Search NASA⌕ Search

SEARCH · Search NASA

Results for “doping effect”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Effects of Cr doping on the magnetic properties of multiferroic YMnO{sub 3}

We have synthesized a series of YMn{sub 1−x}Cr{sub x}O{sub 3} (0 ≤ x ≤ 0.1) samples and study the effect of Cr-doping on their magnetic properties. The magnetic characterization indicates that with increasing Cr-content up to 0.1, the antiferromagnetic (AFM) transition temperature increases from 73 to 89 K. Our experiment results also indicate that the Cr-doped samples exhibit the characteristics of spin-glass state at low temperature. Moreover, the magnetic hysteresis curves of the doped samples show a weak ferromagnetic (FM) behavior. It is found that the spin-glass state of the Cr-doped samples is due to the competition between AFM superexchange and FM double-exchange interaction, induced by the Cr doping.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Fe doping on structural and impedance properties of PZTFN ceramics

An attempts have been made to synthesis the ceramics Pb{sub 1-3x/2} Fe{sub x}(Zr{sub 0.52}Ti{sub 0.48}){sub 1-5y/4} NbyO{sub 3} abbreviated as (PFZTN) for x = 1-6 mol% and y = 5.5 mol% by a semi-wet route. In the present paper, we have investigated the effect of Fe doping on structural and electrical properties of the PFZTN ceramics. X-ray diffraction (XRD) patterns reveal that PFZTN ceramics are single phase in nature. However, for x = 0.05 and 0.06, a secondary phase appears as discernible from the XRD profiles. Rietveld analysis of the powder diffraction data shows the presence of coexistence of tetragonal (P4mm space group) and rhombohedral phases (R3c space group) occurs near the morphotropic phase boundary (MPB) at x ≥ = 0.05. The log-log plots show that the conductivity increases with increase of temperature. The ac conductivity becomes sensitive at high frequency region and shifted towards higher frequency side with increasing temperature. It is observed that the activation energy (Ea) decreases with increasing frequency. This complex perovskite structure can be used as a multilayer ceramic capacitors and electromechanical transducers.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Crystal structures of LaO{sub 1−x}F{sub x}BiS{sub 2} (x∼0.23, 0.46): Effect of F doping on distortion of Bi–S plane

The crystal structures of superconducting LaO{sub 1−x}F{sub x}BiS{sub 2} (x∼0.23, 0.46) were determined by single-crystal X-ray diffraction analysis. Their space group was P4/nmm. Distortion of the Bi–S plane changed when the F content was increased from 0.23 to 0.46, and a nearly flat Bi–S plane was formed at x∼0.46. Computational calculations supported this effect of F doping on distortion of Bi–S plane. LaO{sub 1−x}F{sub x}BiS{sub 2} with higher F contents were computationally predicted to be thermodynamically more unstable under ambient pressure. We discussed the bonding, conductivities, and synthetic routes of LaO{sub 1−x}F{sub x}BiS{sub 2}. - Graphical abstract: Distortion of the Bi–S plane in LaO{sub 1−x}F{sub x}BiS{sub 2} changed when the F content was increased from 0.23 to 0.46, and a nearly flat Bi–S plane was formed at x∼0.46 with the appearance of superconductivity. - Highlights: • Crystal structure of LaO{sub 1−x}F{sub x}BiS{sub 2} was determined by single-crystal XRD. • Doping amount of F changes the distortion of the Bi–S plane. • Nearly flat Bi–S planes were found in superconductive LaO{sub 1−x}F{sub x}BiS{sub 2} (x∼0.46). • LaO{sub 1−x}F{sub x}BiS{sub 2} with higher F contents was thermodynamically more unstable. • Bonding, superconductivities, and synthetic routes of LaO{sub 1−x}F{sub x}BiS{sub 2} were discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of tin doping on oxygen- and carbon-related defects in Czochralski silicon

Experimental and theoretical techniques are used to investigate the impact of tin doping on the formation and the thermal stability of oxygen- and carbon-related defects in electron-irradiated Czochralski silicon. The results verify previous reports that Sn doping reduces the formation of the VO defect and suppresses its conversion to the VO{sub 2} defect. Within experimental accuracy, a small delay in the growth of the VO{sub 2} defect is observed. Regarding carbon-related defects, it is determined that Sn doping leads to a reduction in the formation of the C{sub i}O{sub i}, C{sub i}C{sub s}, and C{sub i}O{sub i}(Si{sub I}) defects although an increase in their thermal stability is observed. The impact of strain induced in the lattice by the larger tin substitutional atoms, as well as their association with intrinsic defects and carbon impurities, can be considered as an explanation to account for the above observations. The density functional theory calculations are used to study the interaction of tin with lattice vacancies and oxygen- and carbon-related clusters. Both experimental and theoretical results demonstrate that tin co-doping is an efficient defect engineering strategy to suppress detrimental effects because of the presence of oxygen- and carbon-related defect clusters in devices.

36 MATERIALS SCIENCE↗

Effect of Carbon Doping on CO 2 –Reduction Activity of Single Cobalt Sites in Graphitic Carbon Nitride

Single atom catalysts have demonstrated interesting activity in a variety of applications. In this study, we prepared single C o2+ sites on graphitic carbon nitride (C 3 N 4 ), which was doped with carbon for enhanced activity in visible-light CO 2 reduction. The synthesized materials were characterized with a variety of techniques, including microscopy, X-ray powder diffraction, UV-vis spectroscopy, infrared spectroscopy, photoluminescence spectroscopy, and X-ray absorption spectroscopy. Here, doping C 3 N 4 with carbon was found to have profound effect on the photocatalytic activity of the single Co 2+ sites. At relatively low levels, carbon doping enhanced the photoresponse of C 3 N 4 in the visible region and improved charge separation upon photoactivation, thereby enhancing the photocatalytic activity. Furthermore, high levels of carbon doping were found to be detrimental to the photocatalytic activity of the single Co 2+ sites by altering the structure of C 3 N 4 and generating defect sites responsible for charge recombination.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of manganese doping of BaSrTiO{sub 3} on diffusion and domain wall pinning

In the present paper, the influence of manganese doping on the dielectric properties of BaSrTiO{sub 3} thin films is presented. The real and imaginary parts of the material's permittivity have been measured in a large frequency range (100 Hz–1 MHz) and as a function of the electric field. The tunability and the figure of merit of the material have been obtained from the measurement of the permittivity under an applied DC bias electric field. For the undoped material, the dielectric losses become important for a large DC bias which leads to breakdown. At a suitable dopant rate, this effect disappears. In order to better understand the origin of the related phenomena, we measure the permittivity as a function of the AC excitation amplitude and we decompose the obtained permittivity with the hyperbolic law. This enables to extract the different contributions of the bulk (low frequency diffusion and high frequency lattice relaxation) and of the domain wall motions (vibration and pinning/unpinning) to the material's dielectric permittivity and to understand the effect of manganese doping on each contribution. Knowledge of the related mechanisms allows us to establish the optimum dopant rate (mainly conditioned by the lattice contribution) and to reduce the domain wall motion, which finally is beneficial for the desired properties of the ferroelectric thin film. A particular attention is paid to low frequency diffusion, an especially harmful effect when a DC biasing is mandatory (tunable electronic component in mobile telecommunication devices for example)

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Electronic confinement in modulation doped quantum dots

Modulation doping, an effective way to dope quantum dots (QDs), modifies the confinement energy levels in the QDs. We present a self-consistent full multi-grid solver to analyze the effect of modulation doping on the confinement energy levels in large-area structures containing Si QDs in SiO{sub 2} and Si{sub 3}N{sub 4} dielectrics. The confinement energy was found to be significantly lower when QDs were in close proximity to dopant ions in the dielectric. This effect was found to be smaller in Si{sub 3}N{sub 4}, while smaller QDs in SiO{sub 2} were highly susceptible to energy reduction. The energy reduction was found to follow a power law relationship with the QD size.

36 MATERIALS SCIENCE↗

Unusual effects of Be doping in the iron-based superconductor FeSe

Recent superconducting transition temperatures (T c ) over 100 K for monolayer FeSe on SrTiO 3 have renewed interest in the bulk parent compound. In KCl:AlCl 3 flux-transport-grown crystals of FeSe 0.94 Be 0.06 , FeSe 0.97 Be 0.03 and, for comparison, FeSe, this work reports doping of FeSe using Be—among the smallest of possible dopants, corresponding to an effective 'chemical pressure'. According to lattice parameter measurements, 6% Be doping shrank the tetragonal FeSe lattice equivalent to a physical pressure of 0.75 GPa. Using this flux-transport method of sample preparation, 6% of Be was the maximum amount of dopant achievable. At this maximal composition of FeSe 0.94 Be 0.06 , the lattice unit cell shrinks by 2.4%, T c —measured in the bulk via specific heat—increases by almost 10%, the T c versus pressure behavior shifts its peak T$onset\atop{c}$downwards by ~1 GPa, the high temperature structural transition around T S = 89 K increases by 1.9 K (in contrast to other dopants in FeSe which uniformly depress T S), and the low temperature specific heat γ increases by 10% compared to pure FeSe. Also, upon doping by 6% Be the residual resistivity ratio, ρ(300 K)/ρ(T → 0), increases by almost a factor of four, while ρ(300 K)/ρ(T=$+\atop{c}$) increases by 50%.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of deposition temperature on the effectiveness of hydrogen doping in Ga-doped ZnO thin films

Gallium-doped zinc oxide thin films were prepared on glass substrates by dc magnetron sputtering under various hydrogen contents in sputtering ambient. The carrier concentration of the films deposited at low-temperatures (80 and 160 deg. C) was increased due to the incorporation of hydrogen atoms, acting as shallow donors. A low resistivity of 4.0x10{sup -4} {Omega} cm was obtained for the film grown at 160 deg. C with H{sub 2} 10%, which has a carrier concentration of 8.2x10{sup 20}/cm{sup 3}. The beneficial effect of hydrogen doping was not observed for the films deposited at 270 deg. C. Both carrier concentration and mobility were decreased by the addition of hydrogen gas in the sputtering ambient. Variations in the electrical transport properties upon vacuum annealing showed that the difference is attributed to the thermal stability of interstitial hydrogen atoms in the films. The hydrogen incorporation was found to induce the lattice expansion and the free carrier absorption in near infrared range. The investigation of the structural and optical properties of the films upon annealing also revealed that the incorporated hydrogen atoms are unstable at high temperature, which is consistent with the results obtained in the electrical properties.

36 MATERIALS SCIENCE↗

Effect of Mg doping on the structural and free-charge carrier properties of InN films

We present a comprehensive study of free-charge carrier and structural properties of two sets of InN films grown by molecular beam epitaxy and systematically doped with Mg from 1.0 × 10{sup 18} cm{sup −3} to 3.9 × 10{sup 21} cm{sup −3}. The free electron and hole concentration, mobility, and plasmon broadening parameters are determined by infrared spectroscopic ellipsometry. The lattice parameters, microstructure, and surface morphology are determined by high-resolution X-ray diffraction and atomic force microscopy. Consistent results on the free-charge carrier type are found in the two sets of InN films and it is inferred that p-type conductivity could be achieved for 1.0 × 10{sup 18} cm{sup −3} ≲ [Mg] ≲ 9.0 × 10{sup 19} cm{sup −3}. The systematic change of free-charge carrier properties with Mg concentration is discussed in relation to the evolution of extended defect density and growth mode. A comparison between the structural characteristics and free electron concentrations in the films provides insights in the role of extended and point defects for the n-type conductivity in InN. It further allows to suggest pathways for achieving compensated InN material with relatively high electron mobility and low defect densities. The critical values of Mg concentration for which polarity inversion and formation of zinc-blende InN occurred are determined. Finally, the effect of Mg doping on the lattice parameters is established and different contributions to the strain in the films are discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of thallium doping on the mobility of electrons in Bi{sub 2}Se{sub 3} and holes in Sb{sub 2}Te{sub 3}

The Shubnikov–de Haas effect and the Hall effect in n-Bi{sub 2–x}Tl{sub x}Se{sub 3} (x = 0, 0.01, 0.02, 0.04) and p-Sb{sub 2–x}Tl{sub x}Te{sub 3} (x = 0, 0.005, 0.015, 0.05) single crystals are studied. The carrier mobilities and their changes upon Tl doping are calculated by the Fourier spectra of oscillations. It is found shown that Tl doping decreases the electron concentration in n-Bi{sub 2–x}Tl{sub x}Se{sub 3} and increases the electron mobility. In p-Sb{sub 2–x}Tl{sub x}Te{sub 3}, both the hole concentration and mobility decrease upon Tl doping. The change in the crystal defect concentration, which leads to these effects, is discussed.

36 MATERIALS SCIENCE↗

Characterizing the Effects of Etch-induced Material Modification on the Crystallization Properties of Nitron Doped Ge2Sb2Te5

The chemical and structural effects of processing on the crystallization of nitrogen doped Ge{sub 2}Sb{sub 2}Te{sub 5} is examined via x-ray photoelectron spectroscopy (XPS), x-ray absorption spectroscopy (XAS), time resolved laser reflectivity, and time resolved x-ray diffraction (XRD). Time resolved laser reflectivity and XRD show that exposure to various etch and ash chemistries significantly reduces the crystallization speed while the transition temperature from the rocksalt to the hexagonal phase is increased. XPS and XAS attribute this to the selective removal and oxidization of N, Ge, Sb, and Te, thus altering the local bonding environment to the detriment of device performance.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Ab initio prediction of FeCr sigma (001)/FCC Fe(111) interfacial energy: Effect of interfacial doping of C, B, and N

Interfacial energy plays a crucial role for high-temperature material systems in determining their microstructure evolution and mechanical properties. Optimizing the interfacial energy through doping can improve the stability, performance, and overall functionality of these materials. Here, the present study delivers theoretical investigation on the sigma FeCr (001)//FCC Fe (111) interfacial energy using ab initio methods, focusing on the implications of interfacial doping with important interstitial elements carbon (C), boron (B), and nitrogen (N). The calculated interfacial energy without doping is 0.183J/m 2 . Upon doping, notable reductions in interfacial energy were observed. Doping with B decreased the interfacial energy to 0.046J/m 2 , with single C doping to 0.126J/m 2 , with two C doping to 0.098J/m 2 , and with a single N doping to 0.071J/m 2 . These findings not only shed light on the atomistic origin for the effect of stabilizing the microstructure of stainless steel at elevated temperatures by interstitial doping, but also present a systematic, thorough ab initio approach to predict interfacial doping properties and guide alloy design to enhance the performance and stability.

FeCr sigma phase↗

Investigation into the effect of Si doping on the cell symmetry and performance of Sr{sub 1−y}Ca{sub y}FeO{sub 3−δ} SOFC cathode materials

In this paper we report the successful incorporation of silicon into Sr{sub 1−y}Ca{sub y}FeO{sub 3−δ} perovskite materials for potential applications as electrode materials for Solid Oxide Fuel Cells. It is observed that Si doping leads to a change from a tetragonal or orthorhombic structure (with partial ordering of oxygen vacancies) to a cubic one (with the oxygen vacancies disordered). The structures of the phases, SrFe{sub 0.85}Si{sub 0.15}O{sub 3−δ}, Sr{sub 0.75}Ca{sub 0.25}Fe{sub 0.85}Si{sub 0.15}O{sub 3−δ} and Sr{sub 0.5}Ca{sub 0.5}Fe{sub 0.85}Si{sub 0.15}O{sub 3−δ}, were analysed using neutron powder diffraction. The data confirmed the cubic unit cell, with no long range oxygen vacancy ordering. Conductivity measurements showed an improvement in the conductivity on Si doping, especially for samples with high Ca content. Composite electrodes comprising 50% Ce{sub 0.9}Gd{sub 0.1}O{sub 1.95} and 50% Sr{sub 1−y}Ca{sub y}(Fe/Si)O{sub 3−δ} on dense Ce{sub 0.9}Gd{sub 0.1}O{sub 1.95} pellets were therefore examined in air. An improvement in the area specific resistances (ASR) values is observed for the Si-doped samples with respect to the undoped samples. Thus the results show that silicon can be incorporated into Sr{sub 1−y}Ca{sub y}FeO{sub 3−δ}-based materials and can have a beneficial effect on the performance, making them potentially suitable for use as cathode material in Solid Oxide Fuel Cells (SOFC). - Graphical abstract: X-ray diffraction patterns for: (left) Sr{sub 0.75}Ca{sub 0.25}Fe{sub 1−x}Si{sub x}O{sub 3−δ} (x=0, 0.05, 0.10 and 0.15) and (right) Sr{sub 0.25}Ca{sub 0.75}Fe{sub 1−x}Si{sub x}O{sub 3−δ} (x=0, 0.05, 0.10 and 0.15), showing the stabilization of the cubic form of these series through silicon doping. For the latter Sr{sub 0.25}Ca{sub 0.75}Fe{sub 1−x}Si{sub x}O{sub 3−δ} phase, the stabilisation is not quite complete at 15% Si doping. - Highlights: • In Sr{sub 1−y}Ca{sub y}Fe{sub 1−x}Si{sub x}O{sub 3−δ} materials Si doping results in a change from tetragonal or orthorhombic symmetry. • An improvement in the conductivity is observed on Si doping. • An improvement in the area specific resistances (ASR) values is observed on Si doping. • Silicon can have a beneficial effect on the performance in perovskite materials.

36 MATERIALS SCIENCE↗

Effect of Sn doping on the room temperature magnetodielectric properties of yttrium iron garnet

The structures, magnetic properties, permittivity spectra, and magnetodielectric (MD) effects of polycrystalline Y{sub 3}Fe{sub 5−x}Sn{sub x}O{sub 12} compounds prepared by solid state reactions were systematically investigated. The substitution of Sn{sup 4+} leads to lattice expansion and the donation of excess electrons in ceramics, which affects the concentration of Fe{sup 2+}, space charge, and electric dipole. As a result, as the amount of Sn dopant increases, so does saturation magnetization and permittivity in the low frequency band. The MD coefficient ([ε{sub r}(H) − ε{sub r}(0)]/ε{sub r}(0)) of lightly doped samples (x ≤ 0.05) is negative in the entire frequency band, reaching −2.3% at 350 MHz and 0.6 T for Y{sub 3}Fe{sub 4.95}Sn{sub 0.05}O{sub 12} ceramics. The MD coefficient of heavily doped samples (x > 0.05) is positive in the low frequency band, reaching 0.83% at 10 MHz and 0.6 T for Y{sub 3}Fe{sub 4.925}Sn{sub 0.075}O{sub 12} ceramics, and then decreasing with the increasing frequency, gradually becoming negative in the high frequency band. A detailed explanation is provided based on the origin of permittivity. This study provides a new methodology according to which the MD materials may be designed in order to satisfy the requirements of engineering applications.

36 MATERIALS SCIENCE↗

Effect of copper doping on kinetic phenomena in n-Bi{sub 2}Te{sub 2.85}Se{sub 0.15}

In single crystals of copper-doped and undoped Bi{sub 2}Te{sub 2.85}Se{sub 0.15} solid solutions with an electron concentration close to 1 x 10{sup 19} cm{sup -3}, the temperature dependences are investigated for the Hall (R{sub 123}, R{sub 321}) and Seebeck (S{sub 11}) kinetic coefficients, the electrical-conductivity ({sigma}{sub 11}), Nernst-Ettingshausen (Q{sub 123}), and thermal conductivity (k{sub 11}) coefficients in the temperature range of 77-400 K. The absence of noticeable anomalies in the temperature dependences of the kinetic coefficients makes it possible to use the one-band model when analyzing the experimental results. Within the framework of the one-band model, the effective mass of density of states (m{sub d} {approx} 0.8m{sub 0}), the energy gap ({epsilon}{sub g} {approx} 0.2 eV), and the effective scattering parameter (r{sub eff} {approx} 0.2) are estimated. The obtained value of the parameter r{sub eff} is indicative of the mixed electron-scattering mechanism with the dominant scattering by acoustic phonons. Data on the thermal conductivity and the lattice resistivity obtained by subtracting the electron contribution according to the Wiedemann-Franz law are presented.

36 MATERIALS SCIENCE↗

Effect of sulfur doping on thermoelectric properties of tin selenide – A first principles study

In this work we present the thermoelectric properties of tin selenide (SnSe) and sulfur doped tin selenide(SnSe{sub (1-x)}S{sub x}, x= 0.125 and 0.25) obtained using first principles calculations. We investigated the electronic band structure using the FP-LAPW method within the sphere of the density functional theory. Thermoelectric properties were calculated using BOLTZTRAP code using the constant relaxation time approximation at three different temperatures 300, 600 and 800 K. Seebeck coefficient (S) was found to decrease with increasing temperature, electrical conductivity (σ/τ) was almost constant in the entire temperature range and thermal conductivity (κ/τ) increased with increasing temperature for all samples. Sulfur doped samples showed enhanced seebeck coefficient, decreased thermal conductivity and decreased electrical conductivity at all temperatures. At 300 K, S increased from 1500 µV/K(SnSe) to 1720μV/K(SnSe{sub 0.75}S{sub 0.25}), thermal conductivity decreased from 5 × 10{sup 15} W/mKs(SnSe) to 3 × 10{sup 15} W/mKs(SnSe{sub 0.75}S{sub 0.25}), electrical conductivity decreased from 7 × 10{sup 20}/Ωms(SnSe) to 5 × 10{sup 20} /Ωms(SnSe{sub 0.75}S{sub 0.25}). These calculations show that sulfur doped tin selenide exhibit better thermoelectric properties than undoped tin selenide.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of heteroatom doping on hydrogen uptake in tungsten oxide

Redox-active transition metal oxides (TMOs) that can undergo proton-insertion coupled electron transfer (PICET) are promising candidates for catalyzing molecular conversion reactions which require the transfer of hydrogen atoms (or the thermochemical equivalent, H + , e − ). Herein, we studied the effects of isovalent (Mo 6+ ) and aliovalent (V 5+ and Nb 5+ ) heteroatom doping on the electrochemical PICET behavior of monoclinic tungsten oxide (WO 3 ). Cyclic voltammetry in aqueous acidic electrolytes shows that the addition of redox-active heteroatoms (Mo 6+ and V 5+ ) leads to systematic shifts in redox couple half-wave potentials (E 1/2 ), broadening, and an overall decrease in the current response. Conversely, the non-redox active heteroatom (Nb 5+ ) only reduces the current response with no observable peak-current broadening. This broadening is attributed to changes in the proton binding affinities of oxygen in different chemical environments, i.e., bridging different pairs of redox-active transition metal cations. We determined the hydrogen bond dissociation free energy (H BDFE) values to elucidate the thermodynamic effect of heteroatom substitution. Density functional theory calculations reveal a differentiation in the hydrogen binding and oxygen vacancy formation energies between heteroatom doped structures. The PICET-induced structural phase transitions of the pristine and doped samples were further probed with operando electrochemical X-ray diffraction (EC-XRD) and with ex situ chemical reduction. The broadening of the potential-dependent current response with increased heteroatom doping manifests in the operando EC-XRD results as prolonged structural regions where multiple hydrogen bronze phases exist and the appearance of cubic bronze phases at lower degrees of reduction compared to pristine WO 3 .

Holzapfel, Noah P. [North Carolina State Universit↗