The Mechanical Response of High Burnup 17x17 PWR Fuel Rods Under Bending

As a part of the US Department of Energy Office of Nuclear Energy High Burnup Spent Fuel Data Project, Oak Ridge National Laboratory has performed 4pt-bend tests on a series of 17x17 PWR fuel rods that were discharged with rod average burnups between 50 and 60 GWd/MTU. The rods include four different kinds of fuel cladding: standard Zircaloy-4 (Zirc-4), low-tin (LT) Zirc-4, ZIRLO, and M5. Six rods of each type (combining Zirc-4 and LT Zirc-4 as one type) were tested to failure at room temperature and 200 oC. Three of each type experienced a full-length heat treatment cycle from RT to 400 oC to RT with an 8 hr soak at 400 oC to simulate the expected limiting vacuum drying condition, which potentially induces hydride reorientation and causes some annealing of irradiation damage in the cladding. Overall, the fuel rods show significant capacity to deflect in bending and exhibit non-linear deformation before failing. The calculated failure strains range from 1.5% to 3.8%. The simulated vacuum drying heat treatment had the largest effect on fuel rods with ZIRLO and M5 cladding. In both cases the heat treatment caused increases in the plastic strain at failure, suggesting some annealing of irradiation damage is occurring. The finite element modeling of the 4pt bending test assume the pellet is a collection of pellet wedge pieces. The results for the Zircaloy-4 rods suggest that the pellets are bonded to the cladding and friction controls the relative motion of the pellet wedge pieces.

Cantonwine, Paul↗

Electrical heating tests of uranium dioxide external fuel configuration at emitter temperature of 1900 K

Testing of two fuel clad specimens for thermionic reactor application is described. The annular UO2 fuel was clad on both sides with tungsten; heat rejection was radially inward. The tests were intended to study inner clad stability, fuel redistribution, and fuel melting problems. The specimens were tested in a vacuum chamber using electron bombardment heating. Fuel structural changes were studied using periodic gammagraphs and posttest metallography. The first specimen test was terminated at 50 hours because of a braze failure. The second specimen was tested for 240 hours when an outer clad leak developed due to a tungsten-water reaction. The fuel developed numerous cracks on cooldown but the inner clad remained dimensionally stable. The fuel cover gas did not impede the rate of fuel redistribution. Posttest examination showed the fuel had not melted during operation.

Diianni, D. C.↗

Regulatory Perspective on Potential Fuel Reconfiguration and Its Implication to High Burnup Spent Fuel Storage and Transportation - 13042

The recent experiments conducted by Argonne National Laboratory on high burnup fuel cladding material property show that the ductile to brittle transition temperature of high burnup fuel cladding is dependent on: (1) cladding material, (2) irradiation conditions, and (3) drying-storage histories (stress at maximum temperature) [1]. The experiment results also show that the ductile to brittle temperature increases as the fuel burnup increases. These results indicate that the current knowledge in cladding material property is insufficient to determine the structural performance of the cladding of high burnup fuel after it has been stored in a dry cask storage system for some time. The uncertainties in material property and the elevated ductile to brittle transition temperature impose a challenge to the storage cask and transportation packaging designs because the cask designs may not be able to rely on the structural integrity of the fuel assembly for control of fissile material, radiation source, and decay heat source distributions. The fuel may reconfigure during further storage and/or the subsequent transportation conditions. In addition, the fraction of radioactive materials available for release from spent fuel under normal condition of storage and transport may also change. The spent fuel storage and/or transportation packaging vendors, spent fuel shippers, and the regulator may need to consider this possible fuel reconfiguration and its impact on the packages' ability to meet the safety requirements of Part 72 and Part 71 of Title 10 of the Code of Federal Regulations. The United States Nuclear Regulatory Commission (NRC) is working with the scientists at Oak Ridge National Laboratory (ORNL) to assess the impact of fuel reconfiguration on the safety of the dry storage systems and transportation packages. The NRC Division of Spent Fuel Storage and Transportation has formed a task force to work on the safety and regulatory concerns in relevance to high burnup fuel storage and transportation. This paper discusses the staff's preliminary considerations on the safety implication of fuel reconfiguration with respect to nuclear safety (subcriticality control), radiation shielding, containment, the performance of the thermal functions of the packages, and the retrievability of the contents from regulatory perspective. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

An approach to grid-to-rod fretting wear modeling using dynamic mortar contact

This article presents the development of a grid-to-rod fretting (GTRF) modeling methodology that utilizes dynamic mortar contact. Here, we leverage a recently developed computational framework for modeling thermomechanical contact in dynamic simulations from the nuclear fuel performance code Bison. Usage of mortar contact ensures a smooth distribution of normal and frictional contact forces, displacements, and velocities on the contact interface, thus facilitating an accurate computation of wear. The integration within an advanced nuclear fuel performance code enables analysis of complex interactions between the fuel, cladding, and spacer grid. Such interactions include swelling, creep, fuel fragmentation, burnup, plenum pressure, and fission gas release. Our methodology is demonstrated via the modeling of two spacer grid geometries and the influence of fuel-cladding mechanical contact on the generation of fretting wear.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Unlocking the Vault - Accelerated Delivery Through the Application of Innovation and Collaboration - 19011

The Pile Fuel Cladding Silo (PFCS) at Sellafield was built in 1949/50 to receive and store fuel cladding from reprocessing of Windscale Pile fuel; it has been used to store this material and other waste from the UK nuclear programme ever since. The Silo is unsuitable for indefinite storage; this along with uncertainty in the make-up and condition of the inventory combine to rank the facility alongside the most hazardous in Western Europe. Sellafield Ltd, began working with its supply chain partners Bechtel Cavendish Nuclear Solutions (BCNS - a joint venture between Bechtel Inc and Cavendish Nuclear Ltd) in 2012, to execute a suite of projects to create an access route to the waste and a capability to retrieve waste from the silo for the first time ever. However, the challenge of providing this capability, while maintaining ongoing safe storage of the waste, and underpinning future performance of both the silo and the waste packages for many hundreds of years, proved to be too much for traditional Sellafield Ltd delivery models. With both cost and schedule forecasts doubling from initial estimates, a new approach was clearly required. The team recognised that success would require all of the experience and expertise of each organisation working together to a common goal. Therefore, significant effort was expended to build a collaborative team environment into which an innovative approach to both the engineering of what was provided and the delivery methods for doing it could be launched. Focussing on collaborative culture in which innovation and fit for purpose thinking were encouraged has completely rebuilt stakeholder confidence. The project is now almost complete; 17 months ahead of schedule and British Pounds 100 m less than the approved cost. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

FeCrAl fuel/clad chemical interaction in light water reactor environments

This article investigates the fuel-cladding chemical interaction (FCCI) behavior of two commercial FeCrAl alloys, APMT composition (Fe-21Cr-5Al-3Mo wt.%) and C35M (Fe-13Cr-5Al-2Mo-0.2Si-0.03Y wt.%), after neutron irradiation. “H-cup” diffusion multiples of FeCrAl alloys and ceramic UO 2 fuel were irradiated at a temperature of ~300 °C to a total estimated burnup of 26 GWd/tHM. Post-irradiation Examination results demonstrate the excellent degradation resistance of FeCrAl alloys as accident tolerant fuel (ATF) cladding materials in light water reactor conditions. The study concludes that there was no irradiation-induced defects observed in either of the two commercial FeCrAl claddings. The formation of amorphous Al/U mixed oxide was observed at the fuel-clad interface, which can serve as a tritium permeation barrier and protect against potential chemical attack from the fuel. Finally, the study attributed the formation of amorphous Al/U mixed oxide to the low temperature and limited time of neutron irradiation. APMT forms more distinct Cr and Cr-Fe intermetallic at the FeCrAl-UO 2 interface than C35M due to the higher bulk Cr:Al ratio.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Zirconium Sludge Criticality Calculations in Large Process Tanks

The Savannah River Site’s H-Canyon facility has been tasked with accelerating the disposition of used research reactor fuels. • Future missions will involve dissolution of “Non-Aluminum” clad fuels – not easily dissolved – Nitric acid is not capable of dissolving stainless steel, Zirconium, and Hastelloy, clad fuels by itself • The electrolytic dissolver has been (re) selected as a disposition path for these fuels. 2

Devine, Nathan P.↗

Parametric and experimentally informed BWR Severe Accident Analysis Utilizing FeCrAl - M3FT-17OR020205041

Iron-chromium-aluminum (FeCrAl) alloys are being considered as advanced fuel cladding concepts with enhanced accident tolerance. At high temperatures, FeCrAl alloys have slower oxidation kinetics and higher strength compared with zirconium-based alloys. FeCrAl could be used for fuel cladding and spacer or mixing vane grids in light water reactors and/or as channel box material in boiling water reactors (BWRs). There is a need to assess the potential gains afforded by the FeCrAl accident-tolerant-fuel (ATF) concept over the existing zirconium-based materials employed today. To accurately assess the response of FeCrAl alloys under severe accident conditions, a number of FeCrAl properties and characteristics are required. These include thermophysical properties as well as burst characteristics, oxidation kinetics, possible eutectic interactions, and failure temperatures. These properties can vary among different FeCrAl alloys. Oak Ridge National Laboratory has pursued refined values for the oxidation kinetics of the B136Y FeCrAl alloy (Fe-13Cr-6Al wt %). This investigation included oxidation tests with varying heating rates and end-point temperatures in a steam environment. The rate constant for the low-temperature oxidation kinetics was found to be higher than that for the commercial APMT FeCrAl alloy (Fe-21Cr-5Al-3Mo wt %). Compared with APMT, a 5 times higher rate constant best predicted the entire dataset (root mean square deviation). Based on tests following heating rates comparable with those the cladding would experience during a station blackout, the transition to higher oxidation kinetics occurs at approximately 1,500°C. A parametric study varying the low-temperature FeCrAl oxidation kinetics was conducted for a BWR plant using FeCrAl fuel cladding and channel boxes using the MELCOR code. A range of station blackout severe accident scenarios were simulated for a BWR/4 reactor with Mark I containment. Increasing the FeCrAl low-temperature oxidation rate constant (3 times and 10 times that of the rate constant for APMT) had a negligible impact on the early stages of the accident and minor impacts on the accident progression after the first relocation of the fuel. At temperatures below 1,500°C, increasing the rate constant for APMT by a factor of 10 still resulted in only minor FeCrAl oxidation. In general, the gains afforded by the FeCrAl enhanced ATF concept with respect to accident sequence timing and combustible gas generation are consistent with previous efforts. Compared with the traditional Zircaloy-based cladding and channel box system, the FeCrAl concept could provide a few extra hours of time for operators to take mitigating actions and/or for evacuations to take place. A coolable core geometry is retained longer, enhancing the ability to stabilize an accident. For example, a station blackout was simulated in which cooling water injection was lost 36 hours after shutdown. The timing to first fuel relocation was delayed by approximately 5 h for the FeCrAl ATF concept compared with that of the traditional Zircaloy-based cladding and channel box system.

36 MATERIALS SCIENCE↗

THERMAL SAFETY MARGIN CALCULATION OF THE MP-2 EXPERIMENT IN THE ADVANCED TEST REACTOR

The Mini-Plate 2 (MP-2) irradiation test is a fueled experiment designed for irradiation in multiple test locations in the Advanced Test Reactor (ATR) at the Idaho National Laboratory (INL). The experiment is a drop-in test where small aluminum-clad fuel plate samples (mini plates) are cooled directly by the ATR Primary Coolant System (PCS) water. The MP-2 fuel plate experiment will be irradiated in several different irradiation locations of the ATR. This fueled experiment contains aluminum-clad fuel mini plates consisting of monolithic U-Mo. Four different types of fuel plates with fuel meat thickness and cladding are part of the MP-2 test. A thermal analysis has been performed on the MP-2 experiment. A method for calculating Departure from Nucleate Boiling Ratio (DNBR) and Flow Instability Ratio (FIR) during a reactivity transient using the commercial finite element and heat transfer code ABAQUS is discussed. At the start of an ATR cycle the heat generation rate of the fueled experiment is high and the heat rate multiplier from the outer shim control cylinders is low, while the reverse is true at the end of the ATR cycle. Thermal analyses at 10 day increments during the cycle calculate the DNBR and FIR during a reactivity transient. This technique calculates DNBR for the fuel plate surfaces and FIR for all water components for each finite element surface and node at various times during the ATR cycle. Heat rates vary with time during the transient calculation that are provided by a detailed physics analysis. Oxide growth on the fuel plates is also incorporated Results from the transient calculations are displayed with the ABAQUS post processor. By calculating these parameters at each location in the finite element model, conservatism is replaced with accuracy. This allows for a greater margin for the thermal hydraulic safety parameters.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Behavior under LOCA conditions on enhanced accident tolerant chromium coated zircaloy-4 claddings

For enhanced accident tolerant fuels for light water reactors application, chromium coatings on zirconium based nuclear fuel claddings are developed and studied at CEA in the framework of the French CEA-EDF-AREVA collaborative program. The results obtained so far, mainly on Zircaloy-4 substrate, show very good corrosion resistance in nominal conditions and significant enhancement of the resistance of the material to oxidation in steam at high temperature (HT), up to 1300 Celsius degrees, with a drastic decrease of hydrogen release and/or pick-up. The present paper reports some new results obtained on chromium coated Zircaloy-4 claddings tested in loss-of-coolant accident (LOCA) conditions. In order to investigate the potential effect of the coating on the cladding mechanical behavior at HT and the capacity of the coating to sustain significant substrate deformation (i.e., during ballooning until burst occurrence) without generalized cracking/peeling, a preliminary limited set of internal pressure creep and temperature ramp tests have been performed in steam environment thanks to the EDGAR facility. The thermal-mechanical tests were done for testing/burst temperatures ranging from 600 C. degrees (α{sub Zr} phase domain) up to 1000 C. degrees (β{sub Zr} phase domain) on 50 cm long low-tin Zircaloy-4 cladding samples with a 15 μm thick outer chromium coating. It is shown that: -) whatever the applied temperature/pressure values, the chromium coating is still fully adherent after having experienced ballooning and burst, including at the vicinity of the burst opening where the Zircaloy-4 clad substrate is highly deformed; -) a HT strengthening effect of the coating on the overall creep clad behavior is evidenced when compared to uncoated Zircaloy-4 cladding materials tested in the same conditions; -) as a consequence, it is observed that, in the 600-750 C. degrees temperature range (α{sub Zr} phase domain) and after burst occurrence, the balloon sizes (i.e., 'uniform' and maximum hoop strains) are generally reduced when compared to uncoated materials; -) regarding the burst mechanism in the β{sub Zr} phase temperature range (1000 C. degrees), it is interesting to observe that, even if some ballooning occurred prior to the cladding failure, the actual burst openings are generally very small (in the order of 1 mm{sub 2} or less), reducing the risk of fuel fragments dispersal in the coolant.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A Standardized Analysis Process Using Digital Image Correlation to Calculate In Situ Cladding Strain from Modified Burst Tests for Fuel Performance Code Validation

Historical data collection on nuclear fuel cladding materials has focused on generating a statistically significant amount of data to assess the material and its failure behavior. Furthermore, data generated to support material model and failure criteria development were previously posttest evaluations, so a large number of tests was required to gain new understanding. A way to expedite this process is to develop techniques capable of generating large, high-fidelity data sets from a single test with lower uncertainty or quantified uncertainty. One such example of this approach is Oak Ridge National Laboratory’s use of modified burst tests (MBTs) to analyze the mechanical behavior and failure conditions of cladding during a simulated reactivity-initiated accident (RIA). Each test incorporates digital image correlation (DIC) analysis techniques that are used to assess the accumulated strain in situ, as well as eventual cladding failure. This work has been fruitful in defining strain-to-failure conditions for materials like silicon carbide (SiC) fiber–reinforced/SiC matrix composite tubes (SiC/SiC), iron-chromium-aluminum (FeCrAl) alloy tubes, and chromium-coated Zircaloy-4 tubes. However, there are numerous DIC software available, including open-source and proprietary software. The different DIC software use various algorithms to process images and calculate displacement values. Using these different software and algorithms can lead to varying results, and perhaps larger-than-expected uncertainties. In the present study, previously published MBT data encompassing a variety of test conditions were reanalyzed with two different DIC software to assess the variance in the calculated strain results. The data consisted of SiC/SiC, FeCrAl, and chromium-coated Zircaloy-4 tubes. Plots of the calculated strains during the transient revealed good agreement between the two DIC software. The average root-mean-square errors between the two software was 0.20% strain, which is slightly larger than a previously reported error value for these tests. In conclusion, this variance in results is low enough that this analysis method can be used for code validation.

Reactivity-initiated accident↗

Measuring the elastic tensor of a monolithic SiC hollow cylinder with resonant ultrasound spectroscopy

Resonant Ultrasound Spectroscopy (RUS) has become a standard tool in material science to measure nondestructively the elastic properties of materials. The widespread adoption of this tool for applications related to nondestructive testing and structural health monitoring in the industry and other places has been restricted thus far by some requirements imposed by RUS on the sample to be tested, in particular the fact that the sample geometry should be relatively simple (e.g., cuboid, cylinder, or sphere). Here, we use RUS to determine the baseline material properties of a hollow cylinder made of monolithic SiC, a surrogate material and geometry representing nuclear fuel cladding for this study. Typically, elastic properties of the nuclear fuel cladding samples are inspected destructively (e.g., indentation) or with acoustic techniquesrequiring multiple and cumbersome measurements. Here, a relatively new RUS approach specifically developed to measure the elastic tensor of samples with arbitrary geometries is used. The results obtained from this RUS approach are compared to values reported in the literature. As a second verification step, vibrational mode shapes computed numerically with the elastic constants are compared to those measured on the sample using a 3D laser Doppler vibrometer, showing an excellent agreement.

36 MATERIALS SCIENCE↗

Amplicon Sequencing Reveals Microbiological Signatures in Spent Nuclear Fuel Storage Basins

Water quality is an important determinant for the structural integrity of alloy cladded fuels and assemblies during long-term wet storage. Detailed characterization of a water filled storage basin for spent nuclear reactor fuel was performed following the formation and proliferation of an amorphous white flocculent. White precipitant was sampled throughout the storage basin for chemical and spectroscopic characterization, and eDNA was extracted for pyrosequencing of bacterial rRNA gene diversity. Accordingly, spectroscopic analyses indicated the precipitant to be primarily amorphous to crystalline aluminum (oxy) hydroxides with minor associated elemental components including Fe, Si, Ti, and U. High levels of dissolved carbon were co-localized with the precipitant relative to bulk water. Bacterial densities were highly variable between sampling locations and with depth; cell numbers (log scale) ranged from 5.6 to 4.89 cells / mL. Bacterial diversity that was physically associated with the aluminum (oxy) hydroxide complexes exceeded an estimated 4,000 OTUs / amplicon library (3% cutoff) and the greatest percent majority of sequences were aligned to the families Burkholderiales (23%), Nitrospiraceae (23%), Hyphomicrobiaceae (17%), and Comamonadaceae (6%). We surmise that episodic changes in the physical and chemical properties of the basin contribute to the polymerization of aluminum (oxy) hydroxides, which in turn can chemisorb nutrients, carbon ligands and bacterial cells from the surrounding bulk aqueous phase. As such, these precipitants should establish favorable microhabitats for bacterial colonization and growth. Comparative analyses of 16S rRNA gene amplicon libraries across diverse environmental landscapes were performed and microbiological signatures unique to the spent nuclear fuel storage basin environment were revealed. These insights could spur the development of tractable bioindicators that are specific of and diagnostic for water quality at discrete locations and finer scales of resolution, marking an important contribution for improved water quality and management of spent nuclear fuel storage facilities.

aluminum↗

The Development and Production of a Functionally Graded Composite for Pb-Bi Service

A material that resists lead-bismuth eutectic (LBE) attack and retains its strength at 700°C would be an enabling technology for LBE-cooled reactors. No single alloy currently exists that can economically meet the required performance criteria of high strength and corrosion resistance. A Functionally Graded Composite (FGC) was developed with layers engineered to perform these functions. F91 was chosen as the structural layer of the composite for its strength and radiation resistance. Fe-12Cr-2Si, an alloy developed from previous work in the Fe-Cr-Si system, was chosen as the corrosion-resistant cladding layer because of its chemical similarity to F91 and its superior corrosion resistance in both oxidizing and reducing environments. Fe-12Cr-2Si experienced minimal corrosion due to its self-passivation in oxidizing and reducing environments. Extrapolated corrosion rates are below one micron per year at 700ï°C. Corrosion of F91 was faster, but predictable and manageable. Diffusion studies showed that 17 microns of the cladding layer will be diffusionally diluted during the three year life of fuel cladding. 33 microns must be accounted for during the sixty year life of coolant piping. 5 cm coolant piping and 6.35 mm fuel cladding preforms were produced on a commercial scale by weld-overlaying Fe-12Cr-2Si onto F91 billets and co-extruding them. An ASME certified weld was performed followed by the prescribed quench-and-tempering heat treatment for F91. A minimal heat affected zone was observed, demonstrating field weldability. Finally, corrosion tests were performed on the fabricated FGC at 700ï°C after completely breaching the cladding in a small area to induce galvanic corrosion at the interface. None was observed. This FGC has significant impacts on LBE reactor design. The increases in outlet temperature and coolant velocity allow a large increase in power density, leading to either a smaller core for the same power rating or more power output for the same size core. This FGC represents an enabling technology for LBE cooled fast reactors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

An Investigation of Liquefaction in Irradiated TRIGA Fuel Exposed to Relatively High Temperatures

This report presents the findings of an investigation into high temperature fuel cladding chemical interactions (FCCI) in Training, Research, Isotopes, General Atomics (TRIGA) fuel rods. A TRIGA fuel-rod core or meat is principally composed of uranium (U) particles dispersed in a zirconium hydride (Zr H) matrix. The fuel is clad in sealed 304SS or Incoloy 800 tubes. At high temperatures, the fuel will interact with the cladding, resulting in FCCI. To investigate the FCCI (in this case, liquefaction), irradiated TRIGA fuel rods were exposed to relatively high temperatures in furnace tests. The tests were performed at different temperatures using segments from an irradiated TRIGA fuel rod at the Hot Fuel Examination Facility located at Idaho National Laboratory (INL). The data from this study is important for developing a better understanding of the performance of U-ZrH fuel type during transient events (e.g., a Loss of Coolant Accident (LOCA) event) that may result in high temperatures while operating a TRIGA reactor. Furnace tests were run for 6 hours at 730, 800, 900, 950, and 1,000°C. One test was run for 12 hours at 950°C. Post-test microstructural characterization was performed on the heat-treated samples using optical metallography to look for evidence of liquefaction. Additionally, microstructural characterization was performed using scanning electron microscopy to investigate the microstructure of the as-irradiated fuel before heat treatment and the microstructural changes that occurred after heat treating for the 730 and 950°C heat treatments for 6 hours. Results of the analysis were compared to those produced during diffusion studies performed using unirradiated TRIGA fuel meat and type 304 stainless steel. A gap is typically present in as-irradiated fuel that limits any possibility for chemical interaction between the fuel and cladding. Optical metallography (OM) was used to identify areas in the specimens heat treated at 950 and 1000°C where fuel and cladding contact was satisfactory for the FCCI to transpire. The bulk of the interaction zones that form due to FCCI developed in the fuel meat and not as much in the cladding. Even in the sample tested at 1,000°C, no evidence was found that gross fuel meat or cladding melting had occurred. Only limited porosity was found in the fuel meat that possibly could have been due to melting of a particular precipitate phase or phases that had formed during FCCI. These results agreed with those reported for the unirradiated diffusion couple studies.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermal Model for Horizontal In-Water and In-Air Mini-Plate Experiments in the Advanced Test Reactor

Mini-Plate (MP) irradiation tests are a fueled experiment designed for irradiation in multiple test locations in the Advanced Test Reactor (ATR) at the Idaho National Laboratory (INL). MP experiments are considered a non-instrumented drop-in test where small aluminum-clad fuel plate samples are cooled directly by the ATR Primary Coolant System (PCS) water. These fueled experiments contain aluminum-clad fuel mini plates consisting of monolithic U-10Mo. Previous thermal analyses have been documented concerning oxide growth[1] and thermal safety margin[2] for the MP-2 experiment. A thermal analysis has been performed on the MP-2 experiment using a new technique for calculating the necessary time after the experiment has been irradiated and reactor shutdown necessary to not exceed the 95% lower bound blister threshold temperature for the fuel in a horizontal in air configuration. A horizontal in water model has also been analyzed and will be discussed. After the experiment is irradiated in the ATR, it is necessary to calculate the fuel meat temperatures at 12 hours after shutdown. This is done to assure that at the 12 hour mark, if this experiment is removed from the reactor and accidentally dropped onto the working tray and is in the most severe geometrical configuration of horizontal (minimum heat transfer) that fission products will not be released. The blister threshold temperature is considered this safety limit. The horizontal in air analysis is also performed considering that the experiment is horizontal in a drained canal and filled with air and natural convection heat transfer with air on the outside. The initial mini-plate testing campaign known as MP-1 [3] has been irradiated and its purpose was to form the base fuel specimens fabricated by various processes so that a single process can be down-selected for qualification. MP-2 will then serve to populate a comprehensive fuel performance data set for the down-selected fabrication process. The MP-2 experiment will be irradiated in several locations of the ATR as shown in Figure 1. The fuel plate thickness and geometry is identical to the MP-1 experiment [3], with the only variable being the fuel meat thickness. This model of the B-12 position is treated as encompassing the I-21, I-24, and B-9 positions since it has more fuel and higher total heat than the other positions. Since the blister threshold temperature is a function of fission density, a series of fission densities is calculated for the B-12 position to cover the other three positions. The B 12 position specifically uses fuel meat that is 0.016 in thick by 3.25 in long and 0.75 in tall. The total plate thickness is 0.050 in. Aluminum cladding forms the barrier between the PCS and the fuel meat. The purpose of this paper is to demonstrate this new technique developed to calculate the necessary decay time after shutdown for a series of fission densities using the ABAQUS [4] finite element and heat transfer code.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Report on DIC Cyclic Dryout Testing of ATF Cladding Materials

Boiling water reactors can experience anticipated operational occurrences, where an expected deviation from normal operating conditions is witnessed for short time scales. One example of such transients arises from cladding dryout, where stable boiling becomes unstable, resulting in cladding heat up before re-wetting occurs. To understand the impact of such transients on fuel cladding lifetime and performance, cyclic dryout conditions were imposed upon fresh fuel cladding in the absence of irradiation. Pressurized cladding tube segments were exposed to rapid temperature increases to intermediate temperatures below a cladding rupture threshold and deformation was monitored in situ via 3-D digital image correlation. The impact of cycle frequency on cladding deformation was assessed. A clear understanding of elastic and plastic strain responses were developed for Zr alloy deformation under temperature transients, and these results can be used to support material model development and validate fuel performance codes.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗