Oxidation of chemically-vapor-deposited silicon nitride and single-crystal silicon

The present 1000 C and 1300 C oxidation tests on 111-oriented single-crystal Si and dense CVD Si3N4 notes the oxidation rates of the latter in wet O2, dry O2, wet inert gas, and steam atmosphere conditions to be several orders of magnitude lower than the rates for the former in identical atmospheric conditions. Although the parabolic rate constant for Si increased linearly as the water vapor pressure increased, the parabolic rate constant for Si3N4 exhibited a nonlinear dependency on water vapor pressure in the presence of O2. NO and NH3 formation at the reaction interface of Si3N4, and the counterpermeation of these reaction products, are noted to dominate reaction kinetics.

Choi, Doo J.↗

The effect of hydrogen on the deformation and fracture behavior of a single crystal nickel-base superalloy

The room temperature and 300 C tensile behavior of a single crystal superalloy, PWA 1480, has been studied as a function of internal hydrogen concentration and microstructure. Hydrogen is trapped at the porosity and eutectic gamma/gamma in the microstructure, and the effect of these trapping sites on the tensile behavior will be discussed. There is no effect of hydrogen on strength, however, the strain to failure decreases steadily with increasing hydrogen content up to 200 ppm. Cleavage of the eutectic gamma/gamma occurs without hydrogen, but the presence of internal hydrogen causes cracking in the eutectic gamma/gamma at a much earlier stage of deformation leading to a small total strain. In contrast to many superalloys with a high volume fraction of gamma precipitates, there was no evidence of shearing of the gamma, and it was found that at all strains the dislocations are trapped in the gamma matrix. The effect of hydrogen on this behavior and its relation to fracture is described.

Walston, W. S.↗

Factors Affecting the Ductility and Strength of NaCl Single Crystals Tested in Flexure

An experimental investigation has revealed that the initial deformation of NaCl single crystals is anelastic rather than Hookean. This anelastic deformation is manifested by a low slope foot in the load‐deflection curve. The magnitude of the foot is dictated by the pretreatment given the specimen. Treatments which increase or decrease the fresh dislocation density respectively increase or decrease the length of the initial anelastic foot. The order of increasing ductility and strength with specimen pretreatment was found to be (1) heated at 135 C, (2) as cleaved, (3) coated with silver, (4) heated at 135 C and then water polished, (5) water polished and then coated with silver, (6) water polished, (7) water polished and then heated at 135 C, (8) annealed at 700 C, and (9) annealed at 700 C and then water polished. The experimental results have been discussed in terms of the role played in deformation and fracture by surface cracks, grown‐in dislocations, and fresh dislocations.

Stearns, C. A.↗

The low cycle fatigue deformation response of a single-crystal superalloy at 650 C

The cyclic stress-strain response and the associated deformation structure of the single crystal nickel-base superalloy PWA 1480 were investigated. Specimens of various crystallographic orientations were tested in low-cycle fatigue (LCF) at 650 C, resulting in a significant tension-compression anisotropy in initial yield strength associated with the shearing of gamma-prime precipitates by dislocation pairs, and a LCF cyclic hardening of the crystals associated with dislocation interactions occurring in the gamma phase. In specimens deforming by slip on a single slip system, dislocations of the primary slip system accumulated in the gamma matrix and formed seesile entanglements. In specimens deforming by slip on several slip systems, the dislocations of the different operative slip systems intersected in the gamma matrix and formed sessile arrangements.

Gabb, T. P.↗

An Atomistic Simulation of Crack Propagation in a Nickel Single Crystal

The main objective of this paper is to determine mechanisms of crack propagation in a nickel single crystal. Motivation for selecting nickel as a case study is because we believe that its physical properties are very close to that of nickel-base super alloy. We are directed in identifying some generic trends that would lead a single crystalline material to failure. We believe that the results obtained here would be of interest to the experimentalists in guiding them to a more optimized experimental strategy. The dynamic crack propagation experiments are very difficult to do. We are partially motivated to fill the gap by generating the simulation results in lieu of the experimental ones for the cases where experiment can not be done or when the data is not available.

Majid Karimi↗

The adsorption and early stages of condensation of Ag and Au on W single-crystal surfaces

Silver and gold were evaporated up to several monolayers in thickness onto W single-crystal surfaces of the 110 and 100 plane types in the temperature range between 300 and 1300 K. The mode of growth and the structure of the layers were studied by Auger electron spectroscopy and low-energy electron diffraction. The results are compared with thermal desorption spectroscopy data and work-function change measurements. They show certain similarities but also some striking differences between the two systems Ag/W and Au/W as well as a strong crystallographic anisotropy of adsorption and condensation.

Bauer, E.↗

Friction and wear behavior of single-crystal silicon carbide in sliding contact with various metals

Sliding friction experiments were conducted with single-crystal silicon carbide in contact with various metals. Results indicate the coefficient of friction is related to the relative chemical activity of the metals. The more active the metal, the higher the coefficient of friction. All the metals examined transferred to silicon carbide. The chemical activity of the metal and its shear modulus may play important roles in metal transfer, the form of the wear debris and the surface roughness of the metal wear scar. The more active the metal, and the less resistance to shear, the greater the transfer to silicon carbide and the rougher the wear scar on the surface of the metal. Hexagon shaped cracking and fracturing formed by cleavage of both prismatic and basal planes is observed on the silicon carbide surface.

Miyoshi, K.↗

Friction and wear behavior of single-crystal silicon carbide in sliding contact with various metals

Sliding friction experiments were conducted with single-crystal silicon carbide in contact with various metals. Results indicate the coefficient of friction is related to the relative chemical activity of the metals. The more active the metal, the higher the coefficient of friction. All the metals examined transferred to silicon carbide. The chemical activity of the metal and its shear modulus may play important roles in metal-transfer, the form of the wear debris and the surface roughness of the metal wear scar. The more active the metal, and the less resistance to shear, the greater the transfer to silicon carbide and the rougher the wear scar on the surface of the metal. Hexagon-shaped cracking and fracturing formed by cleavage of both prismatic and basal planes is observed on the silicon carbide surface.

Miyoshi, K.↗

Anisotropic constitutive model for nickel base single crystal alloys: Development and finite element implementation

A tool for the mechanical analysis of nickel base single crystal superalloys, specifically Rene N4, used in gas turbine engine components is developed. This is achieved by a rate dependent anisotropic constitutive model implemented in a nonlinear three dimensional finite element code. The constitutive model is developed from metallurigical concepts utilizing a crystallographic approach. A non Schmid's law formulation is used to model the tension/compression asymmetry and orientation dependence in octahedral slip. Schmid's law is a good approximation to the inelastic response of the material in cube slip. The constitutive equations model the tensile behavior, creep response, and strain rate sensitivity of these alloys. Methods for deriving the material constants from standard tests are presented. The finite element implementation utilizes an initial strain method and twenty noded isoparametric solid elements. The ability to model piecewise linear load histories is included in the finite element code. The constitutive equations are accurately and economically integrated using a second order Adams-Moulton predictor-corrector method with a dynamic time incrementing procedure. Computed results from the finite element code are compared with experimental data for tensile, creep and cyclic tests at 760 deg C. The strain rate sensitivity and stress relaxation capabilities of the model are evaluated.

Dame, L. T.↗

Growth of Solid Solution Single Crystals

The objective of the study is to establish the effects of processing semiconducting, solid solution, single crystals in a microgravity environment on the metallurgical, compositional, electrical, and optical characteristics of the crystals. The alloy system being investigated is the solid solution semiconductor Hg(1-x)Cd(x)Te, with x-values appropriate for infrared detector applications in the 8 to 14 mm wavelength region. Both melt and Te-solvent growth are being performed. The study consists of an extensive ground-based experimental and theoretical research effort followed by flight experimentation where appropriate. The ground-based portion of the investigation also includes the evaluation of the relative effectiveness of stabilizing techniques, such as applied magnetic fields, for suppressing convective flow during the melt growth of the crystals.

Lehoczky, Sandor L.↗

Friction and metal transfer for single-crystal silicon carbide in contact with various metals in vacuum

Sliding friction experiments were conducted with single-crystal silicon carbide in contact with transition metals (tungsten, iron, rhodium, nickel, titanium, and cobalt), copper, and aluminum. Results indicate the coefficient of friction for a silicon carbide-metal system is related to the d bond character and relative chemical activity of the metal. The more active the metal, the higher the coefficient of friction. All the metals examined transferred to the surface of silicon carbide in sliding. The chemical activity of metal to silicon and carbon and shear modulus of the metal may play important roles in metal transfer and the form of the wear debris. The less active and greater resistance to shear the metal has, with the exception of rhodium and tungsten, the less transfer to silicon carbide.

Miyoshi, K.↗

Elevated temperature creep-rupture behavior of the single crystal nickel-base superalloy NASAIR 100

The creep and rupture behavior of 001-line-oriented single crystals of the nickel-base superalloy NASAIR 100 was investigated at temperatures of 925 and 1000 C. In the stress and temperature ranges studied, the steady state creep rate, time to failure, time to the onset of secondary creep, and the time to the onset of tertiary creep all exhibited power law dependencies on the applied stress. The creep rate exponents for this alloy were between seven and eight, and the modulus-corrected activation energy for creep was approximately 350 kjoule/mole, which was comparable to the measured activation energy for Ostwald ripening of the gamma-prime precipitates. Oriented gamma-prime coarsening to form lamellae perpendicular to the applied stress was very prominent during creep. At 1000 C, the formation of a continuous gamma-gamma-prime lamellar structure was completed during the primary creep stage. Shear through the gamma-gamma-prime interface is considerd to be the rate limiting step in the deformation process. Gradual thickening of the lamellae appeared to be the cause of the onset of tertiary creep. At 925 C, the fully developed lamellar structure was not achieved until the secondary or tertiary creep stages. At this temperature, the gamma-gamma-prime lamellar structure did not appear to be as beneficial for creep resistance as at the higher temperature.

Nathal, M. V.↗