At least 415 records · Page 23

Discerning Cell Surface Defects with 3D Optical Profilometry

This investigation seeks to establish better criteria that can be used for qualitative visual screening of cylindrical battery cells through exploration of various defects across multiple cylindrical Lithium-Ion battery cells. This investigation focuses on INR18650s and INR21700s cells from Molicel, LG, and Samsung. The principal instrument used is a high-definition 3D optical profilometer with measurement accuracy less than 0.5 microns. Through this effort, a catalog was built discerning minor surface imperfections from significant flaws. The catalog generated covers a comparison of axial and radial scratches, less than 5 microns, greater than 5 microns and greater than 15 microns, as well as the difference between surface discoloration, early-stage pitting, and late stages of corrosion. An exploration is made into cell button defects and crimp shoulder defects. When ultra-high-power optical magnification and three-dimension topological tools are not immediately available, this catalog will help determine if an individual cell is usable, worth further investigation, or failing. The purpose of this catalog is to be a field guide used for quick reference of a potential issue, with the goal of increasing screening throughput while reducing the need for costly examination. Trade names and trademarks are used in this abstract for identification only. Their usage does not constitute an official endorsement, either expressed or implied, by the National Aeronautics and Space Administration.

battery↗

Discerning Cell Surface Defects with 3D Optical Profilometry

This investigation seeks to establish better criteria that can be used for qualitative visual screening of cylindrical battery cells through exploration of various defects across multiple cylindrical Lithium-Ion battery cells. This investigation focuses on INR18650s and INR21700s cells from Molicel, LG, and Samsung. The principal instrument used is a high-definition 3D optical profilometer with measurement accuracy less than 0.5 microns. Through this effort, a catalog was built discerning minor surface imperfections from significant flaws. The catalog generated covers a comparison of axial and radial scratches, less than 5 microns, greater than 5 microns and greater than 15 microns, as well as the difference between surface discoloration, early-stage pitting, and late stages of corrosion. An exploration is made into cell button defects and crimp shoulder defects. When ultra-high-power optical magnification and three-dimension topological tools are not immediately available, this catalog will help determine if an individual cell is usable, worth further investigation, or failing. The purpose of this catalog is to be a field guide used for quick reference of a potential issue, with the goal of increasing screening throughput while reducing the need for costly examination. Trade names and trademarks are used in this abstract for identification only. Their usage does not constitute an official endorsement, either expressed or implied, by the National Aeronautics and Space Administration.

battery↗

Localized corrosion of low-carbon steel at the nanoscale

Abstract Mitigating corrosion remains a daunting challenge due to localized, nanoscale corrosion events that are poorly understood but are known to cause unpredictable variations in material longevity. Here, the most recent advances in liquid-cell transmission electron microscopy were employed to capture the advent of localized aqueous corrosion in carbon steel at the nanoscale and in real time. Localized corrosion initiated at a triple junction formed by a solitary cementite grain and two ferrite grains and then continued at the electrochemically-active boundary between these two phases. With this analysis, we identified facetted pitting at the phase boundary, uniform corrosion rates from the steel surface, and data that suggest that a re-initiating galvanic corrosion mechanism is possible in this environment. These observations represent an important step toward atomically defining nanoscale corrosion mechanisms, enabling the informed development of next-generation inhibition technologies and the improvement of corrosion predictive models.

36 MATERIALS SCIENCE↗

Long-term interactive corrosion between International Simple Glass and stainless steel

The interactive corrosion between stainless steel 316 (SS) and International Simple Glass (ISG) has been studied for 12 months. The samples were placed in intimate contact to create crevice corrosion conditions on SS in a 0.6 M NaCl solution with and without 142 ppm dissolved silica species enriched in 29 Si. Corrosion on SS was observed with large pits located close to the crevice mouth at the end of 1 year in 0.6 M NaCl solution. The SS corrosion was also associated with the dissolution of nearby glass in a highly localized manner. When the leaching solution was saturated with silica species, the corrosion rate of SS was suppressed. However, the presence of SS enhances ISG dissolution in both conditions. The implications of the observed phenomena on the long-term storage of nuclear waste are discussed.

36 MATERIALS SCIENCE↗

Influences of Quench Cooling Rate on Microstructure and Corrosion Resistance of Al-Cu-Mg Alloy Based on the End-Quenching Test

To investigate the effects of the quench cooling rate on corrosion resistance of Al-Cu-Mg alloy, an end-quenching test was conducted and the microstructures at different cooling rates were observed by SEM and TEM. Additionally, the corrosion resistance was characterized by an intergranular corrosion test and electrochemical test. Moreover, the finite element method was applied to simulate the end quenching process. The results indicate that the actual end quenching process can be approximated as one-dimensional heat transfer, and the cooling rate varies at different cooling distances. By affecting the microstructures, decreasing the cooling rate leads to a decline in the corrosion properties. Low cooling rates coarsen the constituent particles and grain boundary particles, resulting in a wide precipitation-free zone and an increase in the intensity of corrosion reactions. A high cooling rate concentrates on the intragranular precipitant, which can reduce the pitting depth and represents a conversion from localized corrosion to general corrosion.

36 MATERIALS SCIENCE↗

SRNL report for the tank waste disposition integrated flowsheet: Corrosion testing

A series of cyclic potentiodynamic polarization (CPP) tests were performed in support of the Tank Waste Disposition Integrated Flowsheet (TWDIF). The focus of the testing was to assess the effectiveness of the SRNL model for predicting the amount of nitrite inhibitor needed to prevent pitting induced by increasing halide concentrations. The testing conditions were selected to simulate the dilute process stream that is proposed to be returned to tank farms from treating the off-gas from the low activity waste melter in the Waste Treatment and Immobilization Plant.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Elevated-Temperature Tribo-Corrosion Response of Eutectic High-Entropy Alloy

The combination of elevated temperature and tribo-corrosion leads to the accelerated degradation of structural components used in many extreme environments. Recently developed high-entropy alloys (HEAs) with multiple principal elements have the potential for superior degradation resistance compared with presently used structural alloys. Here, we demonstrate the microstructural stability, pitting resistance, and superior tribo-corrosion degradation resistance of the AlCoCrFeNi 2.1 eutectic HEA in comparison with duplex stainless steel 2205 in deionized water (controlled low-ionic-strength electrolyte) at 25 °C, 50 °C and 100 °C. The AlCoCrFeNi 2.1 HEA showed excellent microstructural stability and tribo-corrosion resistance at all three temperatures, an order-of-magnitude lower wear rate, and a lower coefficient of friction compared with duplex 2205 steel. The lowest wear volume loss and wear rate for both AlCoCrFeNi 2.1 and duplex steel were recorded at 50 °C, which was attributed to temperature-assisted passivation and formation of a comparatively stable tribological surface condition. These results suggest superior performance of eutectic HEAs in tribo-corrosion applications compared with currently used dual-phase steels and motivate future evaluation in ion-containing industrial water chemistries.

36 MATERIALS SCIENCE↗

Stress induced growth of Sn nanowires in a single step by sputtering method

Sn nanowires in aluminum film have been synthesized in a single step by co-sputtering of Al and Sn targets. Due to immiscibility of Sn and Al, co-sputtering leads to generation of stress in the composite film. In order to attain thermodynamic equilibrium, Sn separates from Al and diffuses towards the grain boundaries. External perturbation due to ambient atmosphere leads to corrosion at the grain boundaries forming pits which provide path for Sn to evolve. Owing to this, extrusion of Sn nanowires from Al film occurs to release the residual stress in the film.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of the corrosion resistance of several alloys to dilute biologically active solutions

Sulfate reducing bacteria and acid producing bacteria/fungi detected in hygiene waters increased the corrosion rate in aluminum alloy. Biologically active media enhanced the formation of pits on metal coupons. Direct observation of gas evolved at the corrosion sample, coupled with scanning electron microscopy (SEM) and energy dispersive x-ray analysis of the corrosion products indicates that the corrosion rate is increased because the presence of bacteria favor the reduction of hydrogen as the cathodic reaction through the reaction of oxygen and water. SEM verifies the presence of microbes in a biofilm on the surface of corroding samples. The bacterial consortia are associated with anodic sites on the metal surface, aggressive pitting occurs adjacent to biofilms. Many pits are associated with triple points and inclusions in the aluminum alloy microstructure. Similar bacterial colonization was found on the stainless steel samples. Fourier transform Infrared Spectroscopy confirmed the presence of carbonyl groups in pitted areas of samples exposed to biologically active waters.

Walsh, Daniel W.↗

SNL API-653 In-Service Tank Inspection and Evaluation Tank ID: 981-A2-T0 (West)

An API Standard 653 In-Service inspection was completed on Tank 981-A2-T0 (West) located at the Sandia National Laboratories TAIV tank farm in Albuquerque, NM on September 22, 2015. The inspection was completed to collect data to evaluate the mechanical integrity and fitness for continued service of the tank. No indication or records of any previous inspection were identified for this tank. The inspection and engineering evaluation were completed using API-653, 5 th Edition and conservative engineering practices. The tank was not removed from service, so an internal inspection could not be completed. The tank was also fully insulated. The insulation was removed in specified areas of the tank shell and tank chime to accommodate an acoustic emission scan of the tank and an ultrasonic thickness evaluation of portions of the tank. The acoustic emission scan resulted in a grade of B / I - II indicating an overall TANKPAC grade B and composite grade II indicating minor active damage with highly concentrated sources related to corrosion found in the southeast and west side section of the tank. Eight Potential Localized Damage sources were found mainly in the west side (re-test in 2 years). The tank chime could not be inspected due to the configuration of the insulation welded angle support. An ultrasonic guided bulk wave inspection was completed on the tank shell to assess the lower shell section. At the time of the inspection the limited data collected showed minimal material loss from the shell at the thickness monitoring locations, however, visual inspection and pit depth gauge measurements showed > 3/16” inch pitting and significant general external surface corrosion on the shell at the shell to floor joint. This corrosion is caused by the insulation sheeting support welded angle iron trapping moisture and dirt against the tank shell. This tank should be removed from service, internally inspected, and repaired. Ultrasonic thickness measurement locations were established on this tank and the data is included in this report. The limited data collected indicated minimal material loss at these locations, with the only noted corrosion occurring on the tank shell to floor joint as noted above. An API-653 Annex B Evaluation of Tank Bottom Settlement was completed and the results are included in this report. No significant settlement issues were identified.

42 ENGINEERING↗

Effect of thermal treatments on electrochemical behavior of binder jetted 17-4 PH stainless steel

Binder jetted 17–4 PH stainless steel was post-processed to relate heat treatment, microstructure, and corrosion in 3.5 wt% NaCl. Specimens were sintered at 1380 or 1400 °C, solution-annealed at 1055 °C for 1 h, and aged at 482 °C for 1 h. Here, as-sintered parts showed α′-martensitic matrix with a δ-ferrite network and Cu-rich precipitates in ferrite; inclusions (MnS, NbC) promoted localized attack. solutionizing redistributed elements and reduced ferrite, while aging generated coherent Cu nano-precipitates. Corrosion resistance was highly sensitive to post-processing in which aged specimens exhibited the lowest corrosion current density and formed a thicker, stable Cr 2 O 3 -rich passive film, whereas sintered specimens degraded most. Pitting potential depended on sintering temperature and microstructure, with 1400 °C sintering yielding more positive pitting potentials and the best overall performance after aging. Although the 1400-solutionized condition showed a relatively noble pitting response versus 1380-solutionized, it displayed unstable corrosion kinetics attributed to an imperfect passive film linked to higher NbC density. XPS depth profiles corroborated these trends, showing thicker, more continuous Cr 2 O 3 in aged states and discontinuous/thinning oxides in less resistant conditions. Practically, high-temperature sintering (∼1400 °C) followed by solutionizing and aging is recommended, with further gains expected from reducing NbC/MnS populations and porosity via powder and process control.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Laser-Brazed Surface Made by Joining of AA6082 and Galvanized Steel

In the present study, a galvanized steel and a AA6082 aluminum alloy sheet of 2 mm thick were weld-brazed by applying laser and using 2-mm-diameter solid Al-12% Si filler wire at 2.5 m/min wire feed rate and 2 m/min laser scan speed at varying laser power (4.0, 3.5, 3.0 kW) in flange configuration. The microstructural investigation of the laser weld-brazed joints revealed the presence of two-layered intermetallic compound at steel/braze seam interface. The corresponding x-ray diffraction analysis of the steel/braze seam interface showed the presence of Al-Fe-Si-based ternary intermetallic phases. SEM and EDS analysis of the braze seam revealed the presence of α-Al grains surrounded by Mg{sub 2}Si phase in the grain boundary region. Fine intermetallic layer was observed at lower heat-input condition. The corrosion performance of the brazed joints was studied with the help of immersion, salt spray, and electrochemical polarization tests in different electrolytes containing NaCl salt. Brazed joints experienced galvanic corrosion during immersed in corrosive media. From the salt spray test, it was revealed that galvanized steel was highly susceptible to corrosion compared to Al-rich phase. The polarization results showed a substantial change in corrosion resistance from steel interface to the brazed region due to the variation in microstructure. The samples brazed with low heat-input showed better corrosion resistance as compared to the joints made with high heat-input. Post-corrosion microstructure revealed intergranular corrosion at the brazed joint along with pit formation.

36 MATERIALS SCIENCE↗

In-service Inspection of Radioactive Waste Tanks at the Savannah River Site – 15410

Liquid radioactive wastes from the Savannah River Site (SRS) separation process are stored in large underground carbon steel tanks. The high level wastes are processed in several of the tanks and then transferred by piping to other site facilities for further processing before they are stabilized in a vitrified or grout waste form. Based on waste removal and processing schedules, many of the tanks will be required to be in service for times exceeding the initial intended life. Until the waste is removed from storage, transferred, and processed, the materials and structures of the tanks must maintain a confinement function by providing a barrier to the environment and by maintaining acceptable structural stability during design basis events, which include loadings from both normal service and abnormal (e.g., earthquake) conditions. A structural integrity program is in place to maintain the structural and leak integrity functions of these waste tanks throughout their intended service life. In-service inspection (ISI) is an essential element of a comprehensive structural integrity program for the waste tanks at the Savannah River Site (SRS). The ISI program was developed to determine the degree of degradation the waste tanks have experienced due to service conditions. As a result of the inspections, an assessment can be made of the effectiveness of corrosion controls for the waste chemistry, which precludes accelerated localized and general corrosion of the waste tanks. Ultrasonic inspections (UT) are performed to detect and quantify the degree of general wall thinning, pitting and cracking as a measure of tank degradation. The results from these inspections through 2013, for the 27 Type III/IIIA tanks, indicate no reportable in-service corrosion degradation in the primary tank (i.e., general, pitting, or cracking). The average wall thickness for all tanks remains above the manufactured nominal thickness minus 0.25 millimeter and the largest pit identified is approximately 1.70 millimeter deep (i.e., less than 10% through-wall). Improvements to the inspection program were recently instituted to provide additional confidence in the degradation rates. Thickness measurements from a single vertical strip along the accessible height of the primary tank have been used as a baseline to compare historical measurements. Changes in wall thickness and pit depths along this vertical strip are utilized to estimate the rate of corrosion degradation. An independent review of the ISI program methodology, results, and path forward was held in August 2009. The review recommended statistical sampling of the tanks to improve the confidence of the single strip inspection program. The statistical sampling plan required that SRS increase the amount of area scanned per tank. Therefore, in addition to the baseline vertical strip that is obtained for historical comparisons, four additional randomly selected vertical strips are inspected. To date, a total of 104 independent vertical strips along the height of the primary tank have been completed. A statistical analysis of the data indicates that at this coverage level there is a 99.5% confidence level that one of the worst 5% of all the vertical strips was inspected. That is, there is a relatively high likelihood that the SRS inspection program has covered one of the most corroded areas of any of the Type III/IIIA waste tanks. These data further support the conclusion that there are no significant indications of wall thinning or pitting. Random sampling will continue to increase the confidence that one of the worst 5% has been inspected. In order to obtain the additional vertical strips, and minimize budget and schedule impacts, data collection speed for the UT system was optimized. Prior to 2009, the system collected data at a rate of 32 square centimeters per minute. The scan rate was increased to 129 - 160 square centimeters per minute by increasing the scanner step and pixel sizes in the data acquisition set-up. Laboratory testing was utilized to optimize the scan index/pixel size such that the requirements for wall thinning and pit detection were still maintained. SRS continues to evaluate improvements to ultrasonic equipment.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrosion of carbon steel and the passivating properties of corrosion films formed under high-PT geothermal conditions

Corrosion is a major obstacle to a safe implementation of geotechnical applications. Here, using a novel approach that includes vertical scanning interferometry (VSI) and electrochemical impedance spectroscopy (EIS) we discuss time-dependent carbon steel corrosion and film formation at geothermally relevant temperatures (80-160 °C) in CO 2 -saturated mildly acidic Na—Cl brine. Iron dissolution kinetics follows a logarithmic rate at 80 and 160 °C and a linear rate at 120 °C. At 80 °C, high initial corrosion rates (first 24 h) generate H 2 at a minimum rate of 12 μmol h -1 cm -2 and lead to the formation of a continuous ~100 μm thick porous corrosion film. It exhibits a duplex structure with a crystalline outer FeCO 3 layer and an inner layer composed of a skeletal network of Fe 3 C impregnated with FeCO 3 . Being an electrical conductor we hypothesize the Fe 3 C to strongly enhance corrosion rates by providing additional cathodic sites. Pseudo-passivity due to an anodic film-forming reaction (presumably Fe-oxide) was observed at 120 and 160 °C, soon followed by the initiation of pitting at 120 °C. Steady-state corrosion rates at 160 °C are at least one order of magnitude lower than for 120 °C. Lastly, our experimental approach demonstrated potential for general applicability in studying corrosion-related phenomena.

36 MATERIALS SCIENCE↗

RESULTS OF EXPERIMENT TO DETERMINE CORROSION RATES FOR 304L IN HB-LINE DISSOLVER VESSEL VENTILATION SYSTEM

Radioactive material being processed as part of the DE3013 program for HB-Line will result in the presence of chlorides, and in some cases fluorides, in the dissolver. Material Science and Technology developed an experimental plan to evaluate the impact of chloride on corrosion of the dissolver vessel ventilation system. The plan set test variables from the proposed operating parameters, previous test results, and a desired maximum chloride concentration for processing. The test variables included concentrations of nitric acid, fluorides and chlorides, and the presence of a welded and stressed metal coupon. Table 1 contains expected general corrosion rates in the HB-Line vessel vent system from dissolution of 3013 contents of varying nitric acid and chloride content. These general corrosion rates were measured upstream of the condenser in the experiment's offgas system near the entrance to the dissolver. However, they could apply elsewhere in the offgas system, depending on factors not simulated in the testing, including offgas system temperatures and airflow. Localized corrosion was significant in Tests One, Two, and Three. This corrosion is significant because it will probably be the first mode of penetration of the 304L steel in several places in the system. See Table 2. For Tests One and Three, the penetration rate of localized corrosion was much higher than that for general corrosion. It was approximately four times higher in Test One and at least 45 times higher in Test Three, penetrating an entire coupon thickness of 54 mils in 186 hours or less. There was no significant difference in corrosion between welded areas and un-welded areas on coupons. There was also no significant attack on stressed portions of coupons. It is probable that the lack of corrosion was because the stressed areas were facing downwards and offered no place for condensation or deposits to form. Had deposits formed, pitting may have occurred and led to stress corrosion cracking. The significant localized corrosion observed was usually associated with deposits. General corrosion on the offgas coupons was extremely high for the test containing 10,000 ppm chloride in the dissolver solution. Localized corrosion caused deep penetration of coupon surfaces with a solution of 2000 ppm chloride, both at 12 M and 8 M nitric acid. We recommend that when processing chloride-containing solutions, the pre-condenser side of the vessel vent system be inspected at a frequency calculated from acceptable material losses and expected general corrosion rate. The presence of deposits and heavy condensation during inspection should be taken as indicators of possibly severe localized corrosion.

36 MATERIALS SCIENCE↗

Mitigation of Galvanic Corrosion in Bolted Joint of AZ31B and Carbon Fiber-Reinforced Composite Using Polymer Insulation

The use of polymer insulation to mitigate galvanic corrosion was examined for bolted joints of AZ31B Mg alloy and carbon fiber-reinforced composite. To assess the corrosion behaviors of bolted joints with and without polymer insulation, solution immersion and salt spray exposure (ASTM B117) tests were conducted, and the corrosion depths and volumes were determined for the joint specimens after the tests. The polymer-insulated bolted joints exhibited much lower corrosion depths and volumes, highlighting the effective mitigation of galvanic corrosion. The reductions of joint strength in the post-corrosion joint specimens were relatively small (up to ~10%) in the polymer-insulated group but greater (up to 90%) in the group with no insulation. Cross-sectional characterization of post-corrosion joints with polymer insulation revealed local pits developed on AZ31B under galvanic influence, indicating that limited galvanic attack (that did not decrease the joining integrity significantly) could still occur during a long salt spray exposure (~1264 h) owing to the permeation of an aqueous corrosive medium.

36 MATERIALS SCIENCE↗

Synchrotron Infrared Reflectance Microspectroscopy Study of Film Formation and Breakdown on Copper

This work demonstrates the utility of synchrotron infrared reflectance microspectroscopy in the far- and mid-IR for the determination of the composition of electrogenerated surface films formed during the general and localized corrosion of copper in alkaline and bicarbonate solutions. Back-reflection geometry has been employed to identify the anodic film formed on copper in 0.1 M NaOH solution at 0.3 V (versus a Ag/AgCl reference) to be mainly CuO. In 0.01 M NaHCO{sub 3} solution general corrosion occurs with passive film formation below 0.2 V. The surface film at 0.2 V consisted mainly of bicarbonate, copper carbonate dihydroxide or malachite [CuCO{sub 3} {center_dot} Cu(OH){sub 2}], Cu(OH){sub 2} and possibly some CuO. At higher potentials the passive film breaks down and localized corrosion occurs leading to the formation of pits. The composition of the surface films inside the pits formed at 0.6 V was found to be essentially the same as that outside but the relative amount of Cu(OH){sub 2} appears to be higher.

36 MATERIALS SCIENCE↗

Pit depth analysis using automated software for three containers with complete imaging

The 3013 surveillance program is tasked with ensuring the long term safety of plutonium storage in 3013-compliant containers. One component of this task is to understand corrosion features found on the interior sidewall of the inner container closure weld region (ICCWR). To this end, three containers were selected to have laser confocal microscope (LCM) 20X imaging of the entire ICCWR. This report describes the analysis of the LCM pit depth data using the automated corrosion analysis software. The analysis included determining maximum pit depths and distributions of pit depths, volumes, and diameters for all pit features identified on the three containers. Results provided insight into possible corrosion mechanisms and were consistent with previous pit growth model predictions.

36 MATERIALS SCIENCE↗