SEARCH · Search NASA
Results for “SOLDERING”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
The Challenges of Pb-free Electronics Technology for the Aerospace and Defense (A&D) Industries: "Beyond the Solder Joint".
Abstract not provided.
High-cycle Fatigue (HCF) Test Development to Assess Solder Joints.
Abstract not provided.
High-Cycle Fatigue Test Development to Assess Solder Joints.
Abstract not provided.
Statistical strength analysis of soldered metal/ceramic joints
Explore the source record for details and available documents.
OLED Lighting Substrate and Encapsulation System for Breakthrough Cost Reductions
OLED lighting is predicted to contribute a significant part of the US energy savings that will result from the implementation of Solid-State Lighting (SSL). OLED lighting adoption is predicted to reach approximately 5% of the lighting market by 2020. The primary purpose of this study was to address a barrier in OLED lighting adoption, this being OLED production costs. This project enabled the elimination of the anode patterning steps, by physically insulating the cathode contact area from the blanket coated ITO anode. Furthermore, this technology eliminates the need to change shadow masks between the organic materials and the cathode, making the OLED deposition machines simpler, lower cost, and less prone to particle generation. Finally, the process developed here permits the creation of a perfectly hermetic seal thereby eliminating the cost of desiccant materials. In this project, we successfully developed an ultrasonic soldering process to create a perfectly hermetic metal-on-glass bond. This required the evaluation of many ultrasonic solder materials, soldering parameters, and solder hardware configurations. In addition, methods to evaluate the hermeticity of the solder seal were developed and successfully tested. Our work demonstrated the ability to make a hermetic solder seal between a device glass and a cover glass using a Cerasolzer 155 ultrasonic solder. The resulting process could be leveraged to almost any OLED configuration. As we did not have the opportunity to produce a significant quantity of OLED devices for environmental testing, hermeticity was verified by measuring helium leakage rates through the seal. A second facet of this project required the development of a patterned glass frit insulating barrier over surface of the anode. To accomplish this, the appropriate insulator formulation and geometry needed to be established. In addition, this insulator needed to be robust enough to hold up to the ultrasonic soldering process previously mentioned. Given the aggressive nature of the ultrasonic soldering process, it was a significant challenge to develop an insulator which would withstand the resulting solder cavitation. The frit material and firing process turned out to be quite expensive and time consuming which was a major contributor to the higher than anticipated cost of this technology. In the end, it was found that a Vanadium Phosphate glass frit provided the most reliable insulator over the ITO.
Thermal Testing Quality Assurance of 24LCC & 3LCC Electronic Packages
The purpose of this project is to experimentally validate the thermal fatigue life of solder interconnects for a variety of surface mount electronic packages. Over the years, there has been a significant amount of research and analysis in the fracture of solder joints on printed circuit boards. Solder is important in the mechanical and electronic functionality of the component. It is important throughout the life of the product that the solder remains crack and fracture free. The specific type of solder used in this experiment is a 63Sn37Pb eutectic alloy. Each package was manufactured with conformal coating along with and without an underfill material below the device. Conformal coating helps protect the board from environments such as electrostatic discharge and humidity. It is commonly used in broad types of engineering disciplines such as commercial, military, research and development, etc. Conformal coating can also pose a risk for the life of the board because of its high thermal expansion coefficient. This can greatly decrease the life of the product if it regularly sees high temperature variations. This leads to a shorter fatigue life of the solder. The fatigue life is a common mechanical problem in the field of electronic devices. Adding underfill can help increase the fatigue life of the solder. However, applying underfill adds time to manufacturing and production. This ultimately increases the cost per unit. The study of conformal coated printed circuit boards with and without underfill was done on two different surface mount electronic packages. The electronic packages studied were 24 and 3 contact Leadless Ceramic Chips packages. When the package was not underfilled, the coating was allowed to flow underneath. The assembly was analyzed and tested to obtain the best available combination of conformal coating, underfill, and potting to design the most robust and reliable circuit board while keeping in mind certain factors such as cost, manufacturing time, and need. Different types of conformal coatings were considered with and without underfill for each device. 29 of each component were manufactured to have a large sample size and for the sake of individual defects and imperfections. Finite Element Analysis (FEA) was performed by an engineer at Sandia National Laboratories for both Leadless Ceramic Chips. From the FEA results, a test acceleration profile was derived and the number of temperature cycles to fail the solder interconnects were found for three different cases. Experimentation was done as a secondary measure to validate this data to show confidence in the theoretical analysis. Accelerated testing functions as a quality check for the product. Accelerated testing is extremely useful in the research and development phase of engineering. It can save money from the potential of early life defects and the costs that come along with warranties. Accelerated testing makes a weaker design more robust and checks the reliability of a strong design in a shorter period of time. It is extremely helpful in a world where deliverables are in high demand and scheduling is tight. Accelerated testing helps the engineer gain an understanding of what needs to be improved and what works well. There are many different types of accelerated tests. Our circuit boards were accelerated inside a closed thermal chamber because of the high number of use cycles. The ultimate goal of this experimentation is to help identify what will prevent any premature cracking or fracturing in the solder alloy. It is important to understand that underfilling each component may or may not be needed. If underfill is not needed, there are several production benefits.
Metallurgy, thermal stability, and failure mode of the commercial Bi-Te-based thermoelectric modules.
Bi-Te-based thermoelectric (TE) alloys are excellent candidates for power generation modules. We are interested in reliable TE modules for long-term use at or below 200 C. It is known that the metallurgical characteristics of TE materials and of interconnect components affect the performance of TE modules. Thus, we have conducted an extensive scientific investigation of several commercial TE modules to determine whether they meet our technical requirements. Our main focus is on the metallurgy and thermal stability of (Bi,Sb){sup 2}(Te,Se){sup 3} TE compounds and of other materials used in TE modules in the temperature range between 25 C and 200 C. Our study confirms the material suite used in the construction of TE modules. The module consists of three major components: AlN cover plates; electrical interconnects; and the TE legs, P-doped (Bi{sub 8}Sb{sub 32})(Te{sub 60}) and N-doped (Bi{sub 37}Sb{sub 3})(Te{sub 56}Se{sub 4}). The interconnect assembly contains Sn (Sb {approx} 1wt%) solder, sandwiched between Cu conductor with Ni diffusion barriers on the outside. Potential failure modes of the TE modules in this temperature range were discovered and analyzed. The results show that the metallurgical characteristics of the alloys used in the P and N legs are stable up to 200 C. However, whole TE modules are thermally unstable at temperatures above 160 C, lower than the nominal melting point of the solder suggested by the manufacture. Two failure modes were observed when they were heated above 160 C: solder melting and flowing out of the interconnect assembly; and solder reacting with the TE leg, causing dimensional swelling of the TE legs. The reaction of the solder with the TE leg occurs as the lack of a nickel diffusion barrier on the side of the TE leg where the displaced solder and/or the preexisting solder beads is directly contact the TE material. This study concludes that the present TE modules are not suitable for long-term use at temperatures above 160 C due to the reactivity between the Sn-solder and the (Bi,Sb){sup 2}(Te,Se){sup 3} TE alloys. In order to deploy a reliable TE power generator for use at or below 200 C, alternate interconnect materials must be used and/or a modified module fabrication technique must be developed.
Circularly Polarized Microwave Antenna Element with Very Low Off-Axis Cross-Polarization
The goal of this work was to improve off-axis cross-polarization performance and ease of assembly of a circularly polarized microwave antenna element. To ease assembly, the initial design requirement of Hexweb support for the internal circuit part, as well as the radiating disks, was eliminated. There is a need for different plating techniques to improve soldering. It was also desirable to change the design to eliminate soldering as well as the need to use the Hexweb support. Thus, a technique was developed to build the feed without using solder, solving the lathing and soldering issue. Internal parts were strengthened by adding curvature to eliminate Hexweb support, and in the process, the new geometries of the internal parts opened the way for improving the off-axis cross-polarization performance as well. The radiating disks curvatures were increased for increased strength, but it was found that this also improved crosspolarization. Optimization of the curvatures leads to very low off-axis cross-polarization. The feed circuit was curved into a cylinder for improved strength, eliminating Hexweb support. An aperture coupling feed mechanism eliminated the need for feed pins to the disks, which would have required soldering. The aperture coupling technique also improves cross-polarization performance by effectively exciting the radiating disks very close to the antenna s central axis of symmetry. Because of the shape of the parts, it allowed for an all-aluminum design bolted together and assembled with no solder needed. The advantage of a solderless design is that the reliability is higher, with no single-point failure (solder), and no need for special plating techniques in order to solder the unit together. The shapes (curved or round) make for a more robust build without extra support materials, as well as improved offaxis cross-polarization.
Popcorning Failures in Polymer and MnO2 Tantalum Capacitors
Popcorning is a well-known effect in plastic encapsulated microcircuits (PEM) and it occurs in chip tantalum capacitors. The sensitivity of components to the presence of moisture during soldering is characterized by the moisture sensitivity level (MSL); however, contrary to PEMs, there is no standard procedure for establishing MSL for tantalum capacitors.The effect of absorbed moisture on soldering related degradation and failures in tantalum capacitors have not been studied properly yet, and there is no sufficient information regarding the difference in the sensitivity to soldering between polymer and MnO2 capacitors. In this work, 16 types of polymer and 9 types of MnO2 tantalum capacitors with different moisture content have been tested before and after reflow soldering. The level of moisture release during soldering has been estimated and thermo-mechanical analysis used to assess deformation of capacitorsduring soldering simulations. Results show that moisture uptake in similar parts is approximately two times greater in polymer than in MnO2 capacitors. Cracking of the case and degradation of parameters can occur in both types of parts, but MnO2 capacitors are much more likely to fail catastrophically with a short circuit and possible ignition during the first power-on cycle. This type of failure in MnO2 capacitors is lot-related, can occur even at derated voltages and relatively low levels of moisture sorption that corresponds to room conditions. Baking before soldering is an effective measure to prevent failures even in lots susceptible to popcorning damage.
NASA-DoD Lead-Free Electronics Project: Vibration Test
Vibration testing was conducted by Boeing Research and Technology (Seattle) for the NASA-DoD Lead-Free Electronics Solder Project. This project is a follow-on to the Joint Council on Aging Aircraft/Joint Group on Pollution Prevention (JCAA/JG-PP) Lead-Free Solder Project which was the first group to test the reliability of lead-free solder joints against the requirements of the aerospace/miLItary community. Twenty seven test vehicles were subjected to the vibration test conditions (in two batches). The random vibration Power Spectral Density (PSD) input was increased during the test every 60 minutes in an effort to fail as many components as possible within the time allotted for the test. The solder joints on the components were electrically monitored using event detectors and any solder joint failures were recorded on a Labview-based data collection system. The number of test minutes required to fail a given component attached with SnPb solder was then compared to the number of test minutes required to fail the same component attached with lead-free solder. A complete modal analysis was conducted on one test vehicle using a laser vibrometer system which measured velocities, accelerations, and displacements at one . hundred points. The laser vibrometer data was used to determine the frequencies of the major modes of the test vehicle and the shapes of the modes. In addition, laser vibrometer data collected during the vibration test was used to calculate the strains generated by the first mode (using custom software). After completion of the testing, all of the test vehicles were visually inspected and cross sections were made. Broken component leads and other unwanted failure modes were documented.
Study of the oxidation effects on isothermal solidification based high temperature stable Pt/In/Au and Pt/In/Ag thick film interconnections on LTCC substrate
The objective of the presented paper is to determine the oxidized phase compositions of indium lead-free solders during solidification at 190 ° C under room environment with the help of X-ray diffraction (XRD) and Energy dispersive spectroscopy (EDX). Many lead-free solders alloys available oxidizes and have poor wetting properties. The oxidation of pure indium solder foil, Au, Pt, and Ag alloys were identified and investigated, in the process of isothermal solidification based solder joints construction at room environment and humidity. Both EDX and XRD characterization techniques were performed to trace out the amount of oxide levels and variety of oxide formations at solder interface respectively. The paper also aims to report the isothermal solidification technique to provide interconnections to pads on Low temperature co-fired ceramic (LTCC) substrate. It also elaborates advantages of isothermal solidification over the other methods of interconnection. Scanning electron microscope (SEM) used to identify the oxidized spots on the surface of Pt, Ag substrates and In solder. The identified oxides were reported.