At least 397 records · Page 22

Effect of annealing temperature on titania nanoparticles

Titania polycrystalline samples are prepared by using sol-gel route hydrolyzing a alkoxide titanium precursor under acidic conditions. The as prepared samples are treated with different calcination temperatures. The anatase phase of titania forms when treated below 600°C, above that temperature the anatase phase tends to transform into the rutile phase of titania. The experimental determination of average grain size, phase formation, lattice parameters and the crystal structures of titania samples at different calcinations is done using X-ray diffraction (XRD). Fourier Transform Infra-red Spectroscopy (FTIR), UV-vis-NIR spectroscopy and Scanning Electron Microscopy (SEM) and Energy Dispersive Analysis X-ray are used to characterize the samples to bring impact on the respective properties.

36 MATERIALS SCIENCE↗

Effects of graphene oxide concentration on optical properties of ZnO/RGO nanocomposites and their application to photocurrent generation

The effects of different concentrations of graphene oxide (GO) on the structure and optical properties of ZnO nanoparticles (NPs) were investigated. The nanocomposites were synthesized via the sol-gel method in a gelatin medium. X-ray diffraction patterns (XRD) and Fourier transform infrared spectroscopy indicated that the GO sheets were reduced and changed to reduced GO (RGO) during the calcination of the nanocomposites at 400 °C. In addition, the XRD patterns of the NPs indicated a hexagonal (wurtzite) structure for all the products. Microscopic studies showed that the NPs were decorated and dispersed on the RGO sheets very well. However, these studies revealed that the RGO concentration had an effect on the crystal growth process for the ZnO NPs. Furthermore, these studies showed that the NPs could be grown with a single crystal quality in an optimum RGO concentration. According to the XRD results that were obtained from pure ZnO NPs, the calcinations temperature was decreased by the RGO. UV–vis and room temperature photoluminescence studies showed that the optical properties of the ZnO/RGO nanocomposite were affected by the RGO concentration. Finally, the obtained ZnO/RGO nanocomposite was used to generate a photocurrent. Observations showed that the photocurrent intensity of the nanocomposite was significantly increased by increasing the RGO, with an optimum RGO concentration.

36 MATERIALS SCIENCE↗

Integrated Mg/TiO{sub 2}-ionic liquid system for deep desulfurization

A series of Mg/TiO{sub 2} photocatalysts were prepared using wet impregnation method followed by calcination at 300, 400 and 500°C for 1 h. The photocatalysts were characterized using Thermal Gravimetric Analysis, Fourier-Transform Infrared Spectroscopy, X-Ray Diffraction, and Field Emission Scanning Electron Microscopy. The performance for deep desulfurization was investigated using model oil with 100 ppm sulfur (in the form of dibenzothiophene). The integrated system involves photocatalytic oxidation followed by ionic liquid-extraction processes. The best performing photocatalyst was 0.25wt% Mg loaded on titania calcined at 400°C (0.25Mg400), giving 98.5% conversion of dibenzothiophene to dibenzothiophene sulfone. The highest extraction efficiency of 97.8% was displayed by 1,2-diethylimidazolium diethylphosphate. The overall total sulfur removal was 96.3%.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Controlled synthesis and magnetic properties of monodispersed ceria nanoparticles

In the present study, monodispersed CeO{sub 2} nanoparticles (NPs) of size 8.5 ± 1.0, 11.4 ± 1.0 and 15.4 ± 1.0 nm were synthesized using the sol-gel method. Size-dependent structural, optical and magnetic properties of as-prepared samples were investigated by X-ray diffraction (XRD), field emission scanning electron microscope (FE-SEM), high resolution transmission electron microscopy (HR-TEM), ultra-violet visible (UV-VIS) spectroscopy, Raman spectroscopy and vibrating sample magnetometer (VSM) measurements. The value of optical band gap is calculated for each particle size. The decrease in the value of optical band gap with increase of particle size may be attributed to the quantum confinement, which causes to produce localized states created by the oxygen vacancies due to the conversion of Ce{sup 4+} into Ce{sup 3+} at higher calcination temperature. The Raman spectra showed a peak at ∼461 cm{sup -1} for the particle size 8.5 nm, which is attributed to the 1LO phonon mode. The shift in the Raman peak could be due to lattice strain developed due to variation in particle size. Weak ferromagnetism at room temperature is observed for each particle size. The values of saturation magnetization (Ms), coercivity (Hc) and retentivity (Mr) are increased with increase of particle size. The increase of Ms and Mr for larger particle size may be explained by increase of density of oxygen vacancies at higher calcination temperature. The latter causes high concentrations of Ce{sup 3+} ions activate more coupling between the individual magnetic moments of the Ce ions, leading to an increase of Ms value with the particle size. Moreover, the oxygen vacancies may also produce magnetic moment by polarizing spins of f electrons of cerium (Ce) ions located around oxygen vacancies, which causes ferromagnetism in pure CeO{sub 2} samples.

36 MATERIALS SCIENCE↗

Synthesis and characterization of CuO nano particles using precipitation method

A simple and efficient synthesis of CuO nanoparticles was carried out by precipitation method using copper metal chips as precursor and sodium hydroxide as a stabilizing agent at different calcinations temperatures (100°C, 150°C, and 175°C). The products were characterized by powder X-ray diffraction (XRD), scanning electron microscopy (SEM), and Fourier Transform Infrared Spectroscopy (FTIR). XRD indicated monoclinic structure of CuO. SEM indicated the variation in nanostructures with the heating temperatures and FTIR inidcated Cu-O stretching frequencies. The CuO nanostructures with the average particle size of about 16.52 nm were prepared at 100°C for 3 hr. When the calcinations temperature was increased to 150°C and 175°C, CuO nanostructures with the particle size of about 17.41 nm, and 18.44 nm were obtained respectively. This aqueous precipitation method can give a large scale production of CuO nanoparticles easily.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Combustion synthesis and structural analysis of nanocrystalline nickel ferrite at low temperature regime

Combustion synthesis of single phase Nickel ferrite was successfully achieved at low temperature regime. The obtained powders were calcinated to increase the crystallinity and their characterization change due to calcinations is investigated in detail. Citric acid used as a chelating agent for the synthesis of nickel ferrite. Pure single phase nickel ferrites were found at this low temperature. The average crystalline sizes were measured by using powder XRD measurements. Surface morphology was investigated through Transmission Electron Microscope (TEM). Particle size calculated in XRD is compared with TEM results. Magnetic behaviour of the samples is analyzed by using Vibrating Sample Magnetometer (VSM). Saturation magnetization, coercivity and retentivity are measured and their results are discussed in detail.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study of phase transformation and microstructure of alcohol washed titania nanoparticles for thermal stability

Nanostructured titania have been successfully synthesized by hydrolysis of alkoxide at calcination temperatures 500 °C, 600 °C and 700 °C. As the calcination temperature increases, alcohol washed samples show lesser rutile content as compared to water washed samples. Morphology and Particle sizes was determined by field emission scanning electron microscopy (FESEM), while thermogravimetric-differential scanning calorimetry (TG-DSC) was used to determine thermal stability. Alcohol washed samples undergo 30% weight loss whereas 16% in water washed samples was observed. The mean particle sizes were found to be increase from 37 nm to 100.9 nm and 35.3 nm to 55.2 nm for water and alcohol washed samples respectively. Hydrolysis of alkoxide was shown to be an effective means to prepare thermally stable titania by using alcohol washed samples as a precursor.

36 MATERIALS SCIENCE↗

Fast crystallization of amorphous Gd{sub 2}Zr{sub 2}O{sub 7} induced by thermally activated electron-beam irradiation

We investigate the ionization and displacement effects of an electron-beam (e-beam) on amorphous Gd{sub 2}Zr{sub 2}O{sub 7} synthesized by the co-precipitation and calcination methods. The as-received amorphous specimens were irradiated under electron beams at different energies (80 keV, 120 keV, and 2 MeV) and then characterized by X-ray diffraction and transmission electron microscopy. A metastable fluorite phase was observed in nanocrystalline Gd{sub 2}Zr{sub 2}O{sub 7} and is proposed to arise from the relatively lower surface and interface energy compared with the pyrochlore phase. Fast crystallization could be induced by 120 keV e-beam irradiation (beam current = 0.47 mA/cm{sup 2}). The crystallization occurred on the nanoscale upon ionization irradiation at 400 °C after a dose of less than 10{sup 17} electrons/cm{sup 2}. Under e-beam irradiation, the activation energy for the grain growth process was approximately 10 kJ/mol, but the activation energy was 135 kJ/mol by calcination in a furnace. The thermally activated ionization process was considered the fast crystallization mechanism.

36 MATERIALS SCIENCE↗

Synthesis of anatase and rutile TiO{sub 2} nanostructures from natural ilmenite

Nanostructure anatase and rutile type TiO{sub 2} were synthesized from dissolution roasted ilmenite from natural ilmenite sand as the starting materials. Anatase TiO{sub 2} and rutile TiO{sub 2} (high crystallinity) with the diameters of 20–100 nm were obtained by calcined soluble ilmenite sand produced by leaching process. Calcinations of the xerogel TiO{sub 2} from liquor products were conducted for 4 hours at temperature of 450 °C. The samples were characterized by XRD (X-ray diffraction), STA (simultant thermal analysis), TEM (Transmission Electron Microscopy), and BET surface area. Titania Anatase-Rutile form as a mixture were produced by titania slag with the hydrolysis product. While, in another route, complete titania anatase phase was produced through hydrolysis and condensation steps of leach liquors. This synthesis methods provide a simple route to fabricate nanostructure TiO{sub 2} from low cost material.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of microwave-assisted sintering on dielectric properties of CaCu{sub 3}Ti{sub 4}O{sub 12} ceramic

In this present work, CaCu{sub 3}Ti{sub 4}O{sub 12} (CCTO) was synthesized by conventional solid-state reaction technique. The synthesis process was carried out in two phases; by conventional process (calcination and sintering at 1080°C for 10 hours) and phase II involves the micro assisted pre sintering of conventionally calcined CCTO for very short soaking time of 30 min at 1080°C in a microwave furnace followed by sintering at 1080°C for 10 hours in conventional furnace. X-ray diffraction (XRD) patterns confirmed the formation of single phase ceramic. Dielectric properties were studied over the frequency range from 50Hz -5MHz at temperatures (273K-343K). It was observed that pre- microwave sintering enhance the dielectric constant values from 10900 to 11893 and respectively reduces the dielectric loss values from 0.49 to 0.34 at room temperature(1 KHz). CCTO ceramics which are found desirable for many technological applications. The effect is more pronounced at low frequencies of applied electric field.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Temperature Dependent Raman Spectroscopic Study of the Fe Doped La{sub 0.67}Sr{sub 0.33}MnO{sub 3} Prepared Using Ball Milling Method

Polycrystalline samples of La{sub 0.67}Sr{sub 0.33}Mn{sub 0.65}Fe{sub 0.35}O{sub 3} (LSMFO) were synthesized using the standard ball mill method with different calcination temperatures ranging from 800 to 1100°C for 7 h. The phase purity of these samples was confirmed using X-ray diffraction (XRD) patterns. All samples were found to have rhombohedral crystal structure with R 3-bar c space group. The lattice parameters, cell volume, bond angle and bond length have been obtained using the Rietveld refinement by FullProf software. The average crystallite size calculated using the Debye-Scherrer formula was found between 27 and 60 nm. Surface morphology of the prepared samples has been examined using a scanning electron microscope (SEM). SEM images show the formation of well-arranged grain sizes distributed from 240 to 400 nm, much larger than one estimated using the Scherrer formula. All tiny particles are highly agglomerated with the increasing temperature and porosity decreases with increasing temperature. An analysis of the frequency and peak broadening of Raman modes as a function of temperature clearly shows the significant temperature effect on the A{sub 1g} and E{sub g} modes of LSMFO. The shifts and broadening of the A{sub 1g} and E{sub g} modes are discussed in light of the oxygen sublattice distortion. Our study shows the reduction in distortion with increasing calcination temperature, which suggests a decrease in the JT effect.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Aqueous Chloride Operations Overview: Plutonium and Americium Purification/Recovery

These are a set of slides intended for an information session as part of recruiting activities at Brigham Young University. It gives an overview of aqueous chloride operations, specifically on plutonium and americium purification/recovery. This presentation details the steps taken perform these processes, from plutonium size reduction, dissolution, solvent extraction, oxalate precipitation, to calcination. For americium recovery, it details the CLEAR (chloride extraction and actinide recovery) Line, oxalate precipitation and calcination.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Demonstration of Scaled-Production of Rare Earth Oxides and Critical Materials from U. S. Coal-Based Sources (Final Report)

The project objective was to demonstrate scaled production of high purity rare earth oxides (REO), nominally exceeding 90% grade, from coal refuse sources using innovative technologies that reduce cost and improve environmental outcomes relative to traditional rare earth processing technologies. The project utilized a critical material pilot plant constructed and tested as part of a previous U.S. Department of Energy project. Target performance criteria was a 50% reduction in production cost based on previous optimum values, 150% increase in recovery and greater than 2% concentrates of rare earth oxides, cobalt and manganese. Concentrate production goals were to produce a rare earth mix oxide product at a rate of 200 grams per day having a minimum purity of 50% as well as products of cobalt and manganese having a minimum purity of 2%. A previous pilot plant investigation identified acid cost as the major contributor to an operating cost that made the recovery of rare earth and other critical metals from bituminous coal sources economically challenging. As such, acid cost reduction was a major target using bio-oxidation reactors to produce sulfuric acid from naturally occurring coal pyrite. Based on laboratory data, a bio-oxidation circuit was designed for the pilot plant to produce 7.5 l/min of acid using two 11-m3 (3000 gallon) reactors equipped with 40 hp aerators for air dispersion. The pilot-scale tests revealed that acid concentration equivalent to as high as 1.0 M sulfuric acid could be continuously produced. However, the bio-acid contained exceptionally high iron concentrations, which complicated downstream processing of the pregnant leach solution (PLS). A TEA of the bio-oxidation circuit showed that production cost was approximately $0.13 per kg acid equivalent if produced using a four-day retention time in the reactors. This value represents a 48% reduction from that of purchased bulk sulfuric acid. Calcination (or roasting) studies were conducted on coarse refuse from West Kentucky No. 13 and Fire Clay coal seam sources. The test results revealed the potential to increase recovery by nearly 100% using temperatures between 500°C to 700°C with light REE recovery value being the most improved. Acid baking of the calcined products using sulfuric acid at 250°C increased heavy rare earth recovery from around 40% to 80% while decreasing the acid requirements by over 50%. The existing pilot plant was upgraded for the pilot scale demonstration of REE and CM recovery. The primary feedstocks were West Kentucky No.13 and heap leach pregnant leach solution (PLS) while a secondary feedstock was a lignite waste material from a construction sand operation. The pilot scale operation started with PLS generation through leaching followed by iron and aluminum removal, nominally at 3.3 and 4.5 pH, respectively. Leaching lixiviants used for the test were industrial grade sulfuric acid or bio-acid generated at the pilot scale facility. For most of the tests, the solid feed rate was 200 lb/hr whereas lixiviant was added at 2 gpm to provide an optimal residence time of 45 minutes. Following the contaminant removal step, several different process schematics were tested with the goal of maximizing REE recovery and purity. In the first test, direct processing of aluminum precipitation raffinate for REE recovery using oxalic acid at pH 1.5 was investigated. Overall REE recovery was approximately 45%. Unfortunately, elevated calcium content in the PLS significantly impacted the RE-Oxide product grade. Similarly, high calcium content decreased both the product purity and grades of CM products. As such, a new flowsheet was tested with the same initial process schematic but different precipitation stages for REEs and CMs at pH 6.0 and 9.0, respectively. It was noted that the overlapping precipitation behavior of Co, Ni and Zn with REEs limited the applicability of this process schematic. While this change increased the RE-Oxide grade from 36% in the first test to 87%, the loss of critical metals to the REE cake and bypass of the REEs to the CM cake significantly impacted the recovery of both REEs and CMs. Therefore, the modified process flowsheet combined oxalic acid precipitation stage raffinate and redissolved CM cake filtrate to maximize both the recovery and purity of the products. Consequently, a RE-Oxide product with 85% purity and CM cakes with over 19% Co, 38% Ni, 14% Zn and 9% Mn content were generated with significantly higher recoveries. While the modified process flowsheet improved recoveries and grades, elemental losses observed in separate precipitation and redissolution losses inspired the adaptation of a single precipitation stage at pH 9.0 for both REEs and CMs. This change was anticipated to maximize the REE recovery while minimizing the costs associated with separated redissolution and processing stages. As expected, REE recovery in this new circuit arrangement was over 56% with a product grade of over 87% RE-Oxide content. Similarly, Co, Ni, Mn, and Zn recoveries of 54%, 40%, 67%, and 66%, respectively, were achieved. Unfortunately, the elevated calcium content present in the solution due to its precipitation at pH 9.0 caused a decrease in the CM cake quality. Therefore, the final process flowsheet involved the addition of calcium oxalate precipitation following the oxalic acid precipitation stage, which effectively eliminated calcium contamination of the CM products. Finally, the pilot scale experiments conducted using bio-acid achieved comparable REE leaching recoveries to the conventional sulfuric acid leaching. Elevated iron concentration in the solution caused the co-precipitation of REEs with the iron and aluminum cake, resulting in the REE losses. Furthermore, elevated iron content bypassing the iron and aluminum precipitation stages contaminated the metal sulfide and manganese cake, respectively. A techno-economic analysis was performed based on a commercial facility capable of treating 500 tph of coal-based material. The production cost for West Kentucky No. 13 coarse refuse material ranged from approximately $500-$700/kg of total rare earth oxide whereas the lignite source had significantly lower production cost of $100-$300/kg. The significant difference in cost was due to the easier leaching characteristics of the lignite material and the higher feed concentrations. All process scenarios resulted in a negative net present value (NPV). For the lignite feedstock, laboratory REE leach recovery values were about 30% higher than the pilot plant data. Using the lab leach results, a positive net present value was achieved and the production cost decreased from $100-$300 $/kg to less than $150/kg of total REO.

01 COAL, LIGNITE, AND PEAT↗

The character of W-doped one-dimensional VO{sub 2} (M)

The one-dimensional W-doped VO{sub 2} (M) solid solutions with a various doped content were successfully synthesized under hydrothermal condition and subsequent calcination for the first time, and physical-chemical and phase transformation character were explored, subsequently. DSC analyses displayed that the phase-transition temperature of VO{sub 2} (M) solid solution could be linearly tuned with the doped content. Promisingly, the one-dimensional W-doped VO{sub 2} (M) had a good thermochromic property. - Graphical Abstract: One-dimensional W-doped VO{sub 2} (M) solid solutions with a various doped content were synthesized under hydrothermal condition and subsequent calcination. The physical-chemical and phase transformation character were explored, subsequently.

36 MATERIALS SCIENCE↗

Porous cobalt oxide (Co{sub 3}O{sub 4}) nanorods: Facile syntheses, optical property and application in lithium-ion batteries

We developed a facile synthetic route of porous cobalt oxide (Co{sub 3}O{sub 4}) nanorods via a microemulsion-based method in combination with subsequent calcination process. The porous structure was formed by controlled decomposition of the microemulsion-synthesized precursor CoC{sub 2}O{sub 4} nanorods without destruction of the original morphology. The as-prepared Co{sub 3}O{sub 4} nanorods, consisting of small nanoparticles with diameter of 80-150 nm, had an average diameter of 200 nm and a length of 3-5 {mu}m. The morphology and structure of synthesized samples were characterized by transmission electron microscopy and scanning electron microscopy. The phase and composition were investigated by X-ray powder diffraction and X-ray photoelectron spectroscopy. The optical property of Co{sub 3}O{sub 4} nanorods was investigated. Moreover, the porous Co{sub 3}O{sub 4} nanorods exhibited high electrochemical performance when applied as cathode materials for lithium-ion batteries, which gives them good potential applications. - Graphical abstract: The porous Co{sub 3}O{sub 4} nanorods synthesized via a microemulsion-based method in combination with subsequent calcination were applied in the negative electrode materials for lithium-ion batteries and exhibited high electrochemical performance.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

An alternative solid-state method to prepare pyrochlore-free KTaO{sub 3} at low temperature

Perovskite-type KTaO{sub 3} powder was synthesized by an alternative solid-state method at low temperature. Stoichiometric ammonium tantalum hydroxide, K{sub 2}C{sub 2}O{sub 4} and KF were mixed in water and then dried at room temperature. The crude product was formed by calcining the dried mixture at different temperatures. Pyrochlore-free KTaO{sub 3} powder was successfully synthesized after treating the crude product with water. KF plays an important role to inhibit the formation of pyrochlore K{sub 2}Ta{sub 2}O{sub 6} during the calcination process of ammonium tantalum hydroxide/K{sub 2}C{sub 2}O{sub 4}/KF mixture. X-ray diffraction (XRD), scanning electron microscopy (SEM), Fourier-transform infrared (FTIR) spectroscopy, UV-vis diffuse reflectance (UV-vis) spectroscopy and thermogravimetric (TG) analysis were used to characterize the precursor compound and as-prepared samples. XRD results show that pyrochlore-free KTaO{sub 3} powder can be obtained at 600 deg. C. SEM results reveal that the as-prepared products are agglomerated and each of the agglomerations consists of many small grains with 10-30 nm in diameter. - Graphical abstract: Pyrochlore-free KTaO{sub 3} powder was prepared at 600 deg. C using tantalum hydroxide/K{sub 2}C{sub 2}O{sub 4}/KF raw materials. Pyrochlore K{sub 2}Ta{sub 2}O{sub 6} and perovskite KTaO{sub 3} coexist at 600 deg. C using tantalum hydroxide/K{sub 2}C{sub 2}O{sub 4} raw materials. Highlights: > In-situ degradation of TaO{sub x}(OH){sub 5-x}(NH{sub 4}){sub x}, K{sub 2}C{sub 2}O{sub 4} and KF promotes the reaction. > Synthesis of KTaO{sub 3} displayed a two-step reaction path with the intermediate formation of K{sub 2}TaO{sub 3}F. > Formation of intermediate K{sub 2}TaO{sub 3}F benefits to prepare pyrochlore-free KTaO{sub 3} at low temperature. > Pyrochlore-free KTaO{sub 3} is prepared at 600 deg. C, which is the lowest temperature reported so far by hard chemistry method. > Synthetic method is a facile, rapid, low price and environment friendly route.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Evaluation of Adsorption Properties for Cs and Sr Selective Adsorbents-13171

The development of effective treatment and disposal methods is very urgent and important subject. Tohoku University and UNION SHOWA have developed various selective adsorbents (zeolites, zeolite sheets and composites loaded with insoluble ferrocyanides) for the effective decontamination of radioactive Cs{sup +} and Sr{sup 2+} As for Cs{sup +} adsorption, CST, chabazite and insoluble ferrocyanides composites had relatively large distribution coefficients (K{sub d}) above 10{sup 3} cm{sup 3}/g and excellent adsorption kinetics in seawater. Even after high temperature calcination at 1,100 deg. C, cesium was still immobilized in the calcined products of Cs{sup +}-zeolites, suggesting high immobilization ability of zeolites for Cs{sup +}. As for Sr{sup 2+} adsorption, A and X zeolites had relatively large K{sub d} values around 10{sup 2} cm{sup 3}/g, and zeolite sheet (A zeolite) exhibited excellent adsorption kinetics in seawater. Considering the decontamination of radioactive Sr{sup 2+} in groundwater, the effects of Ca{sup 2+} and Mg{sup 2+} ions on the K{sub d} value of Sr{sup 2+} were further examined by batch method. The K{sub d} value of Sr{sup 2+} was almost independent of Mg{sup 2+} concentration up to 2,500 ppm, while gradually lowered in the presence of Ca{sup 2+} above 200 ppm, due to the differences in the ionic radius of hydrated ion. The Cs{sup +} and Sr{sup 2+} adsorption ability for KNiFC-A (composite of A zeolite loaded with insoluble ferrocyanides) was examined by batch method. Here the matrix of composite (A zeolite) and loaded ferrocyanides (KNiFC) have high selectivity towards Sr{sup 2+} and Cs{sup +}, respectively. The K{sub d} values of Sr{sup 2+} and Cs{sup +} in seawater were estimated to be above 10{sup 2} and 10{sup 3} cm{sup 3}/g, respectively, indicating the effectiveness for the decontamination of both Sr{sup 2+} and Cs{sup +}. The basic data on the Cs{sup +} and Sr{sup 2+} adsorption properties for selective adsorbents are effective for the practical decontamination processes of these metal ions in seawater and groundwater. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗