been limited to non-flowing and/or bench-scale analysis, to give confidence in their potential application as advanced deposition prevention tools.

03 NATURAL GAS↗

Sinter formation during directed energy deposition of titanium alloy powders

During directed energy deposition (DED) additive manufacturing, powder agglomeration and sintering can occur outside of the melt pool when using titanium alloy powders. Using in situ synchrotron radiography we investigate the mechanisms by which sintering of Ti6242 powder occurs around the pool, performing a parametric study to determine the influence of laser power and stage traverse speed on sinter build-up. The results reveal that detrimental sinter can be reduced using a high laser power or increased stage traverse speed, although the latter also reduces deposition layer thickness. The mechanism of sinter formation during DED was determined to be in-flight heating of the powder particles in the laser beam. Calculations of particle heating under the processing conditions explored in this study confirm that powder particles can reasonably exceed 700 °C, the threshold for Ti surface oxide dissolution, and thus the powder is prone to sintering if not incorporated into the melt pool. The build-up of sinter powder layer on deposit surfaces led to lack of fusion pores. To mitigate sinter formation and its detrimental effects on DED component quality, it is essential that the powder delivery spot area is smaller than the melt pool, ensuring most powder lands in the melt pool.

36 MATERIALS SCIENCE↗

An operando synchrotron study on the effect of wire melting state on solidification microstructures of Inconel 718 in wire-laser directed energy deposition

Directed energy deposition (DED) with a coaxial wire-laser configuration has gained significant attention in recent years for the production of large-scale metallic components because of its low directional dependence, fast deposition rate, high feedstock efficiency, and low manufacturing costs. This work studies the coaxial wire-laser DED process of Inconel 718 alloy under a stable deposition condition with a relatively low input volumetric energy density (55.5J/mm 3 ). Post characterization reveals a cluster of refined grains at the center-bottom region of the as-printed track. Operando high-energy synchrotron X-ray experiments and multi-physics modeling are applied innovatively to study the fundamental mechanism responsible for the formation of this microstructure. The X-ray diffraction experiment provides direct evidence, which is supported by the simulation, that the feeding wire can reach the melt pool bottom and release solid particles (primarily carbides) near the mushy zone owing to insufficient melting. Consequently, these sub-micron sized particles suppress the growth of large columnar grains and cause the formation of unique microstructural heterogeneity. In conclusion, this discovery offers new opportunities for tailoring the solidification microstructure by controlling the melting state of the feedstock wire in DED process, in addition to commonly known factors such as the thermal gradient and solidification velocity.

42 ENGINEERING↗