Workability of High-Strength Automobile Steel at High Temperatures Using Hot Processing Maps and Electron Backscatter Diffraction

Hot deformation behavior of a high-strength steel Docol 1500 Bor was investigated by compression tests on a thermal–mechanical simulator Gleeble 3500. The workability of tested steel was analyzed by building processing maps at three strains based on the test results of flow stresses. The essential deformation mechanism was further studied based on the deformation texture analysis on a scanning electronic microscope with a TSL-OIM™EBSD system. It was found that that strain can affect the workability of the tested steel remarkably. At the engineering strain of 0.6, obvious textures in martensite mainly include recrystallization textures <110>//ND and other texture components <110>//RD and {001} <100>, etc. Dynamic recrystallization and recrystallization texture component <111>//ND in deformed austenite can contribute to increasing the workability of a steel Docol 1500 Bor. Finally, the optimized deformation conditions of the tested steel were obtained.

36 MATERIALS SCIENCE↗

Multimodal Analysis of Spatially Heterogeneous Microstructural Refinement and Softening Mechanisms in Three-Pass Friction Stir Processed Al4Si Alloy

Multiple thermally and thermomechanically induced microstructural refinement mechanisms can be activated in metallic alloys when subjected to solid phase processing methods such as friction stir processing (FSP). In this work, we provide detailed descriptions of the relationship between region-specific microstructural refinement mechanisms and the variation in microhardness, through a systematic and multimodal microstructural characterization of an FSP-processed 75% cold-rolled Al-4 at.% Si model binary alloy. Spatially resolved high-energy synchrotron X-ray diffraction, electron backscattered diffraction, and scanning transmission electron microscopy were used to understand the spatially heterogeneous microstructural evolution due to FSP. Results provide insights into how mechanisms such as static recovery, static recrystallization, dynamic recovery and recrystallization, geometric and continuous dynamic recrystallization, and particle-stimulated static or dynamic grain nucleation may occur heterogeneously in the microstructure as a function of the distance from the stir zone in processed alloys, directly influencing the degree of softening. The systematic analysis of microstructures and hardness in the FSP-processed model binary alloy given in this work highlights the rich microstructural domains that can be uniquely harnessed through solid phase processing of metallic alloys.

Al4Si, Friction Stir Processing, Geometric Dynamic↗

Neutron irradiation-enhanced grain growth in tungsten and tungsten alloys

Herein, to understand the microstructural stability of candidate plasma-facing materials under fusion-relevant environments, neutron irradiation of W and W-3%Re alloys with and without K and La dopants was performed in the mixed-spectrum High Flux Isotope Reactor at nominal temperatures of ~850 °C and ~1100 °C to calculated doses between 0.42 and 0.47 dpa. To the best of our knowledge, this study presents the first experimental evidence of radiation-enhanced recrystallization in W and undoped W–Re alloys at ~850 °C, conditions where thermal annealing does not cause any grain growth in a similar timescale. Potassium- or lanthanum-doped tungsten alloys showed more resistance to radiation-enhanced grain growth. We explain the acceleration of grain growth by analyzing the self-diffusion constant under atomic displacement environments. The microstructural observations of the studied W variants suggest that La doping is more effective than K doping for mitigating recrystallization. This study also found that radiation-enhanced recrystallization is an important consideration when designing and applying W to plasma-facing components in future nuclear fusion reactors.

36 MATERIALS SCIENCE↗

Synthesis of hexagonal wurtzite Cu{sub 2}ZnSnS{sub 4} prisms by an ultrasound-assisted microwave solvothermal method

Wurtzite Cu{sub 2}ZnSnS{sub 4} (CZTS) hexagonal prisms were synthesized by a simple ultrasound-microwave solvothermal method. The product was characterized by XRD, FESEM, EDS, TEM, Raman and UV–vis spectrometer. The hexagonal prisms were 0.5–2 μm wide and 5–12 μm long. The PVP played an important role in the formation of the CZTS hexagonal prisms. In addition, the ultrasound-assisted microwave process was helpful for synthesis of wurtzite rather than kesterite phase CZTS. A nucleation–dissolution–recrystallization mechanism was also proposed to explain the growth of the CZTS hexagonal prisms. - Graphical abstract: Wurtzite Cu{sub 2}ZnSnS{sub 4} hexagonal prisms were synthesized by ultrasound-microwave solvothermal method. The ultrasound-assisted microwave process and PVP were useful to the growth of CZTS. A nucleation–dissolution–recrystallization growth mechanism was also proposed. - Highlights: • Wurtzite Cu{sub 2}ZnSnS{sub 4} was prepared by ultrasound-assisted microwave solvothermal method. • The wurtzite CZTS hexagonal prisms are demonstrated a band gap of 1.49 eV. • Synergistic effect of ultrasound and microwave is helpful to prepare Wurtzite CZTS. • PVP plays an important role in the formation of the CZTS hexagonal prisms. • Nucleation–dissolution–recrystallization growth mechanism of the CZTS was proposed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Hot deformation behavior of 7150 aluminum alloy during compression at elevated temperature

Hot compression tests of 7150 aluminum alloy were preformed on Gleeble-1500 system in the temperature range from 300 deg. C to 450 deg. C and at strain rate range from 0.01 s{sup -1} to 10 s{sup -1}, and the associated structural changes were studied by observations of metallographic and transmission electron microscope. The results show that the true stress-true strain curves exhibit a peak stress at a critical strain, after which the flow stresses decrease monotonically until high strains, showing a dynamic flow softening. The peak stress level decreases with increasing deformation temperature and decreasing strain rate, which can be represented by a Zener-Hollomon parameter in the hyperbolic-sine equation with the hot deformation activation energy of 229.75 kJ/mol. In the deformed structures appear the elongated grains with serrations developed in the grain boundaries, decreasing of Z value leads to more adequate proceeding of dynamic recrystallization and coarser recrystallized grains. The subgrains exhibit high-angle sub-boundaries with a certain amount of dislocations and large numbers of dynamic precipitates in subgrain interiors as increasing Z value. The dynamic recovery and recrystallization are the main reasons for the flow softening at low Z value, but the dynamic precipitates and successive dynamic particles coarsening have been assumed to be responsible for the flow softening at high Z value.

36 MATERIALS SCIENCE↗

Microstructure and nanohardness distribution in a polycrystalline Zn deformed by high strain rate impact

Polycrystalline Zn with an average grain size of about 300 {mu}m was deformed by direct impact Hopkinson pressure bar at a velocity of 29 m/s. An inhomogeneous grain structure was found consisting of a center region having large average grain size of 20 {mu}m surrounded by a fine-grained rim with an average grain size of 6 {mu}m. Transmission electron microscopy investigations showed a significant dislocation density in the large-grained area while in the fine-grained rim the dislocation density was negligible. Most probably, the higher strain yielded recrystallization in the outer ring while in the center only recovery occurred. The hardening effect of dislocations overwhelms the smaller grain size strengthening in the center part resulting in higher nanohardness in this region than in the outer ring. - Graphical Abstract: (a): EBSD micrograph showing the initial microstructure of polycrystalline Zn that was subsequently submitted to high strain rate impact. (b): an inhomogeneous grain size refinement was obtained which consists of a central coarse-grained area, surrounded by a fine-grained recrystallized rim. The black arrow points to the disc center. Research Highlights: {yields} A polycrystalline Zn specimen was submitted to high strain rate impact loading. {yields} Inhomogeneous grain refinement occurred due to strain gradient in impacted sample. {yields} A fine-grained recrystallized rim surrounded the coarse-grained center of specimen. {yields} The coarse-grained center exhibited higher hardness than the fine-grained rim. {yields} The higher hardness of the center was caused by the higher dislocation density.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and texture evolution of AZ31 alloy containing trace levels of strontium

The effect of low levels of Sr (0.01, 0.03, 0.05 wt.%) on the microstructure, mechanical properties and texture of AZ31 magnesium alloy has been investigated. Thermodynamic modeling has been used to study the effect of Sr on phase precipitation at different temperatures. Cooling curve analysis reveals a decrease in solidification superheat with the addition of 0.03 wt.% Sr to AZ31. The as-cast microstructures of the alloys have been studied using optical microscopy (OM) and electron probe micro analysis (EPMA). Results show the refining effect of Sr on the grain size and on the {beta}-Mg{sub 17}Al{sub 12} precipitates through growth poisoning and inoculation, respectively. To investigate the mechanical properties of the alloys, as-cast samples were compression tested at elevated temperatures. Hot compression peak stress ({sigma}{sub max}) and critical strain before recrystallization ({epsilon}{sub c}) initially drop but then increase. {sigma}{sub max} first decreases due to the depletion of Al from solid solution and then increases when the amount of the Al-Sr precipitates reach a significant amount. {epsilon}{sub c} drops due to the acceleration of dynamic recrystallization kinetics as a result of grain refinement. It increases with increasing Sr when the concentration Sr in solid solution is increased leading to dislocation pinning and retardation of recrystallization. X-ray texture measurements on the hot compressed and extruded samples show a decrease in maximum intensity of the basal pole figures with increasing Sr as a result of reduced twining and the changes in Al and Sr concentrations in solid solution. - Research Highlights: {yields} Microstructures/precipitates of AZ31+trace levels of Sr were examined by OM and EPMA. {yields} Thermodynamic calculations and cooling curve analysis were used to predict ppt formation. {yields} It has been shown that Sr refines the grains and Mg17Al12 precipitates. {yields} Mechanical properties and texture were studied using hot compression and X-ray diffraction. {yields} Different micro-mechanisms were responsible for mechanical and texture changes.

36 MATERIALS SCIENCE↗

Characteristic of copper matrix simultaneously reinforced with nano- and micro-sized Al{sub 2}O{sub 3} particles

The effect of the simultaneous presence of nano- and micro-sized Al{sub 2}O{sub 3} particles on the microstructure and properties of copper matrix was the object of this study. The mixture of inert gas-atomized prealloyed copper powder (with 1 wt.% Al) and 0.6 wt.% commercial Al{sub 2}O{sub 3} powder (serving as micro-sized particles) was used as the starting materials. Strengthening of the copper matrix was performed by treating the powders in the air for up to 20 h in the planetary ball mill. During milling of the prealloyed powder, finely dispersed nano-sized Al{sub 2}O{sub 3} particles were formed in situ by internal oxidation. The approximate size of these particles was between 30 and 60 nm. The highest values of microhardness were reached in compacts processed from 10 h-milled powders. The microhardness of compact obtained from 10 h-milled powder was 3 times higher than the microhardness of compact processed from as-received and non-milled prealloyed powder. At the maximum microhardness the grain size reaches the smallest value as a result of the synergetic effect of nano- and micro-sized Al{sub 2}O{sub 3} particles. Recrystallization, which occurred during prolonged milling, was the main factor influencing the decrease in microhardness. The increase in electrical conductivity of compacts after 15 h of milling is the result of the decrease in microhardness and activated recrystallization processes. Highlights: Black-Right-Pointing-Pointer Copper matrix was reinforced with nano- and micro-sized Al{sub 2}O{sub 3} particles. Black-Right-Pointing-Pointer The twofold role of coarse Al{sub 2}O{sub 3} particles in matrix strengthening exists. Black-Right-Pointing-Pointer During shorter milling time these particles contribute to increase of microhardness. Black-Right-Pointing-Pointer At longer milling time decrease in microhardness is related to recrystallization.

36 MATERIALS SCIENCE↗

Microstructural characterization in dissimilar friction stir welding between 304 stainless steel and st37 steel

In the present study, 3 mm-thick plates of 304 stainless steel and st37 steel were welded together by friction stir welding at a welding speed of 50 mm/min and tool rotational speed of 400 and 800 rpm. X-ray diffraction test was carried out to study the phases which might be formed in the welds. Metallographic examinations, and tensile and microhardness tests were used to analyze the microstructure and mechanical properties of the joint. Four different zones were found in the weld area except the base metals. In the stir zone of the 304 stainless steel, a refined grain structure with some features of dynamic recrystallization was evidenced. A thermomechanically-affected zone was characterized on the 304 steel side with features of dynamic recovery. In the other side of the stir zone, the hot deformation of the st37 steel in the austenite region produced small austenite grains and these grains transformed to fine ferrite and pearlite and some products of displacive transformations such as Widmanstatten ferrite and martensite by cooling the material after friction stir welding. The heat-affected zone in the st37 steel side showed partially and fully refined microstructures like fusion welding processes. The recrystallization in the 304 steel and the transformations in the st37 steel enhanced the hardness of the weld area and therefore, improved the tensile properties of the joint. - Highlights: Black-Right-Pointing-Pointer FSW produced sound welds between st37 low carbon steel and 304 stainless steel. Black-Right-Pointing-Pointer The SZ of the st37 steel contained some products of allotropic transformation. Black-Right-Pointing-Pointer The material in the SZ of the 304 steel showed features of dynamic recrystallization. Black-Right-Pointing-Pointer The finer microstructure in the SZ increased the hardness and tensile strength.

36 MATERIALS SCIENCE↗

Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel

An Fe-6.5 wt.% Si-0.3 wt.% Al as-cast sheet was produced by twin-roll strip casting process, then treated with hot rolling, warm rolling and annealing. A detailed study of the microstructure and texture evolution at different processing stages was carried out by optical microscopy, X-ray diffraction and electron backscattered diffraction analysis. The initial as-cast strip showed strong columnar grains and pronounced < 001 >//ND texture. The hot rolled and warm rolled sheets were characterized by large amounts of shear bands distributed through the thickness together with strong < 110 >//RD texture and weak < 111 >//ND texture. After annealing, detrimental < 111 >//ND texture almost disappeared while beneficial (001)<210 >, (001)<010 >, (115)<5 − 10 1 > and (410) < 001 > recrystallization textures were formed, thus the magnetic induction of the annealed sheet was significantly improved. The recrystallization texture in the present study could be explained by preferred nucleation and grain growth mechanism. - Highlights: • A high silicon as-cast strip with columnar structure was produced. • A thin warm rolled sheet without large edge cracks was obtained. • Microstructure and texture evolution at each stage were investigated. • Beneficial (001)<210 >, (001)<010 >, (410)<001 > recrystallization textures were formed. • The magnetic induction of annealed sheet was significantly improved.

36 MATERIALS SCIENCE↗

Effect of the pre-existing carbides on the grain boundary network during grain boundary engineering in a nickel based alloy

Grain boundary engineering was carried out on an aging-treated nickel based Alloy 690, which has precipitated carbides at grain boundaries. Electron backscatter diffraction technique was used to investigate the grain boundary networks. Results show that, compared with the solution-annealed samples, the aging-treated samples with pre-existing carbides at grain boundaries need longer duration or higher temperature during annealing after low-strain tensile deformation for forming high proportion of low-Σ coincidence site lattice grain boundaries (more than 75%). The reason is that the primary recrystallization is inhibited or retarded owing to that the pre-existing carbides are barriers to grain boundaries migration. - Highlights: • Study of GBE as function of pre-existing GB carbides, tensile strain and annealing • Recrystallization of GBE is inhibited or retarded by the pre-existing carbides. • Retained carbides after annealing show the original GB positions. • More than 80% of special GBs were formed after the modification of GBE processing. • Multiple twinning during recrystallization is the key process of GBE.

36 MATERIALS SCIENCE↗

Abnormal grain growth in AISI 304L stainless steel

The microstructural evolution during abnormal grain growth (secondary recrystallization) in 304L stainless steel was studied in a wide range of annealing temperatures and times. At relatively low temperatures, the grain growth mode was identified as normal. However, at homologous temperatures between 0.65 (850 °C) and 0.7 (900 °C), the observed transition in grain growth mode from normal to abnormal, which was also evident from the bimodality in grain size distribution histograms, was detected to be caused by the dissolution/coarsening of carbides. The microstructural features such as dispersed carbides were characterized by optical metallography, X-ray diffraction, scanning electron microscopy, energy dispersive X-ray analysis, and microhardness. Continued annealing to a long time led to the completion of secondary recrystallization and the subsequent reappearance of normal growth mode. Another instance of abnormal grain growth was observed at homologous temperatures higher than 0.8, which may be attributed to the grain boundary faceting/defaceting phenomenon. It was also found that when the size of abnormal grains reached a critical value, their size will not change too much and the grain growth behavior becomes practically stagnant. - Highlights: • Abnormal grain growth (secondary recrystallization) in AISI 304L stainless steel • Exaggerated grain growth due to dissolution/coarsening of carbides • The enrichment of carbide particles by titanium • Abnormal grain growth due to grain boundary faceting at very high temperatures • The stagnancy of abnormal grain growth by annealing beyond a critical time.

36 MATERIALS SCIENCE↗

Annealing texture of nanostructured IF steel

In the present work, the evolution of annealing texture in nanostructured interstitial free steel fabricated via accumulative roll bonding (ARB) process was investigated. Textural evolution after post-annealing of ARB-processed samples was evaluated using X-ray diffraction. There were several texture transitions in the γ-fiber and ζ-fiber during ARB and post-annealing treatment. It was found that with increasing the number of ARB cycles, the volume fraction of the low angle grain boundary decreased and the high angle grain boundary fraction increased. Also, the shear texture was dominant after the first cycle, while for other samples, the rolling texture was dominant. The one-cycle sample clearly indicated a weak α-fiber and γ-fiber and a relatively strong ζ-fiber. In addition, during the recrystallization and before the grain growth, the intensity of α-fiber and γ-fiber decreased, the intensity of ζ-fiber increased, and the intensity of (011)〈100〉 orientation in the ε-fiber and η-fiber increased. Moreover, it was concluded that the transition from the rolling texture to the shear one was a sign of occurrence of the recrystallization (before the grain growth). Finally, with increasing the number of ARB cycles, the intensity of rolling and shear textures saturated and a stable texture formed. - Highlights: • There were texture transitions in the γ-fiber and ζ-fiber. • When the number of cycles increased, the low angle grain boundaries decreased. • The shear texture was dominant after the first cycle. • Transition from rolling texture to shear one was a sign of recrystallization. • With increasing the number of ARB cycles, a stable texture formed.

36 MATERIALS SCIENCE↗

Effect of wheel speed and annealing temperature on microstructure and texture evolution of Ni{sub 45}Mn{sub 36.6}In{sub 13.4}Co{sub 5} ribbon

Ni{sub 45}Mn{sub 36.6}In{sub 13.4}Co{sub 5} magnetic shape memory alloy was successfully produced as preferentially textured ribbon by melting spinning with different wheel speed. X-ray diffraction (XRD) and electron back scatter diffraction (EBSD) were used to study structure and texture evolution of these melt-spun ribbons. The thickness of melt-spun ribbon is 42 μm, 65 μm and 30 μm depending on wheel speed of 1 0 m/s, 15 m/s and 20 m/s, respectively. Density of α fiber texture (〈100〉//ND) vary with wheel speed changes, and is most intensive in the ribbon with wheel speed of 15 m/s. Grains of the ribbons grow after being annealed at 873 K, 973 K, 1073 K and 1173 K, recrystallization was not observed in ribbons after being annealed at 873 K but occurred in ribbons after being annealed at higher temperatures. The α fiber texture becomes weaker to some extent after annealing at different temperatures, due to new recrystallization texture formed at the process of annealing. - Highlights: •Sectional part of shape memory ribbon is firstly investigated by EBSD method. •Thickness and texture of ribbons vary with wheel speed. •Annealing temperature affect texture and microstructure evolution greatly. •Recrystallization textures were observed in ribbons after being annealed.

36 MATERIALS SCIENCE↗

Electron backscatter and X-ray diffraction studies on the deformation and annealing textures of austenitic stainless steel 310S

We studied the texture evolution of thermo-mechanically processed austenitic stainless steel 310S. This alloy was cold rolled up to 90% reduction in thickness and subsequently annealed at 1050 °C. At the early stages of deformation, strain-induced martensite was formed from deformed austenite. By increasing the deformation level, slip mechanism was found to be insufficient to accommodate higher deformation strains. Our results demonstrated that twinning is the dominant deformation mechanism at higher deformation levels. Results also showed that cold rolling in unidirectional and cross rolling modes results in Goss/Brass and Brass dominant textures in deformed samples, respectively. Similar texture components are observed after annealing. Thus, the annealing texture was greatly affected by texture of the deformed parent phase and martensite did not contribute as it showed an athermal reversion during annealing. Results also showed that when the fraction of martensite exceeds a critical point, its grain boundaries impeded the movement of austenite grain boundaries during annealing. As a result, recrystallization incubation time would increase. This caused an incomplete recrystallization of highly deformed samples, which led to a rational drop in the intensity of the texture components. - Highlights: •Thermo-mechanical processing through different cold rolling modes can induce different textures. •Martensite reversion is athermal during annealing. •Higher fraction of deformation-induced martensite can increase the annealing time required for complete recrystallization. •Annealing texture is mainly influenced by the deformation texture of austenite.

36 MATERIALS SCIENCE↗

Hot-worked microstructure and hot workability of cold-work tool steels

Highlights: • Hot compression tests were conducted for D2 and an 8% Cr steel. • Processing maps were constructed for the evaluation of their hot workability. • They had similar hot workability concerning the flow instability. • The 8% Cr steel exhibited a larger resistance to dynamic recrystallization. - Abstract: The hot workability of two cold-work tool steels were evaluated and compared. A D2 and an advanced alloy based on 8% Cr steels (TDx) were deformed at high temperatures between 900 and 1100 °C with strain rates 0.001–10 s{sup − 1} via hot compression test. From the flow curves, processing maps were constructed based on the dynamic material model. The deformed microstructures were observed and compared in various scales with respect to the deformation conditions. Although the two alloys exhibited a large similarity in the flow instability consideration of the processing map, their behavior in microstructure evolution was different. While both alloys exhibited a tendency of strain localization in the conditions of instability, the efficiency of power dissipation in the processing maps showed an intricate correlation with the progress of dynamic recrystallization and carbide precipitation. TDx showed a distinctive behavior of carbide precipitation and a larger resistance to dynamic recrystallization, which implied a requirement on more delicate control of hot working conditions.

36 MATERIALS SCIENCE↗

Influence of differential speed rolling ratio on the ridging behavior of ultra purified 17%Cr ferritic stainless steel

Highlights: • Differential rolling process improves ridging resistance of ferritic stainless steel. • Texture orientation inhomogeneity were attributed to non-uniform deformation. • Shear bands results in homogeneous deformation and recrystallization nucleation. • Uniform recrystallization grains and random orientation grains were obtained. - Abstract: The effect of the differential speed rolling on the ridging resistance and the crystallographic texture evolution of ultra purified 17%Cr ferritic stainless steel was investigated in order to select the optimal procedure for improving the surface quality. In the present study, the three different cold rolling processes were carried out: a conventional cold rolling and two different speed ratios asymmetric rolling. In the conventional cold rolling, the ridging of ferritic stainless steel was pronounced due to the band-like clusters of grains with similar crystallographic orientations. For differential speed rolling, ridging depth decreased and ridging was less pronounced when a higher different speed ratio was applied. The results show that severe ridging is attributed to the presence of band-like clusters of γ-fiber (<111>//ND) oriented grains. The shear bands introduced by differential speed rolling can enhance the nucleation for recrystallization both in grain interiors and grain boundaries, which can fragment the band-like clusters of similar orientation effectively, promoting the random grain orientation and improving surface quality.

36 MATERIALS SCIENCE↗

Effects of annealing parameters on microstructural evolution of a typical nickel-based superalloy during annealing treatment

Highlights: • Adopting an annealing treatment after deformation can improve the homogeneity of microstructure. • Heterogeneous grains become homogeneous firstly, and then heterogeneous with increasing annealing time. • The optimum annealing parameters are the temperature of 980 °C and the time of 10 min. - Abstract: It is usually one of important goals to obtain the homogeneous microstructure for forgings by hot working, such as hot die forging. However, there is always a large inhomogeneous deformation in die forgings during hot deformation. It often results in an inhomogeneous microstructure of forging due to the different dynamic recrystallization (DRX) fractions and grain sizes in different strain regions. In this study, a method was proposed to improve the homogeneity of deformed microstructure by annealing treatment. The microstructural evolution of a typical nickel-based superalloy during annealing treatment has been investigated. The Optical Microscope (OM), Electron Backscatter Diffraction (EBSD) and Scanning Electron Microscope (SEM) technologies were applied to observe microstructures. It is found that adopting an annealing treatment after deformation can effectively improve the homogeneity of microstructure due to the static recrystallization. There is an incubation period which is not less than 5 min for the occurrence of static recrystallization. The initial heterogeneous grains become homogeneous firstly, and then heterogeneous again when the annealing time is increased from 5 to 30 min. The deformation accelerates the dissolution of delta phase in annealing treatment. The fraction of delta phase decreases at the early stage of annealing whether the temperature exceeds the solution temperature. Based on a comprehensive consideration of all factors, the optimum annealing parameters, which are the temperature of 980 °C and the time of 10 min, have been obtained.

36 MATERIALS SCIENCE↗