At least 397 records · Page 22

Demystify radiation-enhanced hydrogen isotope diffusion in Fe-Ni-Cr austenitic stainless steels

Understanding and containing hydrogen isotope diffusion is crucial for many nuclear applications. In situ experiments have consistently shown that radiation significantly enhances isotope diffusion in austenitic stainless steels. Despite extensive research, the mechanism behind this phenomenon remains elusive, as most radiation-induced defects (e.g., vacancies, dislocations, and grain boundaries) typically trap hydrogen, thereby slowing diffusion. While grain boundaries may increase in-plane diffusivity and interstitials may enhance diffusion due to material swelling, these effects are relatively minor. Utilizing an Fe-Ni-Cr-H interatomic potential for stainless steels, we conducted extensive molecular dynamics simulations to investigate the origins of radiation-enhanced diffusion. Here, our findings reveal that when a system is resolidified, mimicking defects created by radiation displacements, the resulting structure contains a mixture of phases, boundaries, and dislocation networks. This defective structure significantly increases hydrogen diffusivity, enhancing it by approximately 1.7 times at 900 K. These results suggest that the complex defect structures formed during radiation displacements are the primary drivers of the observed diffusion enhancement, providing valuable insights into the mechanisms underlying radiation-enhanced diffusion in nuclear materials.

36 MATERIALS SCIENCE↗

Chemical interaction and compatibility of uranium mononitride and alumina forming austenitic stainless steel

Uranium mononitride (UN) and alumina forming austenitic (AFA) stainless steel are a potential fuel-cladding combination for the lead-cooled fast reactor (LFR). Chemical compatibility between UN and AFA steel needs to be verified before implementation in a nuclear reactor. Diffusion couple experiments at 823 K and 1023 K were conducted for nonirradiated UN samples in contact with as-cast (no thermally grown Al 2 O 3 ) and preoxidized (with thermally grown Al 2 O 3 ) AFA for 500 and 1000 h in an inert environment. Preoxidized AFA exhibited little to no interaction with all UN samples tested at both 823 K and 1023 K, displaying the stability and capability of the Al 2 O 3 layer to prevent chemical interaction and inter-diffusion with UN. Chemical interaction occurs between UN and as-cast AFA. At 1023 K, an aluminum and nitrogen rich phase (likely AlN) formed along the interface of as-cast AFA and UN samples. At 823 K the AlN phase was not prominently observed due to the reduced diffusivity of aluminum through AFA. The aluminum and nitrogen-enriched phase was also observed in a high temperature pressure-assisted test sample of UN and as-cast AFA thermally treated at 1373 K. Finally, in UN samples doped with a low weight percent of UO 2 (< 3 wt%), AlN was not detected along the interface at either temperatures, and an Al 2 O 3 layer likely formed along the interface and prevented further chemical interaction between UN and as-cast AFA.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of friction stir weld performed on neutron-irradiated 304L steel with helium

As nuclear power plants (NPPs) approach or exceed 40–60 years of service, it may become necessary to repair damaged neutron-irradiated components to prolong longevity. However, fusion welding repair of irradiated steels and metallic materials is challenging because of helium-induced cracking. This study used friction stir welding (FSW) to address helium-related issues, such as helium bubble formation and grain boundary cracking. The microstructure, helium-induced degradation, and mechanical properties of a friction stir weld produced on neutron-irradiated 304L stainless steel with approximately 5.2 appm of helium were characterized. The analysis focused on variations in grain size, texture, and the morphology of helium-induced damage in the friction stir weld. Mechanical properties were characterized on the irradiated base metal (BM) and metallurgical zones of the friction stir weld: the stir zone (SZ), the thermo-mechanically affected zone (TMAZ), and the heat affected zone (HAZ). Only minor scattered porosity in the SZ and TMAZ and a few short microcracks (below 20 μm in length) in the TMAZ were observed, indicating limited helium-induced degradation. Tensile tests revealed good mechanical properties and fractography analysis demonstrated predominantly ductile fracture. In conclusion, the results highlight the immediate and substantial benefits of the FSW approach for repairing or joining helium-containing irradiated materials in NPPs.

36 MATERIALS SCIENCE↗

Influence of fabrication on microstructure and heat affected zone width in weldments of nuclear reactor pressure vessel steel

Advanced manufacturing routes such as electron beam welding and powder metallurgy with hot isostatic pressing are increasingly used across energy and aerospace industries, where the reliable prediction of weld behavior and heat affected zone (HAZ) evolution is critical. This study examines how fabrication routes and post-weld heat treatments influence phase distribution, crystallite size, microstrain, and dislocation density in nuclear reactor pressure vessel steels using synchrotron X-ray diffraction (SXRD). Retained austenite occurs only in samples that did not undergo austenitization, whereas an austenitizing heat treatment fully eliminates retained austenite and produces a more uniform microstructure across the weldment in terms of phase fraction, dislocation density, and microstrain. The Rosenthal solution underestimates the HAZ width for powder metallurgy samples. A newly proposed modified Rosenthal solution, reducing density by accounting for porosity, matches the SXRD-measured HAZ width with a 0.65% error. Structure–property correlations reveal that dislocation density correlates strongly with nanohardness in homogenous microstructures, while in heterogenous weldments nanohardness is further influenced by the presence of dissimilar phase boundaries. These findings provide new insight into the thermal and microstructural response of powder metallurgy fabricated steels and offer a framework for optimizing welding procedures and heat treatments in advanced manufacturing applications.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Microstructure-based prediction of thermal aging strength reduction factors for grade 91 ferritic-martensitic steel

This study aimed to develop a microstructure-based mechanistic approach to address the long-term thermal aging effect on yield stress and ultimate tensile strength and to provide a physical basis for developing thermal aging factors for G91 for a design life of 60 years. Several heats of G91 steel were examined. Controlled aging experiments were conducted on two heats at temperatures of 550, 600, and 650 °C for times up to ~64,000 h. Specimens were also taken from archived creep-tested specimens of G91 and from a tube removed from the Kingston coal-fired power plant to obtain data that cover a wide range of temperatures and for aging times up to 155,000 h. Thermal aging caused significant subgrain recovery, coarsening of M 23 C 6 carbides at subgrain boundaries and MX carbonitrides within subgrains. The intermetallic Laves phase forms during aging and grows rapidly. The growth rate of the subgrain width and MX mean size during thermal aging were described by kinetic models. Thermal aging results in the reductions in the yield stress and the ultimate tensile strength of G91. The effects of thermal aging on the reductions in yield stress and ultimate tensile strength were well described by the microstructure-strength model that considers three superimposed strengthening mechanisms, namely, sub-boundary strengthening, MX precipitation hardening, and Mo solid solution strengthening. Furthermore, the model was independently validated by the ASME Code values and is being used by the ASME to develop the aging-induced strength reduction factors for G91 steel for a design life of 60 years.

36 MATERIALS SCIENCE↗

Experimental evaluation of localized creep deformation in grade 91 steel weldments

Spatially resolved measurement of localized creep deformation in heterogeneous creep resistant steel weldments is crucial but challenging for lifetime assessments of critical steam components in power plants. Here, experimental approaches were established to quantitatively evaluate commonly observed localized creep deformation in multi-pass Grade 91 steel weldments. An in-situ digital image correlation (DIC) system was utilized with a creep testing frame to monitor and measure both full-field strain and localized strain accumulation across the weldments during long-term creep testing at elevated temperatures. The in situ DIC method measured not only the creep deformation behavior of the weld metal, heat affected zone (HAZ), and base metal, but also creep strain evolution for each sub-region within the HAZ itself, including coarse-grained HAZ, fine-grained HAZ (FGHAZ), and intercritical HAZ (ICHAZ). The DIC results revealed that local creep strain in the ICHAZ reached up to 90% strain before final rupture, whereas nominal creep strain measured by the standard extensometer of the tested cross-weld specimen was below 10%, indicative of Type IV cracking of the Grade 91 weld. Microstructural analyses revealed that the faster creep degradation/deformation in the HAZ was caused mainly by accelerated matrix grain recrystallization/growth and a reduced pinning effect from the segregated and coarsened precipitates in the FGHAZ and ICHAZ. The ultimate creep rupture occurred in the ICHAZ owing to its lowest creep resistance induced by the largest recrystallized grain size, the lowest fraction of coincidence site lattice, and the lowest local strain energies/dislocation densities.

36 MATERIALS SCIENCE↗

Degradation of a Cr-Mo steel by carbide precipitation over long-term service

Microstructure of the 40-year service-exposed 1Cr-0.5Mo steel extracted from pressure vessels through the boat sampling technique was characterized using x-ray diffraction, field-emission scanning electron microscopy, energy dispersive spectrometry, electron backscatter diffraction, focused ion beam, and transmission electron microscopy. The microstructure degradation during long-term service was identified. Statistical crystal plastic ity models were developed to correlate the microstructure and mechanical properties quantitatively. The steel is found significantly strengthened but slightly embrittled. Nanoscale Mo 2 C carbides have nucleated within the ferrite matrix over the long-term service, resulting in significant strengthening of the matrix. The coarser grain boundary Cr 23 C 6 carbides, on the other hand, act as the damage accumulation sites and lead to the degradation.

36 MATERIALS SCIENCE↗

In-situ measurement and control of the tool-workpiece interface temperature during friction stir processing of 304/304L stainless steel

Friction stir processing of 304/304L stainless steel is an area of interest for repair of spent nuclear fuel canisters. To enable repair without canister deflection or fracture, it is necessary to define the limitations for the depth of the processing zone which will be critically dependent on the thermal history of the material. Here, this work provides the first direct measurement of the interface temperature for friction stir processing of steel. The measured temperature is in the range of 850–1050 °C which is 20–30 % higher than previously reported values. Notably, the peak temperature occurs at the pin tip which is attributed to a higher sticking fraction and subsequently higher strain rate near the tool axis of rotation. Furthermore, a clear correlation between the temperature, grain size, and hardness is established within a single weld nugget and across different processing conditions. In the future, this data may lead to improved process modelling through direct validation and allow for property optimization through direct microstructure control.

304 stainless steel↗

Measurement of G-phase volume fraction and number density in duplex stainless steels using transmission electron microscopy

Duplex stainless steels (DSS) have a high toughness and strength due the presence of both austenitic and ferritic phases. These alloys have had limited use in power production applications due to thermal embrittlement caused by spinodal decomposition and development of G-phase precipitates in the ferrite. Lean grade DSS alloys (e.g., 2101, 2003) may offer improved thermal stability due to the reduction of Cr- and Ni-equivalent elements when compared to standard grade compositions (e.g., 2205, 2209). The abundance of the G-phase was measured in five duplex stainless steels, three wrought alloys (2101, 2003, 2205) and their matching filler metals (2101-w, 2209-w), after aging at 427 °C for 1000 h and 10,000 h. The G-phase volume fraction, number density, size, and precipitate spacing were found using quantitative analysis of transmission electron microscopy dark field images and the composition of G-phase precipitates on other clusters were characterized with atom probe tomography (APT). In the welded alloys, the G-phase was found to develop rapidly, relative to the wrought material. A positive correlation was found between the nickel equivalent composition of the alloy and the G-phase volume fraction. The alloys 2205, 2209, and 2101-w, which are higher in Cr and Ni, all showed significant G-phase precipitation, further strengthening the hypothesis that lean grade DSS alloys are more thermally stable against precipitation in the ferrite. Electron diffraction showed a secondary phase present in the 2101 wrought alloy at 10,000 h, but it was not crystallographically consistent with the G-phase; APT showed the presence of nanoclusters rich in both nickel and copper for this alloy. In conclusion, no secondary phases or clusters were found in 2003 after 10,000 h of aging, so it may be a candidate alloy for applications that require long-life times at high operating temperatures.

36 MATERIALS SCIENCE↗

Understanding the effect of friction stir processing on electrical steel: Microstructural changes and mechanical transformations

Raising Si beyond 3.5 wt% reduces core loss but embrittles electrical steels, constraining processing and application. Here we assess friction stir processing (FSP) as a solid‑state route to enable Fe–4.0 wt% Si with improved mechanical performance. Temperature‑controlled FSP with a PcBN tool produced a defect‑free processed zone. SEM/EBSD revealed dynamic recrystallization and grain refinement from an average 110 μm in the base material to ∼20 μm in the processed region, with ∼ 80% of grains < 40 μm and a reduction in high‑angle boundary fraction to ∼65% (vs >85% in the base). Comparative mechanical property analysis shows a moderate increase in yield strength in FSP samples relative to the base material, with a significant improvement in ductility (∼35–50%). Post‑fracture EBSD identified 60° twin boundaries in the base while sub-grain formation with elevated KAM in the FSP sample. Fractography revealed a shift from quasi‑cleavage in the Base-faceted planes with river patterns, steps, and occasional secondary cracks—to ductile micro void coalescence after FSP. Following FSP, the material retains soft‑magnetic behavior, with modest shifts in saturation magnetization consistent with grain refinement and stored strain, accompanied by a clear gain in formability. These results indicate that FSP provides a viable route to deploy higher‑Si electrical steels with concurrent gains in strength and ductility.

Electrical steel↗

Force reduction of friction stir welding and processing of steel

Friction stir welding and processing (FSW&P) is considered as a new fabrication method for canisters and repair of existing dry cask storage system canisters (generally made of austenitic stainless steel). Low heat input compared to fusion joining processes and grain refinement associated with low-temperature FSW&P result in a material with improved mechanical properties and equivalent generalized corrosion performance relative to the base metal. But FSW&P of austenitic stainless steel requires significant tool forge axis force to produce a weld (or a run). Exploratory runs utilizing forge axis force control were conducted to investigate the minimum force required to achieve defect-free runs. The correlation between forge axis force and resultant plunge depth was also investigated. Furthermore, detailed microstructural characterization was conducted to display the microstructural variation within the nugget zone.

36 MATERIALS SCIENCE↗

A critical review of irradiation-induced changes in reactor pressure vessel steels

A large body of work has been conducted to investigate the embrittlement and degradation of reactor pressure vessel (RPV) steels. This includes experiments on alloys with different compositions, performed in research and test reactors and ion accelerators that span various temperatures, fluxes, and fluences. In this paper, we perform a critical review of the published experimental data and compile experimentally reported values for dislocation loop size/density, precipitate size/density and yield stress into an easily downloadable format that can be used by both experimentalists and modelers. This thorough experimental review is complemented by a brief review of simulation efforts at atomistic and mesoscopic length scales. Finally, this paper highlights key aspects of the behavior of RPV steels under irradiation, identifies gaps or discrepancies in current understanding, and identifies priority future research directions.

36 MATERIALS SCIENCE↗

Electric current-induced precipitation hardening in advanced high-strength steel

Effect of electric current on precipitation hardening for advanced high-strength steel is investigated based on mechanical testing and microscopic observation. Complex-phase steel containing nano-sized Nb-bearing carbides was used. By comparing the flow stress between uniaxial tension with applied electric current (pulsed tension) and without electric current (nonpulsed tension) at various elevated temperatures, the influence of electric current on precipitation hardening was confirmed. A higher values of Vickers hardness and full-width-at-half-maximum were obtained in the pulsed tensile specimen compared to the identically heat treated specimen after the same deformation. Small angle neutron scattering analysis showed that the volume fraction and mean diameter of newly formed precipitates in the pulsed tensile specimen were higher and larger than those in the induction heat treated specimen, respectively. In conclusion, it clearly shows that additional precipitation hardening could be induced by the athermal effect of electric current, which is distinct from the thermal effect of Joule heating.

36 MATERIALS SCIENCE↗

Genesis of Nanogalvanic Corrosion Revealed in Pearlitic Steel

Nanoscale, localized corrosion underpins billions of dollars in damage and material costs each year; however, the processes responsible have remained elusive due to the complexity of studying degradative material behavior at nanoscale liquid–solid interfaces. Recent improvements to liquid cell scanning/transmission electron microscopy and associated techniques enable this first look at the nanogalvanic corrosion processes underlying this widespread damage. Nanogalvanic corrosion is observed to initiate at the near-surface ferrite/cementite phase interfaces that typify carbon steel. In minutes, the corrosion front delves deeper into the material, claiming a thin layer of ferrite around all exposed phase boundaries before progressing laterally, converting the ferrite to corrosion product normal to each buried cementite grain. Over the following few minutes, the corrosion product that lines each cementite grain undergoes a volumetric expansion, creating a lateral wedging force that mechanically ejects the cementite grains from their grooves and leaves behind percolation channels into the steel substructure.

36 MATERIALS SCIENCE↗

Microstructure and creep strength of simulated intercritical heat-affected zone of grade 91 steel

The intercritical heat affected zone (ICHAZ) has been reported as one of the most Type IV cracking susceptible regions in 9Cr creep-resistant steel weldments. However, creep degradation mechanisms within the ICHAZ itself need further clarifications. In this work, two ICHAZ specimens of Grade 91 steel, low-temperature ICHAZ (LT-ICHAZ) and high-temperature ICHAZ (HT-ICHAZ), were simulated using the Gleeble thermomechanical system by exposing to two peak temperatures (860 °C and 900 °C) between $A_{C1}$ and $A_{C3}$. Dramatically different creep strengths of two simulated ICHAZs were observed and studied. We report dilation curve analysis indicates a high fraction of newly transformed martensite formed in the HT-ICHAZ, which results in a much higher hardness (360 HV0.5) of the HT-ICHAZ than 266 HV0.5 of LT-ICHAZ. Precipitates, especially $M_{23}C_6$ carbides, were not fully dissolved in both ICHAZ specimens. After a typical postweld heat treatment (760 °C-2 hours), the faster recovery of low-carbon martensite and reduced precipitation strengthening due to $M_{23}C_6$ carbides coarsening in the HT-ICHAZ led to a significant hardness reduction. These microstructural degradations in the HT-ICHAZ made its creep lifetime about 36 times shorter than that of the LT-ICHAZ tested at 650 °C. The remaining tempered martensite from base metal in the LT-ICHAZ was the primary contributor to maintain its high creep resistance.

36 MATERIALS SCIENCE↗

Additive Manufacturing of Cryogenic Austenitic Steel JK2LB via Wire-Fed Directed Energy Deposition (DED) for Fusion Energy Applications

This study explores the feasibility of fabricating cryogenic austenitic steel JK2LB via both laser-based directed energy deposition (laser-DED) and arc-based directed energy deposition (arc-DED) additive manufacturing processes for potential application in fusion reactors. JK2LB, a low-nickel, high-manganese stainless steel developed for ITER, offers excellent cryogenic toughness, radiation resistance, and decay-to-clearance characteristics. Although JK2LB was originally designed to endure cyclic stresses at cryogenic temperatures in tokamaks, its low-temperature mechanical integrity and radiation tolerance also make it a promising candidate for structural components, such as the coil case/support structure in nonplanar high-temperature superconducting magnet assemblies in stellarators. Directed energy deposition (DED) additive manufacturing was selected for this study due to its capability to fabricate large structures with complex geometries. Here, to address the long lead time and high cost associated with acquiring conventional JK2LB solid wire, JK2LB powder-cored wire was developed as the feedstock material. Testing blocks were then fabricated using both wire-fed laser-DED and arc-DED processes. Microstructural and compositional analyses revealed that both DED approaches yield fully austenitic phase and columnar grain structures. Mechanical testing at room temperature revealed that both DED routes achieved yield strength and elongation comparable to those of conventionally processed JK2LB via vacuum melting, electroslag remelting, extrusion, and drawing, though ultimate tensile strength was reduced due to Mn loss and large columnar grains. As a study mainly focusing on the additive manufacturing process, this work demonstrates the potential of additive manufacturing for fusion energy applications and provides a basis for optimization and future cryogenic mechanical evaluation.

Cryogenic steel↗

Cascaded Sapphire Fiber Bragg Gratings Inscribed by Femtosecond Laser for Molten Steel Studies

This research reports a distributed fiber optic high-temperature sensing system tailored for applications in the steel industry and various other sectors. Recent advancements in optical sensor technology have led to the exploration of sapphire crystal fibers as a solution for sensing in harsh environments. Utilizing a femtosecond (fs) laser, cascaded fiber Bragg gratings (FBGs) were meticulously fabricated within a multimode sapphire optical fiber. These FBGs endowed the system with distributed sensing capabilities and underwent rigorous testing under extreme temperatures, reaching up to 1800 °C. Here, the study delves into the investigation of the FBG reflection spectrum, facilitated by the development of a sophisticated multimode demodulation system, which contributed to the attainment of precise temperature measurements with a performance accuracy of 99.9%. Demonstrating exceptional thermal stability, the sapphire FBGs endured temperatures of 1600 °C for a sustained duration of 22 h. Furthermore, this article explores the application of distributed temperature sensing employing multiple sapphire FBGs, showcasing their utility in temperature measurements related to molten steel studies.

47 OTHER INSTRUMENTATION↗

4D evolution of Cr 23 C 6 precipitates in neutron-irradiated and annealed HT-UPS steel observed via synchrotron micro-computed tomography

High-temperature-ultrafine precipitate strengthened (HT-UPS) steel is a potential structural material for advanced nuclear reactors; however, its irradiation response is not well understood. This research provides insight into irradiation-induced effects, such as precipitate evolution mechanisms and four-dimensional morphological evolution, in HT-UPS steel using synchrotron micro-computed tomography. Identical specimens were characterized pre-irradiation and post-irradiation following neutron exposure up to 0.3 displacements per atom at 600 °C. Irradiation effects were also differentiated from the annealing response of precipitates. Following neutron irradiation, the average Cr 23 C 6 precipitate size reduced, affected by the synergy of nucleation and growth, ballistic dissolution, and inverse coarsening, which was observed at fluences an order of magnitude lower than previously observed. Annealing at 600 °C for 32 h increased the average Cr 23 C 6 precipitate size and decreased the phase fraction, attributed to precipitate coarsening. The precipitate morphology evolution and resultant mechanisms can be utilized to parameterize and validate microstructural models simulating radiation damage or annealing.

36 MATERIALS SCIENCE↗