Search NASA⌕ Search

SEARCH · Search NASA

Results for “ceramic processing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Ink-based laser powder bed fusion of barium titanate

Barium titanate (BTO) is a lead-free functional ceramic that is widely used in sensors, transducers, and actuators. The increasing demand for complex geometries and quick design iterations motivates the use of additive manufacturing techniques. Laser powder bed fusion (L-PBF) additive manufacturing technique enables the net-shape or near-net-shape fabrication of metals and alloys. Ceramic L-PBF remains challenging due to their high melting temperature. Here, to address this challenge, a nanoparticle ink feedstock was incorporated into the L-PBF process to allow low power melting of BTO. Key print parameters (i.e. laser power, scanning speed, and hatching spacing) were optimized to fabricate millimeter-scale BTO parts. The printed BTO samples possessed an inhomogeneous equiaxed-columnar-cellular microstructure. Semiconducting current-voltage behavior was observed in as-printed samples, which was attributed to the creation of oxygen vacancies. The piezoelectric d 33 coefficient was measured to be 4.6 pC/N.

Dielectrics↗

Dielectric and ferroelectric analysis of nanoparticle/nanocrystalline barium titanate and PLZT.

Attractive for numerous technological applications, ferroelectronic oxides constitute an important class of multifunctional compounds. Intense experimental efforts have been made recently in synthesizing, processing and understanding ferroelectric nanostructures. This work will present the systematic characterization and optimization of barium titanate and lead lanthanum zirconate titanate nanoparticle based ceramics. The nanoparticles have been synthesized using several solution and pH-based synthesis processing routes and employed to fabricate polycrystalline ceramic and nanocomposite based components. The dielectric and ferroelectric properties of these various components have been gauged by impedance analysis and electromechanical response and will be discussed.

36 MATERIALS SCIENCE↗

Investigation of the additive induced doping effects in gelcast soft lead zirconate titanate ceramics

Due to the high sensitivity of the electrical properties of electronic ceramics to various factors, knowledge about the possible influence of the processing procedure on their electrical performance is critical for applying a new technique to the fabrication of the materials. In this study, various electrical parameters, complex impedance spectra, ferroelectric hysteresis loops, and microstructures of soft lead zirconate titanate (PZT) ceramics formed by the gelcasting technique from suspensions with various dispersants were investigated in comparison with those of the conventional dry pressed ones. We found that the sodium ion, which is the main cation in many commercial surfactants, exhibited obvious hard doping effects; thus causing deteriorated performance of the gelcast PZT ceramics. While a certain impurity ion introduced by a dispersant was also found to induce soft doping characteristics and improve the electrical performance of the materials. The results suggest that the doping effects of the metal ions or impurities introduced by the dispersants, or other additives, should be generally considered for applying a wet processing technique to forming multicomponent electronic ceramics.

36 MATERIALS SCIENCE↗

Tailorable Micelle Morphology in Self-Assembling Block Copolymer Gels for Templating Nanoporous Ceramics

The self-assembly of block copolymers offers opportunities for the facile organization and templating of inorganic nanomaterials. Here, we describe a morphology map for a poly(methyl methacrylate)-b-poly(n-butyl acrylate)-b-poly(methyl methacrylate) (PMMA-b-PnBA-b-PMMA) block copolymer/polycarbosilane system that allows for tunable control over nanoscale micelle geometry via manipulation of the preceramic polymer content. We produced gels with spherical, wormlike, and bicontinuous morphologies, which were processed to create silicon carbide-based ceramic structures with tunable nanoscale porosities. The role of the constituent polymers in influencing the structure and rheology of this system is discussed. The PMMA-b-PnBA-b-PMMA block copolymer/preceramic polymer system offers a number of advantages including: (i) commercial availability, (ii) rapid self-assembly kinetics, and (iii) successful conversion of the self-assembled nanostructure to ceramic via pyrolysis. Finally, this system may be useful for catalytic, structural, or thermal applications in both industrial and academic settings because of its ease of use and relatively inexpensive reagents.

36 MATERIALS SCIENCE↗

Synthesis of monodisperse CeO 2 -ZrO 2 particles exhibiting cyclic superelasticity over hundreds of cycles

Nano- and microscale CeO 2 –ZrO 2 (CZ) shape memory ceramics are promising materials for smart micro-electro-mechanical systems (MEMS), sensing, actuation and energy damping applications, but the processing science for scalable production of such small volume ceramics has not yet been established. Herein, we report a modified sol-gel method to synthesize highly monodisperse spherical CZ particles with diameters in the range of ~0.8-3.0 μm. Synchrotron X-ray micro-diffraction (μSXRD) confirmed that most of the particles are single crystal after annealing at 1450°C. Having a monocrystalline structure and a small specimen length scale, the particles exhibit significantly enhanced shape memory and superelasticity properties with up to ~4.7% compression being completely recoverable. Highly reproducible superelasticity through over five hundred strain cycles, with dissipated energy up to ~40 MJ/m 3 per cycle, is achieved in the CZ particles containing 16 mol% ceria. This cycling capability is enhanced by ten times compared with our first demonstration using micropillars (only 50 cycles in Lai et al, Science, 2013, 341, 1505). Furthermore, the effects of cycling and testing temperature (in 25°C-400°C) on superelasticity have been investigated.

36 MATERIALS SCIENCE↗

A new Bi{sub 0.5}Na{sub 0.5}TiO{sub 3} based lead-free piezoelectric system with calculated end-member Bi(Zn{sub 0.5}Hf{sub 0.5})O{sub 3}

The phase structure, dielectric and piezoelectric properties of a new lead-free piezoelectric system (1 − x)Bi{sub 0.5}Na{sub 0.5}TiO{sub 3}–xBi(Zn{sub 0.5}Hf{sub 0.5})O{sub 3} [(1 − x)BNT–xBZH, x = 0, 0.01, 0.02, 0.03, and 0.04] were investigated. The structure of Bi(Zn{sub 0.5}Hf{sub 0.5})O{sub 3} was calculated using first-principles method and (1 − x)BNT–xBZH ceramics were fabricated by conventional solid-state process. At room temperature, a morphotropic phase boundary (MPB) from rhombohedral to pseudocubic is identified near x = 0.02 by the analysis of X-ray diffraction patterns. The ceramics with MPB near room temperature exhibit excellent electrical properties: the Curie temperature, maximum polarization, remnant polarization, and coercive field are 340 °C, 56.3 μC/cm{sup 2}, 43.5 μC/cm{sup 2}, and 5.4 kV/mm, respectively, while the maximum positive bipolar strain and piezoelectric coefficient are 0.09% and 92 pC/N, respectively. In addition, a linear relationship between the MPB phase boundary composition and the calculated tetragonality of non-BNT end-member was demonstrated. Thus, this study not only shows a new BNT-based lead-free piezoelectric system but also suggest a new way to predict the composition at MPB a priori when designing new lead-free piezoelectric system.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Hot-Isostatic Pressing of Sellafield SIXEP Sand/Clinoptilolite Wastes - 18281

Clinoptilolite is an ion-exchange material currently in use at the SIXEP plant (Sellafield, UK) to remove radioactive Cs and Sr from aqueous solution. Clinoptilolite material exists in a granular form that requires consolidation prior to disposal in a Geological Disposal Facility (GDF). The existing baseline treatment technology is to produce cementitious waste packages, which is not ideal due to the large increase in waste volume and poor quality of the wasteform produced. Hot-Isostatic Pressing (HIPing) has been investigated as an alternative treatment method to immobilise this material. This paper presents the results of an investigation that illustrates the capability to process clinoptilolite into a durable, monolithic glass-ceramic wasteform, which should be considered suitable for GDF disposal. The product of HIPing SIXEP sand /clinoptilolite materials is a dense vitreous wasteform with a small quantity of crystalline inclusions, primarily in the form of quartz/cristobalite. Under PCT testing the wasteform produced was shown to be at least an order of magnitude more durable than glasses currently used for the immobilisation of High-Level Wastes (HLW). It was calculated that the treatment of SIXEP sand/clinoptilolite wastes using HIP technology will provide at least a 6.3-fold reduction in the number of waste packages which require management and disposal. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Waste Management Approach for a Potential Future U.S. Closed Fuel Cycle - 16233

The U.S. Department of Energy, Office of Nuclear Energy has chartered an effort to develop technologies to enable safe and cost effective recycle of commercial used nuclear fuel (UNF) in the U.S. Part of this effort includes the evaluation of exiting waste management technologies for effective treatment of wastes in the context of current U.S. regulations and development of waste forms and processes with significant cost and/or performance benefits over those existing. This study summarizes the results of these ongoing efforts with a focus on the highly radioactive primary waste streams. The primary streams considered and the recommended waste forms include: - Tritium separated from either a low volume gas stream or a high volume water stream. The recommended waste form is low-water cement in high integrity containers. - Iodine-129 separated from off-gas streams in aqueous processing. There are a range of potentially suitable waste forms. As a reference case, a glass composite material (GCM) formed by the encapsulation of the silver Mordenite (AgZ) getter material in a low-temperature glass is assumed. A number of alternatives with distinct advantages are also considered including a fused silica waste form with encapsulated nano-sized AgI crystals. - Carbon-14 separated from LWR fuel treatment off-gases and immobilized as a CaCO{sub 3} in a cement waste form. - Krypton-85 separated from LWR and SFR fuel treatment off-gases and stored as a compressed gas. - An aqueous reprocessing high-level waste (HLW) raffinate waste which is immobilized by the vitrification process in one of three forms: a single phase borosilicate glass, a borosilicate based glass ceramic, or a multi-phased titanate ceramic [e.g., synthetic rock (Synroc)]. - An undissolved solids (UDS) fraction from aqueous reprocessing of LWR fuel that is either included in the borosilicate HLW glass or is immobilized in the form of a metal alloy in the case of glass ceramics or titanate ceramics. - Zirconium-based LWR fuel cladding hulls and stainless steel (SS) fuel assembly hardware that are washed and super-compacted for disposal or as an alternative Zr purification and reuse (or disposal as low-level waste, LLW) by reactive gas separations. - Electrochemical process salt HLW which is immobilized in a glass bonded Sodalite waste form known as the ceramic waste form (CWF). - Electrochemical process UDS and SS cladding hulls which are melted into an iron based alloy waste form. Mass and volume estimates for each of the recommended waste forms based on the source terms from a representative flowsheet are reported. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Dielectric and nonlinear electrical behaviors of La-doped CaCu{sub 3}Ti{sub 4}O{sub 12} ceramics

We prepared La doped of CaCu{sub 3}Ti{sub 4}O{sub 12} ceramics by a solid-state sintering process and observed nonlinear electrical varistor and high dielectric behaviors. Phase composition analyses show that the La can substitute on the Ca sites completely, and have no influence on the phase composition. The impedance spectroscopy at room temperature indicates that the La doping can maintain the dielectric permittivity of CaCu{sub 3}Ti{sub 4}O{sub 12} (approx10{sup 4}). The relationships between electrical current density versus applied electrical field show that these ceramic samples exhibit nonlinear varistor characteristics, which should be ascribed to the existing potential barrier height at the grain boundary.

36 MATERIALS SCIENCE↗

The effects of composition and sintering temperature on the silica foam fabricated by slurry method

Reticulated ceramic or open pore ceramic foam is a well-known material which exhibits extremely high porosities, with a significant degree of interconnectivity that makes them desirable in a wide range of applications. There were broad types of ceramic foam fabrication method such as polymeric sponge method, direct foaming, and starch consolidation. In this study, the slurry method has been chosen to fabricate Silica (SiO{sub 2}) foam. In this process, Polyurethane (PU) foam template was dipped into ceramic slurry and followed by drying and sintering to obtain foam which contains porosity in the range of 50% to 70%. The compositions of SiO{sub 2} were varied starting from 55 wt.%, 60 wt.%, 65 wt.% and 70 wt.%. The samples of SiO{sub 2} that have been dipped and dried were sintered at 900°C, 1000°C, 1100°C, and 1250°C. The sintered SiO{sub 2} ceramic foam samples were characterized to observe their morphology, and physical properties. Thus, the microstructure of the SiO{sub 2} ceramic foams samples was examined by Scanning Electron Microscopy (SEM), and Electron Dispersive Spectroscopy (EDS). Meanwhile, the physical properties of the SiO{sub 2} ceramic foam samples such as the total porosity (%) and bulk density were determined using Archimedes method. It was found that the density of ceramic foam produced was in the range of 0.25 g/cm{sup 3} up to 0.75 g/cm{sup 3}, whereas the level of porosity percentage was in the range of 61.81% to 82.18% with the size of open pore or window cells were in between 141 µm up to 626 µm.

36 MATERIALS SCIENCE↗

Development of ITM Oxygen Technology for Low-cost and Low-emission Gasification and Other Industrial Applications

Air Products carried out a scope of work under DOE Award No. DE-FE0012065 “Development of ITM Oxygen Technology for Low-cost and Low-emission Gasification and Other Industrial Applications” with subcontractors Ceramatec, Penn State, and WorleyParsons. The scope of work under this award was aimed at furthering the development of the Ion Transport Membrane (ITM) Oxygen production process toward a demonstration-scale facility known as the Oxygen Development Facility (ODF). Specific activities will help to enable design and construction of the ODF through advancement of a number of challenging technical elements that are required to manage risk in the initial deployment of ITM technology. Major objectives of the work included developing ITM Oxygen ceramic membrane materials with improved performance and reliability, optimizing ceramic module geometry and fabrication methods, testing module performance, trialing the improved fabrication process at commercial scale in the Ceramic Membrane Module Fabrication Facility (CerFab), and advancing engineering development of the ITM oxygen production process, including vessel design and contaminant control measures to prepare for deployment of the ODF. The comprehensive report that follows details the team’s work, which includes several notable accomplishments: 1) compressive creep, a likely limiter of ceramic module lifetime in service, was demonstrated to be retarded by an order of magnitude by changes in material formulation, module joining dimensions, and internal wafer geometry; 2) two promising new materials were shown to be superior to the incumbent ITM material in a key material parameter related to oxygen flux; 3) module degradation mechanisms were identified following operation in large pilot-scale equipment; 4) options for utilizing ITM in a coal-to-liquids (CTL) facility to enable liquids production with carbon capture were identified and studied; and 5) the benefits of potential improvements to the technology were assessed for their cost impact on ITM Oxygen applications to clean power, fuels, and other applications.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Development of ITM Oxygen Technology for Low-cost and Low-emission Gasification and Other Industrial Applications

Air Products carried out a scope of work under DOE Award No. DE-FE0012065 “Development of ITM Oxygen Technology for Low-cost and Low-emission Gasification and Other Industrial Applications” with subcontractors Ceramatec, Penn State, and WorleyParsons. The scope of work under this award was aimed at furthering the development of the Ion Transport Membrane (ITM) Oxygen production process toward a demonstration-scale facility known as the Oxygen Development Facility (ODF). Specific activities will help to enable design and construction of the ODF through advancement of a number of challenging technical elements that are required to manage risk in the initial deployment of ITM technology. Major objectives of the work included developing ITM Oxygen ceramic membrane materials with improved performance and reliability, optimizing ceramic module geometry and fabrication methods, testing module performance, trialing the improved fabrication process at commercial scale in the Ceramic Membrane Module Fabrication Facility (CerFab), and advancing engineering development of the ITM oxygen production process, including vessel design and contaminant control measures to prepare for deployment of the ODF. The comprehensive report that follows details the team’s work, which includes several notable accomplishments: 1) compressive creep, a likely limiter of ceramic module lifetime in service, was demonstrated to be retarded by an order of magnitude by changes in material formulation, module joining dimensions, and internal wafer geometry; 2) two promising new materials were shown to be superior to the incumbent ITM material in a key material parameter related to oxygen flux; 3) module degradation mechanisms were identified following operation in large pilot-scale equipment; 4) options for utilizing ITM in a coal-to-liquids (CTL) facility to enable liquids production with carbon capture were identified and studied; and 5) the benefits of potential improvements to the technology were assessed for their cost impact on ITM Oxygen applications to clean power, fuels, and other applications.

42 ENGINEERING↗

Structure and Hardness of Ceramics Produced through High-Temperature Nitridation of Titanium Foil

We have studied the variation in the phase composition, elemental composition, and microstructure of rolled titanium samples during thermal annealing in a nitrogen atmosphere at 1300, 1500, 1700, and 2000°C. The results demonstrate that the nitridation process can yield compact titanium nitride-based ceramics or TiN/TiN{sub x}/α-Ti〈N〉 heterostructures. X-ray diffraction data for the near-surface region of the samples before and after nitridation and those for cross-sectional fracture surfaces of heterostructures are used to infer orientation relationships between the TiN phase and α-Ti〈N〉 solid solution. Scanning electron microscopy results for cross-sectional fracture surfaces indicate that complete nitridation of the samples leads to the formation of a three-layer microstructure.

36 MATERIALS SCIENCE↗

Waste Management Approach for a Potential Future U.S. Closed Fuel Cycle - 16233

The U.S. Department of Energy, Office of Nuclear Energy has chartered an effort to develop technologies to enable safe and cost effective recycle of commercial used nuclear fuel (UNF) in the U.S. Part of this effort includes the evaluation of exiting waste management technologies for effective treatment of wastes in the context of current U.S. regulations and development of waste forms and processes with significant cost and/or performance benefits over those existing. This study summarizes the results of these ongoing efforts with a focus on the highly radioactive primary waste streams. The primary streams considered and the recommended waste forms include: •Tritium separated from either a low volume gas stream or a high volume water stream. The recommended waste form is low-water cement in high integrity containers. •Iodine-129 separated from off-gas streams in aqueous processing. There are a range of potentially suitable waste forms. As a reference case, a glass composite material (GCM) formed by the encapsulation of the silver Mordenite (AgZ) getter material in a low-temperature glass is assumed. A number of alternatives with distinct advantages are also considered including a fused silica waste form with encapsulated nano-sized AgI crystals. •Carbon-14 separated from LWR fuel treatment off-gases and immobilized as a CaCO3 in a cement waste form. •Krypton-85 separated from LWR and SFR fuel treatment off-gases and stored as a compressed gas. •An aqueous reprocessing high-level waste (HLW) raffinate waste which is immobilized by the vitrification process in one of three forms: a single phase borosilicate glass, a borosilicate based glass ceramic, or a multi-phased titanate ceramic [e.g., synthetic rock (Synroc)]. •An undissolved solids (UDS) fraction from aqueous reprocessing of LWR fuel that is either included in the borosilicate HLW glass or is immobilized in the form of a metal alloy in the case of glass ceramics or titanate ceramics. •Zirconium-based LWR fuel cladding hulls and stainless steel (SS) fuel assembly hardware that are washed and super-compacted for disposal or as an alternative Zr purification and reuse (or disposal as low-level waste, LLW) by reactive gas separations. •Electrochemical process salt HLW which is immobilized in a glass bonded Sodalite waste form known as the ceramic waste form (CWF). •Electrochemical process UDS and SS cladding hulls which are melted into an iron based alloy waste form. Mass and volume estimates for each of the recommended waste forms based on the source terms from a representative flowsheet are reported.

Fuel Cycle↗

Design Methods, Tools, and Data for Ceramic Solar Receivers

This report presents the development of tools and methods for evaluating the reliability and performance of ceramic materials in high temperature solar receivers. As Concentrating Solar Power (CSP) technologies aim for higher operating temperatures to enhance efficiency and meet industrial process heat requirements, current high temperature metallic materials face challenges in maintaining structural integrity. This report explores advanced ceramics as a promising alternative, given their superior high temperature strength and lower thermal expansion, compared to metals. To address the need for effective ceramic receiver design tools, this report integrates statistical failure models of ceramics into the existing srlife tool: an open-source software package designed to estimate the life of high temperature CSP components. These failure models account for the inherent variability and flaw distribution in ceramics, as well as the impact of subcritical crack growth under high temperature cyclic loads. The report also presents experimental data collected for a commercially available ceramic material, SiC, and details the process of estimating reliability model parameters from these data. A comparative design analysis is then performed between ceramic (SiC) and metallic (current nickel-based superalloys A740H and A282) receiver. This comparison demonstrates that SiC receivers can achieve service life exceeding 30 years under high incident heat flux conditions, compared to just a few years for metallic receivers.

14 SOLAR ENERGY↗

NEXT GENERATION MELTER(S) FOR VITRIFICATION OF HANFORD WASTE STATUS AND DIRECTION

Vitrification technology has been selected to treat high-level waste (HLW) at the Hanford Site, the West Valley Demonstration Project and the Savannah River Site (SRS), and low activity waste (LAW) at Hanford. In addition, it may potentially be applied to other defense waste streams such as sodium bearing tank waste or calcine. Joule-heated melters (already in service at SRS) will initially be used at the Hanford Site's Waste Treatment and Immobilization Plant (WTP) to vitrify tank waste fractions. The glass waste content and melt/production rates at WTP are limited by the current melter technology. Significant reductions in glass volumes and mission life are only possible with advancements in melter technology coupled with new glass formulations. The Next Generation Melter (NGM) program has been established by the U.S. Department of Energy's (DOE's), Environmental Management Office of Waste Processing (EM-31) to develop melters with greater production capacity (absolute glass throughput rate) and the ability to process melts with higher waste fractions. Advanced systems based on Joule-Heated Ceramic Melter (JHCM) and Cold Crucible Induction Melter (CCIM) technologies will be evaluated for HLW and LAW processing. Washington River Protection Solutions (WRPS), DOE's tank waste contractor, is developing and evaluating these systems in cooperation with EM-31, national and university laboratories, and corporate partners. A primary NGM program goal is to develop the systems (and associated flowsheets) to Technology Readiness Level 6 by 2016. Design and testing are being performed to optimize waste glass process envelopes with melter and balance of plant requirements. A structured decision analysis program will be utilized to assess the performance of the competing melter technologies. Criteria selected for the decision analysis program will include physical process operations, melter performance, system compatibility and other parameters.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Fully Ceramic Microencapsulated fuel in prismatic high-temperature gas-cooled reactors: Sensitivity of reactor behavior during design basis accidents to fuel properties and the potential impact of the SiC defect annealing process

We conducted reactor performance calculations to assess the potential design basis accident performance of HTGR fuel designs. Three Fully Ceramic Microencapsulated (FCM) fueled HTGR designs were developed in a previous work (Lu et al., 2018). The maximum fuel temperature in the cores fueled by these three FCM fuels was predicted to be higher than that in the reference 350-MWt mHTGR core in both normal operating conditions and during representative design basis accidents (Lu and Brown, 2019). To better understand the potential safety margins in mHTGR design basis accidents, we performed thermal-hydraulics sensitivity studies to investigate how maximum fuel temperature varies considering various parameters, e.g. thermal properties, within the ranges corresponding to the differences between the FCM-fueled prismatic mHTGR cores and the reference core with conventional fuel compacts. We found that the difference in the steady-state axial power distribution contributed the most to the difference in the maximum fuel temperature, in both normal operation and design basis accidents.Experimental data suggested that the annealing process of irradiation defects in SiC would be rapid at mHTGR relevant fuel temperatures. The bounding potential impact of the SiC annealing on the maximum fuel temperature was analyzed considering both the thermal conductivity recovery and the Wigner energy release due to the annealing of SiC. We found that the defect annealing process in SiC would at most increase the peak maximum fuel temperature of an FCM-fueled core by 40 K in loss of forced cooling accidents and by 10 K in a control rod withdrawal accident. Finally, additional experiments on the SiC defect annealing kinetics and Wigner energy release in more relevant conditions are needed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗