Search NASA⌕ Search

SEARCH · Search NASA

Results for “Eutectics”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Microstructural modification of a high-pressure die-cast A380 alloy through friction stir processing and its effect on mechanical properties

Aluminum alloy A380 is one of the major high-pressure die-cast (HPDC) alloys fabricated in the die casting sector. However, microstructural features such as shrinkage and gas porosity, entrapped oxide inclusions, change in the morphology of eutectic Si particles as a function of casting location, and the presence of multiple second phase particulates, especially Fe-bearing phases in HPDC A380 alloy results in limited ductility, thus, affecting its structural application. However, through proper modification of the as-cast microstructure, it is possible to improve the mechanical performance of alloy A380. In this study, we report the effect of friction stir processing (FSP), a well-known severe plastic deformation (SPD) and thermomechanical processing tool for selective microstructural modification, on A380. FSP effectively refines the as-cast microstructure and breaks down the coarse Si particles, creating a homogenized distribution of equiaxed Si particles in the aluminum matrix. Additionally, FSP eliminates porosity that acts as crack initiation sites, leading to improved mechanical strength and ductility.

Friction stir processing, Aluminum alloys, Mechani↗

Exploring Fission–Fusion Synergies to Accelerate Compatibility Understanding

To address the significant commercial interest in fusion energy, it will be necessary to accelerate the compatibility research associated with liquid breeders including Li, eutectic Pb–Li and LiF-BeF 2 (FLiBe) molten salt. Particularly for FLiBe, compatibility understanding is limited especially for fusion relevant materials such as reduced activation ferritic-martensitic steels, SiC and V alloys. The historical knowledge associated with molten salt reactors (MSRs) and recent work to commercialize MSRs can benefit fusion research. Recent experimental and modeling work has improved understanding and this knowledge can be applied to fusion relevant materials. For liquid metals (LMs), the comparisons to Li and Pb–Li are less direct but nevertheless can help guide the pathway toward commercialization. For Pb–Li, Al-rich coatings have been shown to inhibit dissolution and potentially increase operating temperatures. For commercialization, the experience with sensors and on-line cleanup can help guide future developments. Thus, it is worth considering the potential for fission-related research with LMs and molten salts to help accelerate fusion research.

36 MATERIALS SCIENCE↗

A New Recycled Al–Si–Mg Alloy for Sustainable Structural Die Casting Applications

The use of secondary aluminum for structural components in the automotive industry is limited by the high Fe contents in recycled alloys which often result in the formation of brittle β-Al 5 FeSi phase which reduces the ductility of aluminum castings. In this study, a new secondary Al-Si-Mg alloy with high Fe content (about 0.44 wt.%) was developed for die casting applications. Based on thermodynamic modeling, manganese was added to obtain a designed Fe-to-Mn ratio of 2 which successfully suppressed the formation of β-Al 5 FeSi phase, by forming α-Al 15 (Fe,Mn) 3 Si 2 phase with rounded or hexagonal morphology. Additionally, a fine needle-like π-Al 8 FeMg 3 Si 2 phase was also formed within the eutectic regions. The new recycled alloy showed comparable mechanical properties in as-cast and heat treated (T5 and T6) conditions to three major primary die cast alloys (≤ 0.2 wt.% Fe) with similar composition. Ductility up to 7.4% from tensile elongation was achieved in as-cast recycled alloy due to the modification and refinement of α-Al 15 (Fe,Mn) 3 Si 2 by Mn and Sr additions. Tensile elongation was further improved to 9.1% after T6 treatment as a result of dissolution of π-Al 8 FeMg 3 Si 2 phase, defragmentation of α-Al 15 (Fe,Mn) 3 Si 2 and the spheroidization of Si phase. This new alloy provides a promising path for increasing usage of recycled aluminum with high Fe content in structural die castings for automotive and other applications.

36 MATERIALS SCIENCE↗

Strontium Effects on the Formation of Iron-Intermetallic Phases in Secondary Al–9Si–0.6Fe Alloys

The presence and morphology of Fe-containing intermetallic phases affect the mechanical properties of aluminum alloys, especially in secondary Al–Si-based cast alloys. Although strontium (Sr) addition of 50 to 500 ppm is known to refine the needle-type eutectic silicon structure, the influence of Sr on the formation of Fe-intermetallic phases remains unclear. The present work investigates the combined additions of Sr and Mn to Al–9Si–0.6Fe–0.35Mg (All compositions are in wt pct except otherwise stated.) alloys on the formation of Fe-intermetallic phases at different solidification rates from ~ 1.5 to ~ 60 °C/s. Long and branched-type AlFeSi phase with size ranging from 50 to 120 µm are more common when solidified at the rate of 1.5 °C/s regardless of Sr and Mn additions. However, at the fast solidification rate of 60 °C/s, a 60 ppm Sr addition significantly reduced the average length of needle-shaped AlFeSi phase to less than 3 to 5 µm. Thermodynamic simulations have been performed using CALculation of PHAse Diagrams (CALPHAD) models to predict the formation of various phases and their possible interactions during solidification. The results indicated that the combination of a high solidification rate and about 60 ppm of Sr is beneficial to refining the δ-Al 3 FeSi 2 phase in Al–Si–Mg alloys containing 0.6 pctFe. As a result, this unexpected finding of Fe-intermetallic refinement by low Sr addition (~60 ppm) provides an important guide in designing secondary alloys for sustainable casting applications.

36 MATERIALS SCIENCE↗

The Beneficial Effect of Iron in Aluminum-Cerium-Based Cast Alloys

Iron (Fe) has been considered a major impurity since it is detrimental to the mechanical properties of many cast aluminum alloys due to the formation of Fe-containing brittle intermetallic phases. Fe is found naturally as an impurity in bauxite ore, resulting in Fe contamination of aluminum alloys with increasing contamination from current recycling practices. The Al–Ce–Fe system was investigated using CALPHAD (CALculation of PHAse Diagrams) modeling and experimental casting techniques. It was found that additions of Fe to the Al–Ce system are beneficial to the strength (slightly) and ductility (significantly) of the ternary alloys, which is attributed to the formation of fine metastable Al 8 CeFe 2 phase with aggregate morphology and equilibrium Al 10 CeFe 2 phase, suppressing coarse proeutectic Al 11 Ce 3 phase in near-eutectic Al–Ce alloys. Heat treatment study showed that the metastable Al 8 CeFe 2 phase transforms to predicted equilibrium Al 10 CeFe 2 phase at 500 °C, with essentially no intermetallic or grain coarsening; thus, the alloy displayed excellent property retention. The Al–Ce–Fe alloy system offers opportunities for sustainable, recyclable alloy development using low-cost Fe and low-cost cerium (a byproduct of rare-earth extraction).

42 ENGINEERING↗

Phase Selection During Solidification and Solid-State Phase Transformations in an Al-10Ce-8Mn (wt pct) Alloy

In multicomponent Al-Ce alloys, and especially after additive manufacturing (AM), complex and metastable solidification microstructures are frequently observed. Here, in this research, the relationship between solidification conditions and phase selection are explored for an Al-10Ce-8Mn (wt pct) alloy using a systematic study of laser melting conditions. Three solidification modes were observed: primary Al 10 Mn 2 Ce; primary Al 20 Mn 2 Ce; and eutectic FCC Al + Al 20 Mn 2 Ce. These solidification modes were correlated to specific liquid-solid interface velocities using a simple thermal model, showing the change in primary solidification phase for low (< 6.8 × 10 −4 m/s), moderate (between 8.2 × 10 −4 and 5.9 × 10 −2 m/s) and high solidification velocities (> 6.2 x 10 −2 m/s) for the above three solidification microstructures, respectively. These results were rationalized by using interface response function (IRF) theory to describe the solidification undercooling for the possible primary intermetallic phases. The implication of the local phase selection from differing solidification conditions is summarized by a comparison of hardness which demonstrates the potential variance of Vickers hardness from 101 to 242 (VHV) by changing the laser velocity from 1 to 83 mm/s. Interestingly, on heat treatment at 400°C, the decomposition pathways of the solidification microstructure and hardness were also found to be different, thereby opening multiple pathways for spatial microstructure and property control within AM components.

Sisco, Kevin↗

Effects of Post-sintering Annealing on (NdLa)-(FeCo)-B Magnets

A common limitation of La substitutions into (Nd, La) 2 Fe 14 B magnets is the reduction of the anisotropy field (H a ), which decreases magnet coercivity (H cj ). In this study, adding a small amount of Pr-Cu to a La-containing neo magnet may modify the grain boundary (GB), which can help recover a fraction of the degraded H cj . An optimal GB modification requires a carefully designed post-sinter heat treatment, which is the focus of this work on characterizing the effects of multi-step post-sintering annealing on the evolutions of microstructure and magnetic properties. We find that Nd and Cu concentrations at GBs and triple junctions (TJs) increase when the annealing temperatures are lowered. Annealing temperatures of 580°C and 480°C (near rare-earth-rich eutectic temperatures) enabled the development of a thick and continuous GB phase, which helps to magnetically decouple the grains, and, thus, enhance H cj . For the alloy with 25% Nd replaced by La, and with the addition of 7.5 wt.% of Pr 68 Cu 32 as GB modifier, the optimized multi-step post-sinter annealing improved the H cj from 4.8 kOe to 9 kOe.

36 MATERIALS SCIENCE↗

Microstructural Coarsening Kinetics and Mechanical Property Changes in Long-Term Aged Sn–Pb–Sb Solder Joints

Tin-lead-antimony (50Sn–47Pb–3Sb wt.%) soldered assemblies were mechanically tested approximately 30 years after initial production and found to have solder joints of reduced strength. The microstructure of this solder alloy exhibits a ternary eutectic structure with Sn-rich, Pb-rich, and SnSb phases. Accelerated aging was performed to evaluate solder microstructural coarsening and associated strength of laboratory solder joints to correlate these properties to the “naturally aged” solder joints. Isothermal aging was conducted at room temperature, 55, 70, 100, and 135 °C and aging times that ranged from 0.1 to 365 days. The coarsening kinetics of the Pb-rich phase were determined through optical microscopy and image analysis methods established in previous studies on binary Sn–Pb solder. A kinetic equation was developed with time exponent n of 0.43 and activation energy of 24000 J/mol, suggesting grain boundary diffusion or other fast diffusion pathways controlling the microstructural evolution. Compression testing and Vickers microhardness showed significant strength loss within the first 20–30 days after soldering; then, the microstructure and mechanical properties changed more slowly over long periods of time. Further, by combining accelerated aging data and the microstructure-based kinetics, strength predictions were made that match well with the properties of the actual soldered assemblies naturally aged for 30 years. However, aging at the highest temperature of 135 °C produced anomalous behavior suggesting that extraneous aging mechanisms are active. Therefore, data obtained at this temperature or higher should not be used. Overall, the combined microstructural and mechanical property methods used in this study confirmed that the observed reduction in strength of ~ 30-year-old solder joints can be accounted for by the microstructural coarsening that takes place during long-term solid-state aging.

36 MATERIALS SCIENCE↗

Stress relaxation cracking susceptibility evaluation in 347H stainless steel welds

Abstract Stress relaxation cracking (SRC) has been reported as a dominant failure mechanism for 347H stainless steel welds at elevated service temperatures, occurring in either the heat-affected zone (HAZ) or fusion zone (FZ). In this study, SRC susceptibility of physically simulated HAZ and cross-welded E347-347H stainless steel welds was studied using a four-step accelerated SRC test with a thermomechanical physical simulator. The stress and temperature range studied represents weld-induced residual stress at 150–600 MPa and post-weld heat treatment temperatures between 800 and 1050 °C. For all temperature conditions, the cross-welded samples failed at a lower critical stress threshold than the simulated HAZ. A finite element model of a 50.8-mm-thick single-V groove weld was used to generate the residual stress maps induced by a 40-pass welding procedure, which in combination with the experimental threshold stress map predicted potential SRC failure locations. Postmortem microstructural evaluations were performed to identify contributing characteristics to SRC. It was found that HAZ samples exhibited a combination of creep void development, secondary cracks with intergranular fracture near grain boundary carbides, and eutectic phases. FZ samples showed brittle fracture with cracks propagating along straight, non-tortuous interdendritic grain boundaries.

42 ENGINEERING↗

How Cerium and Lanthanum as Coproducts Promote Stable Rare Earth Production and New Alloys

The largest outputs of rare earth mining are the low-value byproducts cerium and lanthanum, which burden rare earth supply chains because they must be separated from more desirable rare earths used in magnet production. Promoting demand for cerium and lanthanum can potentially diversify the economics of rare earth mining and improve supply chain stability for all rare earth elements. A promising avenue for increasing byproduct rare earth element demand is their use in aluminum alloys; an application for cerium and lanthanum offering multiple benefits to manufacturing such as energy reduction and improved throughput. Experimental materials science and economic implications of Al-rare earth element alloys will be discussed. We show that Al–La/Ce alloys have elevated mechanical strength compared to more traditional aluminum alloys, in some formulations can be used without heat treatment, and possess a highly castable eutectic microstructure. This report presents the use of cerium and lanthanum in aluminum alloys as an example of how supply chain focused approaches to technological development can benefit stakeholders at every step in production.

36 MATERIALS SCIENCE↗

Corrosion in Other Liquid Metals (Li, PbLi, Hg, Sn, Ga)

A wide range of liquid metals have been considered for application in nuclear fission and fusion reactors. Liquid mercury (Hg) was tested as a coolant and working fluid for nuclear fission reactors and as a neutron source target. Liquid lithium and lead lithium eutectic (Li and PbLi) have been extensively studied for fusion reactor designs including plasma facing components (PFCs). Liquid tin and gallium (Sn and Ga) have recently gained attention as alternative PFCs due to their low vapor pressure and chemical stability. To enable successful application of these less common liquid metals, corrosion compatibility with containment materials needs to be investigated. For this purpose, this article reviews corrosion behavior and structural material compatibility, including ferrous alloys, refractory metals, and ceramics, by liquid Li, PbLi, Sn, Ga, and Hg.

Jun, Jiheon↗

Liquid metal walls

Here, the plasma performance of fusion devices depends strongly on the chosen wall materials. Solid plasma-facing components (PFCs) are predominantly used in present devices, and are the most investigated candidates for fusion designs. High-Z materials such as tungsten (W) are the leading solid PFC material candidates. To date, a material choice that scales to steady-state reactor conditions has not been identified. Moreover, if plasma transient events such as edge-localized modes and disruptions cannot be altogether avoided or sufficiently mitigated, the projected peak heat and particle loads far exceed the power exhaust capabilities of solids. Liquid metal (LM) PFCs represent an intrinsic self-healing boundary that are both resilient to surface damage from transients, and that could handle high steady-state heat and particle fluxes. Flowing LM PFCs can be designed to remove “slag,” the buildup of material erosion due to plasma-material interactions, including charge exchange sputtering in the main chamber. Further, LM offer the prospect to manage hydrogenic species otherwise retained in the PFCs, which is important from a safety and inventory standpoint. The two most promising LMs are lithium (Li) and tin (Sn), although Sn–Li eutectics may be considered. While Sn offers a higher temperature window with low vapor pressure and low hydrogen retention, Li offers the prospect of enhanced energy confinement and higher acceptable core contamination limits, and this section focuses on Li PFCs. An LM PFC development research program developed LM PFC concepts for a nuclear fusion device via engineering design calculations, single-effect experiments, and staged prototypical experiments. A self-consistent design window was identified with liquid Li flow speeds ~5–10 m/s; plasma contamination was negligible for predicted Li evolution rates. While these preconceptual designs hold promise, there is substantial R&D needed to advance the technical readiness levels of LM PFCs for application to fusion power plants.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Theory-guided design of duplex-phase multi-principal-element alloys

Density-functional theory (DFT) is used to identify phase-equilibria in multi-principal-element and high-entropy alloys (MPEAs/HEAs), including duplex-phase and eutectic microstructures. Here, a combination of composition-dependent formation energy and electronic-structure-based ordering parameters were used to identify a transition from FCC to BCC favoring mixtures, and these predictions experimentally validated in the Al-Co-Cr-Cu-Fe-Ni system. A sharp crossover in lattice structure and dual-phase stability as a function of composition were predicted via DFT and validated experimentally. The impact of solidification kinetics and thermodynamic stability was explored experimentally using a range of techniques, from slow (castings) to rapid (laser remelting), which showed a decoupling of phase fraction from thermal history, i.e., phase fraction was found to be solidification rate-independent, enabling tuning of a multi-modal cell and grain size ranging from nanoscale through macroscale. Strength and ductility tradeoffs for select processing parameters were investigated via uniaxial tension and small-punch testing on specimens manufactured via powder-based additive manufacturing (directed-energy deposition). This work establishes a pathway for design and optimization of next-generation multiphase superalloys via tailoring of structural and chemical ordering in concentrated solid solutions.

36 MATERIALS SCIENCE↗

Multi-scale microstructural investigation of a laser 3D printed Ni-based superalloy

The heterogeneous microstructure of a laser 3D printed Ni-based superalloy was examined at multiple length scales. The sub-millimeter-sized columnar crystal grains are composed of micron-sized cellular colonies. The crystal grains grow in epitaxy with the substrate under the large temperature gradient and high cooling rate. The cell boundaries, decorated with γ/γ' eutectics, μ-phase precipitates and high density of dislocations, show enrichment of γ' forming elements and low-angle misorientations. Dislocations trapped in the intra-cellular regions are characterized as statistically stored dislocations with no detectable contribution to lattice curvature, and are the results of the interaction between dislocations and γ' precipitates.

36 MATERIALS SCIENCE↗

Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing

Required microstructural attributes of an alloy vary with structural applications. The microstructural fine-tuning capability of laser-powder bed fusion (L-PBF) additive manufacturing (AM) enables application specific manufacture of the components. Such manufacture with L-PBF AM requires alloys that exhibit wide processing window and are amenable to multiple deformation mechanisms. However, high hot cracking susceptibility of Al alloys poses a barrier to such printability-performance synergy. In this work we show that an integration of, a) grain refinement through heterogeneous nucleation, and b) eutectic solidification, leads to crack-free parts at wide range of process parameters, microstructural heterogeneity, and hierarchy in the Al-Ni-Ti-Zr alloy. Such an integration targets hot cracking at multiple stages of solidification in L-PBF as opposed to the contemporary alloy design strategies that target hot-cracking at only specific stages of solidification. The Al-Ni-Ti-Zr alloy exhibits excellent printability and a high as-built tensile performance. Due to the wide processing window and amenability to multiple deformation mechanisms, the alloy microstructure and subsequently the performance, can be fine-tuned. Here, such strategy opens the gateway for application-specific manufacture of Al alloys with L-PBF AM and establishes a fundamental shift in current methodologies for design of these alloys for L-PBF AM.

36 MATERIALS SCIENCE↗

Synergy of tensile strength and high cycle fatigue properties in a novel additively manufactured Al-Ni-Ti-Zr alloy with a heterogeneous microstructure

Alloy design strategies in additive manufacturing (AM) to achieve grain refinement and terminal eutectic solidification have been introduced to engineer Al alloys having microstructural hierarchy and heterogeneity. Such alloy design strategies enable crack-free builds with an expanded AM processing window and pushed the strength limit in Al alloys. However, fatigue performance of Al alloys made by AM is restricted by the presence of process induced defects and its stochasticity. In this work, tensile and high cycle fatigue (HCF) behavior of a novel Al-Ni-Ti-Zr alloy with a heterogeneous microstructure is studied in the as-built condition, supplemented by detailed microstructural and mechanical characterization. Excellent strength-ductility synergy of 342 MPa and 16% failure strain achieved in the alloy was associated with the microstructural attributes that pertain to the novel alloy. Additionally, the alloy showed excellent HCF performance with a fatigue endurance limit to ultimate tensile strength ratio of 0.29 in flexural fatigue mode. The study revealed the existence of multiple crack retardation mechanisms and favorable crack propagation pathways through the fine-grained regions which enabled good fatigue performance to the alloy. Further, a probabilistic model has been used to estimate the fatigue life of the alloy as a function of the stochastic microstructure by utilizing the statistical distribution of pores, solid-state inclusions, and grains in the AM Al alloy. Finally, the model parametric trends are consistent with the experimental observations.

36 MATERIALS SCIENCE↗

Hypereutectic Al-Ce-X (X=Mn, Cr, V, Mo, W) alloys fabricated by laser powder-bed fusion

Here, we characterize the microstructures and high-temperature mechanical properties of Al-2Ce and ternary Al-2Ce-1X (at.%) alloys fabricated by laser powder-bed fusion (LPBF), where X = Mn, Cr, V, Mo, and W are slow-diffusing transition metals. All ternary alloys show a hypereutectic microstructure in the as-LPBF state, containing an interconnected network of eutectic Al 11 Ce 3 phases (~10 vol.%) and an additional population of submicron, equiaxed Al 20 CeX 2 primary precipitates (~10 vol.%) which are isomorphous among these five alloys. Similar microstructures are present in arc-melted rods and atomized powders but are coarser due to the slower cooling rates in these processes. The hardness of the as-LPBF ternary Al-Ce-X alloys (1300–1400 MPa) is higher than that of the binary Al-Ce alloy (~1100 MPa) due to the higher volume fraction of strengthening phases. Furthermore, during exposure at 400 °C for up to three months, greater hardness retention is achieved in the ternary Al-Ce-X alloys (65–75%) than in the binary Al-Ce alloy (~55%), which is attributed to the extreme coarsening resistance of the Al 20 CeX 2 precipitates imparted by the very slow-diffusing ternary solute. These coarsening-resistant Al 20 CeX 2 precipitates also substantially improve alloy creep resistance, increasing the threshold stress for dislocation creep at 300°C from ~32 MPa for the binary Al-Ce alloy to ~77–100 MPa for the ternary Al-Ce-X alloys, and at 400°C from <10 MPa for the binary Al-Ce alloy to >40 MPa for the ternary Al-Ce-V alloy.

36 MATERIALS SCIENCE↗