Search NASA⌕ Search

SEARCH · Search NASA

Results for “recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

The effect of chemical composition and austenite conditioning on the transformation behavior of microalloyed steels

In this investigation, by using continuous cooling torsion (CCT) testing, the transformation behavior of four microalloyed steels under two circumstances of austenite conditioning and non-conditioning was studied. A full scale hot-rolling schedule containing a 13-pass deformation was employed for the conditioning of the austenite. The CCT tests were then employed till temperature of {approx} 540 Degree-Sign C and the flow curves obtained from this process were analyzed. The initial and final microstructures of the steels were studied by optical and electron microscopes. Results show that alloying elements would decrease the transformation temperature. This effect intensifies with the gradual increase of Mo, Nb and Cu as alloying elements added to the microalloyed steels. As well, austenite conditioning increased the transformation start temperature due mainly to the promotion of polygonal ferrite formation that resulted from a pancaked austenite. The final microstructures also show that CCT alone would decrease the amount of bainite by inducing ferrite transformation in the two phase region. In addition, after the transformation begins, the deformation might result in the occurrence of dynamic recrystallization in the ferrite region. This could lead to two different ferrite grain sizes at the end of the CCT. Moreover, the Nb bearing steels show no sign of decreasing the strength level after the transformation begins in the non-conditioned situation and their microstructure is a mix of polygonal ferrite and bainite indicating an absence of probable dynamic recrystallization in this condition. In the conditioned cases, however, these steels show a rapid decrease of the strength level and their final microstructures insinuate that ferrite could have undergone a dynamic recrystallization due to deformation. Consequently, no bainite was seen in the austenite conditioned Nb bearing steels. The pancaking of austenite in the latest cases produced fully polygonal ferrite structures. - Highlights: Black-Right-Pointing-Pointer Adding alloying elements would decrease the transformation temperatures. Black-Right-Pointing-Pointer Austenite conditioning increases the transformation start temperature. Black-Right-Pointing-Pointer Deformation could induce the occurrence of dynamic recrystallization in ferrite region.

36 MATERIALS SCIENCE↗

Precipitation in cold-rolled Al–Sc–Zr and Al–Mn–Sc–Zr alloys prepared by powder metallurgy

The effects of cold-rolling on thermal, mechanical and electrical properties, microstructure and recrystallization behaviour of the AlScZr and AlMnScZr alloys prepared by powder metallurgy were studied. The powder was produced by atomising in argon with 1% oxygen and then consolidated by hot extrusion at 350 °C. The electrical resistometry and microhardness together with differential scanning calorimetry measurements were compared with microstructure development observed by transmission and scanning electron microscopy, X-ray diffraction and electron backscatter diffraction. Fine (sub)grain structure developed and fine coherent Al{sub 3}Sc and/or Al{sub 3}(Sc,Zr) particles precipitated during extrusion at 350 °C in the alloys studied. Additional precipitation of the Al{sub 3}Sc and/or Al{sub 3}(Sc,Zr) particles and/or their coarsening was slightly facilitated by the previous cold rolling. The presence of Sc,Zr-containing particles has a significant antirecrystallization effect that prevents recrystallization at temperatures minimally up to 420 °C. The precipitation of the Al{sub 6}Mn- and/or Al{sub 6}(Mn,Fe) particles of a size ∼ 1.0 μm at subgrain boundaries has also an essential antirecrystallization effect and totally suppresses recrystallization during 32 h long annealing at 550 °C. The texture development of the alloys seems to be affected by high solid solution strengthening by Mn. The precipitation of the Mn-containing alloy is highly enhanced by a cold rolling. The apparent activation energy of the Al{sub 3}Sc particles formation and/or coarsening and that of the Al{sub 6}Mn and/or Al{sub 6}(Mn,Fe) particle precipitation in the powder and in the compacted alloys were determined. The cold deformation has no effect on the apparent activation energy values of the Al{sub 3}Sc-phase and the Al{sub 6}Mn-phase precipitation. - Highlights: • The Mn, Sc and Zr additions to Al totally suppresses recrystallization at 550 °C. • The Sc,Zr-containing particle precipitation is slightly facilitated by cold rolling. • The Mn-containing particle precipitation is highly enhanced by cold rolling. • Cold rolling has no effect on activation energy of the Al{sub 3}Sc and Al{sub 6}Mn precipitation. • The texture development is affected by high solid solution strengthening by Mn.

36 MATERIALS SCIENCE↗

Investigation on phase transformation mechanism of zeolite NaY under alkaline hydrothermal conditions

The phase transformation mechanism of zeolite NaY under alkaline hydrothermal conditions was investigated by UV Raman spectroscopy, X-ray diffraction, X-ray fluorescence and scanning electron microscopy techniques. The results revealed that the products and transformation rate are dependent on the alkalinities. All of the starting and resulting zeolites are constructed with the 4-ring and 6-ring secondary building units. The products have lower Si/Al ratio, higher framework density and smaller pore size, which are more stable under alkaline hydrothermal condition. During the phase transformation the fragments of faujasite are formed, then the fragments combine to form different zeolites depending on basicity. Zeolite NaY crystals are consumed as the reservoir for the transformation products during the recrystallization process. For the first time, a 4-membered ring intermediate was found at the early stage of the recrystallization process. A cooperative interaction of liquid and solid phases is required for inducing the phase transformation. - Graphical Abstract: Phase transformation of NaY zeolite under alkaline hydrothermal condition is achieved by the cooperative interaction of the liquid and solid phases. A 4-membered ring species is an intermediate for recrystallization process. Highlights: • The products and transformation rate are dependent on the alkalinity. • A 4-membered ring species is an intermediate for recrystallization process. • A cooperative interaction of liquid and solid phases is required.

36 MATERIALS SCIENCE↗

Effect of Zr on microstructures and mechanical properties of an Al-Mg-Si-Cu-Cr alloy prepared by low frequency electromagnetic casting

The Al-1.6Mg-1.2Si-1.1Cu-0.15Cr (all in wt. %) alloys with and without Zr addition prepared by low frequency electromagnetic casting process were investigated by using the optical microscope, scanning electron microscope and transmission electron microscope equipped with energy dispersive analytical X-ray. The effects of Al{sub 3}Zr phases on the microstructures and mechanical properties during solidification, homogenization, hot extrusion and solid solution were studied. The results show that Al{sub 3}Zr phases reduce the grain size by ∼ 29% and promote the formation of an equiaxed grain structure during solidification. Numerous spherical Al{sub 3}Zr dispersoids with 35–60 nm in diameters precipitate during homogenization, and these fine dispersoids change little during subsequent hot extrusion and solid solution. Adding 0.15 wt. % Zr results in no recrystallization after hot extrusion and partial recrystallization after solid solution, while the recrystallized grain size is 400–550 μm in extrusion direction in the Zr-free alloy. In addition, adding 0.15 wt. % Zr can obviously promote Q′ phase precipitation, while the β″ phases are predominant in the alloy without Zr. Adding 0.15 wt. % Zr, the ultimate tensile strength of the T6 treated alloy increases by 45 MPa, while the elongation remains about 16.7%. - Highlights: • Minor Zr can refine as-cast grains of the LFEC Al-Mg-Si-Cu-Cr alloy. • L1{sub 2} Al{sub 3}Zr phases with 35–60 nm in diameter precipitate during homogenization. • L1{sub 2} and DO{sub 22} Al{sub 3}Zr phases result in partial recrystallization after solid solution. • Minor Zr can promote the precipitation of Q′ phases. • Mechanical properties of Al-Mg-Si-Cu-Cr-Zr alloy are higher than those of AA7005.

36 MATERIALS SCIENCE↗

Characterization of microstructure and texture across dissimilar super duplex/austenitic stainless steel weldment joint by austenitic filler metal

The evolution of microstructure and texture across an as-welded dissimilar UNS S32750 super duplex/UNS S30403 austenitic stainless steel joint welded by UNS S30986 (AWS A5.9 ER309LMo) austenitic stainless steel filler metal using gas tungsten arc welding process was evaluated by optical micrography and EBSD techniques. Due to their fabrication through rolling process, both parent metals had texture components resulted from deformation and recrystallization. The weld metal showed the highest amount of residual strain and had large austenite grain colonies of similar orientations with little amounts of skeletal ferrite, both oriented preferentially in the < 001 > direction with cub-on-cube orientation relationship. While the super duplex stainless steel's heat affected zone contained higher ferrite than its parent metal, an excessive grain growth was observed at the austenitic stainless steel's counterpart. At both heat affected zones, austenite underwent some recrystallization and formed twin boundaries which led to an increase in the fraction of high angle boundaries as compared with the respective base metals. These regions showed the least amount of residual strain and highest amount of recrystallized austenite grains. Due to the static recrystallization, the fraction of low degree of fit (Σ) coincident site lattice boundaries, especially Σ3 boundaries, was increased in the austenitic stainless steel heat affected zone, while the formation of subgrains in the ferrite phase increased the content of < 5° low angle boundaries at that of the super duplex stainless steel. - Graphical abstract: Display Omitted - Highlights: • Extensive grain growth in the HAZ of austenitic stainless steel was observed. • Intensification of < 100 > orientated grains was observed adjacent to both fusion lines. • Annealing twins with Σ3 CSL boundaries were formed in the austenite of both HAZ. • Cub-on-cube OR was observed between austenite and ferrite in the weld metal. • Weld metal had the lowest texture intensity and ratio of low angle and CSL boundaries.

36 MATERIALS SCIENCE↗

Study of grain structure evolution during annealing of a twin-roll-cast Mg alloy

The evolution of microstructure under static annealing was studied for mid-thickness section of a twin-roll-cast (TRC) magnesium alloy. Annealing was performed at 300 °C and 500 °C for different times. Microstructural evolution was quantitatively analyzed, from optical micrographs, using grain path envelope analysis. Additional information from electron backscatter diffraction (EBSD) was used for addressing the possible mechanism(s). It was found that the TRC structure had a bimodal grain size, which was preserved even after annealing at 300 °C. However, the annealing at 500 °C led to a unimodal grain size. This difference in the grain size distribution created a contrasting behavior in the normalized standard deviations. This was primarily attributed to a competition between recovery and recrystallization, and their respective dominance at 300° and 500 °C. A deformation induced recrystallization recovery (DIRR) model was proposed. The proposed model could successfully address the experimental microstructural evolution. - Highlights: • Annealing of twin roll cast (TRC) magnesium alloy was done at temperatures of 300 °C and 500 °C. • TRC had bimodal structure. Bimodality preserved for annealing at 300 °C. Annealing at 500 °C led to unimodal structure. • Grain evolution was described based on the competition between recovery and recrystallization. • Deformation induced recrystallization recovery (DIRR) mechanistic model was developed.

36 MATERIALS SCIENCE↗

Development of microstructure and texture during single and multiple pass friction stir processing of a strain hardenable aluminium alloy

Highlights: • Development of microstructure and texture during single and multiple pass FSP of a strain hardenable aluminium alloy • Strain induced boundary migration (SIBM) is the dominant nucleation mechanism for recrystallization • Weak crystallographic texture development influenced by SIBM with the relative dominance of shear texture components • Stable microstructure and texture development after multiple pass FSP • FSP is a promising method for the secondary processing of strain hardenable aluminium alloys - Abstract: In the present study, microstructure and texture development during single and multiple pass friction stir processing (FSP) of a strain hardenable wrought AlMg alloy (AA5086) was investigated. Subtle differences were observed while comparing with heat treatable alloys in the nucleation mechanism of the recrystallized microstructure observed in the nugget zone. Strain induced boundary migration was the dominant mechanism of microstructure evolution in the alloy, which influenced the crystallographic texture development by weakening it. Micro-texture measurements reveal variations in the crystallographic texture along the thickness of the sample. Recrystallization texture components were observed in the nugget zone indicative of a pronounced static recrystallization in the alloy as compared to the heat treatable alloys. Bulk texture measurements within the nugget zone of the optimally processed sample reveal a relatively dominant C component of shear texture. Average grain size in the nugget zone remained the same and the bulk crystallographic texture components were retained during multiple-pass FSP. The lower strain energies involved and the enhanced recovery processes due to the high temperature materials processing of the alloy during FSP resulted in a stable microstructure and texture. In summary, FSP could be promoted as a competent and suitable secondary processing technique for the bulk production of ultra-fine-grained materials in strain hardenable aluminium alloys.

36 MATERIALS SCIENCE↗

Investigation of annealing temperature on microstructure and texture of Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel

Highlights: • Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel was investigated. • Shear bands provided recrystallization nucleation sites. • Annealing temperature can affect microstructure and texture. • r-bar increased to a maximum value (1.69) and then decreased to 1.42. - Abstract: The evolution of microstructure and texture of Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel annealed at different temperatures was investigated using a combination of X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). EBSD investigations confirm that the in-grain shear bands provide more recrystallization nucleation sites to γ-fiber recrystallization grains with high Taylor factor orientations during cold rolling requiring further annealing for a more homogenous equiaxied grain structure. As the annealing temperatures increase, the grains in center layer are oriented towards {110}∥ND, and the recrystallization grains at 1050 °C are dominated by the uniform and equiaxial γ-fiber grains favourable for the improvement of r-values, while the occurrence of {100} <011> texture detrimental to r-values indicates that an exorbitant annealing temperature can reduce the intensity of γ-fiber textures affecting the formability, accordingly, the average plastic strain ratio of ferritic stainless steel increases sharply up to a maximum value (1.69) and then decreases to a certain value (1.42).

36 MATERIALS SCIENCE↗

Non-equilibrium approach to prediction of microstructure evolution for metals undergoing severe plastic deformation

Highlights: • New consistent physically-based model of dynamic recrystallization. • The model is based on evolution of fraction of high-angle grain boundaries. • Possibility to predict the evolution of dislocation cells and grain boundaries. • The model is implemented for FEM simulations. • Results demonstrate inhomogeneous distribution of strain within the sample. - Abstract: Available models of dynamic recrystallization have a number of disadvantages that in most cases make them inapplicable for practical predictions of material microstructure evolution. Both the microstructural and the empirically based approaches do not reflect physical processes leading to evolution of material defect structure in the process of plastic deformation. This work presents an attempt to develop a consistent physically-based model of dynamic recrystallization. This model, accounting for physical nature of processes of material defect structure evolution, should provide a possibility to predict evolution of several different experimentally measurable parameters of material microstructure without introduction of big number of fitting parameters. It is suggested that such a model should be based on equation for evolution of fraction of high-angle grain boundaries (HAGBs) in the process of deformation. It is shown, that the new model gives a possibility to predict the evolution of dislocation cells and grain boundaries in copper-based alloys providing good coincidence with experimental observations. Full 3-dimensional numerical simulation of multidirectional forging of copper is performed utilizing the developed dynamic recrystallization model. The same 3D simulations demonstrate new noteworthy effects connected to inhomogeneous distribution of plastic strain within the bulk of the material and material strain hardening.

36 MATERIALS SCIENCE↗

Comparative study of Sc and Er addition on microstructure, mechanical properties, and electrical conductivity of Al-0.2Zr-based alloy cables

Highlights: • The comprehensive properties of Al-0.2Zr-0.1Sc were better than those of Al-0.2Zr-0.1Er alloy cable. • The microstructures evolved from fibrous grains to equiaxed grains with increasing annealing time. • The Zener drag force increased with increasing ratio of volume fraction (F{sub V}) to average diameter F{sub V}/ d-bar . • The capability to inhibit recrystallization was as follows: Al{sub 3}(Zr, Sc) > Al{sub 3}(Zr, Er) > Al{sub 3}Zr. - Abstract: The effect of the addition of 0.1 wt% Sc and 0.1 wt% Er on the deformation microstructure, Vickers microhardness, and electrical conductivity of Al-0.2 wt% Zr-based alloy cables annealed at 400 °C for different times was investigated. The comprehensive properties of Al-0.2Zr-0.1Sc were better than those of Al-0.2Zr-0.1Er. The optimal conditions for the Al-0.2Zr-01Sc alloy cable were a microhardness of 575 MPa, an electrical conductivity of 34.5 MS/m for an annealing time of 36 h, and those for the Al-0.2Zr-0.1Er alloy cable were a microhardness of 550 MPa, an electrical conductivity of 33.6 MS/m for an annealing time of 8 h. During the annealing process, dispersed Al{sub 3}(Zr,Sc/Er) precipitates were generated, which substantially impeded recrystallization by Zener pining of grain boundaries. Based on the ratio of volume fraction (F{sub V}) to average diameter ( d-bar ) of the precipitates, their capability to inhibit recrystallization was as follows: Al{sub 3}(Zr, Sc) > Al{sub 3}(Zr, Er) > Al{sub 3}Zr. Moreover, the electrical conductivity of Al-0.2Zr-0.1Sc was better than that of Al-0.2Zr-0.1Er, probably because Sc could better inhibit recrystallization than Er, leading to fewer grain boundaries and hence lesser electron scattering.

36 MATERIALS SCIENCE↗

Evolution of microstructure and microtexture during hot deformation in an advanced P/M nickel base superalloy

Highlights: • Microstructural evolution of PM superalloy sensitive to temperature and strain rate. • Highest DRX with finer grained structure at higher temperatures and strain rates. • Dominance of DDRX showed by serrated grain boundaries and misorientation gradient. • Weak microtextural evolution inclined towards [110] fiber compression texture seen. In the present study, the effect of hot deformation parameters on the microstructural evolution is investigated for an experimental powder metallurgy nickel superalloy. The hot isostatically pressed (HIPed) alloy is isothermally hot compressed at constant true strain rate over wide temperatures (1000 °C, 1050 °C, 1100 °C, 1150 °C) and strain rates (0.001 s{sup −1}, 0.01 s{sup −1}, 0.1 s{sup −1}, 1 s{sup −1}) regimes. Electron Back-Scattered Diffraction (EBSD) characterization of the hot deformed samples is carried out to evaluate the microstructural evolution, grain boundary characteristics, and microtextural behaviour. The strong dependence of dynamic recrystallization characteristics on the hot deformation conditions is divulged through EBSD derived colour inverse pole figure maps endorsed by grain/twin boundary characteristics and misorientation gradient. Dynamic recrystallization (DRX) is maximized at higher deformation temperatures, whereas limited DRX is observed at lower deformation temperatures, especially at higher strain rates. The dominance of discontinuous dynamic recrystallization (DDRX) is manifested through bulged/serrated grain boundaries resulting in the formation of necklace microstructure corroborated by grain boundary cumulative misorientation gradient. Although random microtexture is revealed in both deformed and recrystallized microstructures, the tendency towards the formation of 110 fiber compression texture is apparently evident.

36 MATERIALS SCIENCE↗

Additive friction stir deposition of SS316: Effect of process parameters on microstructure evolution

Solid state nature of additive friction stir deposition (AFSD) additive manufacturing process is very advantageous in terms of defect formation and microstructural refinement in the material. Current study presents the process optimization, microstructural evolution and kinetics of recrystallization for AFSD deposited low stacking fault energy material - SS316. As deposited microstructure shows equiaxed ultra fine grains with an average grain size of ~5.0 ± 0.5 μm. Shear deformation at high temperature during processing leads to the operation of restoration mechanisms. Observation of necklace type microstructure in the as deposited SS316 is attributed to discontinuous dynamic recrystallization during processing. Recrystallization kinetics of the AFSD SS316 is characterized using Johnson-Mehl-Avarami-Kolmogorov (JMAK) model. Deformation – thermal cycling during AFSD process resulted in inconsistent recrystallization kinetics. Variation in strain, strain rate and temperature during processing with processing parameters result in varying microstructure and tool wear. Further, high strength-ductility combination and sustained work hardening in as deposited SS316 appear to arise from transformation and twinning during deformation, leading to the formation of hierarchical twins and martensitic phase after deformation.

36 MATERIALS SCIENCE↗

Steam-assisted crystallization of TPA{sup +}-exchanged MCM-41 type mesoporous materials with thick pore walls

Highlights: ► Mesoporous Ti-containing silica with thicker pore walls was synthesized. ► Ion-exchange and steam-assisted crystallization led to MCM-41/MFI composite. ► The introduction of Ti inhibited the formation of separated MFI particles. ► Lower temperature favored retaining mesoporous characteristics and morphology. -- Abstract: Hierarchical MCM-41/MFI composites were synthesized through ion-exchange of as-made MCM-41 type mesoporous materials with tetrapropylammonium bromide and subsequent steam-assisted recrystallization. The obtained samples were characterized by powder X-ray diffraction (XRD), UV–vis diffuse reflectance spectroscopy, scanning electron microscopy (SEM), transmission electron microscopy (TEM), thermogravimetric analysis, FT-IR, {sup 1}H–{sup 13}C CP/MAS and nitrogen adsorption–desorption. The XRD patterns show that the MCM-41/MFI composite possesses both ordered MCM-41 phase and zeolite MFI phase. SEM and TEM images indicate that the recrystallized materials retained the mesoporous characteristics and the morphology of as-made mesoporous materials without the formation of bulky zeolite, quite different from the mechanical mixture of MCM-41 and MFI structured zeolite. Among others, lower recrystallization temperature and the introduction of the titanium to the parent materials are beneficial to preserve the mesoporous structure during the recrystallization process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Temperature dependence of electron-beam induced effects in amorphous apatite

Irradiation effects on pre-amorphized Sr2Nd8(SiO4)6O2 have been investigated under 200 and 300 keV electron-beam irradiation at 130 and 480 K using in situ transmission electron microscopy. At 480 K, recrystallization occurred from the amorphous/crystalline interface under both 200 and 300 keV e-beam irradiation. At 130 K, the 200 keV e-beam irradiation induced recrystallization only; however, 300 keV e-beam irradiation induced both recrystallization and an electron hammering effect in the amorphous material that resulted in radial expansion perpendicular to the incident electron-beam direction and shrinkage parallel to the electron-beam direction. Ionization-induced processes and knock-on displacement damage are suggested to be the mechanisms for the recrystallization and the electron hammering effect, respectively.

58 GEOSCIENCES↗

Mechanisms for pressure-induced crystal-crystal transition, amorphization, and devitrification of SnI{sub 4}

The pressure-induced amorphization and subsequent recrystallization of SnI{sub 4} have been investigated using first principles molecular dynamics calculations together with high-pressure {sup 119}Sn nuclear resonant inelastic x-ray scattering measurements. Above ∼8 GPa, we observe a transformation from an ambient crystalline phase to an intermediate crystal structure and a subsequent recrystallization into a cubic phase at ∼64 GPa. The crystalline-to-amorphous transition was identified on the basis of elastic compatibility criteria. The measured tin vibrational density of states shows large amplitude librations of SnI{sub 4} under ambient conditions. Although high pressure structures of SnI{sub 4} were thought to be determined by random packing of equal-sized spheres, we detected electron charge transfer in each phase. This charge transfer results in a crystal structure packing determined by larger than expected iodine atoms.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

An investigation of the microstructure and ductility of annealed cold-rolled tungsten

Tungsten is notoriously brittle metal at room temperature. Furthermore, contrary to most metals, plastic deformation increases ductility and recrystallization decreases ductility of tungsten. The fundamentals that govern this behavior have challenged academia and industry for decades. This paper focuses on understanding the controlling factors of ductility through a systematic investigation of the changes in microstructure and mechanical properties of cold-rolled tungsten that occur during annealing. Cold-rolled tungsten samples were annealed at temperatures up to 1400 °C, and mechanical testing and microstructural analysis was performed before and after annealing. Furthermore, a dislocation mobility model based on the Orowan equation was applied. The mechanisms of deformation are discussed within the context of deformed and annealed microstructures. The high fraction of low angle grain boundaries and high density of edge dislocations were found to be the most important factors for ductility. Although there were gradual changes in microstructure and mechanical properties, the ductility of cold-rolled tungsten was maintained up to 1300 °C. The material recrystallized when annealed above this temperature, had no ductility, and suffered brittle fracture. Microstructural characterizations of the as-rolled material revealed a typical BCC texture, with grains elongated in rolling direction and a large amount of edge dislocations and low angle grain boundaries. The level of texturing and the fraction of low angle grain boundaries diminished after recrystallization. It was found that, compared to the recrystallized material, as-rolled tungsten can accommodate over 7 orders of magnitude higher deformation velocity due to the high density of edge dislocations.

36 MATERIALS SCIENCE↗

Stabilization and transformation of selenium during the Fe(II)-induced transformation of Se(IV)-adsorbed ferrihydrite under anaerobic conditions

Selenium (Se) is an essential nutrient for human beings at trace concentrations, but also a hazardous contaminant at high concentrations. As an important geological adsorbent, the transformation of 2-line ferrihydrite (Fh) strongly influences the geochemical behavior of selenium. However, little is known about the effect of the recrystallization of Fh on the fate of adsorbed Se(IV) in the reducing environments. We investigated the redistribution and transformation of Se(IV) during the recrystallization of Se(IV)-adsorbed Fh accelerated by Fe(II) under anaerobic conditions. Synchrotron based X-ray absorption near edge structure (XANES) spectroscopy was utilized to characterize oxidation state of Se. Results revealed that the adsorbed Se(IV) inhibited the Fe(II)-catalyzed recrystallization of ferrihydrite to goethite. Transmission electron microscopy (TEM) images showed that pH and the presence of Se(IV) had significant impacts on the morphology of the produced goethite. Approximately 30–75% adsorbed Se(IV) transformed to phosphate-unextractable form, indicating that the adsorbed Se transformed to more stable phase during the recrystallization of Fh. The XANES results indicated that a small fraction of Se(IV) was reduced to elemental Se. Our study demonstrated that the stability of adsorbed Se(IV) on ferrihydrite could be enhanced during Fe(II)-catalytic transformation of Fh under anoxic environments.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fabrication of hierarchical Lewis acid Sn-BEA with tunable hydrophobicity for cellulosic sugar isomerization

Lewis acid Sn-BEA catalysts with tunable morphology and hydrophobicity were successfully synthesized by the recrystallization of post-synthetic Sn-BEA in the presence of ammonium fluoride (NH4F) and tetraethylammonium bromide (TEABr). Three-dimensionally ordered mesoporous imprinted (3DOm-i) and nanocrystalline Sn-BEA catalysts with hydrophobic surface were synthesized for the first time by the method. This recrystallization method includes the dissolution of crystalline zeolite BEA by fluoride ions and the rearrangement of different types of silanol defects in the presence of TEABr. The method allows the final products to simultaneously inherit the morphology of their parent Al-BEA zeolites, and significantly reduce silanol defects within the catalysts. The Sn-BEA catalysts synthesized from the recrystallization method show largely enhanced catalytic performance for both glucose isomerization and bulky lactose isomerization in different solvents, which is presumably due to the hydrophobic surface and improved molecular transport property in the hierarchical zeolites. The recrystallization approach is a facile and reliable strategy to improve the hydrophobicity of zeolite catalysts with tunable morphologies ranging from nanocrystals to hierarchical structures.

bio-inspired↗