Search NASA⌕ Search

SEARCH · Search NASA

Results for “ELECTROMECHANICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Flexoelectricity of a Calamitic Liquid Crystal Elastomer Swollen with a Bent-core Liquid Crystal

We have measured the electric current induced by mechanical distortion of a calamitic liquid crystal elastomer (LCE) swollen with a low molecular weight bent-core nematic (BCN) liquid crystal, and have determined, for the first time, the bend flexoelectric coefficient e{sub 3} of such a BCN-LCE composite. In one method, we utilize air-pressure to induce a mechanical bend deformation and flexoelectric polarization in a BCN-LCE film, and then measure the polarization current as a function of time. An alternative technique uses a rotary-motor driven scotch yoke to periodically flex the BCN-LCE; in this case, the magnitude and phase of the induced current are recorded via a lock-in amplifier. The flexoelectric coefficient, e{sub 3}, was found to be {approx}20 nC/cm{sup 2}, and is stable in magnitude from room temperature to {approx}65 C. It is about one third the value measured in samples of the pure BCN; this fraction corresponds closely to the molar concentration of BCN in the LCE. The flexoelectric current increases linearly with the magnitude of the bend deformation and decays with frequency. These observations indicate a promising way forward towards producing very low-cost, self-standing, rugged electromechanical energy conversion devices.

36 MATERIALS SCIENCE↗

Ionic electroactive polymer actuators as active microfluidic mixers

On-chip sample processing is integral to the continued development of lab-on-a-chip devices for various applications. An active microfluidic mixer prototype is proposed using ionic electroactive polymer actuators (IEAPAs) as artificial cilia. A proof-of-concept experiment was performed in which the actuators were shown to produce localized flow pattern disruptions in the laminar flow regime. Suggestions for further engineering and optimization of a scaled-down, complete device are provided. Furthermore, the device in its current state of development necessitates further engineering, the use of IEAPAs addresses issues currently associated with the use of electromechanical actuators as active microfluidic mixers and may prove to be a useful alternative to other similar materials.

36 MATERIALS SCIENCE↗

Visualization of ion transport in Nafion using electrochemical strain microscopy

The electromechanical response of a Nafion membrane immersed in water was probed using electrochemical strain microscopy (ESM) to redistribute protons and measure the resulting local strain that is caused by the movement of protons. We also measured the relaxation of protons from the surface resulting from proton diffusion. Using this technique, we can visualize and analyze the local strain change resulting from the redistribution and relaxation of hydrated protons.

Kim, Suran↗

Compositional phase diagram and microscopic mechanism of Ba 1-x Ca x Zr y Ti 1-y O 3 relaxor ferroelectrics

With extensive first-principles density-functional calculations, we construct a three-dimensional compositional phase diagram of Ba1-xCaxZryTi1-yO3 (BCZT) with the Ca and Zr content in the ranges of 0 ≤ xCa ≤ 0.2 and 0 ≤ yZr ≤ 1. Our calculations show that, when the Zr content increases, the difference in energy and difference in the structural parameters of the cubic, tetragonal, orthorhombic, and rhombohedral phases of BCZT are reduced. Eventually, all four phases merge into a multiphase with coexisting cubic structures (MPCCS) under Zr-rich conditions, indicating that BCZT undergoes phase transition from a normal ferroelectric (NFE) to a relaxor ferroelectric (RFE), consistent with experimental observations. The 3D diagram shows that the regions of merged and separated energy surfaces correspond to the regions of the RFE and NFE, respectively, which suggests that a MPCCS corresponds to a RFE. In addition, with the MPCCS model and Landau–Devonshire theory, we provide an interpretation of the high electromechanical properties of the BCZT relaxor ferroelectric and apply it to the classical local random field and micro–macro domain transition models.

Liu, Shi-Yu↗

Tailoring the crystal growth of quartz on silicon for patterning epitaxial piezoelectric films

Epitaxial films of piezoelectric α-quartz could enable the fabrication of sensors with unprecedented sensitivity for prospective applications in electronics, biology and medicine. However, the prerequisites are harnessing the crystallization of epitaxial α-quartz and tailoring suitable film microstructures for nanostructuration. Here, we bring new insights into the crystallization of epitaxial α-quartz films on silicon (100) from the devitrification of porous silica and the control of the film microstructures: we show that by increasing the quantity of devitrifying agent (Sr) it is possible to switch from an α-quartz microstructure consisting of a porous flat film to one dominated by larger, fully dense α-quartz crystals. We also found that the film thickness, relative humidity and the nature of the surfactant play an important role in the control of the microstructure and homogeneity of the films. Via a multi-layer deposition method, we have extended the maximum thickness of the α-quartz films from a few hundreds of nm to the μm range. Moreover, we found a convenient method to combine this multilayer approach with soft lithography to pattern silica films while preserving epitaxial crystallization. This improved control over crystallization and the possibility of preparing patterned films of epitaxial α-quartz on Si substrates pave the path to future developments in applications based on electromechanics, optics and optomechanics.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Light–ferroelectric interaction in two-dimensional lead iodide perovskites

The unique physical properties of two-dimensional (2D) metal halide perovskites (MHPs) such as nonlinear optics, anisotropic charge transport, and ferroelectricity have made these materials promising candidates for multifunctional applications. Recently, fluorine derivatives such as 4,4-difluoropiperidinium lead iodide perovskite or (4,4-DFPD, C 5 H 10 F 2 N) 2 PbI 4 have shown strong ferroelectricity as compared to other 2D MHPs. Although it was previously addressed that the ferroelectricity in MHPs can be affected by illumination, the underlying physical mechanisms of light–ferroelectricity interaction in 2D MHPs are still lacking. Here, we explore the electromechanical responses in 4,4-(DFPD) 2 PbI 4 thin films using advanced scanning probe microscopy techniques revealing ferroelectric domain structures. In this work, hysteretic ferroelectric loops measured by contact-Kelvin probe force microscopy are dependent on domain structures under dark conditions, while ferroelectricity weakens under illumination. The X-ray diffraction patterns exhibit significant changes in preferential orientation of individual lattice planes under illumination. Particularly, the reduced intensity of the (1 1 1) lattice plane under illumination leads to transitioning from a ferroelectric to a paraelectric phase. The instability of positive ions, especially molecular organic cations, is observed under illumination by time-of-flight secondary ion mass spectrometry. The combination of crystallographic orientation and chemical changes under illumination clearly contributes to the origin of light–ferroelectricity interaction in 2D (4,4-DFPD, C 5 H 10 F 2 N) 2 PbI 4 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Lead-free acoustic emission sensors

Acoustic emission (AE) sensors have been fabricated using both soft- and hard-type lead-free (Na{sub 0.5}K{sub 0.5})NbO{sub 3}-based ceramics. The acoustic and electromechanical properties of the ceramics have been determined using the resonance technique. The lead-free AE sensors were calibrated using a laser source and compared to a commercial sensor. A lead zirconate titanate (PZT) 5H ceramics AE sensor has also been fabricated and calibrated for comparison. It was found that the sensitivity of lead-free AE sensors is comparable to that of the lead-based PZT sensor. To evaluate the sensors for potential application, they have been used in the detection of AE in an impact test. The lead-free sensors can reproduce AE signals accurately without giving artifacts and have potential use in commercial AE systems.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Piezoelectric properties of K{sub 4}CuNb{sub 8}O{sub 23} modified (Na{sub 0.5}K{sub 0.5})NbO{sub 3} lead-free piezoceramics

Dense K{sub 4}CuNb{sub 8}O{sub 23} modified (Na{sub 0.5}K{sub 0.5})NbO{sub 3} (NKN:KCN) ceramics were synthesized by using conventional oxide mixing process. The maximum mechanical quality factor Q{sub m} of NKN:KCN ceramics reaches up to 1150, the piezoelectric constant d{sub 33} and the planar electromechanical coefficient k{sub p} still maintain relatively high levels, which are about 100 pC/N and 40%, respectively. Middle frequency (455 kHz) lead-free resonators were fabricated by using NKN:KCN, and remarkable improvements in resonance characteristics were found by KCN doping.

36 MATERIALS SCIENCE↗

Special Application Thermoelectric Micro Isotope Power Sources

Promising design concepts for milliwatt (mW) size micro isotope power sources (MIPS) are being sought for use in various space and terrestrial applications, including a multitude of future NASA scientific missions and a range of military applications. To date, the radioisotope power sources (RPS) used on various space and terrestrial programs have provided power levels ranging from one-half to several hundred watts. In recent years, the increased use of smaller spacecraft and planned new scientific space missions by NASA, special terrestrial and military applications suggest the need for lower power, including mW level, radioisotope power sources. These power sources have the potential to enable such applications as long-lived meteorological or seismological stations distributed across planetary surfaces, surface probes, deep space micro-spacecraft and sub-satellites, terrestrial sensors, transmitters, and micro-electromechanical systems. The power requirements are in the range of 1 mW to several hundred mW. The primary technical requirements for space applications are long life, high reliability, high specific power, and high power density, and those for some special military uses are very high power density, specific power, reliability, low radiological induced degradation, and very low radiation leakage. Thermoelectric conversion is of particular interest because of its technological maturity and proven reliability. This paper summarizes the thermoelectric, thermal, and radioisotope heat source designs and presents the corresponding performance for a number of mW size thermoelectric micro isotope power sources.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Thermoelastic Analysis of a Vibrating TiB/Ti Cantilever Beam Using Differential Thermography

Differential thermography has been used to detect the fluctuating temperatures due the thermoelastic effect for a number of years. This paper examines functionally graded TiB/Ti cantilever beams excited on an electromechanical shaker in fully reversed bending. Finite difference analysis of specimens was used to look at the effect of heat conduction, convection and the fundamental frequency on the surface temperature distribution and compared to experimental data. The thermoelastic effect was also used to detect cracking and the stress field at the tip of the fixture during fatigue.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Enhanced active piezoelectric 0-3 nanocomposites fabricated through electrospun nanowires

The use of monolithic piezoceramic materials in sensing and actuation applications has become quite common over the past decade. However, these materials have several properties that limit their application in practical systems. These materials are very brittle due to the ceramic nature of the monolithic material, making them vulnerable to accidental breakage during handling and bonding procedures. In addition, they have very poor ability to conform to curved surfaces and result in large add-on mass associated with using a typically lead-based ceramic. These limitations have motivated the development of alternative methods of applying the piezoceramic material, including piezoceramic fiber composites and piezoelectric 0-3 composites (also known as piezoelectric paint). Piezoelectric paint is desirable because it can be spayed or painted on and can be used with abnormal surfaces. However, the piezoelectric paint developed in prior studies has resulted in low coupling, limiting its application. In order to increase the coupling of the piezoelectric paint, this effort has investigated the use of piezoelectric nanowires rather than spherical piezoelectric particle, which are difficult to strain when embedded in a polymer matrix. The piezoceramic wires were electrospun from a barium titanate (BaTiO{sub 3}) sol gel to produce fibers with 500-1000 nm diameters and subsequently calcinated to acquire perovskite BaTiO{sub 3}. An active nanocomposite paint was formed using the resulting piezoelectric wires and was compared to the same paint with piezoelectric nanoparticles. The results show that the piezoceramic wires produce 0-3 nanocomposites with as high as 300% increase in electromechanical coupling.

36 MATERIALS SCIENCE↗

Bulk dense fine-grain (1-x)BiScO{sub 3}-xPbTiO{sub 3} ceramics with high piezoelectric coefficient

High density fine grain (1-x)BiScO{sub 3}-xPbTiO{sub 3} ceramics were successfully prepared by two-step sintering and their ferroelectric properties were investigated. Experimental evidence indicates the existence of a morphotropic phase boundary at the composition x=0.635, which exhibits a piezoelectric coefficient d{sub 33} of 700 pC/N at room temperature, significantly higher than the reported values to date. Furthermore, a higher electromechanical coupling factor Kp=0.632 and a larger remnant polarization P{sub r}=47.3 {mu}C/cm{sup 2} were obtained. The paraelectric-to-ferroelectric phase transition occurs at 446 deg. C, slightly lower than in the coarse grain ceramics with a similar composition, suggesting a grain size effect. The local effective piezoelectric coefficient d{sub 33}* was estimated to be 795 pC/N at 2.29 V, measured by scanning probe microscopy. Further atomic force microscope observation revealed the existence of 90 deg. domains of about 60-70 nm in width, confirming the previous results that small domain structure enhances the piezoelectric properties.

36 MATERIALS SCIENCE↗

Dielectric and piezoelectric properties of Bi{sub 2}O{sub 3} added (Pb,Ca,Sr)(Ti,Mn,Sb)O{sub 3} ceramics sintered at low temperature

In this study, in order to develop low temperature sintering ceramics for a thickness mode multilayer piezoelectric transformer, (Pb,Ca,Sr)(Ti,Mn,Sb)O{sub 3} ceramics were fabricated using Na{sub 2}CO{sub 3}, Li{sub 2}CO{sub 3}, MnO{sub 2}, and Bi{sub 2}O{sub 3} as sintering aids at 870, 900, and 930 deg. C. Their respective dielectric and piezoelectric properties were investigated according to the amount of Bi{sub 2}O{sub 3} addition. At the sintering temperature of 900 deg. C, the optimum value was shown for the density of 6.94 g/cm{sup 3}, thickness vibration mode electromechanical coupling factor (henceforth, k{sub t}) of 0.497, thickness vibration mode mechanical quality factor (henceforth, Q{sub mt}) of 3162, and dielectric constant (henceforth, {epsilon}{sub r}) of 209 for thickness mode multilayer piezoelectric transformer application.

36 MATERIALS SCIENCE↗

Morphotropic phase boundary and electrical properties of K{sub 1-x}Na{sub x}NbO{sub 3} lead-free ceramics

Lead-free K{sub 1-x}Na{sub x}NbO{sub 3} ceramics with x=0.48-0.54 were prepared by a conventional solid-state reaction method to investigate the influence of the K/Na ratio on phase structures and electrical properties. The results suggest that a typical morphotropic phase boundary exists at x=0.52-0.525, separating the monoclinic and orthorhombic phases. The sample with the composition near x=0.52 shows the maximum values of the piezoelectric constant (d{sub 33}=160 pC/N) and the electromechanical coupling coefficient (k{sub t}=47%). The results provide a helpful guidance to consider the optimal ratio of K to Na for designing and developing new (K,Na)NbO{sub 3}-based ceramics.

36 MATERIALS SCIENCE↗

Investigation of high Curie temperature (1-x)BiSc{sub 1-y}Fe{sub y}O{sub 3}-xPbTiO{sub 3} piezoelectric ceramics

Ceramics around the morphotropic phase boundary (MPB) in the (1-x)BiSc{sub 1-y}Fe{sub y}O{sub 3}-xPbTiO{sub 3} solid solution were fabricated. For y=0.5, ceramics were single phase, and piezoelectric coefficients (d{sub 33}) and electromechanical coupling coefficients (k{sub p}) for MPB compositions were 300 pC/N and 0.49, respectively; a level of piezoelectric activity similar to that of hard, lead zirconate titanate compositions but with T{sub C}approx60 deg. C higher at approx440 deg. C. For ceramics with y>=0.7, dielectric measurements in combination with diffraction contrast transmission electron microscopy revealed the existence of two ferroelectric phases for most PbTiO{sub 3} contents studied. The presence of two ferroelectric phases was associated with a decrease in piezoelectric activity and although raw materials costs for y=0.7 and 0.8 with respect to y=0 were significantly lower (less Sc{sub 2}O{sub 3}) and T{sub C} greater (approx500 deg. C), d{sub 33} (approx100 pC/N) and k{sub p} (0.18) were too low to be commercially useful for actuator applications.

36 MATERIALS SCIENCE↗

Nanoscale manipulation of Ge nanowires by ion irradiation

Nanowires have generated considerable interest as nanoscale interconnects and as active components of both electronic and electromechanical devices. However, in many cases, manipulation and modification of nanowires are required to fully realize their potential. It is essential, for instance, to control the orientation and positioning of nanowires in some specific applications. This work demonstrates a simple method to reversibly control the shape and the orientation of Ge nanowires using ion beams. Crystalline nanowires were amorphized by 30 keV Ga{sup +} implantation. Subsequently, viscous flow and plastic deformation occurred causing the nanowires to bend toward the beam direction. The bending was reversed multiple times by ion implanting the opposite side of the nanowires, resulting in straightening and subsequent bending into that opposite direction. This effect demonstrates the detailed manipulation of nanoscale structures is possible through the use of ion irradiation.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Local Measurements of Preisach Density in Polycrystalline Ferroelectric Capacitors

Polarization switching in polycrystalline ferroelectric capacitors is explored using piezoresponse force microscopy (PFM) based first-order reversal curve (FORC) measurements. The band excitation method facilitates decoupling the electromechanical responses from variations in surface elastic properties. A simulated annealing method is developed to estimate the Preisach densities from PFM FORC data. Microscopic and macroscopic Preisach densities are compared, illustrating good agreement between the two.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

ULTRASONIC MEASUREMENT MODELS FOR SURFACE WAVE AND PLATE WAVE INSPECTIONS

A complete ultrasonic measurement model for surface and plate wave inspections is obtained, where all the electrical, electromechanical, and acoustic/elastic elements are explicitly described. Reciprocity principles are used to describe the acoustic/elastic elements specifically in terms of an integral of the incident and scattered wave fields over the surface of the flaw. As with the case of bulk waves, if one assumes the incident surface waves or plate waves are locally planar at the flaw surface, the overall measurement model reduces to a very modular form where the far-field scattering amplitude of the flaw appears explicitly.

36 MATERIALS SCIENCE↗