Search NASA⌕ Search

SEARCH · Search NASA

Results for “cathode electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 415 records · Page 23

Role of Electrolyte in Overcoming the Challenges of LiNiO 2 Cathode in Lithium Batteries

LiNiO 2 (LNO) is a high-capacity and model cathode first discovered in the 1980s that fell out of favor due to its intrinsic instabilities. However, research activities toward LNO are once again on the rise as the push for higher-energy-density cells marches on. Here we demonstrate here that with appropriate modern electrolytes, major performance improvements can be achieved with LNO with no additional modifications. Cells with a localized high concentration electrolyte (LHCE) deliver 92% capacity retention after 200 cycles compared with 56% capacity retention in a baseline carbonate electrolyte, maintain 94% capacity after high-voltage storage compared with 77% capacity, and display a higher onset temperature of thermal runaway of 244 °C compared with 188 °C. These improvements are attributed to the LHCE’s high oxidative stability and its formation of fluorine-rich interphases. Although further characterization of this new class of electrolyte is necessary, this work demonstrates that modern electrolytes can be drop-in enablers of high-capacity, long-cycle-life cells.

25 ENERGY STORAGE↗

Designing a hybrid electrode toward high energy density with a staged Li + and PF 6 - deintercalation/intercalation mechanism

Existing lithium-ion battery technology is struggling to meet our increasing requirements for high energy density, long lifetime, and low-cost energy storage. Here, a hybrid electrode design is developed by a straightforward reengineering of commercial electrode materials, which has revolutionized the “rocking chair” mechanism by unlocking the role of anions in the electrolyte. Our proof-of-concept hybrid LiFePO 4 (LFP)/graphite electrode works with a staged deintercalation/intercalation mechanism of Li + cations and PF 6 - anions in a broadened voltage range, which was thoroughly studied by ex situ X-ray diffraction, ex situ Raman spectroscopy, and operando neutron powder diffraction. Introducing graphite into the hybrid electrode accelerates its conductivity, facilitating the rapid extraction/insertion of Li + from/into the LFP phase in 2.5 to 4.0 V. This charge/discharge process, in turn, triggers the in situ formation of the cathode/electrolyte interphase (CEI) layer, reinforcing the structural integrity of the whole electrode at high voltage. Consequently, this hybrid LFP/graphite-20% electrode displays a high capacity and long-term cycling stability over 3,500 cycles at 10 C, superior to LFP and graphite cathodes. Importantly, the broadened voltage range and high capacity of the hybrid electrode enhance its energy density, which is leveraged further in a full-cell configuration.

25 ENERGY STORAGE↗

Investigation of the Electrode-Electrolyte Interphase in Ester-Based Electrolytes in NCM523/Graphite Cells

The use of methyl acetate (MA) and methyl propionate (MP) as co-solvents in carbonate/LiPF 6 electrolytes have been investigated in LiNi 0.5 Co 0.2 Mn 0.3 O 2 (NCM523)/graphite cells to improve electrochemical performance at low temperature (−20 °C). Consistent with previous investigations, improved low temperature performance was observed with all electrolyte formulations containing esters. Detailed ex situ surface analysis of the surface films generated with the ester-based electrolytes containing electrolyte additives reveal significant changes to the SEI on graphite upon cycling at moderately elevated temperature (45 °C). In the presence of vinylene carbonate (VC) lithium plating is observed upon cycling at low temperature (−20 °C) which leads to a thicker solid electrolyte interface (SEI) upon cycling at 45 °C. Incorporation of fluoroethylene carbonate (FEC) as an electrolyte additive results in the generation of a thin SEI and alters the structure of the surface film on the NCM523 cathode resulting in stable cycling over a wide temperature range.

Rodrigo, Nuwanthi D. (ORCID:0000000343129536)↗

Electrolyte and Cutoff Potential Effects on Cycle Life of Li4Ti5O12/LiNi0.9Mn0.1O2 Batteries for Behind-the-Meter Storage Applications

Behind-the-Meter Storage (BTMS) is a stationary battery energy storage system that is connected to the electrical distribution system on the customer's side of the utility's service meter. BTMS systems are used to store electrical energy from the grid as well as inconstant, renewable energy, such as local solar and wind generation. A successful BTMS system will allow the customer to pair their energy generation and storage to optimize electrical consumption from the grid, improving reliability and minimizing cost. For BTMS applications, batteries must be designed and optimized with different set of criteria from other leading segments of the Li-ion battery market, like transportation, due the system being stationary and proximal to the residential or commercial building it's benefitting. BTMS applications prioritize safety, cost (low/no-critical materials), reliability (20-year calendar life), and durability (10,000 cycle life), while having the ability to (minimally) compromise energy density and rate capability. Lithium titanate (Li4Ti5O12-, LTO) is a promising anode candidate for BTMS applications due to its high safety and capacity retention, while maintaining a reasonable 160 mAhg-1 reversable capacity and composition of relatively abundant materials. (1) Specifically, LTO has a high working voltage which helps to prevent Li dendrite formation, improving safety. Furthermore, LTO also has negligible lithiation-based volume change, leading to less mechanical pulverization, or loss of active material, upon cycling. For the cathode, materials with little or no Co are of high interest due to the high cost and low abundance of Co. LiMn2O4 (LMO) has been paired with LTO for BTMS applications in the past due to its safety, low cost (abundancy), and reasonably high operating voltage. (2-4) However, the low capacity of LMO limits energy density and specific energy. While not the highest priority for BTMS applications, increasing energy density will enable deployment in space constrained BTMS applications and decrease total cost. LiNi0.9Mn0.1O2 (LN-MO) is a recently developed material with promise due to its high operating voltage and relatively low price. (5) However, Ni-rich layered oxides, including LNMO, tend to struggle with capacity retention during high-voltage cycling due to mechanical pulverization, irreversible phase transitions, and unstable solid-electrolyte interphase. The study presented here focuses on building an understanding of how electrolyte solvent and varied cutoff potentials will impact the cycle life of LTO/LN-MO cells. Specifically, a comparison is provided between ethylene carbonate (EC), ethyl methyl carbonate (EMC), fluoroethylene carbonate (FEC), and Gen2 electrolyte solvents with 1M Lithium hexafluorophosphate (LiPF6) salt, cycling to two upper termination potentials, 2.6V and 2.7V. Electrochemical testing and diagnostics (e.g., differential capacity analysis, area specific impedance, constant voltage hold, and rate capability) and post-mortem characterization will be used to understand the aging behavior and failure mechanisms of the 8 cell combinations (four electrolytes and two voltage cutoffs). Cells with FEC electrolyte showed a lower initial capacity compared to cells with Gen2, EMC, and EC cycling at both voltages; however, the cells with FEC showed consistent trends in capacity retention with 2.6V and 2.7V termination potentials, while the cells with the other electrolytes showed much higher rates of capacity loss when cycling to the higher voltage. These results indicate that FEC may play a role in improving durability of high-voltage, Ni-rich electrode systems for use in high-cycle applications, such as BTMS.

electrolyte↗

Optimized Al Doping Improves Both Interphase Stability and Bulk Structural Integrity of Ni-Rich NMC Cathode Materials

Ni-rich layered transition metal oxide (NMC, LiNi1-x-yMxCoyO2, 1 – x – y = 0.6) is promising for high-energy-density lithium-ion batteries, but its large-scale application is still hindered by several technical challenges, including secondary particle cracking, interfacial instability, and cell degassing during cycling. Here, we report a facile wet-chemical method to modify both the surface and the bulk of the LiNi0.76Mn0.14Co0.10O2 (NMC76) cathode with Al doping to effectively improve the structural/interfacial stability of the cathode, and hence its long-term cycling capability. With only 1 mol% Al doping, the Al-NMC76 electrode delivers a good capacity retention of 79.2% after 500 cycles at a high voltage limit of 4.5 V, which is far better than those of undoped NMC76 under the similar condition. The enhanced performance can be attributed to the Al doping in the NMC76, which not only strengthens the bulk structural stability through doping into the lattice, but also suppresses acidic attack from the electrolyte through altered surface structure of NMC76.

Al doping, capacity retention, high voltage, elect↗

Crack‐Free Single‐Crystalline LiNiO 2 for High Energy Density All‐Solid‐State Batteries

Abstract Single‐crystalline layered oxide (LiNi 1‐ x ‐ y Mn x Co y O 2 ) cathodes have been found to exhibit exceptional electrochemical properties when coupled with various inorganic solid electrolytes (ISEs) in all‐solid‐state batteries (ASSBs). Their advantages stem from the robust morphological integrity with the absence of grain boundaries and the high electrochemical oxidative stability. Here, ASSBs featuring single‐crystalline LiNiO 2 (LNO) with the highest Ni content are reported, offering a high theoretical specific capacity of 275 mAh g ‐1 alongside a high average discharge voltage (3.7 V vs Li + /Li). Through a careful investigation, it is demonstrated that micron‐sized single‐crystalline LNO (µSC‐LNO) composite cathodes with a halide ISE exhibit a high initial discharge capacity of 205 mAh g ‐1 with an outstanding cycle performance over 200 cycles in room‐temperature ASSBs. The significance of engineering parameters is emphasized, such as particle size and specific density, in promoting a homogeneous and fast Li + transport within the composite cathodes. Furthermore, the formation of undesirable interphase between the halide ISE in the cathode and sulfide ISE separator is elucidated, which may be a critical factor impeding long‐term cyclability of ASSBs. This work provides insights into the design of composite cathodes for high‐energy‐density ASSBs.

Chemistry↗

Constructing Robust Electrode/Electrolyte Interphases to Enable Wide Temperature Applications of Lithium-Ion Batteries

The electrolyte generally dictates the working temperature range of lithium ion batteries (LIBs), thus developing new class of electrolytes (primarily functional additives) in LIBs for wide temperature applications will be quite essential for further development of LIBs for electric vehicle market. In this study, we develop new functional electrolytes containing multiple additives to enable the LIBs to perform well in a wide temperature range from -40°C to 60°C. Importantly, those cells based on the above optimized electrolytes have been proven to behave significantly enhanced discharging performance at -40°C, the long-term cycling stability at 25°C (more than 85% of capacity retention after 1000 cycles at 1C/1C rates in 1 Ah pouch cells), as well as the obviously improved cycling stability at 60°C. These remarkable cell performances originate from the highly conductive, uniform and compact passivating films formed on both anode and cathode surfaces by the synergistic effects of the multiple additives. Our finding on the synergistic benefits originating from certain additive combination in the optimized electrolytes would favorably widen the working temperature range of future high-performance LIBs.

Lithium ion battery, electrolyte, additive, electr↗

Influence of Binder Coverage on Interfacial Chemistry of Thin Film LiNi 0.6 Mn 0.2 Co 0.2 O 2 Cathodes

In this work, we explore the influence of binder coverage and chemistry on the interfacial properties of the textured Ni-rich cathode LiNi 0.6 Mn 0.2 Co 0.2 O 2 . We find that the formation of the cathode/electrolyte interphase (CEI) composition varies significantly for cathodes coated with either poly(vinylene fluoride) (PVDF), carboxymethyl cellulose (CMC), or lithium polyacrylate (LiPAA) after cycling to high upper cutoff voltages (4.5 V vs Li/Li). The PVDF-coated samples had a thinner CEI and twice the relative concentration of LiF and Li 2 CO 3 to Li x PO y F z species in the CEI compared to the uncoated sample. This correlated with significantly lower interfacial impedance (285 vs ~1700 Ohm-cm 2 ) and improved capacity retention between cycles of the PVDF-coated samples compared to the other binder compositions and the uncoated sample. CMC-coated samples performed worst, with a CEI comprised of greater amounts of Li x PO y F z . In addition, we find the choice of binder results in the selective protection or promotion of electrolyte reactions at the (104) surface of the 622 cathode. This suggests that the choice of binder can impact the surface chemistry and performance of high voltage cathodes and supports an avenue for interest in multifunctional binders for stabilizing the CEI.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Rational Electrolyte Design for Elevated-Temperature and Thermally Stable Lithium-Ion Batteries with Nickel-Rich Cathodes

As the energy density of lithium-ion batteries (LIBs) increases, the shortened cycle life and the increased safety hazard of LIBs are drawing increasing concerns. To address such challenges, a series of localized high-concentration electrolytes (LHCEs) based on a solvating-solvent mixture of tetramethylene sulfone and trimethyl phosphate and a high flash-point diluent 1H,1H,5H-octafluoropentyl 1,1,2,2-tetrafluoroethyl ether were designed. The LHCEs exhibited non-flammability and greatly suppressed heat release at high temperatures, which would potentially improve the safety performance of the LIBs. Moreover, the optimal LHCE achieved capacity retentions of 87.1% and 81.7% in graphite||LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells after 500 cycles at 25 °C and 45 °C, respectively, which were significantly better than the conventional electrolyte, whose capacity retentions were only 75.2% and 38.5% under the same condition. Mechanistic studies revealed that the LHCE not only formed a more robust solid electrolyte interphase, but also exhibited improved anodic stability, compared with the conventional electrolyte. Further, this work sheds light in rational electrolyte design for high energy density LIBs with high battery performance and low safety concerns.

25 ENERGY STORAGE↗

Lithium‐Containing Hybrid SEI Layer Enabling High Mass Loading and Anode‐Less Sodium Metal Batteries

Abstract The continuous rupturing and rebuilding of unstable solid electrolyte interphase (SEI) layer during cycling would block Na + diffusion and induce Na dendrite formation, ultimately limiting the practical application of high‐energy‐density sodium metal batteries. Herein, a hybrid SEI layer containing Li‐species is dexterously constructed on the surface of sodium metal anode. Li‐containing inorganic components (Li 3 N, LiF, and Li 2 CO 3 ) are introduced to stabilize the Na/electrolyte interface and enhance the mechanical and diffusion kinetic properties of the SEI layer, which can reduce the side reactions and gas generation, regulate Na + flux during cycling and promote rapid Na + migration for uniform dendrite‐free Na deposition. As a result, the constructed Na symmetric cells achieve low overpotential and long cycle life of 5900, 1800, and 500 h at current densities of 3, 10, and 30 mA cm −2 , respectively. Furthermore, the full cells paired with the Na₃V₂(PO₄)₃ cathode demonstrate high specific capacity and excellent cycle stability, even at an ultra‐high cathode loading of 39.3 mg cm −2 and a low N/P ratio (negative/positive electrode capacity ratio of 1.21).

Xia, Li [State Key Laboratory of Physical Chemistr↗

Glass-fiber-reinforced polymeric film as an efficient protecting layer for stable Li metal electrodes

With numerous reports on protecting films for stable lithium (Li) metal electrodes, the key attributes for how to construct these efficient layers have rarely been fully investigated. Here, we report a rationally designed hybrid protective layer (HPL) with each component aligning with one key attribute; i.e., cross-linked poly(dimethylsiloxane) (PDMS) enhances flexibility, polyethylene glycol (PEG) provides homogeneous ion-conducting channels, and glass fiber (GF) affords mechanical robustness. A significant improvement of the electrochemical performance of HPL-modified electrodes can be achieved in Li/HPL@Cu half cells, HPL@Li/HPL@Li symmetric cells, and HPL@Li/LiFePO 4 full cells. Even with an industrial standard LiFePO 4 cathode (96.8 wt % active material), the assembled cell still exhibits a capacity retention of 90% after 100 cycles at 1 C. More importantly, the functionality of each component has been studied comprehensively via electrochemical and physical experiments and simulations, which will provide useful guidance on how to construct efficient protective layers for next-generation energy storage devices.

25 ENERGY STORAGE↗

Effects of Anion Mobility on Electrochemical Behaviors of Lithium–Sulfur Batteries

The electrolyte is a crucial component of lithium-sulfur (Li-S) batteries, as it controls polysulfide dissolution, charge shuttling processes, and solid-electrolyte interphase (SEI) layer formation. Experimentally, the overall performance of Li-S batteries varies with choice of solvent system and Li-salt used in the electrolyte, and a lack of predictive understanding about the effects of individual electrolyte components inhibits the rational design of electrolytes for Li-S batteries. Here we analyze the role of the counter anions of common Li salts (such as TfO-, FSI-, TFSI-, and TDI-) when dissolved in DOL/DME (1:1 vol.) for use in Li-S batteries. The evolution of ion-ion and ion-solvent interactions due to vari-ous anions was analyzed using 17O NMR and pulsed-field gradient (PFG) NMR and then correlated with electrochemi-cal performance in Li-S cells. These data reveal that the for-mation of the passivation layer on the anode and the loss of active materials from the cathode (evidenced by polysulfide dissolution) are related to anion mobility and affinity with lithium polysulfide, respectively. For future electrolyte de-sign, anions with lower mobility and weaker interactions with lithium polysulfides may be superior candidates for increasing the long-term stability of Li-S batteries.

25 ENERGY STORAGE↗

Lithium‐Containing Hybrid SEI Layer Enabling High Mass Loading and Anode‐Less Sodium Metal Batteries

The continuous rupturing and rebuilding of unstable solid electrolyte interphase (SEI) layer during cycling would block Na + diffusion and induce Na dendrite formation, ultimately limiting the practical application of high-energy-density sodium metal batteries. Herein, a hybrid SEI layer containing Li-species is dexterously constructed on the surface of sodium metal anode. Li-containing inorganic components (Li 3 N, LiF, and Li 2 CO 3 ) are introduced to stabilize the Na/electrolyte interface and enhance the mechanical and diffusion kinetic properties of the SEI layer, which can reduce the side reactions and gas generation, regulate Na + flux during cycling and promote rapid Na + migration for uniform dendrite-free Na deposition. As a result, the constructed Na symmetric cells achieve low overpotential and long cycle life of 5900, 1800, and 500 h at current densities of 3, 10, and 30 mA cm −2 , respectively. Furthermore, the full cells paired with the Na₃V₂(PO₄)₃ cathode demonstrate high specific capacity and excellent cycle stability, even at an ultra-high cathode loading of 39.3 mg cm −2 and a low N/P ratio (negative/positive electrode capacity ratio of 1.21).

Diffusion kinetic↗

Self-healing SEI enables full-cell cycling of a silicon-majority anode with a coulombic efficiency exceeding 99.9%

Despite active developments, full-cell cycling of Li-battery anodes with >50 wt% Si (a Si-majority anode, SiMA) is rare. The main challenge lies in the solid electrolyte interphase (SEI), which when formed naturally (nSEI), is fragile and cannot tolerate the large volume changes of Si during lithiation/delithiation. An artificial SEI (aSEI) with a specific set of mechanical characteristics is henceforth designed; we enclose Si within a TiO 2 shell thinner than 15 nm, which may or may not be completely hermetic at the beginning. In situ TEM experiments show that the TiO 2 shell exhibits 5× greater strength than an amorphous carbon shell. Void-padded compartmentalization of Si can survive the huge volume changes and electrolyte ingression, with a self-healing aSEI + nSEI. The half-cell capacity exceeds 990 mA h g -1 after 1500 cycles. To improve the volumetric capacity, we further compress SiMA 3-fold from its tap density (0.4 g cm -3 ) to 1.4 g cm -3 , and then run the full-cell battery tests against a 3 mA h cm -2 LiCoO 2 cathode. Despite some TiO 2 enclosures being inevitably broken, 2× the volumetric capacity (1100 mA h cm -3 ) and 2× the gravimetric capacity (762 mA h g -1 ) of commercial graphite anode is achieved in stable full-cell battery cycling, with a stabilized areal capacity of 1.6 mA h cm -2 at the 100th cycle. The initial lithium loss, characterized by the coulombic inefficiency (CI), is carefully tallied on a logarithmic scale and compared with the actual full-cell capacity loss. In conclusion, it is shown that a strong, non-adherent aSEI, even if partially cracked, facilitates an adaptive self-repair mechanism that enables full-cell cycling of a SiMA, leading to a stabilized coulombic efficiency exceeding 99.9%.

25 ENERGY STORAGE↗

Engineering Solid Electrolyte Interphase Composition by Assessing Decomposition Pathways of Fluorinated Organic Solvents in Lithium Metal Batteries

Studies have shown fluorinated electrolyte solvents can form desirable solid electrolyte interphase (SEI) in lithium metal batteries. In this study, we develop a detailed mechanistic understanding of two high performing electrolytes, Fluoroethylene Carbonate (FEC) and Difluoroethylene Carbonate (DFEC) to demonstrate minimal structural variations can lead to different decomposition products, and thereby the nature of the SEI. Using density functional theory (DFT) calculations, we find different initial bond-breaking mechanisms between FEC and DFEC. We develop free energy diagrams for the decomposition pathways including both electrochemical and chemical steps. Using the computational Li electrode, we identify the largest limiting potential of 1.77 V for FEC decomposition, associated with the formation of lithium fluoride, lithium oxide and FEC oligomers, and 1.53 V for DFEC, which correspond to the formation of polymerized vinylene carbonate and lithium fluoride. We suggest the formation of oligomers in the case of FEC instead of long polymers may lead to better SEI compactness. We also demonstrate the SEI components of FEC and DFEC are not stable on typical cathode voltage (3.87 V). This study presents a unified electrocatalytic perspective on SEI formation and decomposition.

25 ENERGY STORAGE↗

Identification of efficient and stable solid-solid electrochemical interfaces for Li-S batteries. Final Report

The objective of this work is to develop a better understanding of the interactions between battery components that drive the observed battery performance. Using computational tools at the atomistic level, we elucidate molecular, crystal, and amorphous structures, interfacial structures and reactions, and electrochemical behavior. We focus on Li metal anodes, liquid electrolytes, solid electrolytes, S cathodes, and metal-oxide cathodes, and their corresponding interfaces. Within liquid electrolytes, we study their bulk structure and dynamics, as a function of salt concentration. The analysis allows to understand the formation of localized high concentrated regions as the solvent is substituted by a weakly interacting diluent species. Analysis of the electron distribution yields the reactive behavior at interfaces. Moreover, we employ tools that allow the characterization of ion and electron transport at interfaces, during the processes of solvation and desolvation occurring while cycling. For Sulfur cathodes we elucidate synthesis processes and the role of carbon-sulfur and nitrogen-sulfur interactions not only to provide electronic conductivity but also to define alternative reaction pathways during discharge of Li-S batteries. Full-cell simulations offer new insights regarding the integration of all the battery components. Our studies also include solid electrolytes and their interfaces with Li metal, S-C, and metal-oxide electrodes.

25 ENERGY STORAGE↗

3D Artificial Solid-Electrolyte Interphase for Lithium Metal Anodes Enabled by Insulator–Metal–Insulator Layered Heterostructures

Despite considerable efforts to prevent lithium (Li) dendrite growth, stable cycling of Li metal anodes with various structures remains extremely difficult due to the direct contact of the liquid electrolyte with Li. Rational design of solid-electrolyte interphase (SEI) for 3D electrodes is a promising but still challenging strategy for preventing Li dendrite growth and avoiding lithium–electrolyte side reactions in Li-metal batteries. Here, a 3D architecture is constructed with g-C 3 N 4 /graphene/g-C 3 N 4 insulator–metal–insulator sandwiched nanosheets to guide uniform Li plating/stripping in the van der Waals gap between the graphene and the g-C 3 N 4 , and the function of which can be regarded as a 3D artificial SEI. Li deposition on the surface of g-C 3 N 4 is suppressed due to its insulating nature. However, its uniform lithiophilic sites and nanopore channels enable homogeneous lithium plating between the graphene and the g-C 3 N 4 , prohibiting the direct contact of the electrolyte with the Li metal. The use of the g-C 3 N 4 -layer-modified 3D anode enables long-term Li deposition with a high Coulombic efficiency and stable cycling of full cells under high cathode loading, limited Li excess, and lean electrolyte conditions. The concept of a 3D artificial SEI will shed light on developing safe and stable Li-metal anodes.

25 ENERGY STORAGE↗