All-organic self-separating three-dimensionally nanoarchitected electrochemical energy storage devices

This work realizes a three-dimensionally (3D) nanoarchitected, all organic, "self-separating" lithium-ion electrochemical energy storage (EES) device that is cycled as a solid-state full cell. The device is enabled by a monolithic carbon anode with a co-continuous pore network, derived from the structure direction of resols by an ultra-large molar mass block copolymer (BCP), poly(styrene-block-2-dimethylaminoethyl methacrylate) (SA). Electropolymerization of a single-phase conductive and redox-active material, poly((2,3-dihydrothieno[3,4-b][1,4]dioxin-2-yl)methyl 9,10-dioxo-9,10-dihydroanthracene-2-carboxylate) (PAQEDOT), into the pore space provides the cathode of the cell. The device is electronically contacted to the relevant electrode network enabled by the co-continuous nature of each electrode. Electrochemical processing via cycling against external lithium in an electrolyte generates a solid electrolyte interphase (SEI) as a separator and lithiates the cell electrodes, after which the EES device is cycled in the solid state. While the full cell does not demonstrate high cyclability, the best full cell demonstrates a discharge capacity of 267 milliamp hours per gram (mAh/g). This work marks, to the best of knowledge of the authors, the first example of an all-organic materials derived 3D nanoarchitected EES device, as well as the first design of "self-separating" cell fabrication. Furthermore, generalization of the design to another co-continuous carbon form factor is demonstrated.

FOS: Physical sciences↗

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Solid polymer electrolytes based on plastic crystals are promising for solid-state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 -electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, in this study, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non-uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive-embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile-plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome-like Na 0 with thin, amorphous, and fluorine-rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

25 ENERGY STORAGE↗

Catalytic Electrolyte Additive for High-Loading and Lean Electrolyte Li–S Batteries

The cycle life of high-energy Li–S cells is largely constrained by the quick electrolyte depletion. LiNO 3 has been a well-established additive known for protecting the Li metal anode and stabilizing the battery from polysulfide “shuttling”. However, it can be depleted prematurely and can pose safety risks when exposed to carbon, sulfur, or Li metal under harsh conditions. Here, in this study, LiPO 2 F 2 was explored as a safe and durable alternative additive in ether-based electrolytes. LiPO 2 F 2 demonstrates superior performance in Li/S batteries, especially under high sulfur loading (∼4 mg/cm 2 ) and lean electrolyte conditions (E/S = 4), achieving a long-term cycling stability of 40%, compared to 14.7% with LiNO 3 . This additive facilitates the disproportionation of polysulfides, reducing their dissolution and mitigating the shuttle effect. Additionally, LiPO 2 F 2 promotes the formation of a stable solid-electrolyte interphase (SEI) composed of inorganic anion-derived species, improving the battery’s overall stability and functionality. These findings blaze a trail in the design of safer and more durable electrolytes for Li–S batteries.

Li-S batteries↗

Stable Potassium Metal Anodes with an All-Aluminum Current Collector through Improved Electrolyte Wetting

This is the first report of successful potassium metal battery anode cycling with an aluminum-based rather than copper-based current collector. Dendrite-free plating/stripping is achieved through improved electrolyte wetting, employing an aluminum-powder-coated aluminum foil “Al@Al,” without any modification of the support surface chemistry or electrolyte additives. The reservoir-free Al@Al half-cell is stable at 1000 cycles (1950 h) at 0.5 mA cm -2 , with 98.9% cycling Coulombic efficiency and 0.085 V overpotential. The pre-potassiated cell is stable through a wide current range, including 130 cycles (2600 min) at 3.0 mA cm -2 , with 0.178 V overpotential. Al@Al is fully wetted by a 4 m potassium bis(fluorosulfonyl)imide-dimethoxyethane electrolyte (θCA = 0°), producing a uniform solid electrolyte interphase (SEI) during the initial galvanostatic formation cycles. On planar aluminum foil with a nearly identical surface oxide, the electrolyte wets poorly (θCA = 52°). This correlates with coarse irregular SEI clumps at formation, 3D potassium islands with further SEI coarsening during plating/stripping, possibly dead potassium metal on stripped surfaces, and rapid failure. The electrochemical stability of Al@Al versus planar Al is not related to differences in potassiophilicity (nearly identical) as obtained from thermal wetting experiments. Additionally, planar Cu foils are also poorly electrolyte-wetted and become dendritic. The key fundamental takeaway is that the incomplete electrolyte wetting of collectors results in early onset of SEI instability and dendrites.

25 ENERGY STORAGE↗

A dynamically bare metal interface enables reversible magnesium electrodeposition at 50 mAh cm −2

Understanding and facilitating pure magnesium nucleation/growth electrodeposition behavior with ultrahigh Coulombic efficiency is complicated by the phenomenon of solid electrolyte interphase (SEI) formation in state-of-the-art, halogen-free magnesium electrolytes. Defining the electrolyte properties necessary to achieve ideal electrodeposition/stripping (E/S) thus remains elusive. Here, in this work, we reveal for the first time, rapid magnesium electrodeposition behavior that forms densely aligned, micron-sized thin platelets by establishing a dynamic bare magnesium/electrolyte interface during high-rate net plating. This effectively “SEI-free” interface allows facile magnesium diffusion and migration in stripping with near-unity E/S efficiency under demanding conditions over long-term cycling. The intrinsic electrolyte stability of the salt/solvent at the molecular level is the key to forming such an interface. The efficacy of the dynamic bare interface and an electrodeposited, free-standing magnesium anode is demonstrated in a high-areal-capacity full cell. These findings provide new design principles and fundamental understanding of interfacial chemistry in multivalent metal batteries.

Mg full cell↗

High Energy Aqueous Lithium-Ion Batteries (Final Report)

Lithium-ion batteries (LIBs) are a widely used energy storage device. For decades, researchers have been studying aqueous electrolytes due to their non-flammability and environmental friendless. However, the hydrogen evolution reaction (HER) and oxygen evolution reaction (OER) of water greatly limit the voltage window of the aqueous electrolyte. The recent concept of ‘solvent-in-salt’ electrolytes, namely ‘water-in-salt’ electrolytes (WISE) for aqueous batteries and ‘super-concentrated’ electrolytes for non-aqueous batteries, greatly expands the electrochemical window of these battery systems and consequently their energy density. This expansion occurs because the large number of salt aggregates in ‘solvent-in-salt’ electrolytes enables preferential salt decomposition over solvent decomposition to form robust interphase layers on electrodes, thus enhancing their stability in a wide range of operating voltages. However, even when the salt concentration reached 63m, regardless of cost, the cathodic potential of the WISE expanded only to 1.75V with an overall electrochemical stability window of <3.25V. To design the next generation of high energy aqueous LIBs, electrolytes that possess a wider electrochemical stability window and lower cost but still maintain the merit of non-flammability are much needed. In this project, we designed the aqueous LIBs with widened voltage window. We reported a cheap and non-flammable ternary eutectic electrolyte that can form a robust solid electrolyte interface (SEI)so that the cathodic limiting potential can be decreased to <1.5 V for Li 4 Ti 5 O 12 anodes, while maintaining both a high ionic conductivity of >10 -3 S cm –1 and a low viscosity. We demonstrated the super-stable2.5V LiMn 2 O 4 ||Li 4 Ti 5 O 12 pouch cell with mass loading of 2.5 mAh/cm. Further, LiCl-LiBr-Graphite/Li full cells were designed with high energy density. Finally, we use a bi-layer design to enlarge the voltage window of aqueous electrolyte, which can endow the stable cycling of aqueous Lithium metal batteries.

25 ENERGY STORAGE↗

Monofluorinated acetal electrolyte for high-performance lithium metal batteries

High degree of fluorination for ether electrolytes has resulted in improved cycling stability of lithium metal batteries due to stable solid electrolyte interphase (SEI) formation and good oxidative stability. However, the sluggish ion transport and environmental concerns of high fluorination degree drive the need to develop less fluorinated structures. Here, we depart from the traditional ether backbone and introduce bis(2-fluoroethoxy)methane (F2DEM), featuring monofluorination of the acetal backbone. High coulombic efficiency and stable long-term cycling in Li||Cu half cells can be achieved with F2DEM even under fast Li metal plating conditions. The performance of F2DEM is further compared with diethoxymethane (DEM) and 2-[2-(2,2-difluoroethoxy)ethoxy]-1,1,1-trifluoroethane (F5DEE). A significantly lower overpotential is observed with F2DEM, which improves energy efficiency and enables its application in high-rate conditions. Comparative studies of F2DEM with DEM and F5DEE in anode-free lithium iron phosphate (LiFePO4) LFP pouch cells and high-loading LFP coin cells further show improved capacity retention of F2DEM electrolyte, demonstrating its practical applicability. More importantly, we also extensively investigate the underlying mechanism for the superior performance of F2DEM through various techniques, including X-ray photoelectron spectroscopy, scanning electron microscopy, cryogenic electron microscopy, focused ion beam, electrochemical impedance spectroscopy, and titration gas chromatography. Overall, F2DEM facilitates improved Li deposition morphology with reduced amount of dead Li. This enables F2DEM to show superior performance, especially under higher charging and slower discharging rate conditions.

25 ENERGY STORAGE↗

Compositions and Formation Mechanisms of Solid-Electrolyte Interphase on Microporous Carbon/Sulfur Cathodes

We report the formation mechanism and compositions of a solid-electrolyte interphase (SEI) on a microporous carbon/sulfur (MC/S) cathode in Li–S batteries using a carbonate-based electrolyte (1 M LiPF 6 in ethylene carbonate (EC)/dimethyl carbonate, v:v = 1:1). Through characterizations using 1D and 2D solution-phase nuclear magnetic resonance spectroscopy, coupled with model chemical reactions and DFT calculations, we have identified two critical roles of Li + in steering the SEI formation. First, the preferential solvation of Li + by EC in the mixed carbonate electrolyte renders EC as the dominant participant in the SEI formation, and second, Li + coordination to the EC carbonyl alters activation barriers and changes the reaction pathways relative to Na + . The main organic components in the SEI are identified as lithium ethylene monocarbonate and lithium methyl carbonate, which are virtually identical to those formed on Li and graphite anodes of lithium-ion batteries but via a different pathway.

25 ENERGY STORAGE↗

On the crystallography and reversibility of lithium electrodeposits at ultrahigh capacity

Abstract Lithium metal is a promising anode for energy-dense batteries but is hindered by poor reversibility caused by continuous chemical and electrochemical degradation. Here we find that by increasing the Li plating capacity to high values ( e.g ., 10–50 mAh cm −2 ), Li deposits undergo a morphological transition to produce dense structures, composed of large grains with dominantly (110) Li crystallographic facets. The resultant Li metal electrodes manifest fast kinetics for lithium stripping/plating processes with higher exchange current density, but simultaneously exhibit elevated electrochemical stability towards the electrolyte. Detailed analysis of these findings reveal that parasitic electrochemical reactions are the major reason for poor Li reversibility, and that the degradation rate from parasitic electroreduction of electrolyte components is about an order of magnitude faster than from chemical reactions. The high-capacity Li electrodes provide a straightforward strategy for interrogating the solid electrolyte interphase (SEI) on Li —with unprecedented, high signal to noise. We find that an inorganic rich SEI is formed and is primarily concentrated around the edges of lithium particles. Our findings provide straightforward, but powerful approaches for enhancing the reversibility of Li and for fundamental studies of the interphases formed in liquid and solid-state electrolytes using readily accessible analytical tools.

59 BASIC BIOLOGICAL SCIENCES↗

Electrolyte design for Li-ion batteries under extreme operating conditions

The ideal electrolyte for the widely used LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)||graphite lithium-ion batteries is expected to have the capability of supporting higher voltages (≥4.5 volts), fast charging (≤15 minutes), charging/discharging over a wide temperature range (±60 degrees Celsius) without lithium plating, and non-flammability. No existing electrolyte simultaneously meets all these requirements and electrolyte design is hindered by the absence of an effective guiding principle that addresses the relationships between battery performance, solvation structure and solid-electrolyte-interphase chemistry. Here we report and validate an electrolyte design strategy based on a group of soft solvents that strikes a balance between weak Li+-solvent interactions, sufficient salt dissociation and desired electrochemistry to fulfil all the aforementioned requirements. Remarkably, the 4.5-volt NMC811||graphite coin cells with areal capacities of more than 2.5 milliampere hours per square centimetre retain 75 per cent (54 per cent) of their room-temperature capacity when these cells are charged and discharged at -50 degrees Celsius (-60 degrees Celsius) at a C rate of 0.1C, and the NMC811||graphite pouch cells with lean electrolyte (2.5 grams per ampere hour) achieve stable cycling with an average Coulombic efficiency of more than 99.9 per cent at -30 degrees Celsius. The comprehensive analysis further reveals an impedance matching between the NMC811 cathode and the graphite anode owing to the formation of similar lithium-fluoride-rich interphases, thus effectively avoiding lithium plating at low temperatures. Additionally, this electrolyte design principle can be extended to other alkali-metal-ion batteries operating under extreme conditions.

25 ENERGY STORAGE↗

Effect of temperature on capacity fade in silicon-rich anodes

Coin half-cells containing 80 wt% silicon electrodes are assembled and cycled at the similar to C/10 rate in the temperature range of 25-55 degrees C. To the best of our knowledge, this is the first time that the effect of temperature is reported for such high-silicon-containing cells. Two different electrolytes are used in this study, a baseline electrolyte and the baseline electrolyte +10 wt% fluoroethylene carbonate (FEC). Analysis of the capacity vs. cycle count data by curve fitting reveals that the addition of FEC markedly affects the capacity loss mechanism. Without FEC, the kinetic rate law for the capacity loss mechanism can be described as the sum of two logistic growth models. With the addition of FEC, the rate law depends on ln(t). Clearly, the addition of FEC has a profound effect on the mechanism of capacity loss. Interestingly, X-ray photoelectron spectroscopy (XPS) shows that the composition of the solid electrolyte interphase (SEI) layer changes markedly from mostly organic to mostly inorganic in the presence of FEC and how it varies at the different temperatures tested, especially in the absence of FEC.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Nonsacrificial Additive for Tuning the Cathode–Electrolyte Interphase of Lithium-Ion Batteries

Solid–electrolyte interphases is essential for stable cycling of rechargeable batteries. The traditional approach for interphase design follows the decomposition of additives prior to the host electrolyte, which, as governed by the thermodynamic rule, however, inherently limits the viable additives. Here we report an alternative approach of using a nonsacrificial additive. This is exemplified by the localized high-concentration electrolytes, where the fluoroethylene carbonate (FEC) plays a nonsacrificial role for modifying the chemistry, structure, and formation mechanism of the cathode–electrolyte interphase (CEI) layers toward enhanced cycling stability. On the basis of ab initio molecular dynamics simulations, we further reveal that the unexpected activation of the otherwise inert species in the interphase formation is due to the FEC–Li + coordinated environment that altered the electronic states of reactants. In conclusion, the nonsacrificial additive on CEI formation opens up alternative avenues for the interphase design through the use of the commonly overlooked, anodically stable compounds.

25 ENERGY STORAGE↗

Enhanced cycling stability of Ni-rich Li-metal cells enabled by dual vinylene carbonate and tris(trimethylsilyl)borate electrolyte additives

NMC811 (LiNi 0.8 Co 0.1 Mn 0.1 O 2 ) and other high-Ni chemistries are promising cathode candidates for high-performance electric vehicles, owing to their high energy density and reduced cobalt content. However, their long-term cycling stability is hindered by surface degradation, particularly when paired with conventional electrolytes and a lithium metal anode. Electrolyte additives represent a practical approach to enhance interfacial stability and improve overall battery performance by promoting the formation of a robust electrolyte–electrode interphase (EEI). In this study, we revisit the effects of vinylene carbonate (VC) and tris(trimethylsilyl)borate (TMSB) additives on single-crystal SC-NMC811||Li cells. While TMSB only increases the open-circuit voltage and initial overpotential, it delivers superior capacity retention at C/3 compared to cells containing only VC or a dual additive system (VC and TMSB). Notably, under fast-charging conditions (1C, 2C, and 5C), the dual-additive system significantly outperforms other formulations, achieving markedly enhanced long-term capacity retention. Comprehensive electrochemical and spectroscopic analyses reveal that the VC/TMSB dual-additive system suppresses surface transition in NMC811, mitigates structural degradation by forming a thin, LiF-deficient cathode-electrolyte interface (CEI) layer. Moreover, they promote smooth and dense Li deposition and generate a LiF-deficient solid-electrolyte interphase (SEI). Consequently, the synergistic stabilization of both the CEI and SEI effectively limits the overall cell impedance growth during extended cycling. These findings provide key insights into co-additive strategies for engineering stable interfaces in high-energy Ni-rich Li-metal batteries.

36 MATERIALS SCIENCE↗

Lithium oxidation and electrolyte decomposition at Li-metal/liquid electrolyte interfaces

In this work, we examine the evolution of events occurring when a Li metal surface is in contact with a 2 M solution of a Li salt in a solvent or mixture of solvents, via classical molecular dynamics simulations with a reactive force field allowing bond breaking and bond forming. The main events include Li oxidation and electrolyte reduction along with expansion of the Li surface layers forming a porous phase that is the basis for the formation of the solid-electrolyte interphase (SEI) components. Nucleation of the main SEI components (LiF, Li oxides, and some organics) is characterized. The analysis clearly reveals the details of these physical–chemical events as a function of time, during 20 nanoseconds. The effects of the chemistry of the electrolyte on Li oxidation and dissolution in the liquid electrolyte, and SEI nucleation and structure are identified by testing two salts: LiPF 6 and LiCF 3 SO 3 , and various solvents including ethers and carbonates and mixtures of them. The kinetics and thermodynamics of Li 6 F, the core nuclei in the LiF crystal, are studied by analysis of the MD trajectories, and via density functional theory calculations respectively. The SEI formed in this computational experiment is the “native” film that would form upon contact of the Li foil with the liquid electrolyte. As such, this work is the first in a series of computational experiments that will help elucidate the intricate interphase layer formed during battery cycling using metal anodes.

25 ENERGY STORAGE↗

Continuum-Level Modeling of Li-Ion Battery SEI by Upscaling Atomistically Informed Reaction Mechanisms

Understanding and controlling solid-electrolyte interphase (SEI) formation to stabilize cell performance is a significant challenge for next-generation Li-ion battery technologies. In recent years, computational modeling has become an essential tool in providing fundamental insights into SEI properties and dynamics. However, neither atomistic nor continuum-level approaches alone can capture the complexities of SEI chemistry across all relevant length and time scales. In this work, a continuum-level model is developed that is informed by reaction mechanisms obtained from first-principle calculations. The atomistically informed continuum-level model is used to understand electrolyte degradation, including the decomposition of ethylene carbonate (EC), ethyl methyl carbonate (EMC), and fluoroethylene carbonate (FEC). The model presented here is the most chemically complex continuum-level SEI model in the literature to date. The SEI model is calibrated against experimental irreversible leakage currents and shows qualitative agreement with expected SEI growth trends. The model framework is expected to accelerate fundamental understanding of SEI formation, facilitate mechanism development feedback, and dynamically interact with experimental insights.

continuum-level model↗

Multiscale Electrochemomechanics Interaction and Degradation Analytics of Sn Electrodes for Sodium-Ion Batteries

Sodium-ion batteries have emerged as a strong contender among the beyond lithium-ion chemistries due to elemental abundance and the low cost of sodium. Tin (Sn) is a promising alloying electrode with high capacity, redox reversibility, and earth abundance. Tin electrodes, however, undergo a series of intermediate reactions exhibiting multiple voltage plateaus upon sodiation/desodiation. Phase transformations related to incomplete sodiation in tin during cycling, in the presence of a frail solid electrolyte interphase layer, can quickly weaken the structural stability. The structural dynamics and reactivity of the electrode/electrolyte interface, being further dependent on the size and morphology of the active material particle in the presence of different electrolytes, dictate the electrode degradation and survivability during cycling. Here, we paint a comprehensive picture of the underpinnings of the electrochemical and mechanics coupling and electrode/electrolyte interfacial interactions in alloying Sn electrodes. We elicit the fundamental role of electrode/electrolyte complexations in the Sn electrode structure-property-performance relationship based on multimodal analytics, including electrochemical, microscopy, and tomography analyses.

25 ENERGY STORAGE↗

Understanding and controlling lithium morphology in solid polymer and gel polymer systems: mechanisms, strategies, and gaps

Lithium metal anode promises the highest theoretical energy density and may enable high energy designs such as lithium–sulfur and lithium–air batteries. However, stable lithium plating and stripping remains a challenge in all electrolyte systems including liquids, polymers, and ceramic electrolytes. In this perspective, we examine literature studies of lithium morphologies in solid polymer and gel polymer systems and compare that with well-studied liquid electrolytes. In solid polymer electrolytes, current density and mechanical properties are both governing parameters for lithium morphology, differing from conventional liquid electrolytes. Stable lithium electrodeposition may be accomplished by a polymer electrolyte with good stiffness operating at significantly lower current densities than its limiting current density, which is defined by the Sand equation. In gel polymer electrolytes, the reported lithium morphology is more similar to that in liquid electrolytes, suggesting similar nucleation and growth mechanisms. Based on experimental evidence and theoretical guidance, current strategies to control lithium morphology in solid polymer and gel polymer electrolytes are summarized. The limitations of these strategies are discussed. In particular, we note the knowledge gap in understanding the solid electrolyte interphase in solid polymer systems and the critical role it can play in regulating lithium morphologies.

36 MATERIALS SCIENCE↗

Investigation of SiO x anode fading mechanism with limited capacity cycling

Silicon suboxide (SiO x ) is one of the promising anode materials for the next-generation lithium-ion batteries. However, SiO x has a severe capacity fading problem during cycling. It is thus desired to investigate the detailed fading mechanisms of SiO x anode materials. In this study, limited capacity cycling was employed to examine the electrochemical behaviors of the SiO x anode, and the lithiation/delithiation cycling was limited within a range of 10% theoretical capacity. This strategy minimizes the volume variation of SiO x materials upon charging/discharging, which helps to reveal their decay factors other than volume fluctuation. It is demonstrated that the instability of the SiO x surface during cycling was likely a parallel factor of active material fading, which seems to cause unfavored electrode interface rearrangements with lowered electric conductivity.

electric vehicles↗