Search NASA⌕ Search

SEARCH · Search NASA

Results for “PITTING CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Study of localized corrosion in aluminum alloys by the scanning reference electrode technique

Localized corrosion in 2219-T87 aluminum (Al) alloy, 2195 aluminum-lithium (Al-Li) alloy, and welded 2195 Al-Li alloy (4043 filler) have been investigated using the relatively new scanning reference electrode technique (SRET). Anodic sites are more frequent and of greater strength in the 2195 Al-Li alloy than in the 2219-T87 Al alloy, indicating a greater tendency toward pitting for the latter. However, the overall corrosion rates are about the same for these two alloys, as determined using the polarization resistance technique. In the welded 2195 Al-Li alloy, the weld bean is entirely cathodic, with rather strongly anodic heat affected zones (HAZ) bordering both sides, indicating a high probability of corrosion in the HAZ parallel to the weld bead.

Danford, M. D.↗

Pitting Propagation Behavior on Low Alloy AISI 4130 (UNS G41300) Steel Exposed to Various Alkali and Alkaline Earth Metal Chlorides

Pit propagation studies were conducted to elucidate whether alkali and alkali earth metal cations such as Na+ and Rb+ present in the form of metal chloride salts such as RbCl affect pitting behavior in distinctly different manner than NaCl. Pit propagation studies were conducted on a low alloy steel using one-dimensional (1-D) pit method over pit depths from 300-1000 µm. LSV and EIS of planar electrodes of 4130 in a range of Cl- solutions were conducted and revealed no detected differences in impedance, open circuit, corrosion potential (Ecorr), passive current density (ipass), and pitting potential (Epit) as a function of salt type. In the case of one-dimensional pits during fast downward scan rates, the saturation potential (Esat) varied as a function of cation identity when pit depths were shallow. Mass transported limited current density also differed with cations in shallow pits when various alkali metal and alkaline metal cations were present. The limiting current density was increased for RbCl relative to NaCl The pit surface potential (Esurf) of activated pit surfaces reached Ecorr prior to establishing a condition where the pit electrolyte surface concentration (Csurf) was less than the critical concentration for active acidified pitting (i.e. Csurf<Ccrit) in this marginally passivating steel. For various Esurf and pit current density (ipit) combinations at constant Csurf where Ccrit< Csurf < Csat, E-log(i) plots were constructed using the method of Tianshu to create IR ohmic voltage corrected Tafel plots for various fixed pit solution concentrations. Under these conditions, the influence of cation identity on charge transfer controlled kinetics indicated slight differences in Tafel behavior where RbCl was slightly more aggressive than NaCl for low alloy steel oxidation. Differences in metal cation identity exert no effect on passive or breakdown on planar electrodes and only effect pit propagation stage in shallow pits.

Demarest, Chalres↗

Synchrotron Infrared Microspectroscopy Study of Film Formation and Breakdown on Copper

This work demonstrates the utility of synchrotron infrared reflectance microspectroscopy (SIRM), in the far and mid IR, for the determination of the composition of electrogenerated surface films formed during the general and localized corrosion of copper in bicarbonate solution. The back-reflection geometry was used. The anodic passivation film formed on copper at 0.2 V, in 0.01 M NaHCO{sub 3} solution consisted mainly of bicarbonate, copper carbonate dihydroxide or malachite [CuCO{sub 3}.Cu(OH){sub 2}], Cu(OH){sub 2}, and possibly some CuO. At higher potentials, the passive film breaks down and localized corrosion occurs leading to the formation of pits. The composition of the surface films inside the pits formed at 0.6 V was found to be essentially the same as that outside but the relative amount of Cu(OH){sub 2} is higher.

36 MATERIALS SCIENCE↗

FY19 Status of the Full Circumference Examination of the Inner Container Closure Weld Region for Selected 3013 DE Containers

One of the main focus areas of the 3013 Surveillance Program is a thorough evaluation of the inner container closure weld region (ICCWR) opened for destructive examination (DE). As part of the protocol to investigate the corrosion in the ICCWR a laser confocal microscope (LCM) is used to perform close visual examination of the surface and measurements of corrosion features on the surface. In FY17, DE containers from FY13 through FY16 were evaluated to select candidates for a full circumference analysis of the ICCWR. In FY18, the selected DE containers for full circumference evaluation (FCE) were processed according to the ICCWR protocol and LCM data collection was completed for the full circumference only for FY15 DE07. In FY19 the remaining DE containers were completed. The ICCWR protocol was completed as follows: (1) the FCE containers were sectioned into quarters and the weld removed to access the ICCWR; (2) a series of images of the ICCWR full circumference were taken using a stereo microscope and assembled into panoramic views; (3) SEM/EDS analysis performed on selected sections showed what is most likely corrosion products on the surface and chlorides randomly dispersed; (4) the presence of chlorides was also confirmed with ion chromatography of citric acid washes, in which FY15 DE07 and FY16 DE05 showed a significant amount of chlorides with FY15 DE08 showing the less amount of chlorides; (5) dye penetrant examination was performed on the interior and exterior surfaces of all the sidewall sections but reveled no relevant indication of surface-breaking defects, (6) finally, as described above, the full circumference examination of the ICCWR by LCM was completed. The three ICCWRs show general and localized corrosion on the surface. However, FY15 DE08 show more areas with agglomerated pits in Zones 2 and 3 than the other two DEs. The major suspect corrosion events were observed for FY15 DE07 on Sections C1 and C2 and for FY15 DE08 on Section C2. These events correspond to suspect cracks or crack-like features identified with a unique name to easily refer to each feature. FY15 DE07 shows a crack-like feature, identified as Acrux, in Section C1 and three features in Section C2 identified as Bellatrix, Cursa Minor and Cursa Major. Acrux and Bellatrix are located at the boundary of Zone 2 and Zone 3. Cursa Minor and Cursa Major are in Zone 2. FY15 DE08 shows two crack-like features, identified as Denebola and Draco, in Section C2. Both features are located at the boundary of Zone 2 and Zone 3. However, gas analysis and statistical evaluation of the gas compositions and pressures via GEST analyses suggest that leakage between the OI and IC volumes was unlikely. Additional characterization and analysis will be performed on the locations where the cracks were found.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

A potentiodynamic study of aluminum-lithium alloys in an aqueous sodium chloride environment

The characteristics of the potentiodynamic curves for Al-Li alloys in 3.5 percent NaCl aqueous solution are explained and the electrochemical parameters of the potentiodynamic technique are correlated to observed pitting and intergranular cracking behavior. It is shown that the oxygen content of the sodium chloride electrolyte plays an important role in the electrochemical behavior of Al-Li alloys. The potentiodynamic behavior of the alloys is found to be insensitive to variation in compositional content and heat treatment, both of which affect the stress-corrosion behavior. Stringer oxide particle attack and random pitting are observed. It is shown that alternate-immersion exposure prior to potentiodynamic polarization may offer a means of assessing susceptibility to stress-corrosion cracking.

Tsao, C.-H. T.↗

Humidity Effects on Pitting of Ground Stainless Steel Exposed to Sea Salt Particles

The effect of relative humidity (RH) on the corrosion of coarse-ground 304 stainless steel exposed for one year under sea salt particles was investigated. Total corrosion damage accumulation was higher at 40% RH than at 76% RH. At 40% RH, pits were numerous and irregularly shaped with a rough, cross-hatched structure. At 76% RH, pits were much fewer in number and ellipsoidal with crystallographically faceted surfaces. Higher E pit resulting from lower [Cl⁻] impeded initiation at 76% RH. Cathodic resource competition likely limited growth and resulted in lower total volume loss. At 40% RH, lower E pit due to higher [Cl⁻] led to initiation of multiple pits supported by discrete cathodes under individual droplets. Despite more cathodic current available at 76% RH, higher damage accumulation at 40% RH was due to lower anodic stability requirements resulting from higher [Cl⁻]. At 76% RH, pitting proceeded with increasing active area at conditions above critical stability, leading to ellipsoidal pits with facets. The cross-hatched morphology at 40% RH was ascribed to growth at the critical stability conditions, driven by constant current through a fixed active area. Small cracks at the 40% RH pits might have been caused by hydrogen environment assisted cracking.

36 MATERIALS SCIENCE↗

The stress corrosion resistance and the cryogenic temperature mechanical properties of annealed Nitronic 60 bar material

Ambient and cryogenic temperature mechanical properties and the ambient temperature stress corrosion properties of annealed, straightened, and centerless ground Nitronic 60 stainless steel alloy bar material are presented. The mechanical properties of longitudinal specimens were evaluated at test temperatures from ambient to liquid hydrogen. The tensile test data indicated increasing strength with decreasing temperature to -196 C. Below liquid nitrogen temperature the smooth tensile and notched tensile strengths decreased slightly while the elongation and reduction of area decreased drastically. The Charpy V-notched impact energy decreased steadily with decreasing test temperature. Stress corrosion tests were performed on longitudinal tensile specimens and transverse C-ring specimens exposed to: alternate immersion in a 3.5% NaCl bath; humidity cabinet; and a 5% salt spray atmosphere. The longitudinal tensile specimens experienced no corrosive attack. Approximately 3/4 of the transverse C-rings exposed to alternate immersion and to salt spray experienced a pitting attack on the top and bottom ends. Additional stress corrosion tests were performed on transverse tensile specimens. No failures occurred in the 90% stressed specimens exposed for 90 days in the alternate immersion and salt spray environments

Montano, J. W. L.↗

A first-principles study of hydrogen surface coverage on δ-Pu (100), (111), and (110) surfaces

Hydriding corrosion of plutonium leads to surface cracking, pitting, and ultimately structural failure. Laboratory experiments demonstrate that hydriding begins on the surface or near the subsurface of plutonium. However, there has not yet been a systematic evaluation of hydrogen surface coverage on plutonium. In this work, we compute the surface energies of the low facet surfaces of face-centered cubic δ-Pu. The adsorption free energies of expected hydrogen structures at low and high coverage are presented along with the likely progression for filling sites as the H 2 partial pressure increases. Implications for near-equilibrium pressure hydride nucleation and non-equilibrium millibar pressure hydriding are discussed.

36 MATERIALS SCIENCE↗

Improving Corrosion Resistance and Corrosive Wear Resistance of Aluminum Alloy Drill Pipe by Surface Nanocrystallization and Micro-arc Oxidation

To improve the corrosion and wear resistance performance of aluminum alloy drill pipes in geological and petroleum drilling applications, a strengthening coating was prepared on the surface of the 2618 aluminum alloy by combining treatment with ultrasonic cold forging technology (UCFT) and micro-arc oxidation (MAO). The effects of the strengthening coating on the corrosion and wear resistance of the aluminum alloy were evaluated by electrochemical and tribological tests. The results demonstrated that the corrosion and wear resistance of the aluminum alloy were improved by the UCFT and MAO technologies, especially the salt corrosion resistance. The corrosion morphology of the strengthening coating primarily included pitting, micro-cracks and NaCl attachment. In addition, the UCFT + MAO composite coating exhibited the best wear performance. The wear rate of the UCFT + MAO composite coating was lower than that of the aluminum alloy by 94%. The results provided support for this excellent surface treatment technology for the corrosion and wear resistance of aluminum alloy drill pipes, and they also present a feasible evaluation method for drill pipes.

36 MATERIALS SCIENCE↗

Halogen Removal from Tritium Gas Streams

Halogen impurities are poisonous and/or corrosive • Poison for catalysts and equipment • Causes pitting in most austenitic stainless steels • Minimized to prevent damage over time • Prone to appear in certain processes • Appear if certain materials degrade (i.e., elastomers, etc.) • Present as trace impurities in a large number of metals and zeolites (<200 ppm)

Angelette, Lucas M.↗

Design of a Borescope for Extravehicular Non-Destructive Applications

Anomalies such as corrosion, structural damage, misalignment, cracking, stress fiactures, pitting, or wear can be detected and monitored by the aid of a borescope. A borescope requires a source of light for proper operation. Today s current lighting technology market consists of incandescent lamps, fluorescent lamps and other types of electric arc and electric discharge vapor lamp. Recent advances in LED technology have made LEDs viable for a number of applications, including vehicle stoplights, traffic lights, machine-vision-inspection, illumination, and street signs. LEDs promise significant reduction in power consumption compared to other sources of light. This project focused on comparing images taken by the Olympus IPLEX, using two different light sources. One of the sources is the 50-W internal metal halide lamp and the other is a 1 W LED placed at the tip of the insertion tube. Images acquired using these two light sources were quantitatively compared using their histogram, intensity profile along a line segment, and edge detection. Also, images were qualitatively compared using image registration and transformation [l]. The gray-level histogram, edge detection, image profile and image registration do not offer conclusive results. The LED light source, however, produces good images for visual inspection by an operator. Analysis using pattern recognition using Eigenfaces and Gaussian Pyramid in face recognition may be more useful.

Bachnak, Rafic↗

Reverse martensitic transformation on the corrosion behavior of a 2304 lean duplex stainless steel

This study investigates the influence of the reverse martensitic transformation on the corrosion behavior of 2304 lean duplex stainless steel (LDSS) at low temperatures (400–600°C). The steel underwent cold rolling, followed by isochronal annealing for 0.5 h. Phase transformations and microstructures were analyzed using X-ray diffraction, scanning electron microscopy, and transmission electron microscopy. Corrosion resistance was evaluated using a syringe cell with cyclic potentiodynamic polarization in 0.6 M NaCl solution and double-loop electrochemical potentiokinetic reactivation in 0.5 M H 2 SO 4 + 0.001 M KSCN solution. A bimodal breakdown potential behavior, associated with either pitting or transpassivity, was observed in the as-received (AR) and samples annealed at 400°C. Pitting in the AR sample was associated with Al–Mg–Si–Ca–O inclusions, while pitting on the samples annealed at 400°C was linked to local reduced passive film resistance. Severe cold rolling enhanced the pitting resistance of 2304 LDSS. Selective electrochemical etching revealed preferential corrosion at phase interfaces and within the austenite phase. Additionally, annealing at 500°C to 600°C led to a marked decrease in pitting resistance and increased sensitization. Electron backscatter diffraction analysis of the corroded pits in the annealed specimens indicated that pits tend to nucleate and grow in α'-martensite/austenite regions. Furthermore, the nanostructure formed during low-temperature reversion, characterized by dislocation-cell martensite with high dislocation density and stacking faults, may adversely affect corrosion resistance due to heterogeneities associated with alloying element redistribution.

36 MATERIALS SCIENCE↗

In-service inspection of radioactive waste tanks at the Savannah River Site - 15410

Liquid radioactive wastes from the Savannah River Site (SRS) separation process are stored in large underground carbon steel tanks. The high level wastes are processed in several of the tanks and then transferred by piping to other site facilities for further processing before they are stabilized in a vitrified or grout waste form. Based on waste removal and processing schedules, many of the tanks, will be required to be in service for times exceeding the initial intended life. Until the waste is removed from storage, transferred, and processed, the materials and structures of the tanks must maintain a confinement function by providing a barrier to the environment and by maintaining acceptable structural stability during design basis events, which include loadings from both normal service and abnormal (e.g., earthquake) conditions. A structural integrity program is in place to maintain the structural and leak integrity functions of these waste tanks throughout their intended service life. In-service inspection (ISI) is an essential element of a comprehensive structural integrity program for the waste tanks at the Savannah River Site (SRS). The ISI program was developed to determine the degree of degradation the waste tanks have experienced due to service conditions. As a result of the inspections, an assessment can be made of the effectiveness of corrosion controls for the waste chemistry, which precludes accelerated localized and general corrosion of the waste tanks. Ultrasonic inspections (UT) are performed to detect and quantify the degree of general wall thinning, pitting and cracking as a measure of tank degradation. The results from these inspections through 2013, for the 27 Type III/IIIA tanks, indicate no reportable in-service corrosion degradation in the primary tank (i.e., general, pitting, or cracking). The average wall thickness for all tanks remains above the manufactured nominal thickness minus 0.25 millimeter and the largest pit identified is approximately 1.70 millimeter deep (i.e., less than 10% through-wall). Improvements to the inspection program were recently instituted to provide additional confidence in the degradation rates. Thickness measurements from a single vertical strip along the accessible height of the primary tank have been used as a baseline to compare historical measurements. Changes in wall thickness and pit depths along this vertical strip are utilized to estimate the rate of corrosion degradation. An independent review of the ISI program methodology, results, and path forward was held in August 2009. The review recommended statistical sampling of the tanks to improve the confidence of the single strip inspection program. The statistical sampling plan required that SRS increase the amount of area scanned per tank. Therefore, in addition to the baseline vertical strip that is obtained for historical comparisons, four additional randomly selected vertical strips are inspected. To date, a total of 104 independent vertical strips along the height of the primary tank have been completed. A statistical analysis of the data indicates that at this coverage level there is a 99.5% confidence level that one of the worst 5% of all the vertical strips was inspected. That is, there is a relatively high likelihood that the SRS inspection program has covered one of the most corroded areas of any of the Type III/IIIA waste tanks. These data further support the conclusion that there are no significant indications of wall thinning or pitting. Random sampling will continue to increase the confidence that one of the worst 5% has been inspected. In order to obtain the additional vertical strips, and minimize budget and schedule impacts, data collection speed for the UT system was optimized. Prior to 2009, the system collected data at a rate of 32 square centimeters per minute. The scan rate was increased to 129 - 160 square centimeters per minute by increasing the scanner step and pixel sizes in the data acquisition set-up. Laboratory testing was utilized to optimize the scan index/pixel size such that the requirements for wall thinning and pit detection were still maintained. SRS continues to evaluate improvements to ultrasonic equipment. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Quantitative assessment of environmental phenomena on maximum pit size predictions in marine environments

Maximum pit sizes were predicted for dilute and concentrated NaCl and MgCl 2 solutions as well as sea-salt brine solutions corresponding to 40% relative humidity (RH) (MgCl 2 -rich) and 76% RH (NaCl-rich) at 25 °C. A quantitative method was developed to capture the effects of various cathode evolution phenomena including precipitation and dehydration reactions. Additionally, the sensitivity of the model to input parameters was explored. Despite one's intuition, the highest chloride concentration (roughly 10.3 M Cl – ) did not produce the largest predicted pit size as the ohmic drop was more severe in concentrated MgCl 2 solutions. Therefore, the largest predicted pits were calculated for saturated NaCl (roughly 5 M Cl – ). Next, it was determined that pit size predictions are most sensitive to model input parameters for concentrated brines. However, when the effects of cathodic reactions on brine chemistry are considered, the sensitivity to input parameters is decreased. Although there was not one main input parameter that influenced pit size predictions, two main categories were identified. Under similar chloride concentrations (similar RH), the water layer thickness (WL), and pit stability product, (i · x) sf , are the most influential factors. When varying chloride concentrations (RH), changes in WL, the brine specific cathodic kinetics on the external surface (captured in the equivalent current density (i eq )), and conductivity (k o ) are the most influential parameters. Finally, it was noted that dehydration reactions coupled with precipitation in the cathode will have the largest effect on predicted pit size, and cause the most significant inhibition of corrosion damage.

54 ENVIRONMENTAL SCIENCES↗

Corrosion Response of Ni-19Cr-5Fe in Molten NaCl-MgCl 2 Salt

Ni-based alloys are strong candidates for use in high-temperature molten salt reactors due to their superior corrosion resistance and mechanical stability compared to stainless steels. In this study, the static corrosion behavior of a Ni-19Cr-5Fe model alloy was systematically evaluated in a purified molten NaCl-MgCl 2 salt at 700°C for 30, 240, and 500 h. Post-exposure analyses were conducted to assess microstructural evolution, corrosion depth, and elemental depletion profiles. Corrosion rates, quantified by chromium depletion depth, followed an inverse power-law trend with increasing exposure time, indicating diffusion-limited kinetics. This trend is attributed to limitations in mass transport in the static salt and to the progressive local depletion of reactive chromium species. Coupled electron backscatter diffraction and energy dispersive X-ray spectroscopy analysis further revealed that the grain boundary character significantly influences corrosion susceptibility: high-angle grain boundaries exhibited pronounced Cr depletion and pitting, while low-angle and Σ3 boundaries remained comparatively resistant. These results offer valuable insight into the role of microstructure in corrosion processes and reinforce the importance of time-dependent material evaluation in molten salt environments relevant to advanced reactor designs.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evaluation of the stress corrosion cracking resistance of several high strength low alloy steels

The stress corrosion cracking resistance was studied for high strength alloy steels 4130, 4340, for H-11 at selected strength levels, and for D6AC and HY140 at a single strength. Round tensile and C-ring type specimens were stressed up to 100 percent of their yield strengths and exposed to alternate immersion in salt water, salt spray, the atmosphere at Marshall Space Flight Center, and the seacoast at Kennedy Space Center. Under the test conditions, 4130 and 4340 steels heat treated to a tensile strength of 1240 MPa (180 ksi), H-11 and D6AC heat treated to a tensile strength of 1450 MPa (210 ksi), and HY140 (1020 MPa, 148 ksi) are resistant to stress corrosion cracking because failures were not encountered at stress levels up to 75 percent of their yield strengths. A maximum exposure period of one month for alternate immersion in salt water or salt spray and three months for seacoast is indicated for alloy steel to avoid false indications of stress corrosion cracking because of failure resulting from severe pitting.

Humphries, T. S.↗

Variation of the Passive Film on Compositionally Concentrated Dual-Phase Al 0.3 Cr 0.5 Fe 2 Mn 0.25 Mo 0.15 Ni 1.5 Ti 0.3 and Implications for Corrosion

The passive film on a dual-phase Al 0.3 Cr 0.5 Fe 2 Mn 0.25 Mo 0.15 Ni 1.5 Ti 0.3 FCC + Heusler (L2 1 ) compositionally concentrated alloy formed during extended exposure to an applied potential in the passive range in dilute chloride solution was characterized. Each phase, with its own distinct composition of passivating elements, formed unique passive films separated by a heterophase interface. High-resolution, surface sensitive characterization enabled chemical analysis of the passive film formed over individual phases. The film formed over the L2 1 phase had a higher concentration of Al, Ni, and Ti, while the film formed over FCC phase was of similar thickness but contained comparatively higher Cr, Fe, and Mo concentrations, consistent with the differences in bulk microstructure composition. The passive film was continuous across phase boundaries and the distribution of passivating elements (Al, Cr, and Ti) indicated both phases were independently passivated. Spatially resolved analysis of the surface chemistry of the dual-phase CCA revealed that the cation with the highest composition in passive film formed on the FCC phase was Cr (52.4 at. pct) and for the L2 1 phase was Ti (53.1 at. pct) despite the bulk concentration of each element being below 20 at. pct in their respective phases. Al, Cr, and Ti were enriched in both phases within the passive film relative to their respective bulk compositions. In parallel studies, single-phase alloys with compositions representative of the FCC and L2 1 phases were synthesized to evaluate the corrosion behavior of each phase in isolation. The corrosion behavior of the dual-phase alloy showed passivity evidenced by a pitting potential of 0.615 V SCE in 0.01 M NaCl. The pitting potential and other electrochemical parameters suggested a combination of behaviors of both single-phase samples, suggesting that the global corrosion behavior may be represented by a composite theory applied to phases, their area fractions, and interphase length. However, the interphase in the dual-phase CCA was a local corrosion initiation site and may limit localized corrosion protectiveness. The alloy design implications for optimization of second phase structure and morphology are discussed.

36 MATERIALS SCIENCE↗

Corrosion of metals and alloys in sulfate melts at 750 C

The corrosion of Ni, Co, Ni-10Cr, Co-21Cr, and IN738 was studied at 750 C in the presence of molten sulfate mixtures (Na2SO4-Li2SO4 and Na2SO4-CoSO4) and in an atmosphere consisting of O2 + 0.12 percent SO2-SO3. The corrosion was observed to be similar for both Na2SO4-Li2SO4 and Na2SO4-CoSO4 melts. The corrosion of Ni and Co took place by the formation of a mixed oxide plus sulfide scale, very similar to the corrosion in SO2 or SO3 alone. The initial stage for the corrosion of Ni-10Cr involved the formation of a thick NiO + Ni3S2 duplex scale, and Cr sulfide was formed during the later stages. A pitting type of morphology was observed for both Co-21Cr and IN738. The pit was Cr sulfide at the beginning, and subsequently the sulfides oxidized to Cr2O3. A base-metal oxide layer was present above the pit, and this was observed to be formed very early in the corrosion process. A mechanism is proposed to explain this. In general, the formation of sulfides appears to be the primary mode of degradation in mixed sulfide melts.

Misra, A. K.↗