At least 415 records · Page 23

Zeolite-based SCR catalysts and their use in diesel engine emission treatment

A catalyst comprising a zeolite loaded with copper ions and at least one trivalent metal ion other than Al.sup.+3, wherein the catalyst decreases NO.sub.x emissions in diesel exhaust. The trivalent metal ions are selected from, for example, trivalent transition metal ions, trivalent main group metal ions, and/or trivalent lanthanide metal ions. In particular embodiments, the catalysts are selected from Cu--Fe-ZSM5, Cu--La-ZSM-5, Fe--Cu--La-ZSM5, Cu--Sc-ZSM-5, and Cu--In-ZSM5. The catalysts are placed on refractory support materials and incorporated into catalytic converters.

36 MATERIALS SCIENCE↗

Zeolite-based SCR catalysts and their use in diesel engine emission treatment

A catalyst comprising a zeolite loaded with copper ions and at least one trivalent metal ion other than Al.sup.+3, wherein the catalyst decreases NO.sub.x emissions in diesel exhaust. The trivalent metal ions are selected from, for example, trivalent transition metal ions, trivalent main group metal ions, and/or trivalent lanthanide metal ions. In particular embodiments, the catalysts are selected from Cu--Fe-ZSM5, Cu--La-ZSM-5, Fe--Cu--La-ZSM5, Cu--Sc-ZSM-5, and Cu--In-ZSM5. The catalysts are placed on refractory support materials and incorporated into catalytic converters.

36 MATERIALS SCIENCE↗

Ruthenium-lead oxide for acidic oxygen evolution reaction in proton exchange membrane water electrolysis

Developing an active and stable anode catalyst for the proton exchange membrane water electrolyzer (PEM-WE) is a critical objective to enhance the economic viability of green hydrogen technology. However, the expensive iridium-based electrocatalyst remains the sole practical material with industrial-level stability for the acidic oxygen evolution reaction (OER) at the anode. Ruthenium-based catalysts have been proposed as more cost-effective alternatives with improved activity, though their stability requires enhancement. The current urgent goal is to reduce costs and noble metal loading of the OER catalyst while maintaining robust activity and stability. Here, in this study, we design a Ru-based OER catalyst incorporating Pb as a supporting element. This electrocatalyst exhibits an OER overpotential of 201 mV at 10 mA.cm -2 , simultaneously reducing Ru noble metal loading by similar to 40%. Normalization of the electrochemically active surface area unveils improved intrinsic activity compared to the pristine RuO 2 catalyst. During a practical stability test in a PEM-WE setup, our developed catalyst sustains stable performance over 300 h without notable degradation, underscoring its potential for future applications as a reliable anodic catalyst.

Electrocatalysis↗

Monodisperse metal nanoparticle catalysts on silica mesoporous supports: synthesis, characterizations, and catalytic reactions

The design of high performance catalyst achieving near 100% product selectivity at maximum activity is one of the most important goals in the modern catalytic science research. To this end, the preparation of model catalysts whose catalytic performances can be predicted in a systematic and rational manner is of significant importance, which thereby allows understanding of the molecular ingredients affecting the catalytic performances. We have designed novel 3-dimensional (3D) high surface area model catalysts by the integration of colloidal metal nanoparticles and mesoporous silica supports. Monodisperse colloidal metal NPs with controllable size and shape were synthesized using dendrimers, polymers, or surfactants as the surface stabilizers. The size of Pt, and Rh nanoparticles can be varied from sub 1 nm to 15 nm, while the shape of Pt can be controlled to cube, cuboctahedron, and octahedron. The 3D model catalysts were generated by the incorporation of metal nanoparticles into the pores of mesoporous silica supports via two methods: capillary inclusion (CI) and nanoparticle encapsulation (NE). The former method relies on the sonication-induced inclusion of metal nanoparticles into the pores of mesoporous silica, whereas the latter is performed by the encapsulation of metal nanoparticles during the hydrothermal synthesis of mesoporous silica. The 3D model catalysts were comprehensively characterized by a variety of physical and chemical methods. These catalysts were found to show structure sensitivity in hydrocarbon conversion reactions. The Pt NPs supported on mesoporous SBA-15 silica (Pt/SBA-15) displayed significant particle size sensitivity in ethane hydrogenolysis over the size range of 1-7 nm. The Pt/SBA-15 catalysts also exhibited particle size dependent product selectivity in cyclohexene hydrogenation, crotonaldehyde hydrogenation, and pyrrole hydrogenation. The Rh loaded SBA-15 silica catalyst showed structure sensitivity in CO oxidation reaction. In addition, Pt-mesoporous silica core-shell structured NPs (Pt{at}mSiO{sub 2}) were prepared, where the individual Pt NP is encapsulated by the mesoporous silica layer. The Pt{at}mSiO{sub 2} catalysts showed promising catalytic activity in high temperature CO oxidation. The design of catalytic structures with tunable parameters by rational synthetic methods presents a major advance in the field of catalyst synthesis, which would lead to uncover the structure-function relationships in heterogeneous catalytic reactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Infiltrated Sr 0.9 Y 0.1 CoO 2.5+δ nanoparticles as a cathode material for solid oxide fuel cells operated at 450–650 °C

Catalytically active cathode materials are highly desirable for the development of low-temperature solid oxide fuel cells (LT-SOFCs). In the present study, we report the performance of a high-loading Sr 0.9 Y 0.1 CoO 2.5+δ (SYC10) nanoparticles (NPs) as a catalytic cathode infiltrated in Ce 0.8 Gd 0.2 O 2-δ (GDC) backbones for LT-SOFCs and the use of a low-loading SYC10 NPs as a catalyst for promoting the performance of a commercial cathode. The loading and calcination temperature of SYC10 NPs were systematically optimized to achieve the lowest area-specific polarization resistance at ≤650 °C. A significant reduction in polarization resistance of commercial LSCF cathode by SYC NPs has also been demonstrated at 650 °C.

08 HYDROGEN↗

Enhanced Hydrodeoxygenation of m -Cresol over Bimetallic Pt–Mo Catalysts through an Oxophilic Metal-Induced Tautomerization Pathway

Supported bimetallic catalysts consisting of a noble metal (e.g., Pt) and an oxophilic metal (e.g., Mo) have received considerable attention for the hydrodeoxygenation of oxygenated aromatic compounds produced from biomass fast pyrolysis. Here, we report that PtMo can catalyze m-cresol deoxygenation via a pathway involving an initial tautomerization step. In contrast, the dominant mechanism on monometallic Pt/Al 2 O 3 was found to be sequential Pt-catalyzed ring hydrogenation followed by dehydration on the support. Bimetallic Pt 10 Mo 1 and Pt 1 Mo 1 catalysts were found to produce the completely hydrogenated and deoxygenated product, methylcyclohexane (MCH), with much higher yields than monometallic Pt catalysts with comparable metal loadings and surface areas. Over an inert carbon support, MCH formation was found to be slow over monometallic Pt catalysts, while deoxygenation was significant for PtMo catalysts even in the absence of an acidic support material. Experimental studies of m-cresol deoxygenation together with density functional theory calculations indicated that Mo sites on the PtMo bimetallic surface dramatically lower the barrier for m-cresol tautomerization and subsequent deoxygenation. The accessibility of this pathway arises from the increased interaction between the oxygen of m-cresol and the Mo sites in the Pt surface. This interaction significantly alters the configuration of the precursor and transition states for tautomerization. Lastly, a suite of catalyst characterization techniques including X-ray absorption spectroscopy (XAS) and temperature-programmed reduction (TPR) indicate that Mo was present in a reduced state on the bimetallic surface under conditions relevant for reaction. Overall, these results suggest that the use of bifunctional metal catalysts can result in new reaction pathways that are unfavorable on monometallic noble metal catalysts.

09 BIOMASS FUELS↗

New route toward building active ruthenium nanoparticles on ordered mesoporous carbons with extremely high stability

Creating highly active and stable metal catalysts is a persistent goal in the field of heterogeneous catalysis. However, a real catalyst can rarely achieve both of these qualities simultaneously due to limitations in the design of the active site and support. One method to circumvent this problem is to fabricate firmly attached metal species onto the voids of a mesoporous support formed simultaneously. In this study, we developed a new type of ruthenium catalyst that was firmly confined by ordered mesoporous carbons through the fabrication of a cubic Ia3d chitosan-ruthenium-silica mesophase before pyrolysis and silica removal. This facile method generates fine ruthenium nanoparticles (ca. 1.7 nm) that are homogeneously dispersed on a mesoporous carbonaceous framework. This ruthenium catalyst can be recycled 22 times without any loss of reactivity, showing the highest stability of any metal catalysts; this catalyst displays a high activity (23.3 molLAh21 gmetal21 ) during the catalytic hydrogenation of levulinic acid (LA) when the metal loading is 6.1 wt%. Even at an ultralow loading (0.3 wt%), this catalyst still outperforms the most active known Ru/C catalyst. This work reveals new possibilities for designing and fabricating highly stable and active metal catalysts by creating metal sites and mesoporous supports simultaneously.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Hydrodesulfurization Properties of Rhodium Phosphide: Comparison with Rhodium Metal and Sulfide Catalysts

Silica-supported rhodium phosphide (Rh2P/SiO2) catalysts were prepared and characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), 31P solid-state NMR spectroscopy, X-ray photoelectron spectroscopy (XPS), and chemisorption measurements. XRD and TEM analysis of a 5 wt.% Rh2P/SiO2 catalyst confirmed the presence of well-dispersed Rh2P crystallites on the silica support having an average crystallite size of 10 nm. NMR spectroscopy showed unsupported and silica-supported Rh2P to be metallic and XPS spectroscopy yielded a surface composition of Rh1.94P1.00 that is similar to that expected from the bulk stoichiometry. The 5 wt.% Rh2P/SiO2 catalyst exhibited a higher dibenzothiophene (DBT) hydrodesulfurization (HDS) activity than did Rh/SiO2 and sulfided Rh/SiO2 catalysts having a similar Rh loading and was also more active than a commercial NiAMo/Al2O3 catalyst. The Rh2P/SiO2 catalyst showed excellent stability over a 100 h DBT HDS activity measurement and was more S tolerant than the Rh/SiO2 catalyst. The Rh2P/SiO2 catalyst strongly favored the hydrogenation pathway for DBT HDS, while the Rh/SiO2 and sulfided Rh/SiO2 catalysts favored the direct desulfurization pathway.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Pt Particles on a Dynamic TiO 2 Support in Near-Ambient Conditions−Disentangling Size, Pressure, and Support Effects

Platinum particles on reducible oxides are known to form complex and highly dynamic catalyst systems at elevated pressures and temperatures, often adopting active structures that differ from those found at room temperature and under ultrahigh vacuum (UHV). Here, we study the oxidation and structural evolution of subnanometer Pt clusters and nanoparticles supported on rutile TiO 2 (110) across an oxygen pressure range from UHV to 0.1 mbar, using near-ambient pressure X-ray photoelectron spectroscopy (NAP-XPS), scanning tunneling microscopy (STM) under UHV and NAP conditions, and low-energy ion scattering (LEIS). Our results reveal distinct differences in oxidation behavior and thermal stability between Pt nanoparticles and clusters, which are further modulated by the support stoichiometry and oxygen pressure. Small Pt clusters become oxidized even at room temperature but are susceptible to accelerated sintering in 0.1 mbar O 2 at elevated temperatures. In contrast, well-crystallized Pt nanoparticles on near-stoichiometric TiO 2 show weaker oxidation. On a reduced, defective TiO 2 support, Pt instead quickly becomes deeply buried by new titania layers, which are formed during support reoxidation. This process appears to result primarily from interactions of the support with the gas phase, unlike the classical, selflimited encapsulation that is induced by the strong metal−support interaction (SMSI). Finally, we address the full complexity of real catalysts in a direct side-by-side comparison of the single-crystalline model system with a Pt-loaded TiO 2 powder catalyst (P25). We conclude that the stoichiometry of the model supports must be carefully chosen and controlled to accurately reproduce the expected state of powder supports during redox reactions.

metal nanoparticles↗

The effect of PdZn particle size on reverse-water-gas-shift reaction

The effect of PdZn particle size on the catalytic activity of Pd/ZnO catalysts for the reverse-water-gas-shift (RWGS) reaction was studied. The PdZn particle size was varied by adjusting Pd loading and reducing the catalysts at different temperatures. XRD and IR spectroscopy characterization confirmed the absence of metallic Pd on the catalyst surface. Consequently, the effect of PdZn alloy particle size on the RWGS reaction can be unambiguously studied without the complication of reactions catalyzed by metallic Pd. The results indicated that the turnover frequency increases as the PdZn crystallite size decreases. Interestingly, this structure relationship between PdZn particle size and RWGS activity is consistent with that previously observed for the steam reforming of methanol, i.e., higher CO selectivity on smaller PdZn particles. Thus, RWGS has been identified as a likely potential reaction pathway to undesired CO formation in methanol steam reforming on Pd/ZnO catalysts for hydrogen production.

08 HYDROGEN↗

Highly dense atomic Fe–Ni dual metal sites for efficient CO 2 to CO electrolyzers at industrial current densities

Carbon-supported, atomically dispersed, nitrogen-coordinated metal sites (e.g., Fe and Ni) are arguably the most promising catalysts for the electrochemical reduction of CO 2 to CO due to their unique catalytic properties and the use of earth-abundant elements. However, conventional single metal sites are constrained by their structural simplicity, causing either too weak or too strong absorption/desorption of multiple critical intermediates (e.g., *COOH and *CO). Current catalysts also suffer from ultra-low loadings (<1.0 wt%) of atomic metal active sites in catalysts, leading to inadequate performance for CO 2 -to-CO conversion. Here, we develop dual Ni/Fe metal site catalysts with significantly increased atomically dispersed metal loadings (up to 4.8 wt%). A gas-phase chemical vapor deposition (CVD) approach to introducing single Ni sites was integrated with Fe 2 O 3 /ZIF-8 precursors, followed by an optimal thermal activation. The optimized CVD-Ni/Fe–N–C catalyst exhibited remarkable electrocatalytic performance for the CO 2 reduction to CO in a continuous membrane-electrode-assembly electrolyzer, achieving a maximum CO faradaic efficiency (FE CO ) of 96% at a current density of 700 mA cm −2 in a near-neutral electrolyte. Furthermore, a desirable but challenging acidic flow-cell electrolyzer was designed using this dual metal site catalyst to improve CO 2 utilization, accomplishing a FE CO of up to 95% at a CO partial current density close to 600 mA cm −2 . Density functional theory (DFT) calculations suggest a synergetic effect between Fe–Ni pairs facilitating *COOH intermediate formation and *CO desorption simultaneously during CO 2 to CO conversion. This is key to breaking the linear scaling relationship of conventional single-metal site catalysts during the CO 2 reduction reaction.

36 MATERIALS SCIENCE↗

Highly Active, Durable Dispersed Iridium Nanocatalysts for PEM Water Electrolyzers

One of the primary challenges for proton exchange membrane (PEM) electrolyzers is the sluggish kinetics of the oxygen evolution reaction (OER) at the anode, which requires the use of precious metals or metal oxides, such as iridium (Ir) or iridium oxide (IrO x ), as the OER catalyst. This study introduces a one-pot surfactant-free polyol reduction method to disperse iridium nanoparticles on a tungsten doped titanium oxide (W x Ti 1-x O 2 ) support. The polyol reduction approach for the Ir/W x Ti 1-x O 2 catalyst synthesis was systematically investigated to determine the influence of synthesis parameters on the catalysts’ physical properties, and its electrochemical activity and durability. The most promising synthesized catalyst with 38 wt% Ir (Ir 38% /W x Ti 1-x O 2 ) demonstrated five times higher mass activity than an Ir-black baseline (the industry standard catalyst) based on rotating-disk electrode (RDE) studies. When tested in a real water electrolyzer system, the synthesized catalyst enabled the Ir loading to be lowered by an order of magnitude while retaining a similar electrolyzer performance found for the baseline Ir-black catalyst. In conclusion, the Ir 38% /W x Ti 1-x O 2 catalyst also demonstrated remarkable stability, e.g., only small voltage (<20 mV) increase was observed during a 1200-hour durability test at a constant current density of 1500 mA/cm 2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High aspect ratio catalytic reactor and catalyst inserts therefor

The present invention relates to high efficient tubular catalytic steam reforming reactor configured from about 0.2 inch to about 2 inch inside diameter high temperature metal alloy tube or pipe and loaded with a plurality of rolled catalyst inserts comprising metallic monoliths. The catalyst insert substrate is formed from a single metal foil without a central supporting structure in the form of a spiral monolith. The single metal foil is treated to have 3-dimensional surface features that provide mechanical support and establish open gas channels between each of the rolled layers. This unique geometry accelerates gas mixing and heat transfer and provides a high catalytic active surface area. The small diameter, high aspect ratio tubular catalytic steam reforming reactors loaded with rolled catalyst inserts can be arranged in a multi-pass non-vertical parallel configuration thermally coupled with a heat source to carry out steam reforming of hydrocarbon-containing feeds. The rolled catalyst inserts are self-supported on the reactor wall and enable efficient heat transfer from the reactor wall to the reactor interior, and lower pressure drop than known particulate catalysts. The heat source can be oxygen transport membrane reactors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Advantages of MgAlOx over gamma-Al2O3 as a support material for potassium-based high temperature lean NOx traps

MgAlOx mixed oxides were employed as supports for potassium-based lean NOx traps (LNTs) targeted for high temperature applications. Effects of support compositions, K/Pt loadings, thermal aging and catalyst regeneration on NOx storage capacity were systematically investigated. The catalysts were characterized by XRD, NOx-TPD, TEM, STEM-HAADF and in-situ XAFS. The results indicate that MgAlOx mixed oxides have significant advantages over conventional gamma-Al2O3-supports for LNT catalysts, in terms of high temperature NOx trapping capacity and thermal stability. First, as a basic support, MgAlOx stabilizes stored nitrates (in the form of KNO3) to much higher temperatures than mildly acidic gamma-Al2O3. Second, MgAlOx minimizes Pt sintering during thermal aging, which is not possible for gamma-Al2O3 supports. Notably, combined XRD, in-situ XAFS and STEM-HAADF results indicate that Pt species in the thermally aged Pt/MgAlOx samples are finely dispersed in the oxide matrix as isolated atoms. This strong metal-support interaction stabilizes Pt and minimizes the extent of sintering. However, such strong interactions result in Pt oxidation via coordination with the support so that NO oxidation activity can be adversely affected after aging which, in turn, decreases NOx trapping ability for these catalysts. Interestingly, a high-temperature reduction treatment regenerates essentially full NOx trapping performance. In fact, regenerated Pt/K/MgAlOx catalyst exhibits much better NOx trapping performance than fresh Pt/K/Al2O3 LNTs over the entire temperature range investigated here. In addition to thermal aging, Pt/K loading effects were systemically studied over the fresh samples. The results indicate that NOx trapping is kinetically limited at low temperatures, while thermodynamically limited at high temperatures. A simple conceptual model was developed to explain the Pt and K loading effects on NOx storage. An optimized K loading, which allows balancing between the stability of nitrates and exposed Pt surface, gives the best NOx trapping capability.

Environmental Molecular Sciences Laboratory↗

Transformation of Active Sites in Fe/SSZ-13 SCR Catalysts during Hydrothermal Aging: A Spectroscopic, Microscopic, and Kinetics Study

Fe/SSZ-13 catalysts (Si/Al = 12, Fe loadings 0.37% and 1.20%) were prepared via solution ion-exchange, and hydrothermally aged at 600, 700 and 800 C. The fresh and aged catalysts were characterized with surface area/pore volume analysis, Mössbauer, solid-state MAS NMR, NO titration FTIR spectroscopies, and TEM and APT imaging. Hydrothermal aging causes dealumination of the catalysts, and transformation of various Fe sites. The latter include conversion of free Fe2+ ions to dimeric Fe(III) species, the agglomeration of isolated Fe-ions to Fe-oxide clusters, and incorporation of Al into the Fe-oxide species. These changes result in complex influences on standard SCR and NO/NH3 oxidation reactions. In brief, mild aging causes catalyst performance enhancement for SCR, while harsh aging at 800 C deteriorates SCR performance. In comparison to Fe/zeolites more prone to hydrothermal degradation, this study demonstrates that via the utilization of highly hydrothermally stable Fe/SSZ-13 catalysts, more accurate correlations between various Fe species and their roles in SCR related chemistries can be made. The authors gratefully acknowledge the US Department of Energy (DOE), Energy Efficiency and Renewable Energy, Vehicle Technologies Office for the support of this work. The research described in this paper was performed in the Environmental Molecular Sciences Laboratory (EMSL), a national scientific user facility sponsored by the DOE’s Office of Biological and Environmental Research and located at Pacific Northwest National Laboratory (PNNL). PNNL is operated for the US DOE by Battelle.

Environmental Molecular Sciences Laboratory↗

Active Site Dynamics in Molybdenum-Based Silica-Supported Olefin Metathesis Catalysts: Site Renewal and Decay Beyond the Chauvin Cycle

Heterogeneous olefin metathesis catalysts exhibit low active site densities and unpredictable kinetics due to dynamic active site formation and decay processes. Here, in this study, we establish a quantitative framework that captures active site generation, renewal, and decay in olefin metathesis over silica-supported molybdenum oxide catalysts, enabling a mechanistic explanation of catalytic behavior and strategies to achieve high, stable activity. Steady-state active site titrations reveal that 2,3-dimethyl-butene isomers (4MEs) cofeeding increases active site density by up to 4.3-fold, directly correlating with enhanced metathesis rates. Spectroscopic studies demonstrate that 4MEs facilitate Mo(VI) reduction to Mo(IV) and interact strongly with surface Si–OH groups, generating labile protons that promote active site formation via a 1,2-proton shift mechanism. Kinetic modeling indicates that ethylene acts as a decay promoter, shifting kinetic control away from the Chauvin cycle and suppressing metathesis activity. Comparative studies on catalysts with varying Mo loading reveal that promotion is most effective for dispersed molybdate species, with a decline at higher Mo loadings. These findings provide a unified mechanistic framework for heterogeneous olefin metathesis, offering new strategies to enhance active site accessibility, mitigate deactivation, and optimize catalyst design.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Domain Structures of Ni and NiFe (Oxy)Hydroxide Oxygen-Evolution Catalysts from X-ray Pair Distribution Function Analysis

Ni-Fe (oxy)hydroxides, Ni( i-z )Fe z O x H y , are among the fastest-known water oxidation catalysts in alkaline media on a per-cation basis. At current densities relevant for electrolysis (e.g., >0.5 A/cm( -2 )), mass and electron transport through catalyst films with high mass loading are critical and depend substantially on the extended and intermediate catalyst architecture. We use X-ray pair distribution function (PDF) analysis to determine the intermediate nanostructures of electrodeposited Ni( i-z )Fe z O x H y films. We report the effects of electrodeposition technique (pulsed versus continuous), electrochemical cycling, and Fe content on the structure of the catalyst film. The PDF patterns for Ni( i-z )Fe z O x H y films are best simulated by model structures consisting of brucite-like β-Ni(OH) 2 fragments 1 to 3 layers in thickness. Only the oxidation state of the film significantly affects the intralayer scattering behavior (i.e., metal-oxygen bond distance). The interlayer interactions, however, are affected by Fe content and deposition conditions. The domain size of many of the systems are similar, extending to similar to ~5 nm, which are best modeled by sheets containing upward of similar to ~250 metal cations. Smaller domains were found for films deposited through a larger number of electrochemical cathodic current pulses. Films can be cycled between as-deposited, oxidized, and reduced states, with minimal loss of intrasheet coherence, indicating a degree of structural stability. We estimate heterogeneity in the domain structures by modeling the PDF data to linear combinations of oxyhydroxide fragments with different sizes and numbers of layers.

36 MATERIALS SCIENCE↗