Determination of Constraint-Independent Crack Tip Opening Angle for Stable Crack Growth in High-Strength Ductile Steels

The crack tip opening angle (CTOA) is one of fracture toughness parameters that has been used for decades in describing large stable crack growth in thin-walled aerospace structures under the low-constraint conditions. Recently, the pipeline industry has developed a growing interest in using the CTOA parameter to serve as the minimum required fracture toughness to arrest dynamic crack propagation in modern gas transmission pipelines made of high-strength ductile steel. To meet this industrial need, the CTOA test standard ASTM E3039 was therefore developed for measuring the constant critical CTOA. ASTM E3039 recommends a drop weight tearing test (DWTT) specimen with a shallow crack for standard CTOA testing, but its CTOA may depend on the low constraint condition of the DWTT specimen at the crack tip. Verifying the constraint independence of the DWTT-measured CTOA thus becomes indispensable for applying CTOA toughness to the running fracture control in the pipeline design. For this purpose, the present paper evaluates critical CTOA values in a set of fracture toughness tests on single-edge notched bend (SENB) specimens with shallow and deep cracks, based on four CTOA estimation models. Among these, the Ln(P)-LLD linear fit model is similar to that recommended by ASTM E3039 for CTOA calculation. Fracture test data for X80 pipeline steel and HY80 structural steel were considered in the CTOA evaluation. The results showed that the four CTOA models were able to determine a constraint independent CTOA value for stable crack growth in the SENB specimens. As a result, a single, reliable, constant CTOA value could be determined regardless of the specimen geometry or the crack-tip constraint conditions. Therefore, the CTOA measured using ASTM E3039 is constraint-independent and transferable to use in cases of actual cracks propagating in gas transmission pipelines.

36 MATERIALS SCIENCE↗

Experimental Investigation of Steel-Borne Acoustic Pulses for Fault Pinpointing in Pipe-Type Cable Systems: A Scaled-Down Model Approach

Pipe-type cable systems, including high-pressure fluid-filled (HPFF) and high-pressure gas-filled cables, are widely used for underground high-voltage transmission. These systems consist of insulated conductor cables within steel pipes, filled with pressurized fluids or gases for insulation and cooling. Despite their reliability, faults can occur due to insulation degradation, thermal expansion, and environmental factors. As many circuits exceed their 40-year design life, efficient fault localization becomes crucial. Fault location involves prelocation and pinpointing. Therefore, a novel pinpointing approach for pipe-type cable systems is proposed, utilizing accelerometers mounted on a steel pipe to capture fault-induced acoustic signals and employing the time difference of arrival method to accurately pinpoint the location of the fault. The experimental investigations utilized a scaled-down HPFF pipe-type cable system setup, featuring a carbon steel pipe, high-frequency accelerometers, and both mechanical and capacitive discharge methods for generating acoustic pulses. The tests evaluated the propagation velocity, attenuation, and pinpointing accuracy with the pipe in various embedment conditions. The experimental results demonstrated accurate fault pinpointing in the centimeter range, even when the pipe was fully embedded, with the acoustic pulse velocities aligning closely with the theoretical values. These experimental investigation findings highlight the potential of this novel acoustic pinpointing technique to improve fault localization in underground systems, enhance grid reliability, and reduce outage duration. Further research is recommended to validate this approach in full-scale systems.

Moutassem, Zaki↗

A Laboratory Corrosion Inhibition Study of Carbon Steel Using 2-Mercaptobenzothiazole (MBT) Under Post-Combustion CO2 Capture Conditions

Corrosion mitigation is an important aspect of amine-based post-combustion carbon dioxide (CO2) capture operations due to the desire to use less expensive but corrosion-vulnerable materials such as low carbon steels in the construction of a capture system. In this study, the corrosion behavior of A106 (grade B) carbon steel with an in-house proprietary amine-based solvent was investigated in a laboratory environment at 80°C using an organic corrosion inhibitor, 2-mercaptobenzothiazole (MBT). The corrosion inhibition mechanism was interpreted by electrochemical methods and surface analyses. The results revealed that the corrosion rates of carbon steel were significantly retarded using MBT. The critical inhibitor concentration was determined to be lie between 10 ppm and 50 ppm under the tested conditions.

Materials Science↗

Pitting Propagation Behavior on Low Alloy AISI 4130 (UNS G41300) Steel Exposed to Various Alkali and Alkaline Earth Metal Chlorides

Pit propagation studies were conducted to elucidate whether alkali and alkali earth metal cations such as Na+ and Rb+ present in the form of metal chloride salts such as RbCl affect pitting behavior in distinctly different manner than NaCl. Pit propagation studies were conducted on a low alloy steel using one-dimensional (1-D) pit method over pit depths from 300-1000 µm. LSV and EIS of planar electrodes of 4130 in a range of Cl- solutions were conducted and revealed no detected differences in impedance, open circuit, corrosion potential (Ecorr), passive current density (ipass), and pitting potential (Epit) as a function of salt type. In the case of one-dimensional pits during fast downward scan rates, the saturation potential (Esat) varied as a function of cation identity when pit depths were shallow. Mass transported limited current density also differed with cations in shallow pits when various alkali metal and alkaline metal cations were present. The limiting current density was increased for RbCl relative to NaCl The pit surface potential (Esurf) of activated pit surfaces reached Ecorr prior to establishing a condition where the pit electrolyte surface concentration (Csurf) was less than the critical concentration for active acidified pitting (i.e. Csurf<Ccrit) in this marginally passivating steel. For various Esurf and pit current density (ipit) combinations at constant Csurf where Ccrit< Csurf < Csat, E-log(i) plots were constructed using the method of Tianshu to create IR ohmic voltage corrected Tafel plots for various fixed pit solution concentrations. Under these conditions, the influence of cation identity on charge transfer controlled kinetics indicated slight differences in Tafel behavior where RbCl was slightly more aggressive than NaCl for low alloy steel oxidation. Differences in metal cation identity exert no effect on passive or breakdown on planar electrodes and only effect pit propagation stage in shallow pits.

Demarest, Chalres↗

Effects of Accident Thermal Loading on In-Plane Shear Behavior of Steel-Plate Composite Walls

Structural walls in safety-related nuclear facilities are required to be designed for seismic and accident thermal (due to postulated high-energy pipe break events) loading combination. Current U.S. and international codes provide limited guidance for analysis and design of walls for this loading combination. This paper describes the experimental results and observations from tests conducted on a laboratory-scale (1:4 to 1:5) test unit representing steel-plate composite (SC) walls subjected to combined in-plane (seismic) and accident thermal loading. The test unit was subjected to surface temperatures of up to 450°F in combination with cyclic in-plane loading. Results of similar experiments recently conducted in Japan are also summarized (with surface temperatures up to 570°F). Surface heating combined with the low thermal conductivity and high specific heat of concrete resulted in nonlinear thermal gradients through the thickness of the specimens. These nonlinear thermal gradients and the associated self- or internal restraint led to extensive concrete cracking. This concrete cracking reduced the initial and secant stiffness of the specimens. The initial stiffness of the heated specimens reduced to 30 to 40% of the initial stiffness of the control (unheated) specimen. The secant stiffness of the heated specimens reduced up to 50% of the secant stiffness of the control (unheated) specimen. However, the in-plane shear strength of the heated SC specimens was still approximately 10 to 30% greater than the nominal in-plane shear strength calculated, for the limit state of steel plate von Mises yielding, using AISC N690 equations and measured material properties. Evaluation of the experimental results and observations suggests that the in-plane shear strength of SC walls subjected to typical accident surface temperatures (up to 570°F) can be estimated conservatively using the current provisions of AISC N690. The stiffness for accident thermal loading combinations can be considered to reduce from cracked composite stiffness at ambient temperature to fully cracked—that is, steel-only stiffness as the surface temperature increases up to typical accident value.

Construction & Building Technology↗

Susceptibility of irradiated steels to hydrogen embrittlement

Investigation determined whether irradiated pressure-vessel steels 4340 and 212-B are susceptible to hydrogen embrittlement and to catastrophic failure. Hydrogen-charging conditions which completely embrittled 4340 steel had negligible effect on 212-B steel in tensile and delayed-failure tests.

Rossin, A. D.↗

Practical method of diffusion-welding steel plate in air

Method is ideal for critical service requirements where parent metal properties are equaled in notch toughness, stress rupture and other characteristics. Welding technique variations may be used on a variety of materials, such as carbon steels, alloy steels, stainless steels, ceramics, and reactive and refractory materials.

Holko, K. H.↗

Study of hot hardness characteristics of tool steels

Hardness measurements of tool steel materials in electric furnace at elevated temperatures and low oxygen environment are discussed. Development of equation to predict short term hardness as function of intial room temperature hardness of steel is reported. Types of steel involved in the process are identified.

Chevalier, J. L.↗

Physisorption of Ar, Kr, CH4, and N2 on 304 stainless steel at very low pressures.

Determination of physisorption isotherms of these gases on stainless steel by pressure change measurements in very low pressure cryogenic baths where a steel nipple was brought in contact with the test gas at 77 to 90 K in a sealed constant-volume system. The position of the nipple in the gas was changed in such a manner that gas adsorption on a 47.5 sq cm area of the steel surface could be measured. The Dubinin-Radushkevich (DR) equation (1947) was used for an empirical description of isotherms at different temperatures. The mean adsorption energies calculated from the DR plots were 1290, 1545, 1490 and 1903 cal/mol for Ar, Kr, CH4 and N2, respectively, being about 10% higher than the corresponding values on Pyrex.

Troy, M.↗

Explosive welding technique for joining aluminum and steel tubes

Silver sheet is wrapped around aluminum portion of joint. Mylar powder box is wrapped over silver sheet. Explosion welds silver to aluminum. Stainless-steel tube is placed over silver-aluminum interface. Mylar powder box, covered with Mylar tape, is wrapped around steel member. Explosion welds steel to silver-aluminum interface.

Wakefield, M. E.↗

An investigation of the plastic fracture of AISI 4340 and 18 nickel - 200 grade maraging steels

The mechanisms of plastic fracture (dimpled rupture) in high-purity and commercial 18 Ni, 200 grade maraging steels and quenched and tempered AISI 4340 steels have been studied. Plastic fracture takes place in the maraging alloys through void initiation by fracture of titanium carbo-nitride inclusions and the growth of these voids until impingement results in coalescence and final fracture. The fracture of AISI 4340 steel at a yield strength of 200 ksi occurs by nucleation and subsequent growth of voids formed by fracture of the interface between manganese sulfide inclusions and the matrix. The growth of these inclusion-nucleated voids is interrupted long before coalescence by impingement, by the formation of void sheets which connect neighboring sulfide-nucleated voids.

Cox, T. B.↗

The effect of microstructure and strength on the fracture toughness of an 18 Ni, 300 grade maraging steel

A 300 grade maraging steel was chosen as a vehicle by which to understand the inverse relationship between strength and toughness in high strength alloys such as the 18 Ni maraging steels. The 18 Ni, 300 grade maraging material was a commercial grade consumable-electrode, vacuum arc remelted heat obtained in the form of forged and annealed plate. The matrix contained a population of second-phase impurity inclusions which was a product of the casting and hot working processes. These inclusions did not change with subsequent precipitation hardening. Changes in microstructure resulting in strength increases were brought about by variations in aging temperature and time. Maximum strength was attained in the 300 grade maraging steel by aging at 427 C (800 F) for 100 hours. Tensile, fatigue precracked Charpy impact, and plane-strain fracture toughness tests were performed at room temperature, 20 C (68 F). With increasing strength the fracture toughness decreases as smaller and smaller inclusions act as sites for void initiation.

Psioda, J. A.↗

Low-cycle fatigue of Type 347 stainless steel and Hastelloy alloy X in hydrogen gas and in air at elevated temperatures

An investigation was conducted to assess the low-cycle fatigue resistance of two alloys, Type 347 stainless steel and Hastelloy Alloy X, that were under consideration for use in nuclear-powered rocket vehicles. Constant-amplitude, strain-controlled fatigue tests were conducted under compressive strain cycling at a constant strain rate of 0.001/sec and at total axial strain ranges of 1.5, 3.0, and 5.0 %, in both laboratory-air and low-pressure hydrogen-gas environments at temperatures from 538 to 871 C. Specimens were obtained from three heats of Type 347 stainless steel bar and two heats of Hastelloy Alloy X. The tensile properties of each heat were determined at 21, 538, 649, and 760 C. The continuous cycling fatigue resistance was determined for each heat at temperatures of 538, 760, and 871 C. The Type 347 stainless steel exhibited equal or superior fatigue resistance to the Hastelloy Alloy X at all conditions of this study.

Jaske, C. E.↗

Hydrogen enhanced crack growth in 18 Ni maraging steels

The kinetics of sustained-load subcritical crack growth for 18 Ni maraging steels in high-purity hydrogen are examined using the crack-tip stress intensity factor K as a measure of crack driving force. Crack growth rate as a function of stress intensity exhibited a clearly defined K-independent stage (Stage II). Crack growth rates in an 18 Ni (grade 250) maraging steel are examined for temperatures from -6 to +100 C. A critical temperature was observed above which crack growth rates became diminishingly small. At lower temperatures the activation energy for Stage II crack growth was found to be 16.7 plus or minus 3.3 kJ/mole. Temperature and hydrogen partial pressure are shown to interact in a complex manner to determine the apparent Kth (stress intensity level below which no observable crack growth occurs) and the crack growth behavior. Comparison of results on '250' and '300' grades of 18 Ni maraging steel indicate a significant influence of alloy composition and/or strength level on the crack growth behavior.

Hudak, S. J., Jr.↗

Cyclic-load crack growth in ASME SA-105 grade II steel in high-pressure hydrogen at ambient temperature

ASME SA-105 Grade II steel, which is used in high-pressure hydrogen compressor systems, is similar to steels used or considered for use in high-pressure hydrogen storage vessels and pipelines. This paper summarizes the results of a program conducted to provide cyclic-load crack growth rate (da/dN) data for a fracture mechanics analysis of a 15,000 psi hydrogen compressor facility which contains pulse quieter and after-cooler separator vessels constructed of the ASME SA-105 Grade II steel. Included in the program were tests performed to assist in establishing operating procedures that could minimize the effect of hydrogen on crack growth rates during operation.

Walter, R. J.↗

Detection of tightly closed flaws by nondestructive testing (NDT) methods in steel and titanium

X-radiographic, liquid penetrant, ultrasonic, eddy current and magnetic particle testing techniques were optimized and applied to the evaluation of 4340 steel (180 KSI-UTS) and 6Al-4V titanium (STA) alloy specimens. Sixty steel specimens containing a total of 176 fatigue cracks and 60 titanium specimens containing a total of 135 fatigue cracks were evaluated. The cracks ranged in length from .043 cm (0.017 inch) to 1.02 cm (.400 inch) and in depth from .005 cm (.002 inch) to .239 cm (.094 inch) for steel specimens. Lengths ranged from .048 cm (0.019 inch) to 1.03 cm (.407 inch) and depths from 0.010 cm (.004 inch) to .261 cm (0.103 inch) for titanium specimens. Specimen thicknesses were nominally .152 cm (0.060 inch) and 0.635 cm (0.250 inch) and surface finishes were nominally 125 rms. Specimens were evaluated in the "as machined" surface condition, after etch surface and after proof loading in a randomized inspection sequence.

Rummel, W. D.↗

Fabrication of stainless steel clad tubing

The feasibility of producing stainless steel clad carbon steel tubing by a gas pressure bonding process was evaluated. Such a tube product could provide substantial chromium savings over monolithic stainless tubing in the event of a serious chromium shortage. The process consists of the initial assembly of three component tubesets from conventionally produced tubing, the formation of a strong metallurgical bond between the three components by gas pressure bonding, and conventional cold draw and anneal processing to final size. The quality of the tubes produced was excellent from the standpoint of bond strength, mechanical, and forming properties. The only significant quality problem encountered was carburization of the stainless clad by the carbon steel core which can be overcome by further refinement through at least three different approaches. The estimated cost of clad tubing produced by this process is greater than that for monolithic stainless tubing, but not so high as to make the process impractical as a chromium conservation method.

Kovach, C. W.↗