Search NASA⌕ Search

SEARCH · Search NASA

Results for “catalyst layer”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Controlled growth of ultrathin Mo 2 C superconducting crystals on liquid Cu surface

Exhibiting thickness-dependent change in the critical temperature (T c ) for the onset of superconductivity, Mo 2 C is an important new member in the family of two-dimensional atomic crystals. Controllable growth in terms of morphology and thickness is necessary to elucidate its intrinsic properties at the 2D limit. Here we demonstrate the chemical vapor deposition of ultrathin Mo 2 C crystals on liquid Cu surface where the morphology of the crystals can be controlled by tuning the carbon supersaturation. A unique staggered carbon vacancy ordering is discovered in Mo 2 C crystals having particular geometries. Thickness engineering of the crystal can be achieved by controlling the thickness of the Cu catalyst layer, which affords a facile route to grow ultrathin 2D samples. Ultrathin Mo 2 C crystals so obtained, have been characterized using aberration corrected scanning transmission electron microscopy annular dark field imaging, where the co-existence of both AA and AB stacking modes is observed. The high crystallinity of the Mo 2 C crystals synthesized in this work is attested by its characteristic sharp superconducting transition.

36 MATERIALS SCIENCE↗

Understanding Carbon Dioxide Transfer in Direct Methanol Fuel Cells Using a Pore-Scale Model

Abstract The gas flow of carbon dioxide from the catalyst layer (CL) through the microporous layer (MPL) and gas diffusion layer (GDL) has great impacts on the water and fuel management in direct methanol fuel cells (DMFCs). This work has developed a liquid–vapor two-phase model considering the counter flow of carbon dioxide gas, methanol, and water liquid solution in porous electrodes of DMFC. The model simulation includes the capillary pressure as well as the pressure drop due to flow resistance through the fuel cell components. The pressure drop of carbon dioxide flow is found to be about two to three orders of magnitude higher than the pressure drop of the liquid flow. The big difference between liquid and gas pressure drops can be explained by two reasons: volume flowrate of gas is three orders of magnitude higher than that of liquid; only a small fraction of pores (<5%) in hydrophilic fuel cell components are available for gas flow. Model results indicate that the gas pressure and the mass transfer resistance of liquid and gas are more sensitive to the pore size distribution than the thickness of porous components. To buildup high gas pressure and high mass transfer resistance of liquid, the MPL and CL should avoid micro-cracks during manufacture. Distributions of pore size and wettability of the GDL and MPL have been designed to reduce the methanol crossover and improve fuel efficiency. The model results provide design guidance to obtain superior DMFC performance using highly concentrated methanol solutions or even pure methanol.

Electrochemistry↗

Statistical Simulation of the Performance and Degradation of a PEMFC Membrane Electrode Assembly

A 1-D MEA Performance model was developed that considered transport of liquid water, agglomerate catalyst structure, and the statistical variation of the MEA characteristic parameters. The model was validated against a low surface area carbon supported catalyst across various platinum loadings and operational conditions. The statistical variation was found to play a significant role in creating noise in the validation data and that there was a coupling effect between movement in material properties with liquid water transport. Further, in studying the low platinum loaded catalyst layers it was found that liquid water played a significant role in the increasing the overall transport losses. The model was then further applied to study platinum dissolution via potential cycling accelerated stress tests, in which the platinum was found to dissolve nearest the membrane effectively resulting in reaction distribution shifts within the layer.

08 HYDROGEN↗

In-Situ through-Plane Measurements of Ionic Potential Distributions in Non-Precious Metal Catalyst Electrode for PEFC

This manuscript presents micro-scale experimental diagnostics and nano-scale resolution X-ray imaging applied to the study of proton conduction in non-precious metal catalyst (NPMC) fuel cell cathodes. NPMC’s have the potential to reduce the cost of the fuel cell for multiple applications. But, NPMC electrodes are inherently thick compared to the convention Pt/C electrode due to the lower volumetric activity. Thus, the electric potential drop through the Nafion across the electrode thickness can yield significant performance loss. Ionomer distributions in the NPMC electrodes with different ionomer loading are extracted from morphological data using nanoscale X-ray computed tomography (nano-XCT) imaging of the cathode. Microstructured electrode scaffold (MES) diagnostics are used to measure the electrolyte potential at discrete points across the thickness of the catalyst layer. When using that apparatus, the electrolyte potential drop, the through-thickness reaction distribution, and the proton conductivity are measured and correlated with the corresponding Nafion morphology and cell performance.

36 MATERIALS SCIENCE↗

Cerium migration during PEM fuel cell assembly and operation

Cerium migration between PEM fuel cell components is influenced by potential-driven mobility, ionic diffusion, and gradients in water content. These factors were investigated in ex situ experiments and in operating fuel cells. Potential-induced migration was measured ex situ in hydrated window cells. Cerium-containing MEAs were also fabricated and tested under ASTs. MEA disassembly and subsequent XRF analysis were used to observe rapid cerium migration during cell assembly and operation. During MEA hot pressing, humidification, and low RH operation at OCV, ionic diffusion causes uniform migration from the membrane into the catalyst layers. During high RH operation at OCV, in-plane cerium gradients arise due to variations in water content. These gradients may diminish the scavenging efficacy of cerium by reducing its proximity to generated radicals.

08 HYDROGEN↗

(Plenary) Electrochemical Diagnostics and Modeling in Developing the PEMFC Cathode

Reducing the use of precious metal in a proton exchange membrane fuel cell is a key challenge in mass commercialization of fuel cell electric vehicles. However, as Pt loadings are reduced, fuel cell performance losses due to mass transport phenomena become more localized to the Pt and ionomer interface. In this paper, we provide an overview of how we use in-situ electrochemical diagnostics and modeling to understand the performance of low-Pt electrodes, identify their key limiting factors, and guide our catalyst layer development. Furthermore, diagnostics used to quantify the local-Pt oxygen transport resistance and the ionomer adsorption on the Pt surface will be discussed.

25 ENERGY STORAGE↗

Modeling Impedance Caused by Ohmic Losses in High Surface Area Carbons in Polymer Electrolyte Fuel Cells

An analytical model for a blocking porous electrode is derived and used to predict how ohmic resistance inside micropores that host catalyst nanoparticles affects impedance. This paper revisits a widely used approach for estimating ionic conductivities of catalyst layers in fuel cells. An interfacial term associated with resistance in micropores is derived and added to the classical expression for the impedance of a blocking porous electrode at low frequency. The revised model predicts a physically realistic rise in the real component of the impedance at low frequency when reasonable pore dimensions and conductivities are used as inputs.

08 HYDROGEN↗

Direct Utilization of Pure and Denatured Ethanol in Metal Supported Solid Oxide Fuel Cells

Metal supported solid oxide fuel cells (MS-SOFC) are integrated with internal reforming catalyst for direct utilization of ethanol to generate electricity. MS-SOFCs are operated up to 500 h at 700°C, with water-ethanol blend fuel using high-purity ethanol and denatured ethanol. Performance and durability with denatured ethanol varies dramatically with the composition of the denaturant. Cells operated with three denatured ethanol fuels containing small amount of methanol, isopropanol, and denatonium benzoate demonstrate similar and relative stable performance after stabilization, suggesting that these fuels are fit for MS-SOFC operation. No or minimum carbon deposits are observed on the high entropy alloy-based reforming catalyst layer. Denatured ethanol containing gasoline and toluene leads to fast degradation. Here, MS-SOFCs are promising for direct utilization of denatured ethanol, offering a path to rapid-start, carbon-neutral operation with widely-available fuels.

30 DIRECT ENERGY CONVERSION↗

Modeling Oxygen Transport in High Surface Area Carbon Supports for Polymer-Electrolyte Fuel Cells

Here, an analytical model for resistance to oxygen transport in air electrodes containing carbon black supports with high surface area was developed by combining a Thiele modulus—effectiveness factor approach at the agglomerate scale (~150 nm) with nanoscale diffusional resistance in carbon micropores/pits (~5 nm). This paper extends an earlier model for transport resistance to platinum nanoparticles on low surface area carbon. Differences in transport resistances between catalyst layers with high and low surface area carbon blacks predicted by the model with reasonable geometric dimensions and physical properties are consistent with experimental observations.

08 HYDROGEN↗

Elucidating the Role of Hydroxide Electrolyte on Anion-Exchange-Membrane Water Electrolyzer Performance

Many solid-state devices, especially those requiring anion conduction, often add a supporting electrolyte to enable efficient operation. The prototypical case is that of anion-exchange-membrane water electrolyzers (AEMWEs), where addition of an alkali metal solution improves performance. However, the specific mechanism of this performance improvement is currently unknown. This work investigates the functionality of the alkali metal solution in AEMWEs using experiments and mathematical models. The results show that additional hydroxide plays a key role not only in ohmic resistance of the membrane and catalyst layer but also in the reaction kinetics. The modeling suggests that the added liquid electrolyte creates an additional electrochemical interface with the electrocatalyst that provides ion-transport pathways and distributes product gas bubbles; the total effective electrochemical active surface area in the cell with 1 M KOH is 5 times higher than that of the cell with DI water. In the cell with 1 M KOH, more than 80% of the reaction current is associate with the liquid electrolyte. These results indicate the importance of high pH of electrolyte and catalyst/electrolyte interface in AEMWEs. The understanding of the functionality of the alkali metal solution presented in this study should help guide the design and optimization of AEMWEs.

25 ENERGY STORAGE↗

Investigation of Membrane Chemical Degradation as a Function of Catalyst Platinum Loading

Membrane chemical degradation is one of many factors that can impact fuel cell durability. Additionally, the fuel cell’s lifetime heavily depends on the membrane and its ability to maintain chemical and mechanical integrity. Previous studies indicate that chemical degradation is due to the formation of hydroxyl radicals that attack the polymer structure resulting in membrane thinning, pinhole formation, and the release of fluoride and sulfate ions. Membrane durability was investigated using ultra-low Pt electrode loadings (≤ 0.1 mg Pt cm -2 ). Accelerated stress testing (US-DOE protocols) demonstrated that the degradation rate was found to increase with higher Pt loadings. This is most likely due to more heterogeneous sites for radical formation due to hydrogen crossover to the cathode. We also explored membrane degradation rates while varying catalyst layer thickness, ionomer to carbon ratio, and types of carbon support. All of the aforementioned variables impact the membrane degradation rates.

25 ENERGY STORAGE↗

Ionomer Optimization for Hydroxide-Exchange-Membrane Water Electrolyzers Operated with Distilled Water: A Modeling Study

The hydroxide-exchange-membrane water electrolyzer (HEMWE) is a promising means to store intermittent renewable energy in the form of hydrogen chemical energy. The hydroxide-exchange ionomer (HEI) in the gas-evolving electrodes and the hydroxide-exchange membrane (HEM) are key components of HEMWE. In this work, we simulate the cell and examine explicitly the impact of HEI and HEM properties with a focus on improving HEMWE performance when operated with distilled water ( i.e ., no supporting electrolyte). The tradeoff between the ionic conductivity gain and electrochemically active surface area (ECSA) loss is studied. For a constant catalyst loading, distributing more catalyst next to the HEM or making thinner but denser catalyst layer is beneficial for HEMWE performance. The results demonstrate that a higher water diffusion coefficient is desired for HEM to supply reactant water to the cathode. In contrast, a lower water diffusion coefficient is preferred for the cathode HEI to retain the water in the regions with high reaction rates. Overall, the findings provide important insights to optimizing HEI/HEM materials for improved HEMWE performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Degradation of Fuel Cell Membrane Electrode Assemblies from Buses Operated More than 25,000 h

This study investigates the performance losses and degradation of proton-exchange-membrane fuel-cell stacks taken from the Alameda Contra Costa Transit District (AC Transit) bus system (Alameda and Contra Costa counties, California, United States) that were operated for over 25,000 h. Here, we focus on the origin of differences in electrochemical performance between beginning-of-life (BOL) and end-of-life states as well as diagnostic data acquired during the lifetime of the buses. In doing so, we employ in- and ex- situ characterization methods such as polarization curves, electrochemical impedance spectroscopy, electron microscopy, and X-ray characterization. Uniform degradation of the catalyst layer including Pt agglomeration/migration and electrode thinning was observed in all of the post-teardown measurements compared to BOL materials resulting from years of field operation. Despite these changes, the measured post-teardown performance suggests a sufficient output for the expected load, which indicate factors other than degradation of the membrane-electrode assemblies (MEAs) are likely responsible for the decommissioning of the stacks. The findings indicate that these MEA materials can enable long lifetime in fuel-cell vehicles, if the MEAs are not subjected to adverse operating conditions. The results also highlight the need for more in-vehicle diagnostics to maximize the lifetime of fuel cell vehicle (FCV) powerplants.

25 ENERGY STORAGE↗

Microstructural Analysis and Transport Resistances of Low-Platinum-Loaded PEFC Electrodes

In this study, we present microstructural characterization for polymer electrolyte fuel cell (PEFC) cathodes with low platinum loadings (low-PGM). The characterization results are used to quantify the contribution of mass transport resistances to cell voltage losses observed in polarization curve data. Three-dimensional pore morphology and ionomer distribution are resolved using nano-scale X-ray computed tomography (nano-CT). Electrode structural properties are reported along with analysis of the impact of microstructure on the effective charge and reactant transport properties. These characterizations are incorporated with a two-dimensional multi-physics model that accounts for energy, charge, and mass transport along with the effect of liquid water flooding. Defining a total mass transport resistance for the whole polarization curve, contributions of transport mechanisms are identified. Analysis of the experimental polarization curves at different operating pressures and temperatures indicates that the mass transport resistance in the cathode is dominated by the transport processes in the electrode. It is shown that flooding in the electrode is a major contributor to transport losses especially at elevated operating pressures while the pressure-independent resistance at the catalyst surface due to transport through the ionomer film plays a significant role, especially at low temperatures and low catalyst loading. In addition, by performing a parametric study for varying catalyst loadings, the importance of electrode roughness (i.e, electrochemically-active surface area/geometric electrode area) in determining the mass transport losses is highlighted.

25 ENERGY STORAGE↗

Impedance Spectroscopy Characterization of PEM Fuel Cells with Fe-N-C-Based Cathodes

We report impedance spectroscopy analysis of PEM fuel cells built with platinum group metal-free (PGM-free) Fe-N-C cathodes with the catalyst loading and ionomer to catalyst ratio being variable parameters. The dependence of key cathode transport and kinetic parameters on the cell current density J are obtained in the range from 0.025 to 0.4 A cm -2 . The electrode performance is evaluated using the characteristic current densities for proton and oxygen transport in the cathode catalyst layer. Overall, certain electrode configurations demonstrate proton and oxygen transport properties comparable to those of Pt/C systems, making them promising substitutes for platinum at cathodic side of PEM fuel cells.

36 MATERIALS SCIENCE↗

Influence of Proton Activity Gaps between Electrodes on Open-Circuit Potential of H 2 /H 2 and H 2 /Air Cells

Polymer -electrolyte-fuel-cell open-circuit voltages (OCVs) are exactly defined by equation (1), where cathode and anode proton activities [(aH+)cathode and (aH+)anode, respectively] usually are identical, so the third term in the right-hand side of equation (2) is ignored. OCV=E0+RT/2F*ln(a1/2 O2*(a2 H+)cathode/aH2O)-RT/2F*ln((a2 H+)anode/aH2) (1) =E0+RT/2F*ln(a1/2 O2*aH2/aH2O)+RT/2F*ln((a2 H+)cathode/(a2 H+)anode) (2) Water vapor pressure is a colligative property that fundamentally correlates to electrolyte concentrations in aqueous solutions. Proton activity is a function of acid concentration, such as pH, when electrolytes are acids. In polymer-electrolyte membranes, water vapor pressure and acid concentration are understood as relative humidity (RH) and water uptake (λ), respectively, where λ represents number of water molecules per sulfonic acid molecule. Several investigations have reported the relationship between RH and λ, meaning that proton activities and associated water uptakes are intimately related to RH. In actual fuel cell operation, cathode RH is determined by ambient-atmosphere and/or humidifier RH(s), and anode RH depends on hydrogen-circulator RH. Therefore, RH is not always identical at both electrodes, and the difference between electrode RHs is considerable during dry operation of polymer electrolyte fuel cells. Therefore, the third term in the right-hand side of equation (2) may be significant for dry operation. We measured OCVs when hydrogen was supplied to both electrodes at 80°C. One electrode (A) was fixed at 30% RH, while RH at the other electrode (B) was varied (0, 5, 10, 20, and 30%). Measured OCVs varied from 0 to 75 mV. For fuel cell tests, electrode A was supplied with hydrogen at 30% RH; electrode B, oxygen at 0, 5, 10, 20, and 30% RH. OCVs deviated from that measured when RH at electrode B was 30%, increasing from 0 to 60 mV with decreasing RH at electrode B. Results are also shown in Figure 1. Proton activities of both electrodes were thermodynamically calculated. The Gibbs–Duhem relation was applied to obtain molar Gibbs free energies of water and sulfonic acid, and proton activity coefficient was calculated using the Gibbs free energy of sulfonic acid and the relationship between RH and λ1–4, assuming that protons and sulfonic anions show identical ionic-activity coefficients. OCVs were estimated using the third term in the right-hand side of equation (2). Results are shown in Figure 1. Fuel-cell current–voltage performance was poor when RHs at the anode and cathode were 30 and 20%, respectively. To determine kinetic current, we measured the oxygen-reduction reaction (ORR) using a rotating-disk electrode (RDE) in concentrated-acid aqueous solutions, which modeled catalyst-layer ionomers. Kinetic currents decreased with acid concentrations. References T. A. Zawodzinski, Jr., C. Derouin, S. Radzinski, R. J. Sherman, V. T. Smith, T. E. Springer and S. Gottesfeld , J. Electrochem. Soc., 140,1041 (1993) P. K. Das and A. Z. Weber, Proceedings of the ASME 2013 11th Fuel Cell Science, Engineering and Technology Conference, Fuel Cell 18010 (2013) V. A. Sethuraman, J. W. Weidner, A. T. Haug, S. Motupally,b and L. V. Protsailo, J. Electrochem. Soc., 155, B50 (2008) A. Kusoglu and A. Z. Weber, Chem. Rev., 117, 987 (2017) Figure 1

Yoshida, Toshihiko↗

Modeling Synergistic Fuel Cell Membrane Degradation with Mitigating Effects of Cerium

During operation, polymer-electrolyte-membrane (PEM) fuel cells undergo mechanical and chemical degradation mechanisms, which behave synergistically and lead to accelerated membrane degradation over time. This study builds upon previous modeling work on mechanical degradation as described by a pinhole in the membrane and the effects of cerium on chemical degradation.1 By combining these two models, analysis can be carried out on the coupled degradation methods and how the mitigation effects of cerium disrupt the degradation cycle. The mechanical model represents a pinhole in the membrane using an effective void fraction, which allows for increased gas crossover through the membrane and impacts the membrane transport and mechanical properties. A microkinetic model for the chemical degradation is included in the model, including attack of the membrane polymer by hydroxyl radicals as well as the mitigation reaction for quenching of hydroxyl radicals with cerium. A concentrated solution theory approach is used to model the transport of cerium ions throughout the cell.2 The model results show how the location of cerium in the cell can be used to prevent chemical degradation. In addition, the model shows how cerium slows down the rate of pinhole growth by reducing the gas crossover and membrane thinning rate. Finally, the model can be used to optimize the distribution of cerium in the membrane and catalyst layers by balancing trade-offs between lowering degradation rates and decreasing fuel cell performance.

25 ENERGY STORAGE↗

Mathematical Modeling of Hydroxide-Exchange-Membrane Water Electrolyzer

Water electrolyzers can transform intermittent renewable energy like solar energy and wind energy into the chemical energy of hydrogen with zero greenhouse-gas emissions. The hydroxide-exchange membrane electrolyzer (HEME) combines the capability to produce pressurized hydrogen with the advantage of being able to use low or non-platinum group metal (PGM) electrocatalysts in the alkaline environment.1 Hydroxide salts, for example, KOH, are added to the HEME water feed on both anode and cathode to improve its performance. However, the specific mechanism of performance improvement still needs to be further understood. In addition, at high current densities, bubble evolution can result in mass-transport limitations, a less well studied phenomena. Mathematical modeling is ideal to explore these issues as it is cost and time efficient and can deconvolute the physics, processes, and observed phenomena and study the applied-voltage breakdown. In this work, we extend our previously developed 1D two-phase continuum model2 to study the varies processes in the HEME and provide insights on performance optimizations. First, the oxygen evolution reaction (OER) and hydrogen evolution reaction (HER) kinetics at different hydroxide concentrations have been studied by rotating disk electrodes (RDE) and implemented in the model. Then, the model is calibrated and validated against experimental HEME polarization curves for different KOH concentrations as a liquid electrolyte. The model clearly shows a performance increase with increasing KOH concentrations, which is consistent with the experimental results. The reduced ohmic resistance and increased electrochemical active surface area (ECSA) are the two main reasons for performance increase. The large amount of hydroxide in the liquid electrolyte not only helps to distribute the reactant hydroxide throughout the catalyst layer (CL), which reduces ohmic loss, but also enables reaction at the interface between the liquid electrolyte and electrocatalyst, which increases the ECSA. Applied-voltage breakdown demonstrates that the electrolyzer performance is dominated by anode kinetics and ohmic loss. A comparison with the DI water feed shows a more uniform current distribution in the anode CL when KOH is added, which indicates a higher utilization of the CL. Second, we present modeling on the effects of bubble coverage. As gas evolves, part of the ECSA is minimized due to bubble coverage. To account for this effect, an empirical relationship between the fractional bubble coverage and the current density is implemented in the model.3 The model shows this bubble coverage effect is more pronounced at large current densities with DI water feed. Acknowledgements This work was funded under the HydroGEN Consortium by the Energy Efficiency and Renewable Energy, Hydrogen and Fuel Cell Technologies Office, of the U. S. Department of Energy under contract number DE-AC02-05CH11231. References R. Abbasi, B. P. Setzler, S. Lin, J. Wang, Y. Zhao, H. Xu, B. Pivovar, B. Tian, X. Chen, G. Wu and Y. Yan, 31, 1805876 (2019). L. N. Stanislaw, M. R. Gerhardt and A. Z. Weber, ECS Transactions, 92, 767 (2019). H. Vogt and R. J. Balzer, Electrochimica Acta, 50, 2073 (2005).

Liu, Jiangjin↗