Search NASA⌕ Search

SEARCH · Search NASA

Results for “PITTING CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Burner rig corrosion of SiC at 1000 deg C

Sintered alpha-SiC was examined in both oxidation and hot corrosion with a burner rig at 400 kPa (4 atm) and 1000 C with a flow velocity of 310 ft/sec. Oxidation tests for times to 46 hr produced virtually no attack, whereas tests with 4 ppm Na produced extensive corrosion in 13-1/2 hr. Thick glassy layers composed primarily of sodium silicate formed in the salt corrosion tests. This corrosion attack caused severe pitting of the silicon carbide substrate which led to a 32 percent strength decrease below the as-received material. Parallel furnace tests of Na2SO4/air induced attacked yielded basically similar results with some slight product composition differences. The differences are explained in terms of the continuous sulfate deposition which occurs in a burner rig.

Jacobson, N. S.↗

Burner rig corrosion of SiC at 1000 C

Sintered alpha-SiC was examined in both oxidation and hot corrosion with a burner rig at 400 kPa (4 atm) and 1000 C with a flow velocity of 94 m/s. Oxidation tests for times to 46 h produced virtually no attack, whereas tests with 4 ppm Na produced extensive corrosion in 13.5 h. Thick glassy layers composed primarily of sodium silicate formed in the salt corrosion tests. This corrosion attack caused severe pitting on the silicon carbide substrate and led to a 32 percent decrease in strength, compared to the as-received material. Parallel furnace tests of Na2SO4/air-induced attack yielded basically similar results, with slight product composition differences. The differences are explained in terms of the continuous sulfate deposition which occurs in a burner rig.

Jacobson, N. S.↗

Characterization of the Aerosol Source Term in Dry Storage Canisters

As long-term dry storage of used nuclear fuel at independent spent fuel storage installations (ISFSI) trends toward the de facto back end of the US fuel cycle, it becomes appropriate to investigate potential degradation and dispersion scenarios for suitable risk mitigation purposes. Pitting and subsequent stress corrosion cracking of the canister wall is currently viewed as a potential scenario leading to a through-wall pathway for contamination to be transferred from within the storage container to the surrounding environment. While stress corrosion cracking measurements are currently underway to further characterize this scenario, a parallel effort endeavors to perform a consequence analysis of conditions in which through wall cracks are indeed formed. This effort consists of engineering scale modeling using the GOTHIC and MELCOR software packages along with experimental depletion and penetration tests.

spent fuel storage, aerosol deposition, Stress Cor↗

Aging Management Considerations for Dry Cask Storage Canisters - 18472

Dry cask storage systems (DCSSs) are used to store used nuclear fuel (UNF) at independent spent fuel storage installations (ISFSIs) prior to final geologic storage or reprocessing. As storage durations increase beyond the twenty-year period commonly implemented for licensing the storage sites, it is important to consider aging related degradation issues for DCSS components. A large portion of the DCSS designs used throughout the world employ a ventilated concrete overpack with a welded stainless steel canister that confines the UNF. This paper explores key issues related to aging management for these canister components, including: (1) canister environment, (2) inspection limitations, and (3) aging management program guidance and requirements. While the austenitic stainless steel used for the canisters are generally resistant to most forms of environmental attack, it is possible for conditions to arise that lead to pitting and even stress corrosion cracking of the canister systems. A large number of studies related to canister degradation have been performed by industry groups and government researchers, both in the US and worldwide. These advances in the collective knowledge provide insight into risk factors for DCSS. Such information is beneficial to improve ISFSI siting decisions and ensure successful relicensing of existing ISFSIs. This paper highlights relevant research and also discusses applicability to degradation of other equipment and containers used to process and isolate UNF and other nuclear waste streams from the public and the environment. Inspection of the canister surface is an important tool to investigate and evaluate the potential for degradation. Existing DCSS designs typically do not offer ready access to the canister surface in order to perform the inspection. Further complicating inspection efforts are the surface conditions present on the sheltered canisters after extended storage times, including atmospheric debris such as dust and pollen. Given ongoing development efforts, inspection capabilities and associated limitations should be assessed at multiple points in time over the course of an aging management program to incorporate new advances in the field. This paper explores the limitations of currently available capabilities in inspection and delivery, and provides insight into the gaps remaining to be filled to permit an effective inspection program. Recommendations and requirements related to programs for aging management of canisters have been published or are in progress from a variety of groups, including industry groups, regulatory authorities, and Codes and Standards. An effective aging management program should consider the technical bases of these various inputs and maintain compliance with requirements. Given multiple sources, decisions will be required when considering conflicting guidance, and this paper will include discussion of the relative merits of the various approaches. (author)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

LOCALIZED CORROSION OF AUSTENITIC STAINLESS STEELEXPOSED TO MIXTURES OF PLUTONIUM OXIDE AND CHLORIDE SALTS

Laboratory corrosion tests were conducted to investigate the corrosivity of moist plutonium oxide/chloride (PuO{sub 2}/Cl-) salt mixtures on 304L and 316L stainless steel coupons. The tests exposed flat coupons for pitting evaluation and 'teardrop' stressed coupons for stress corrosion cracking (SCC) evaluation at room temperature to various mixtures of PuO{sub 2} and chloride-bearing salts for periods up to 500 days. The two flat coupons were placed so that the solid oxide/salt mixture contacted about one half of the coupon surface. One teardrop coupon was placed in contact with solid mixture; the second teardrop was in contact with the headspace gas only. The mixtures were loaded with nominally 0.5 wt % water under a helium atmosphere. Observations of corrosion ranged from superficial staining to pitting and SCC. The extent of corrosion depended on the total salt concentration and on the composition of the salt. The most significant corrosion was found in coupons that were exposed to 98 wt % PuO{sub 2}, 2 wt % chloride salt mixtures that contained calcium chloride. SCC was observed in two 304L stainless steel teardrop coupons exposed in solid contact to a mixture of 98 wt % PuO{sub 2}, 0.9 wt % NaCl, 0.9 wt % KCl, and 0.2 wt % CaCl{sub 2}. The cracking was associated with the heat-affected zone of an autogenous weld that ran across the center of the coupon. Cracking was not observed in coupons exposed to the headspace gas, nor in coupons exposed to other mixtures with either 0.92 wt% CaCl{sub 2} or no CaCl{sub 2}. The corrosion results point to the significance of the interaction between water loading and the concentration of the hydrating salt CaCl{sub 2} in the susceptibility of austenitic stainless steels to corrosion.

36 MATERIALS SCIENCE↗

ELECTROCHEMICAL CORROSION TESTS FOR TANK 241-AY-101 CORE 325 SEGMENTS 16R1 & 16R2

The interstitial liquid in the double-shell tank 241-AY-101 settled solids layer is below the hydroxide chemistry control limit required by HNF-SD-WM-TSR-006, Tank Farms Technical Safety Requirements, Administrative Control 5.16, 'Corrosion Mitigation Controls'. Operating tanks outside of the specification may increase the propensity corrosion of the carbon steel wall. This report is concerned with generalized electrochemical corrosion mechanism that may occur at specific loci. All cyclic potentiodynamic polarization scans exhibited a negative hysteresis, scan reversing at lower current density, indicating that there was no pitting propensity. The general electrochemical corrosion rates ranged from 4.4E-02 to 1.5E-03 mpy with the first round of coupons, while the second round yielded corrosion rates of 2.5E-03 to 2.9E-02 mpy.

36 MATERIALS SCIENCE↗

Liquid-Air Interface Corrosion Studies at SRS

Philip Zapp of Savannah River Site (SRS) details corrosion studies done at the facility's waste tanks with an emphasis on pitting and the liquid-air interface.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Seacoast stress corrosion cracking of aluminum alloys

The stress corrosion cracking resistance of high strength, wrought aluminum alloys in a seacoast atmosphere was investigated and the results were compared with those obtained in laboratory tests. Round tensile specimens taken from the short transverse grain direction of aluminum plate and stressed up to 100 percent of their yield strengths were exposed to the seacoast and to alternate immersion in salt water and synthetic seawater. Maximum exposure periods of one year at the seacoast, 0.3 or 0.7 of a month for alternate immersion in salt water, and three months for synthetic seawater were indicated for aluminum alloys to avoid false indications of stress corrosion cracking failure resulting from pitting. Correlation of the results was very good among the three test media using the selected exposure periods. It is concluded that either of the laboratory test media is suitable for evaluating the stress corrosion cracking performance of aluminum alloys in seacoast atmosphere.

Humphries, T. S.↗

In-situ visualization of corrosion behavior of Al CoCrFeNi high-entropy alloys during electrochemical polarization

In this study, the corrosion behavior of the Al x CoCrFeNi (x = 0.3, 0.5, 0.7) high-entropy alloys (HEAs) is investigated by an in-situ visualization system. Surface morphology changes on both micro-spatial and temporal scales are monitored in the 3.5 wt% NaCl solution during the potentiodynamic polarization. The microstructures of the Al x CoCrFeNi HEAs are characterized by SEM, EBSD, and EDS. The results show that the microstructure evolves from singe face-centered cubic (FCC) phase to multi-phases by increasing the Al content. The in-situ observations directly reveal the different localized corrosion processes in the AlxCoCrFeNi HEAs. In the single FCC phase Al 0.3 CoCrFeNi HEA, localized corrosion shows in the form of pitting. In the Al 0.5 CoCrFeNi and Al 0.7 CoCrFeNi alloys, which possess FCC and body-centered cubic (BCC) phases, the localized corrosion initiates and propagates in the Cr-depleted BCC phase. In addition, the in-situ visualization uncovers the evolution of current serration, which represents the propagation and repassivation of metastable pit during the polarization. The frequent occurrence of metastable pits indicates distinct repassivation ability of the Al 0.3 CoCrFeNi HEA.

36 MATERIALS SCIENCE↗

Effect of the Heat Treatment on the Corrosion Resistance of Duplex Stainless Steels

Duplex stainless steels (DSS) are biphasic austenitic-ferritic steels in which the best combination of mechanical and corrosion resistance properties is achieved for an almost equal volume fraction of the phases. In this work, the effect of secondary phases precipitation on the corrosion resistance of four DSS grades (2101, 2304, 2205 and 2507), after isothermal aging in the critical temperature range 750-900 °C, was studied. The corrosion resistance was investigated by potentiodynamic polarization tests in both 0.6 M NaCl solution (pH 7) and in an acid chlorinated solution (pH 3) at room temperature. Moreover, the critical pitting temperature was determined according to ASTM G150. The results showed that secondary phases precipitation mainly influenced the resistance to corrosion of the lean duplex grades.

36 MATERIALS SCIENCE↗

LABORATORY TESTING TO SIMULATE VAPOR SPACE CORROSION IN RADIOACTIVE WASTE STORAGE TANKS

Radioactive liquid waste has been stored in underground carbon steel tanks for nearly 70 years at the Hanford nuclear facility. Vapor space corrosion of the tank walls has emerged as an ongoing challenge to overcome in maintaining the structural integrity of these tanks. The interaction between corrosive and inhibitor species in condensates/supernates on the tank wall above the liquid level, and their interaction with vapor phase constituents as the liquid evaporates from the tank wall influences the formation of corrosion products and the corrosion of the carbon steel. An effort is underway to gain an understanding of the mechanism of vapor space corrosion. Localized corrosion, in the form of pitting, is of particular interest in the vapor space. CPP testing was utilized to determine the susceptibility of the steel in a simulated vapor space environment. The tests also investigated the impact of ammonia gas in the vapor space area on the corrosion of the steel. Vapor space coupon tests were also performed to investigate the evolution of the corrosion products during longer term exposures. These tests were also conducted at vapor space ammonia levels of 50 and 550 ppm NH{sub 3} (0.005, and 0.055 vol.%) in air. Ammonia was shown to mitigate vapor space corrosion.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Uncertainty quantification methodologies development for stress corrosion cracking of canister welds

This letter report presents a probabilistic performance assessment model to evaluate the probability of canister failure (through-wall penetration) by SCC. The model first assesses whether environmental conditions for SCC – the presence of an aqueous film – are present at canister weld locations (where tensile stresses are likely to occur) on the canister surface. Geometry-specific storage system thermal models and weather data sets representative of U.S. spent nuclear fuel (SNF) storage sites are implemented to evaluate location-specific canister surface temperature and relative humidity (RH). As the canister cools and aqueous conditions become possible, the occurrence of corrosion is evaluated. Corrosion is modeled as a two-step process: first, pitting is initiated, and the extent and depth of pitting is a function of the chloride surface load and the environmental conditions (temperature and RH). Second, as corrosion penetration increases, the pit eventually transitions to a SCC crack, with crack initiation becoming more likely with increasing pit depth. Once pits convert to cracks, a crack growth model is implemented. The SCC growth model includes rate dependencies on both temperature and crack tip stress intensity factor, and crack growth only occurs in time steps when aqueous conditions are predicted. The model suggests that SCC is likely to occur over potential SNF interim storage intervals; however, this result is based on many modeling assumptions. Sensitivity analyses provide information on the model assumptions and parameter values that have the greatest impact on predicted storage canister performance, and provide guidance for further research to reduce uncertainties.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Review—Effects of Solution and Alloy Composition on Critical Crevice Temperature

Critical temperature for localized corrosion can be a good design parameter because localized corrosion is not likely to occur below that temperature. The critical temperature depends on alloy composition, microstructure, and environment chemistry (including its redox potential). This paper reviews the literature on critical temperature for localized corrosion, expressed either as Critical Pitting Temperature (CPT) or Critical Crevice Temperature (CCT). A history of various testing methods is presented. Different approaches for modeling the temperature of transition to active pit growth are reviewed, including probabilistic aspects of critical temperature. A semi-empirical, electrolyte-based, model is described that can be useful in predicting CCT in service environments that differ from standard laboratory test environments. The model predictions are compared to experimental data for various alloys. The effect of solvent on CCT/CPT is described briefly and future avenues of research are recommended.

02 PETROLEUM↗

Pitting behavior of friction stir repair-welded 304L stainless steel in 3.5% NaCl solution at room temperature: role of grain and defect structures

Stainless steel (SS) canisters used for storing spent nuclear waste are prone to chloride-induced stress corrosion cracking. Friction stir welding (FSW), being a low heat input process, can be used for repair welding of these canisters. In this study, an artificial crack was introduced on the 304L SS coupons by an electric discharge machining process. The artificial crack was repair-welded by FSW by maintaining the tool temperature a constant at two levels (725 and 825 °C). Friction stirring significantly reduced the grain size of the stirred zone (SZ) from about 47 to 2–4 μm. The fraction of low-angle grain boundaries increased in the SZ from 2 to 37–43%. Here, on the other hand, the fraction of special grain boundaries (Σ3 and Σ9) that was ~ 50% in the base metal reduced to < 10% in the SZ. During friction stirring, the oxide layer of artificial crack was broken and aligned to form a spiral defect called lazy-S structure. All these microstructural changes affected the corrosion behavior of the FSW specimens when tested in 3.5% NaCl at room temperature using cyclic polarization, chronoamperometry, and electrochemical impedance spectroscopy. The FSW specimens showed lower polarization resistance and lower transpassive potential than those of the base metal specimens. However, the pitting protection potentials of the FSW specimens were higher than that of the base metal. The pitting behavior of the FSW specimens was influenced more by the preferential attack on the lazy-S region than by passive film breakdown. The flat band potentials of the passive film formed on the FSW specimens were more positive than that of base metal. The charge carrier density of passive film formed on the FSW specimens was higher than that of the base metal. The higher fraction of low-angle grain boundaries present in the FSW specimens could supply more number of misorientation dislocations at the metal/film interface which could form anion vacancies by a climb process leading to formation of oxide at these locations without stressing the substrate. Therefore, low-angle boundaries are considered helpful for formation of stress-free passive films that will be highly stable and enhance both pitting and stress corrosion cracking resistance.

Dry storage canister↗

Overview of zion comparative analysis project for assessment of Boral{sup R} neutron absorber material performance and monitoring in spent fuel pools - 14618

Neutron absorber materials are used in spent fuel pool (SFP) storage racks to control reactivity. In the United States, about half of the operating plants currently use BORAL{sup R} neutron absorber material in SFP racks. Although operational experience spanning more than 25 years has not shown any loss of the BORAL{sup R} core material, corrosion effects, including blisters and pits, have been observed and reported. To improve understanding for the behavior of BORAL{sup R} in SFPs and evaluate the performance of monitoring approaches, EPRI initiated the Zion comparative analysis project in 2014. The Zion project involves three phases. During the first phase of the project, in situ measurements were performed on selected SFP rack panels in December 2014. Panels for in situ measurements were selected after an extensive analysis of each panel in the pool to ensure that the selected panels represented the pool in terms of variation in neutron and gamma dose values. As part of the second phase of the project, the remaining 10 coupons from the Zion SFP were shipped to a Penn State University (PSU) laboratory for analysis in January 2015. During the final phase of the project, a subset of the panels for which in situ measurements were performed will be harvested from the Zion SFP, cut into samples, and analyzed at PSU. The overall scope of this project will allow comparison of in situ measurements to real panel data as well as data obtained from coupon analysis. In this paper, an overview of the Zion comparative analysis project, the criteria and procedure for panel selection for in situ measurements and harvesting, preliminary coupon analysis results and in situ measurement results are presented. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Burner Rig Hot Corrosion of a Single Crystal Ni-48Al-Ti-Hf-Ga Alloy

The hot corrosion resistance of a single crystal Ni-48Al-1Ti-0.5Hf-0.2Ga alloy was examined in a Mach 0.3 burner rig at 900 C for 300 hours. The combustion chamber was doped with 2 ppmw synthetic sea salt. The hot corrosion attack produced a random mound morphology on the surface. Microstructurally, the hot corrosion attack appeared to initiate with oxide-filled pits which were often broad and shallow. At an intermediate stage, the pits increased in size to incorporate unoxidized Ni islands in the corrosion product. The rampant attack stage, which was observed only at sharp sample corners, was characterized by rapid inward growth of alumina in finger-like protrusions incorporating significant amounts of Al-depleted Ni islands. Aluminum consumption in the oxide fingers resulted in the growth of a gamma' layer ahead of the advancing oxide fingers.

Nesbitt, James A.↗

Localized Corrosion of Chromium-Containing Conventional and Multiprincipal Element Alloys in Methanol and Aqueous Chloride Environments

The localized corrosion behavior of Type 304L stainless steel (UNS S30400), Alloy 625 (UNS N06625), and three experimental NiCoCrMo multiprincipal element alloys (MPEA), exposed to methanol/lithium chloride solutions with different water contents, is examined in this paper. Cyclic potentiodynamic polarization tests indicated that water increased the pitting and repassivation potentials and the critical temperature at which localized corrosion occurred in chloride solutions. The effect of water on repassivation potential in methanol-chloride solution depended on the chloride concentration and alloy content. At lower chloride concentration and higher alloy content, water had a greater inhibiting effect on repassivation potential, suggesting a competitive reaction between chloride and water on the metal surface in the pit. The localized corrosion resistance of the MPEAs followed the same trend as that of commercial stainless steels and Ni-base alloys in terms of the effect of alloying elements. The implications of these results on the mechanisms of localized corrosion are discussed.

Materials Science↗

Passive and Semiconducting Properties Assessment of Commercially Pure Tantalum in Hank’s Physiological Solution

In this study, various electrochemical measurements were used to evaluate the passive and semiconducting properties of commercially pure tantalum (Ta) in Hank’s physiological solution at 310 K (37 °C). Potentiodynamic polarization and electrochemical impedance spectroscopy results show that the passivation of pure Ta immersed in Hank’s physiological solution improves over time. Mott–Schottky (M–S) tests indicate that the passive layers of pure Ta in Hank’s physiological solution behave as n-type semiconductors and longer immersion times do not lead to any inversion of semiconducting behavior. Additionally, M–S tests show that as the immersion time increases, the donor density of the passive layer decreases. Finally, scanning electron microscope micrographs and energy-dispersive spectroscopy results reveal that Ta is less likely to experience significant pitting or buildup of undesirable corrosion products after longer immersion times in this physiological solution.

36 MATERIALS SCIENCE↗