Search NASA⌕ Search

SEARCH · Search NASA

Results for “NICKEL ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Dynamic oxidation behavior at 1000 and 1100 C of four nickel-base cast alloys, NASA-TRW VIA, B-1900, 713C, and 738X

The superalloys NASA-TRW VIA, B-1900, 713C, and 738X were tested cyclically and isothermally for resistance to oxidation in high velocity gas streams for 100 hours at specimen temperatures of 1000 C and 1100 C. Alloys VIA and B-1900, which were the most oxidation resistant, displayed slight and very similar weight changes and metal losses. Alloy 713C also sustained only slight metal losses, but it exhibited some tendency to spall. Alloy 738X was found to be the most susceptible to cyclic oxidation; this resulted in heavy spalling, which in turn caused high weight losses and high metal losses. Oxidation test results are related to the amounts of chromium aluminum, and the refractory metals in the alloys investigated.

Sanders, W. A.↗

Solid state welding processes for an oxide dispersion strengthened nickel-chromium-aluminum alloy

Solid-state welding processes were evaluated for joining TD-NiCrAl (Ni-16Cr-4Al-2ThO2) alloy sheet. Both hot-press and resistance spot welding techniques were successfully applied in terms of achieving grain growth across the bond line. Less success was achieved with a resistance seam welding process. In stress-rupture shear and tensile shear tests of lap joints at 1100 C, most failures occurred in the parent material, which indicates that the weld quality was good and that the welds were not a plane of weakness. The overall weld quality was not as good as previously attained with TD-NiCr, probably because the presence of alumina at the faying surfaces and the developmental TD-NiCrAl sheet, which was not of the quality of the TD-NiCr sheet in terms of surface flatness and dimensional control.

Moore, T. J.↗

Several braze filler metals for joining an oxide-dispersion-strengthened nickel-chromium-aluminum alloy

An evaluation was made of five braze filler metals for joining an aluminum-containing oxide dispersion-strengthened (ODS) alloy, TD-NiCrAl. All five braze filler metals evaluated are considered suitable for joining TD-NiCrAl in terms of wettability and flow. Also, the braze alloys appear to be tolerant of slight variations in brazing procedures since joints prepared by three sources using three of the braze filler metals exhibited similar brazing characteristics and essentially equivalent 1100 C stress-rupture properties in a brazed butt-joint configuration. Recommendations are provided for brazing the aluminum-containing ODS alloys.

Gyorgak, C. A.↗

An exploratory study of a zirconium-modified, precipitation-strengthened nickel-30 copper alloy

A precipitation-strengthened alloy has been produced through minor additions of zirconium to a base Ni-30Cu alloy. The results of this exploratory study indicate that thermomechanical processing of a solution-treated Ni-30Cu-0.2Zr alloy produced a dispersion of precipitates. The precipitates have been tentatively identified as a Ni5Zr compound. Comparison of the mechanical properties, as determined by testing in air, of the Zr-modified alloy to those of a Ni-30Cu alloy reveals that the precipitation-strengthened alloy has improved tensile properties to 1200 K and improved stress-rupture properties to 1100 K. The oxidation characteristics of the modified alloy appeared to be equivalent to those of the base Ni-30Cu alloy.

Whittenberger, J. D.↗

A feasibility study of a diffusion barrier between Ni-Cr-Al coatings and nickel-based eutectic alloys

Coating systems have been proposed for potential use on eutectic alloy components in high-temperature gas turbine engines. In a study to prevent the deterioration of such systems by diffusion, a tungsten sheet 25 microns thick was placed between eutectic alloys and an Ni-Cr-Al layer. Layered test specimens were aged at 1100 C for as long as 500 h. Without the tungsten barrier the delta phase of the eutectic deteriorated by diffusion of niobium into the Ni-Cr-Al. Insertion of the tungsten barrier stopped the diffusion of niobium from the delta phase. Chromium diffusion from the Ni-Cr-Al into the gamma/gamma-prime phase of the eutectic was greatly reduced by the barrier. However, the barrier thickness decreased with time, and tungsten diffused into both the Ni-Cr-Al and the eutectic. When the delta platelets were aligned parallel rather than perpendicular to the Ni-Cr-Al layer, diffusion into the eutectic was reduced.

Young, S. G.↗

A multiple linear regression analysis of hot corrosion attack on a series of nickel base turbine alloys

Multiple linear regression analysis was used to determine an equation for estimating hot corrosion attack for a series of Ni base cast turbine alloys. The U transform (i.e., 1/sin (% A/100) to the 1/2) was shown to give the best estimate of the dependent variable, y. A complete second degree equation is described for the centered" weight chemistries for the elements Cr, Al, Ti, Mo, W, Cb, Ta, and Co. In addition linear terms for the minor elements C, B, and Zr were added for a basic 47 term equation. The best reduced equation was determined by the stepwise selection method with essentially 13 terms. The Cr term was found to be the most important accounting for 60 percent of the explained variability hot corrosion attack.

Barrett, C. A.↗

Nickel base coating alloy

Zirconium is added to a Ni-30 Al (beta) intermetallic alloy in the range of 0.05 w/o to 0.25 w/o. This addition is made during melting or by using metal powders. The addition of zirconium improves the cyclic oxidation resistance of the alloys at temperatures above 1100 C.

Barrett, C. A.↗

Tungsten solution kinetics and amorphization of nickel in mechanically alloyed Ni-W alloys

The kinetics of solution of W, and the subsequent amorphization of Ni, in mechanically alloyed Ni-W alloys has been investigated. As W is a highly abrasive material in the energy intensive devices used for mechanical alloying, we studied the above reactions in different mills. One used hardened steel balls as the grinding media, and the other Al2O3. Abrasion is common to both mills, but Fe wear debris from the hardened steel enters into solution in the Ni rich phases whereas Al2O3 debris is present as small dispersoids. The kinetics of W solution and those of subsequent amorphization do not appear strongly affected by the Fe in solution or the Al2O3 dispersoid. Tungsten dissolves in crystalline Ni in amounts in excess of the equilibrium solubility during alloying. Amorphization of the Ni phase occurs if the W content in this phase exceeds ca. 28 at. pct.

Aning, A. O.↗

A comparison of corrosion-resistant steel (18 percent chromium - 8 percent nickel) and aluminum alloy (24st)

In the selection of materials for aircraft application, it is not enough to make the selection on a strength-weight basis alone. A strength-weight comparison is significant but other factors must be considered, for while a material with a high ratio of strength to weight may be perfectly satisfactory for one use, it may be totally unfitted for another. It is essential, among other things, that the probable nature, magnitude, and direction of the principal stresses be given special consideration. The following analysis has therefore been made with this in mind. An attempt has been made to cover insofar as possible the major, but not all the points, that a designer would consider in the use of "18-8", as it is commonly referred to, and 24ST aluminum alloy, as applied to aircraft. 24ST was selected for this comparison as it has practically replaced 17ST for aircraft construction and it appears to have the best combination of properties of the alloys now available for this purpose. The cost of fabrication has not been considered.

Sullivan, J E↗

The Effect of Heat Treatment on Residual Stress and Machining Distortions in Advanced Nickel Base Disk Alloys

This paper describes an extension of NASA's AST and IDPAT Programs which sought to predict the effect of stabilization heat treatments on residual stress and subsequent machining distortions in the advanced disk alloy, ME-209. Simple "pancake" forgings of ME-209 were produced and given four heat treats: 2075F(SUBSOLVUS)/OIL QUENCH/NO AGE; 2075F/OIL QUENCH/1400F@8HR;2075F/OIL QUENCH/1550F@3HR/l400F@8HR; and 2160F(SUPERSOLVUS)/OIL QUENCH/1550F@3HR/ 1400F@8HR. The forgings were then measured to obtain surface profiles in the heat treated condition. A simple machining plan consisting of face cuts from the top surface followed by measurements of the surface profile opposite the cut were made. This data provided warpage maps which were compared with analytical results. The analysis followed the IDPAT methodology and utilized a 2-D axisymmetric, viscoplastic FEA code. The analytical results accurately tracked the experimental data for each of the four heat treatments. The 1550F stabilization heat treatment was found to significantly reduce residual stresses and subsequent machining distortions for fine grain (subsolvus) ME209, while coarse grain (supersolvus) ME209 would require additional time or higher stabilization temperatures to attain the same degree of stress relief.

Gayda, John↗

ECLSS Sustaining Metal Materials Compatibility Final Report, Electrochemical and Crevice Corrosion Test Results

Electrochemical test results are presented for six noble metals evaluated in two acidic test solutions which are representative of waste liquids processed in the Environmental Control and Life Support System (ECLSS) aboard the International Space Station (ISS). The two test solutions consisted of fresh waste liquid which had been modified with a proposed or alternate pretreatment formulation and its associated brine concentrate. The six test metals included three titanium grades, (Commercially Pure, 6Al-4V alloy and 6Al-4V Low Interstitial alloy), two nickel-chromium alloys (Inconel® 625 and Hastelloy® C276), and one high tier stainless steel (Cronidur® 30).

Lee, R. E.↗

Electrochemical, Polarization, and Crevice Corrosion Testing of Nitinol 60, A Supplement to the ECLSS Sustaining Materials Compatibility Study

In earlier trials, electrochemical test results were presented for six noble metals evaluated in test solutions representative of waste liquids processed in the Environmental Control and Life Support System (ECLSS) aboard the International Space Station (ISS). Subsequently, a seventh metal, Nitinol 60, was added for evaluation and subjected to the same test routines, data analysis, and theoretical methodologies. The previous six test metals included three titanium grades, (commercially pure, 6Al-4V alloy and 6Al-4V low interstitial alloy), two nickel-chromium alloys (Inconel(RegisteredTrademark) 625 and Hastelloy(RegisteredTrademark) C276), and one high-tier stainless steel (Cronidur(RegisteredTrademark) 30). The three titanium alloys gave the best results of all the metals, indicating superior corrosive nobility and galvanic protection properties. For this current effort, the results have clearly shown that Nitinol 60 is almost as noble as titanium, being very corrosion-resistant and galvanically compatible with the other six metals electrochemically and during long-term exposure. is also quite noble as it is very corrosion resistant and galvanically compatible with the other six metals from both an electrochemical perspective and long-term crevice corrosion scenario. This was clearly demonstrated utilizing the same techniques for linear, Tafel and cyclic polarization, and galvanic coupling of the metal candidate as was done for the previous study. The high nobility and low corrosion susceptibility for Nitinol 60 appear to be intermediate to the nickel/chromium alloys and the titanium metals with indications that are more reflective of the titanium metals in terms of general corrosion and pitting behavior.

Lee, R. E.↗

Shock- and Corrosion-Resistant Bearings for Space Mechanisms

Nickel-titanium (NiTi) alloys are an emerging class of materials for rolling element bearing applications that require superior corrosion resistance and/or high load capability. Certain space mechanisms fall into one or both of those categories. Often, due to size and mass considerations, space mechanism systems are limited in torque margin and necessarily require small, precision-instrument bearings with very little frictional drag (i.e., low torque). In addition, space mechanism bearings must survive launch conditions without suffering raceway dents known as brinnelling, which would increase operating torque and reduce overall smoothness. Consequently, a bearing material or design that reduces or eliminates brinnelling under high contact stress conditions would represent a beneficial technology advancement. One specific alloy, nickel-titanium-hafnium (NiTi-Hf), under development for several years at the NASA Glenn Research Center as a bearing material, has the potential to mitigate concerns about brinnelling under extreme load conditions due to its unusually high elastic strain capability. In the present work, a sample of small precision bearings produced with three different ball materials (steel, ceramic, and NiTi-Hf) is subjected to a range of load conditions sufficient to dent the races. The dent depth as a function of load is compared and demonstrates that NiTi-Hf has the potential to increase bearing load capacity from the perspective of brinnelling under severe load conditions; additional testing of full NiTi-Hf bearings demonstrates corrosion resistance superior to that of 440C bearings.

Bearings↗