A survey of strength analysis methods for laminates with holes

The methods for predicting the strength of composite laminates with fastener holes are reviewed for the cases of unloaded as well as loaded holes. Three categories of methods are discussed: (1) the hole-boundary stress (HBS) methods which compare the peak stresses and the laminate strength; (2) the linear elastic fracture (LEFM) methods which assume cracks emanating from the hole and predict failure when the stress intensity factor for a crack equals the laminate fracture toughness; and (3) two different two-parameter (TP) methods: the average-stress (ASTP) method, which predicts failure when the average stress over a distance from the hole equals the laminate strength; and the point-stress (PSTP) Whitney-Nuismer (1974) approach, which predicts failure when the stress near the hole equals the material strength. The PSTP is relatively accurate and is by far the most widely used of all the prediction methods. However, for large ranges of variables and cases, the current strength predictions may not always be accurate.

Crews, J. H., Jr.↗

The elasticity problem for a thick-walled cylinder containing a circumferential crack

The elasticity problem for a long hollow circular cylinder containing an axisymmetric circumferential crack subjected to general nonaxisymmetric external loads is considered. The problem is formulated in terms of a system of singular integral equations with the Fourier coefficients of the derivative of the crack surface displacement as density functions. The stress intensity factors and the crack opening displacement are calculated for a cylinder under uniform tension, bending by end couples, and self-equilibrating residual stresses.

Nied, H. F.↗

The elasticity problem for a thick-walled cylinder containing a circumferential crack

The elasticity problem for a long hollow circular cylinder containing an axisymmetric circumferential crack subjected to general nonaxisymmetric external loads is considered. The problem is formulated in terms of a system of singular integral equations with the Fourier coefficients of the derivative of the crack surface displacement as density functions. The stress intensity factors and the crack opening displacement are calculated for a cylinder under uniform tension, bending by end couples, and self-equilibrating residual stresses.

Nied, H. F.↗

Simulated Service and Stress Corrosion Cracking Testing for Friction Stir Welded Spun Form Domes

Damage tolerance testing development was required to help qualify a new spin forming dome fabrication process for the Ares 1 program at Marshall Space Flight Center (MSFC). One challenge of the testing was due to the compound curvature of the dome. The testing was developed on a sub-scale dome with a diameter of approximately 40 inches. The simulated service testing performed was based on the EQTP1102 Rev L 2195 Aluminum Lot Acceptance Simulated Service Test and Analysis Procedure generated by Lockheed Martin for the Space Shuttle External Fuel Tank. This testing is performed on a specimen with an induced flaw of elliptical shape generated by Electrical Discharge Machining (EDM) and subsequent fatigue cycling for crack propagation to a predetermined length and depth. The specimen is then loaded in tension at a constant rate of displacement at room temperature until fracture occurs while recording load and strain. An identical specimen with a similar flaw is then proof tested at room temperature to imminent failure based on the critical offset strain achieved by the previous fracture test. If the specimen survives the proof, it is then subjected to cryogenic cycling with loads that are a percentage of the proof load performed at room temperature. If all cryogenic cycles are successful, the specimen is loaded in tension to failure at the end of the test. This standard was generated for flat plate, so a method of translating this to a specimen of compound curvature was required. This was accomplished by fabricating a fixture that maintained the curvature of the specimen rigidly with the exception of approximately one-half inch in the center of the specimen containing the induced flaw. This in conjunction with placing the center of the specimen in the center of the load train allowed for successful testing with a minimal amount of bending introduced into the system. Stress corrosion cracking (SCC) tests were performed using the typical double beam assembly and with 4-point loaded specimens under alternate immersion conditions in a 3.5% NaCl environment for 90 days. In addition, experiments were conducted to determine the threshold stress intensity factor for SCC (K1SCC) of Al-Li 2195 which to our knowledge has not been determined previously. The successful simulated service and stress corrosion testing helped to provide confidence to continue to Ares 1 scale dome fabrication.

Stewart, Thomas J.↗

Stress intensity and crack displacement for small edge cracks

The weight function method was used to derive stress intensity factors and crack mouth displacement coefficients for small edge cracks (less than 20 percent of the specimen width) in common fracture specimen configurations. Contact stresses due to point application of loads were found to be small but significant for three-point bending and insignificant for four-point bending. The results are compared with available equations and numerical solutions from the literature and with unpublished boundary collocation results.

Orange, Thomas W.↗

Slow Crack Growth Analysis of Brittle Materials with Finite Thickness Subjected to Constant Stress-Rate Flexural Loading

A two-dimensional, numerical analysis of slow crack growth (SCG) was performed for brittle materials with finite thickness subjected to constant stress-rate ("dynamic fatigue") loading in flexure. The numerical solution showed that the conventional, simple, one-dimensional analytical solution can be used with a maximum error of about 5% in determining the SCG parameters of a brittle material with the conditions of a normalized thickness (a ratio of specimen thickness to initial crack size) T > 3.3 and of a SCG parameter n > 10. The change in crack shape from semicircular to elliptical configurations was significant particularly at both low stress rate and low T, attributed to predominant difference in stress intensity factor along the crack front. The numerical solution of SCG parameters was supported within the experimental range by the data obtained from constant stress-rate flexural testing for soda-lime glass microslides at ambient temperature.

Chio, S. R.↗

Fatigue life and crack growth prediction methodology

The capabilities of a plasticity-induced crack-closure model and life-prediction code to predict fatigue crack growth and fatigue lives of metallic materials are reviewed. Crack-tip constraint factors, to account for three-dimensional effects, were selected to correlate large-crack growth rate data as a function of the effective-stress-intensity factor range (delta(K(sub eff))) under constant-amplitude loading. Some modifications to the delta(K(sub eff))-rate relations were needed in the near threshold regime to fit small-crack growth rate behavior and endurance limits. The model was then used to calculate small- and large-crack growth rates, and in some cases total fatigue lives, for several aluminum and titanium alloys under constant-amplitude, variable-amplitude, and spectrum loading. Fatigue lives were calculated using the crack growth relations and microstructural features like those that initiated cracks. Results from the tests and analyses agreed well.

Newman, J. C., Jr.↗

Fatigue life and crack growth prediction methodology

This paper reviews the capabilities of a plasticity-induced crack-closure model and life-prediction code to predict fatigue crack growth and fatigue lives of metallic materials. Crack-tip constraint factors, to account for three-dimensional effects, were selected to correlate large-crack growth rate data as a function of the effective stress-intensity factor range (Delta K(sub eff)) under constant amplitude loading. Some modifications to the Delta K(sub eff)-rate relations were needed in the near threshold regime to fit small-crackgrowth rate behavior and endurance limits. The model was then used to calculate small- and large-crack growth rates, and in some cases total fatigue lives, for several aluminum and titanium alloys under constant-amplitude, variable-amplitude, and spectrum loading. Fatigue lives were calculated using the crack-growth relations and microstructural features like those that initiated cracks. Results from the tests and analyses agreed well.

Newman, J. C., Jr.↗

Fatigue Analyses Under Constant- and Variable-Amplitude Loading Using Small-Crack Theory

Studies on the growth of small cracks have led to the observation that fatigue life of many engineering materials is primarily "crack growth" from micro-structural features, such as inclusion particles, voids, slip-bands or from manufacturing defects. This paper reviews the capabilities of a plasticity-induced crack-closure model to predict fatigue lives of metallic materials using "small-crack theory" under various loading conditions. Constraint factors, to account for three-dimensional effects, were selected to correlate large-crack growth rate data as a function of the effective stress-intensity factor range (delta-Keff) under constant-amplitude loading. Modifications to the delta-Keff-rate relations in the near-threshold regime were needed to fit measured small-crack growth rate behavior. The model was then used to calculate small-and large-crack growth rates, and to predict total fatigue lives, for notched and un-notched specimens under constant-amplitude and spectrum loading. Fatigue lives were predicted using crack-growth relations and micro-structural features like those that initiated cracks in the fatigue specimens for most of the materials analyzed. Results from the tests and analyses agreed well.

Newman, J. C., Jr.↗

Analyses of Fatigue and Fatigue-Crack Growth under Constant- and Variable-Amplitude Loading

Studies on the growth of small cracks have led to the observation that fatigue life of many engineering materials is primarily crack growth from micro-structural features, such as inclusion particles, voids, slip-bands or from manufacturing defects. This paper reviews the capabilities of a plasticity-induced crack-closure model to predict fatigue lives of metallic materials using small-crack theory under various loading conditions. Constraint factors, to account for three-dimensional effects, were selected to correlate large-crack growth rate data as a function of the effective stress-intensity factor range (delta K(sub eff)) under constant-amplitude loading. Modifications to the delta K(sub eff)-rate relations in the near-threshold regime were needed to fit measured small-crack growth rate behavior. The model was then used to calculate small- and large-crack growth rates, and to predict total fatigue lives, for notched and un-notched specimens under constant-amplitude and spectrum loading. Fatigue lives were predicted using crack-growth relations and micro-structural features like those that initiated cracks in the fatigue specimens for most of the materials analyzed. Results from the tests and analyses agreed well.

Newman, J. C., Jr.↗

Quantitative Characterization of Impacts of Coupled Geomechanics and Flow on Safe and Permanent Geological Storage of CO 2 in Fractured Aquifers

This is the final scientific report for the award DE-FE0023305, entitled “Quantitative Characterization of Impacts of Coupled Geomechanics and Flow on Safe and Permanent Geological Storage of CO 2 in Fractured Aquifers.” The work has been divided into six tasks. In Task 2, we characterized rock properties, which are important when developing a quantitative approach for understanding and predicting geomechanical effects on large-scale CO 2 injection and long-term storage in the subsurface. Rock properties of interest for this characterization include porosity, permeability, elastic constants, strength, and heat capacity. We measured rock properties for three different rock types: concrete, sandstone and shale. These properties were obtained from the acoustic measurement, permeability and porosity measurement, Brazilian test, the uniaxial compressive test, and heat capacity measurement. Then, using the Brazilian technique to fracture samples, we measured their permeability under brine injection for varying effective stresses, followed by similar measurements of permeability under sc-CO 2 injection. Permeability to brine and sc-CO 2 decreased as the effective stress increased. The apparent permeability to sc-CO 2 was an order of magnitude less than that for brine, a consequence of CO 2 being the non-wetting fluid. In Task 3, we developed understandings and correlations for CO 2 injection pressure induced fracturing. We initially fractured four eight inch cubes of concrete with brine to establish a standard test procedure. Then, additional concrete samples were fractured using brine. Confining stresses were exerted on the samples and brine was injected at a constant rate into a borehole that was previously drilled into the concrete cube. The borehole pressure was measured and fracture initiation was identified as a peak in the pressure profile. That was followed by fracture propagation, which was identified as a plateau in the pressure profile, and finally the fracture reached the sample surface. The sample surfaces were photographed before and after fracturing, which enabled determination of where the fracture reached the sample surface. Afterwards, aqueous food dye solution was injected into the fractured concrete samples to color the fracture planes. The borehole was filled with food dye solution in advance, a gas pulse was transmitted to the borehole, and the borehole was then shut in to allow the food dye to be driven into existing fractures. Then, the concrete samples were broken down by high-pressure gas injection to reveal the geometry and morphology of the hydraulic fractures. In addition, acoustic measurements were conducted on multiple locations on each face of the concrete samples before and after injection for comparison. This comparison was used to confirm changes in the internal structure of the concrete sample, namely the formation of fractures. There were six concrete samples fractured with brine. Afterwards, concrete samples were fracture using sc-CO 2 . The main change in experimental procedure was the inclusion of temperature control, since in the field, we mostly encounter temperature and pressure conditions above the supercritical point of CO 2 . The concrete samples were pre-heated in an oven to elevate their temperature, and thermal tape was used to heat the CO 2 to a temperature above its supercritical temperature. Two concrete samples were fractured using liquid CO 2 , four concrete samples were fractured using gaseous CO 2 , and twenty two concrete samples were fractured using sc-CO 2 . For the concrete samples fractured using sc-CO 2 , three had pre-existing hydraulic fractures on the surface near the wellbore, and two were water saturated (as opposed to containing only air). Two concrete samples were composite samples, with a high permeability ball in the center, in order to represent CO 2 injection into a high permeability zone surrounded by a low permeability sealing formation. Later, we fractured five shale samples, obtained from the Niobrara shale outcrop, with sc-CO 2 . The injection rate was constant, confining stresses were applied, the shale samples were pre-heated in an oven to the desired temperature, and the sample was then fractured. An analysis of the failure type was done for many of the concrete samples, based on the predicted break down pressure for tensile and shear failure, and it was found that most samples fractured due to shear failure. Also, the presence of induced fractures has little to no effect on the fracture initiation pressure, but significantly changes the fracture morphology. The CO 2 fracturing in water saturated samples behaved much similar to brine induced fracturing. There was a significant difference of breakdown pressure for injection of CO 2 and brine, where the breakdown pressure for CO 2 induced fracturing is generally around the minimum horizontal stress and that for brine is much higher. Finally, the fracture orientation for most samples with large confining stress differential was perpendicular to the minimum horizontal stress. When the stress differential, especially the difference between the two directions with the smallest stresses was small, the fracture orientation was determined not only by the minimum stress direction, but also the magnitude of the confining stress, the tensile strength of the rock, and the breakdown pressure. In Task 4, we modified our coupled flow-geomechanical models to model fracture growth and propagation in storage formations and caprocks. These flow-geomechanical models are TOUGH2-CSM and TOUGH2-FLAC. The TOUGH2-CSM fluid and heat flow formulation is based on the TOUGH2 formulation of mass and energy conservation equations that govern fluid and heat flow in general multiphase, multicomponent, multi-porosity systems. The TOUGH2-CSM simplified geomechanical formulation is based on the linear theory of elasticity applied to multi-porosity non-isothermal (thermo-multi-poroelastic) media. We previously derived, from the fundamental relations of the linear theory of elasticity, an equation relating mean stress, pore pressures, temperatures, and body force (the Mean Stress equation) that we added to the TOUGH2-CSM fluid and heat flow equations. We extended the TOUGH2-CSM simplified geomechanical formulation to calculate the entire stress tensor by deriving equations for stress tensor components from derivatives of the Cartesian thermo-multi-poroelastic Navier equation components. In addition, we derived equations for stress tensor components in rz-coordinates. We solved these geomechanical equations using the integral finite difference method. This method utilizes momentum fluxes obtained by “factoring” a divergence operator out of each geomechanical equation. In Task 5, we did a literature survey to determine suitable correlations for fracture initiation, growth, and propagation. After surveying numerous papers, we modified TOUGH2-CSM to model stress dependent fracture initiation and growth using the Mohr-Coulomb criterion for shear failure in faults and caprock and the condition of negative minimum effective stress for tensile failure. Tensile failure results in a fracture whose width depends on the difference between fracture pressure and minimum stress and whose propagation is based on the difference between the stress intensity factor at the fracture tip and the rock toughness. The TOUGH-FLAC model is based on the FLAC3D ubiquitous joint model, extended for the modeling of permeability changes induced by changes in effective normal stress across fractures as well permeability changes caused by shearing along fractures. In Task 6, we validated our coupled flow-geomechanical models using analytical solutions and problems from the literature. We validated the TOUGH2-CSM modifications using analytical solutions to the displacement from a uniform load on a semi-infinite elastic medium and the two-dimensional Mandel-Cryer effect. Those were followed by a sample problem to test our stress tensor calculations, which was for injection into a single-phase reservoir with constant properties. Comparisons of our simulator to published results were done on for the depletion of a single-phase reservoir with stress dependent porosity, two examples from the In Salah gas project, an axisymmetric baserock–reservoir–caprock system with a normal faulting stress regime that had thermally induced shear stresses, simulations of CO 2 leakage through caprock in a two-dimensional reservoir in Cartesian coordinates, and predictions of caprock failure from CO 2 injection into an axisymmetric reservoir. Finally, we simulated CO 2 injection pressure-induced fracturing from one of our laboratory studies, Sample 39, and obtained a fracture profile. We also validated the TOUGH2-FLAC model for fluid driven fracture growth against solutions based on the KGD model and a case with an inclined fracture that was loaded from the boundaries to achieve wing-crack propagation. The strain softening tensile behavior and softening of modulus considering a simple damage approach was verified by a simulation representing hydraulic fracturing stress measurement around a vertical well. Finally, the model was validated against deep fracture zone opening and surface uplift at In Salah with inverses analysis used to improve the match of simulation with field data. In Task 7, we developed a scheme based on inverse modeling that can be used to identify caprock leakage. Injection of fluid into a reservoir results in a time varying pressure profile that depends on the properties of the rock and the fluid. The presence of significant caprock leakage would effect this pressure profile and we used inverse modeling, namely the Levenberg-Marquardt method, to determine the leakage location from the pressure profile. A two-dimensional and a three-dimensional example based on published data were presented. The published simulation was run and its results were considered as “field” data. In the two-dimensional example, a simulation of CO 2 injection into a two-dimensional aquifer-caprock system, the caprock had a vertical fault through which leakage could occur. The location of this leakage was obtained from our inverse modeling scheme. In the three-dimensional example, the simulation domain had four geological layers, one of which was the injection zone that contained a horizontal injection well. We simulated fractures as high permeability gridblocks, introduced a fracture that spanned the caprock depth, and ran a simulation to obtain “field” data. Then, using our inverse modeling scheme, we obtained the location of that fracture.

58 GEOSCIENCES↗

Limitations to the small scale yielding approximation for crack tip plasticity

Recent finite-element results by S. G. Larsson and A. J. Carlsson suggest a limited range of validity to the 'small scale yielding approximation,' whereby small crack tip plastic zones are correlated in terms of the elastic stress intensity factor. It is shown with the help of a model for plane strain yielding that their results may be explained by considering the non-singular stress, acting parallel to the crack at its tip, which accompanies the inverse square-root elastic singularity. Further implications of the non-singular stress term for crack tip deformations and fracturing are examined. It is suggested that its effect on crack tip parameters, such as the opening displacement and J-integral, is less pronounced than its effect on the yield zone size.

Rice, J. R.↗

Simulated Service and Stress Corrosion Cracking Testing for Friction Stir Welded Spun Formed Domes

Simulated service testing (SST) development was required to help qualify a new 2195 aluminum lithium (Al-Li) alloy spin forming dome fabrication process for the National Aeronautics and Space Administration (NASA) Exploration Development Technology Program. The application for the technology is to produce high strength low weight tank components for NASA s next generation launch vehicles. Since plate material is not currently manufactured large enough to fabricate these domes, two plates are joined by means of friction stir welding. The plates are then pre-contour machined to near final thicknesses allowing for a thicker weld land and anticipating the level of stretch induced by the spin forming process. The welded plates are then placed in a spin forming tool and hot stretched using a trace method producing incremental contours. Finally the dome receives a room temperature contour stretch to final dimensions, heat treatment, quenching, and artificial aging to emulate a T-8 condition of temper. Stress corrosion cracking (SCC) tests were also performed by alternate immersion in a sodium chloride (NaCl) solution using the typical double beam assembly and with 4-point loaded specimens and use of bent-beam stress-corrosion test specimens under alternate immersion conditions. In addition, experiments were conducted to determine the threshold stress intensity factor for SCC (K(sub ISCC)) which to our knowledge has not been determined previously for Al-Li 2195 alloy. The successful simulated service and stress corrosion testing helped to provide confidence to continue to Ares 1 scale dome fabrication

Stewart, Thomas J.↗

Predicting The Propagation Of Cracks

Advanced Crack Propagation Predictive Analysis Program, FLAGR04, developed as aid in predicting growth of preexisting flaws and cracks in structural components. Provides fracture-mechanics analyst with computerized method of evaluation of "safe crack-growth life" capabilities of structural components. Also used to evaluate tolerance-to-damage aspects of given structural design. Predicts growth of crack by use of two-dimensional model independently predicting growth of flaw in two directions based on calculation of stress-intensity factors. Input to FLAGR04 consists of initial definition of crack, type of rate solution, type and geometry of flaw, properties of material, data on load spectrum, load-stress functions, and design-limit stress levels. Output includes echo of input with any error or warning message and history of propagation of crack. Written in FORTRAN IV.

Tianlai, HU↗

The stress field in an edge cracked plate in antiplane deformation

The antiplane strain problem of an edge cracked elastic plate subjected to a surface displacement load is solved, and the surface line loads are obtained using conformal mapping techniques. Results are presented for the yield, stress, strain and displacement distributions, and stress intensity factors in the plate. A superposition technique and Green's functions are used to determine the strain field on the upper plate surface due to arbitrarily applied tensile stress on the lower plate surface.

Li, V. C.↗

Fatigue-Life Prediction Methodology Using Small-Crack Theory

This paper reviews the capabilities of a plasticity-induced crack-closure model to predict fatigue lives of metallic materials using 'small-crack theory' for various materials and loading conditions. Crack-tip constraint factors, to account for three-dimensional state-of-stress effects, were selected to correlate large-crack growth rate data as a function of the effective-stress-intensity factor range (delta K(eff)) under constant-amplitude loading. Some modifications to the delta k(eff)-rate relations were needed in the near-threshold regime to fit measured small-crack growth rate behavior and fatigue endurance limits. The model was then used to calculate small- and large-crack growth rates, and to predict total fatigue lives, for notched and un-notched specimens made of two aluminum alloys and a steel under constant-amplitude and spectrum loading. Fatigue lives were calculated using the crack-growth relations and microstructural features like those that initiated cracks for the aluminum alloys and steel for edge-notched specimens. An equivalent-initial-flaw-size concept was used to calculate fatigue lives in other cases. Results from the tests and analyses agreed well.

Newmann, James C., Jr.↗

Stress Intensity of Delamination in a Sintered-Silver Interconnection: Preprint

In automotive power electronics packages, conventional thermal interface materials such as greases, gels, and phase-change materials pose bottlenecks to heat removal and are also associated with reliability concerns. The industry trend is toward high thermal performance bonded interfaces for large-area attachments. However, because of coefficient of thermal expansion mismatches between materials/layers and resultant thermomechanical stresses, adhesive and cohesive fractures could occur, posing a reliability problem. These defects manifest themselves in increased thermal resistance. This research aims to investigate and improve the thermal performance and reliability of sintered-silver for power electronics packaging applications. This has been experimentally accomplished by the synthesis of large-area bonded interfaces between metalized substrates and copper base plates that have subsequently been subjected to thermal cycles. A finite element model of crack initiation and propagation in these bonded interfaces will allow for the interpretation of degradation rates by a crack-velocity (V)-stress intensity factor (K) analysis. A description of the experiment and the modeling approach are discussed.

30 DIRECT ENERGY CONVERSION↗

Investigation of the effects of manufacturing variations and materials on fatigue crack detection methods in gear teeth

The fatigue life of a gear tooth can be thought of as the sum of the number of cycles required to initiate a crack, N(sub i), plus the number of cycles required to propagate the crack to such a length that fracture occurs, N(sub p). The factors that govern crack initiation are thought to be related to localized stress or strain at a point, while propagation of a fatigue crack is a function of the crack tip parameters such as crack shape, stress state, and stress intensity factor. During a test there is no clear transition between initiation and propagation. The mechanisms of initiation and propagation are quite different and modeling them separately produces a higher degree of accuracy, but then the question that continually arises is 'what is a crack?' The total life prediction in a fracture mechanics model presently hinges on the assumption of an initial crack length, and this length can significantly affect the total life prediction. The size of the initial crack is generally taken to be in the range of 0.01 in. to 0.2 in. Several researchers have used various techniques to determine the beginning of the crack propagation stage. Barhorst showed the relationship between dynamic stiffness changes and crack propagation. Acoustic emissions, which are stress waves produced by the sudden movement of stressed materials, have also been successfully used to monitor the growth of cracks in tensile and fatigue specimens. The purpose of this research is to determine whether acoustic emissions can be used to define the beginning of crack propagation in a gear using a single-tooth bending fatigue test.

Wheitner, Jeffrey A.↗