Search NASA⌕ Search

SEARCH · Search NASA

Results for “Solids Formation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 415 records · Page 23

An analysis of the pull strength behaviors of fine-pitch, flip chip solder interconnections using a Au-Pt-Pd thick film conductor on Low-Temperature, Co-fired Ceramic (LTCC) substrates.

The assembly of the BDYE detector requires the attachment of sixteen silicon (Si) processor dice (eight on the top side; eight on the bottom side) onto a low-temperature, co-fired ceramic (LTCC) substrate using 63Sn-37Pb (wt.%, Sn-Pb) in a double-reflow soldering process (nitrogen). There are 132 solder joints per die. The bond pads were gold-platinum-palladium (71Au-26Pt-3Pd, wt.%) thick film layers fired onto the LTCC in a post-process sequence. The pull strength and failure modes provided the quality metrics for the Sn-Pb solder joints. Pull strengths were measured in both the as-fabricated condition and after exposure to thermal cycling (-55/125 C; 15 min hold times; 20 cycles). Extremely low pull strengths--referred to as the low pull strength phenomenon--were observed intermittently throughout the product build, resulting in added program costs, schedule delays, and a long-term reliability concern for the detector. There was no statistically significant correlation between the low pull strength phenomenon and (1) the LTCC 'sub-floor' lot; (2) grit blasting the LTCC surfaces prior to the post-process steps; (3) the post-process parameters; (4) the conductor pad height (thickness); (5) the dice soldering assembly sequence; or (5) the dice pull test sequence. Formation of an intermetallic compound (IMC)/LTCC interface caused by thick film consumption during either the soldering process or by solid-state IMC formation was not directly responsible for the low-strength phenomenon. Metallographic cross sections of solder joints from dice that exhibited the low pull strength behavior, revealed the presence of a reaction layer resulting from an interaction between Sn from the molten Sn-Pb and the glassy phase at the TKN/LTCC interface. The thick film porosity did not contribute, explicitly, to the occurrence of reaction layer. Rather, the process of printing the very thin conductor pads was too sensitive to minor thixotropic changes to ink, which resulted in inconsistent proportions of metal and glassy phase particles present during the subsequent firing process. The consequences were subtle, intermittent changes to the thick film microstructure that gave rise to the reaction layer and, thus, the low pull strength phenomenon. A mitigation strategy would be the use of physical vapor deposition (PVD) techniques to create thin film bond pads; this is multi-chip module, deposited (MCM-D) technology.

36 MATERIALS SCIENCE↗

Microphysical Modelling of the 1999-2000 Arctic Winter: Impact of Homogeneous Freezing on PSCs - 3

Simulations of the 1999-2000 winter have tested the effect on polar stratospheric clouds (PSCs) of the homogeneous freezing of liquid ternary solutions into nitric acid trihydrate (NAT) and nitric acid dihydrate (NAD). Proposed laboratory-derived volume-based and surface-based homogeneous freezing rates have both been examined, including different assumptions about the extrapolation of laboratory measurements to atmospheric conditions. Widespread PSC formation and denitrification are possible in several of the scenarios examined. However, the simulations are all unable to explain the solid-phase PSCs observed early in the 1999-2000 winter, and are unable to reproduce the measured extent of vortex denitrification. These problems can both be attributed to the relatively cold temperatures, more than 5 K below the NAT condensation point, necessary for effective homogeneous freezing. Therefore synoptic-scale homogeneous freezing appears unlikely to be the primary mechanism responsible for solid-phase PSC formation.

Drdla, K.↗

Stabilizing the Solid‐Electrolyte Interphase with Polyacrylamide for High‐Voltage Aqueous Lithium‐Ion Batteries

Abstract The introduction of “water‐in‐salt” electrolyte (WiSE) concept opens a new horizon to aqueous electrochemistry that is benefited from the formation of a solid‐electrolyte interphase (SEI). However, such SEI still faces multiple challenges, including dissolution, mechanical damaging, and incessant reforming, which result in poor cycling stability. Here, we report a polymeric additive, polyacrylamide (PAM) that effectively stabilizes the interphase in WiSE. With the addition of 5 molar % PAM to 21 mol kg −1 LiTFSI electrolyte, a LiMn 2 O 4 ∥L‐TiO 2 full cell exhibits enhanced cycling stability with 86 % capacity retention after 100 cycles at 1 C. The formation mechanism and evolution of PAM‐assisted SEI was investigated using operando small angle neutron scattering and density functional theory (DFT) calculations, which reveal that PAM minimizes the presence of free water molecules at the anode/electrolyte interface, accelerates the TFSI − anion decomposition, and densifies the SEI.

25 ENERGY STORAGE↗

Tailoring the properties of polymers via formation of a mesophase

The combination of the control of the concentration of stereodefects in isotactic polypropylene using metallocene catalysts and the crystallization via the mesophase is a strategy to tailor the mechanical properties. Stiff materials, flexible materials, and thermoplastic elastomers can be produced depending only on the concentration of rr stereodefects. We show that in the case of isotactic polypropylene (iPP) the material properties can be finely tuned at molecular level via formation of a solid mesophase, characterized by an intermediate degree of order between amorphous and crystalline state. The effect of different degree of stereoregularity on the mesophase formation, thermal stability, morphology, is analyzed at different length scales, using different technique including wide angle X-ray scattering, atomic and optical microscopy. Different morphologies are observed depending on the stereoregularity and conditions of crystallization. In contrast to the lamellar morphology of crystals normally obtained from the melt, the solid mesophase show a nodular morphology.

36 MATERIALS SCIENCE↗

Unveiling the mechanisms of lithium dendrite suppression by cationic polymer film induced solid–electrolyte interphase modification

It is crucial to suppress lithium dendrite formation in lithium metal batteries. Formation of a good solid–electrolyte interphase (SEI) has been considered to be effective in limiting lithium dendrite growth. However, how the SEI may be modified during lithium deposition is hard to resolve due to challenges in in situ investigation of the SEI with fine details. Here, we report an in situ study that uncovers the lithium dendrite suppression mechanism arising from SEI modification by a poly(diallyldimethylammonium chloride) (PDDA) cationic polymer film, using electrochemical liquid cell transmission electron microscopy (TEM). Lithium nanogranules are obtained in the presence of the polymer film. Chemical mapping of the deposits provides remarkable details of the SEI on individual nanogranules. It shows that lithium fluorides are uniformly distributed within the inner SEI layer of individual lithium nanogranules, arising from the instantaneous reaction of the deposited lithium with PF 6 – ions accumulated by the cationic polymer film, and thus the dendritic growth of lithium is prohibited. The ability to directly measure SEI chemistry at the nanoscale down to the individual nanograins in situ and unveil its correlation with the lithium deposition behavior opens future opportunities to explore unsolved mechanisms in batteries.

25 ENERGY STORAGE↗

Methods to avoid post-filtration precipitation in treatment of high-level waste

The Hanford Tank Waste Treatment and Immobilization Plant currently under construction for treating high level waste at the Hanford Site will rely on ultrafiltration to provide solids liquid separation as a core part of the treatment process. A series of bench-scale simulant tests have been performed to evaluate the potential for post-filtration precipitation. These tests focused on identifying precipitation from a range of potential feed compositions and providing the data required to evaluate mitigation options. A series of tests were performed using a variety of simulant samples. These tests identified the expected extent of supersaturation that develops under normal operations and identified and characterized the solids phases that are expected to form when the filtrate solutions are stored. In addition, tests identified the potential to mitigate the formation of these solids through both dilution and the application of increased temperature.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of Carbonate Solvents and Lithium Salts on Morphology and Coulombic Efficiency of Lithium Electrode

The application of lithium (Li) metal anode in rechargeable batteries is hindered by Li dendrite growth during Li deposition and low Li Coulombic efficiency (CE), where the nonaqueous electrolyte plays a critical role. In this work, the effects of different carbonate solvents and Li salts on Li deposition morphology and CE were systematically investigated. Typically cyclic carbonates are found to favor the formation of uniform Li film and improve Li CE than linear carbonates do. Several specific cyclic carbonates that are conventionally used as solid electrolyte interface formation additives in Li ion batteries can also improve the CE of Li anode. Furthermore, among the nine electrolyte salts studied, LiAsF6 and LiBOB lead to the highest CE for Li anode. LiBOB also leads to much smoother Li morphology than other salts do. Considering the better safety of LiBOB as compared to LiAsF6, LiBOB is a promising Li salt for rechargeable Li metal batteries with high CE. By combining the best electrolyte solvent/salt that can lead to high Li CE and novel electrolyte additives that can prevent dendrite formation, it is possible to find an electrolyte that not only prevents Li dendrite formation but also lead to high CE during Li deposition/stripping processes.

Environmental Molecular Sciences Laboratory↗

Melting behavior of the iron-sulfur system and chemical convection in iron-rich planetary cores

We present experimental data on the high-pressure melting behavior of the Fe-S system from a synchrotron x-ray radiography study using the large volume press, with implications for the role of chemical convection in sulfur-bearing planetary cores. At present, Earth, Mercury and Ganymede are the only three solid bodies in the Solar System that possess intrinsic global magnetic fields. Dynamo simulation reveal that chemical buoyancy force associated with the formation of a solid inner core is critical for sustaining the Earth's magnetic field. Fluid motions in Mercury and Ganymede may be partially driven by chemical buoyancy force as well. The style of chemical convection and its influence on the thermal and chemical state and evolution of iron-rich cores are determined in part by the melting behavior of potential core-forming materials. Sulfur is widely accepted as a candidate light element in iron-rich planetary cores. In order to understand the role of chemical convection in sulfur-bearing cores, we studied the high-pressure melting behavior of Fe-S mixtures containing 9 wt% sulfur using the synchrotron x-ray radiographic method in a large volume press.

43 PARTICLE ACCELERATORS↗

Stabilizing the Solid‐Electrolyte Interphase with Polyacrylamide for High‐Voltage Aqueous Lithium‐Ion Batteries

Abstract The introduction of “water‐in‐salt” electrolyte (WiSE) concept opens a new horizon to aqueous electrochemistry that is benefited from the formation of a solid‐electrolyte interphase (SEI). However, such SEI still faces multiple challenges, including dissolution, mechanical damaging, and incessant reforming, which result in poor cycling stability. Here, we report a polymeric additive, polyacrylamide (PAM) that effectively stabilizes the interphase in WiSE. With the addition of 5 molar % PAM to 21 mol kg −1 LiTFSI electrolyte, a LiMn 2 O 4 ∥L‐TiO 2 full cell exhibits enhanced cycling stability with 86 % capacity retention after 100 cycles at 1 C. The formation mechanism and evolution of PAM‐assisted SEI was investigated using operando small angle neutron scattering and density functional theory (DFT) calculations, which reveal that PAM minimizes the presence of free water molecules at the anode/electrolyte interface, accelerates the TFSI − anion decomposition, and densifies the SEI.

Hou, Xu↗

Synthesis of Antiperovskite Solid Electrolytes: Comparing Li 3 SI, Na 3 SI, and Ag 3 SI

Prior calculations have predicted that chalcohalide anti-perovskites may exhibit enhanced ionic mobility compared to oxyhalide anti-perovskites as solid-state electrolytes. Herein, the synthesis of Ag-, Li- and Na-based chalcohalide anti-perovskites is investigated using first-principle calculations and in situ synchrotron X-ray diffraction. These techniques demonstrate that the formation of Ag 3 SI is facilitated by the adoption of a common body centered cubic packing of S 2– and I – in the reactants and products at elevated temperatures, with additional stabilization achieved by the formation of a solid solution of the anions. Further, the absence of these two features appears to hinder the formation of the analogous Li and Na anti-perovskites.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Knowledge-driven design of solid-electrolyte interphases on lithium metal via multiscale modelling

Abstract Due to its high energy density, lithium metal is a promising electrode for future energy storage. However, its practical capacity, cyclability and safety heavily depend on controlling its reactivity in contact with liquid electrolytes, which leads to the formation of a solid electrolyte interphase (SEI). In particular, there is a lack of fundamental mechanistic understanding of how the electrolyte composition impacts the SEI formation and its governing processes. Here, we present an in-depth model-based analysis of the initial SEI formation on lithium metal in a carbonate-based electrolyte. Thereby we reach for significantly larger length and time scales than comparable molecular dynamic studies. Our multiscale kinetic Monte Carlo/continuum model shows a layered, mostly inorganic SEI consisting of LiF on top of Li 2 CO 3 and Li after 1 µs. Its formation is traced back to a complex interplay of various electrolyte and salt decomposition processes. We further reveal that low local Li + concentrations result in a more mosaic-like, partly organic SEI and that a faster passivation of the lithium metal surface can be achieved by increasing the salt concentration. Based on this we suggest design strategies for SEI on lithium metal and make an important step towards knowledge-driven SEI engineering.

25 ENERGY STORAGE↗

Impact of dual-layer solid-electrolyte interphase inhomogeneities on early-stage defect formation in Si electrodes

While intensive efforts have been devoted to studying the nature of the solid-electrolyte interphase (SEI), little attention has been paid to understanding its role in the mechanical failures of electrodes. Here we unveil the impact of SEI inhomogeneities on early-stage defect formation in Si electrodes. Buried under the SEI, these early-stage defects are inaccessible by most surface-probing techniques. With operando full field diffraction X-ray microscopy, we observe the formation of these defects in real time and connect their origin to a heterogeneous degree of lithiation. This heterogeneous lithiation is further correlated to inhomogeneities in topography and lithium-ion mobility in both the inner- and outer-SEI, thanks to a combination of operando atomic force microscopy, electrochemical strain microscopy and sputter-etched X-ray photoelectron spectroscopy. Our multi-modal study bridges observations across the multi-level interfaces (Si/LixSi/inner-SEI/outer-SEI), thus offering novel insights into the impact of SEI homogeneities on the structural stability of Si-based lithium-ion batteries. Severe structural deformation during (de)lithiation is the main factor limiting the stability of Si anodes in Li-ion batteries. Here, a multi-modal approach is used to visualize these deformations in their early-stage and link them to inhomogeneities in the dual-layer solid-electrolyte interphase.

25 ENERGY STORAGE↗

Ionic conductivity and the formation of cubic CaH{sub 2} in the LiBH{sub 4}–Ca(BH{sub 4}){sub 2} composite

LiBH{sub 4}–Ca(BH{sub 4}){sub 2} composites were prepared by ball milling. Their crystal structures and phase composition were investigated using synchrotron X-ray diffraction and Rietveld refinement, and their ionic conductivity was measured using impedance spectroscopy. The materials were found to form a physical mixture. The composites were composed of α-Ca(BH{sub 4}){sub 2}, γ-Ca(BH{sub 4}){sub 2} and orthorhombic LiBH{sub 4}, and the relative phase quantities of the Ca(BH{sub 4}){sub 2} polymorphs varied significantly with LiBH{sub 4} content. The formation of small amounts of orthorhombic CaH{sub 2} and cubic CaH{sub 2} in a CaF{sub 2}-like structure was observed upon heat treatment. Concurrent formation of elemental boron may also occur. The ionic conductivity of the composites was measured using impedance spectroscopy, and was found to be lower than that of ball milled LiBH{sub 4}. Electronic band structure calculations indicate that cubic CaH{sub 2} with hydrogen defects is electronically conducting. Its formation along with the possible precipitation of boron therefore has an effect on the measured conductivity of the LiBH{sub 4}–Ca(BH{sub 4}){sub 2} composites and may increase the risk of an internal short-circuit in the cells. -- Graphical abstract: An Arrhenius plot of the ionic conductivity of the LiBH{sub 4}–Ca(BH{sub 4}){sub 2} composites (red, blue, green). The ionic conductivity of ball milled (gray) and non-milled (black) LiBH{sub 4} is shown for comparison. The filled symbols are measured during heating runs and the empty symbols are measured during subsequent cooling runs. The conductivity of the composites is in all cases higher during cooling, most probably due to the formation of an electronically conducting layer containing defect-rich cubic CaH{sub 2}. Such layer formation could eventually lead to a short circuit in the cell and reveals a general issue of chemical stability that should be attended to in the development of solid electrolyte materials. Highlights: • The LiBH{sub 4}–Ca(BH{sub 4}){sub 2} composite forms a physical mixture rather than a solid solution. • The formation of defect-rich, cubic CaH{sub 2} in a CaF{sub 2}-like structure is observed. • A new layer containing cubic CaH{sub 2} is conducting and may lead to a short-circuit.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Superoxide (Electro)Chemistry on Well-Defined Surfaces in Organic Environments

Efficient chemical transformations in energy conversion and storage systems depend on understanding superoxide anion (O 2 – ) electrochemistry at atomic and molecular levels. Here, in this work, a combination of experimental and theoretical techniques are used for rationalizing, and ultimately understanding, the complexity of superoxide anion (electro)chemistry in organic environments. By exploring the O 2 + e – ↔ O 2 – reaction on well-characterized metal single crystals (Au, Pt, Ir), Pt single crystal modified with a single layer of graphene (Graphene@Pt(111)), and glassy carbon (GC) in 1,2 dimethoxyethane (DME) electrolytes, we demonstrate that (i) the reaction is an outer-sphere process; (ii) the reaction product O 2 – can “attack” any part of the DME molecule, i.e., the C–O bond via nucleophilic reaction and the C–H bond via radical hydrogen abstraction; (iii) the adsorption of carbon-based decomposition products and the extent of formation of a “solid electrolyte interface” (“SEI”) increases in the same order as the reactivity of the substrate, i.e., Pt(hkl)/Ir(hkl) » Au(hkl)/GC > Gaphene@Pt(111); and (iv) the formation of the “SEI” layer leads to irreversible superoxide electrochemistry on Pt(hkl) and Ir(hkl) surfaces. In conclusion, we believe this fundamental insight provides a pathway for the rational design of stable organic solvents that are urgently needed for the development of a new generation of reliable and affordable battery systems.

25 ENERGY STORAGE↗

Direct formation of InAs quantum dots grown on InP (001) by solid-source molecular beam epitaxy

We have developed a growth process that leads to the direct formation of self-assembled InAs quantum dots on InP(001) by solid-source molecular beam epitaxy avoiding the previous formation of quantum wires usually obtained by this technique. The process consists of a periodically alternated deposition of In and As correlated with InAs(4x2){r_reversible}(2x4) surface reconstruction changes. Based on the results obtained by in situ characterization techniques, we propose that the quantum dots formation is possible due to the nucleation of In droplets over the InAs(4x2) surface during the In deposition step and their subsequent crystallization under the As step.

36 MATERIALS SCIENCE↗

Localized high-concentration electrolytes get more localized through micelle-like structures

Liquid electrolytes in batteries are typically treated as macroscopically homogeneous ionic transport media despite having a complex chemical composition and atomistic solvation structures, leaving a knowledge gap of the microstructural characteristics. Here, we reveal a unique micelle-like structure in a localized high-concentration electrolyte, in which the solvent acts as a surfactant between an insoluble salt in a diluent. The miscibility of the solvent with the diluent and simultaneous solubility of the salt results in a micelle-like structure with a smeared interface and an increased salt concentration at the centre of the salt–solvent clusters that extends the salt solubility. These intermingling miscibility effects have temperature dependencies, wherein a typical localized high-concentration electrolyte peaks in localized cluster salt concentration near room temperature and is used to form a stable solid–electrolyte interphase on a Li metal anode. Importantly, these findings serve as a guide to predicting a stable ternary phase diagram and connecting the electrolyte microstructure with electrolyte formulation and formation protocols of solid–electrolyte interphases for enhanced battery cyclability.

25 ENERGY STORAGE↗

Probing the Li 4 Ti 5 O 12 Interface Upon Lithium Uptake by Operando Small Angle Neutron Scattering

The formation of a solid–electrolyte interphase (SEI) on the surface of Li 4 Ti 5 O 12 (LTO) has become a highly controversial topic, with arguments for it and against it. However, prior studies supporting the formation of an SEI layer have typically suggested that a layer forms upon cycling of a cell, although the layer is probed after disassembling. In this study, cubic mesostructured LTO is synthesized with crystallite domain sizes between 3 and 4 nm and uniform pores with diameters ≤8 nm. The mean pore size is controlled between 4–8 nm through the use of a triblock amphipathic copolymer with a tunable hydrophobic block as template and by thermal treatment. The LTO morphology obtained is spherical and evolves upon heat treatment. We report these materials show excellent electrochemical performance, including high rate capability and capacity retention. The LTO material is subjected to operando small-angle neutron scattering and X-ray photoelectron spectroscopy experiments, which reveal that the highly debated SEI forms at potentials as high as 2.2 V, first as a LiF-rich layer and subsequently by the growth of a carbonaceous layer. These SEI products form first on the smaller pores before forming on the mesopores.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗