Search NASA⌕ Search

SEARCH · Search NASA

Results for “cathode electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

432 records · Page 24

Self-healing SEI enables full-cell cycling of a silicon-majority anode with a coulombic efficiency exceeding 99.9%

Despite active developments, full-cell cycling of Li-battery anodes with >50 wt% Si (a Si-majority anode, SiMA) is rare. The main challenge lies in the solid electrolyte interphase (SEI), which when formed naturally (nSEI), is fragile and cannot tolerate the large volume changes of Si during lithiation/delithiation. An artificial SEI (aSEI) with a specific set of mechanical characteristics is henceforth designed; we enclose Si within a TiO 2 shell thinner than 15 nm, which may or may not be completely hermetic at the beginning. In situ TEM experiments show that the TiO 2 shell exhibits 5× greater strength than an amorphous carbon shell. Void-padded compartmentalization of Si can survive the huge volume changes and electrolyte ingression, with a self-healing aSEI + nSEI. The half-cell capacity exceeds 990 mA h g -1 after 1500 cycles. To improve the volumetric capacity, we further compress SiMA 3-fold from its tap density (0.4 g cm -3 ) to 1.4 g cm -3 , and then run the full-cell battery tests against a 3 mA h cm -2 LiCoO 2 cathode. Despite some TiO 2 enclosures being inevitably broken, 2× the volumetric capacity (1100 mA h cm -3 ) and 2× the gravimetric capacity (762 mA h g -1 ) of commercial graphite anode is achieved in stable full-cell battery cycling, with a stabilized areal capacity of 1.6 mA h cm -2 at the 100th cycle. The initial lithium loss, characterized by the coulombic inefficiency (CI), is carefully tallied on a logarithmic scale and compared with the actual full-cell capacity loss. In conclusion, it is shown that a strong, non-adherent aSEI, even if partially cracked, facilitates an adaptive self-repair mechanism that enables full-cell cycling of a SiMA, leading to a stabilized coulombic efficiency exceeding 99.9%.

25 ENERGY STORAGE↗

Engineering Solid Electrolyte Interphase Composition by Assessing Decomposition Pathways of Fluorinated Organic Solvents in Lithium Metal Batteries

Studies have shown fluorinated electrolyte solvents can form desirable solid electrolyte interphase (SEI) in lithium metal batteries. In this study, we develop a detailed mechanistic understanding of two high performing electrolytes, Fluoroethylene Carbonate (FEC) and Difluoroethylene Carbonate (DFEC) to demonstrate minimal structural variations can lead to different decomposition products, and thereby the nature of the SEI. Using density functional theory (DFT) calculations, we find different initial bond-breaking mechanisms between FEC and DFEC. We develop free energy diagrams for the decomposition pathways including both electrochemical and chemical steps. Using the computational Li electrode, we identify the largest limiting potential of 1.77 V for FEC decomposition, associated with the formation of lithium fluoride, lithium oxide and FEC oligomers, and 1.53 V for DFEC, which correspond to the formation of polymerized vinylene carbonate and lithium fluoride. We suggest the formation of oligomers in the case of FEC instead of long polymers may lead to better SEI compactness. We also demonstrate the SEI components of FEC and DFEC are not stable on typical cathode voltage (3.87 V). This study presents a unified electrocatalytic perspective on SEI formation and decomposition.

25 ENERGY STORAGE↗

Identification of efficient and stable solid-solid electrochemical interfaces for Li-S batteries. Final Report

The objective of this work is to develop a better understanding of the interactions between battery components that drive the observed battery performance. Using computational tools at the atomistic level, we elucidate molecular, crystal, and amorphous structures, interfacial structures and reactions, and electrochemical behavior. We focus on Li metal anodes, liquid electrolytes, solid electrolytes, S cathodes, and metal-oxide cathodes, and their corresponding interfaces. Within liquid electrolytes, we study their bulk structure and dynamics, as a function of salt concentration. The analysis allows to understand the formation of localized high concentrated regions as the solvent is substituted by a weakly interacting diluent species. Analysis of the electron distribution yields the reactive behavior at interfaces. Moreover, we employ tools that allow the characterization of ion and electron transport at interfaces, during the processes of solvation and desolvation occurring while cycling. For Sulfur cathodes we elucidate synthesis processes and the role of carbon-sulfur and nitrogen-sulfur interactions not only to provide electronic conductivity but also to define alternative reaction pathways during discharge of Li-S batteries. Full-cell simulations offer new insights regarding the integration of all the battery components. Our studies also include solid electrolytes and their interfaces with Li metal, S-C, and metal-oxide electrodes.

25 ENERGY STORAGE↗

3D Artificial Solid-Electrolyte Interphase for Lithium Metal Anodes Enabled by Insulator–Metal–Insulator Layered Heterostructures

Despite considerable efforts to prevent lithium (Li) dendrite growth, stable cycling of Li metal anodes with various structures remains extremely difficult due to the direct contact of the liquid electrolyte with Li. Rational design of solid-electrolyte interphase (SEI) for 3D electrodes is a promising but still challenging strategy for preventing Li dendrite growth and avoiding lithium–electrolyte side reactions in Li-metal batteries. Here, a 3D architecture is constructed with g-C 3 N 4 /graphene/g-C 3 N 4 insulator–metal–insulator sandwiched nanosheets to guide uniform Li plating/stripping in the van der Waals gap between the graphene and the g-C 3 N 4 , and the function of which can be regarded as a 3D artificial SEI. Li deposition on the surface of g-C 3 N 4 is suppressed due to its insulating nature. However, its uniform lithiophilic sites and nanopore channels enable homogeneous lithium plating between the graphene and the g-C 3 N 4 , prohibiting the direct contact of the electrolyte with the Li metal. The use of the g-C 3 N 4 -layer-modified 3D anode enables long-term Li deposition with a high Coulombic efficiency and stable cycling of full cells under high cathode loading, limited Li excess, and lean electrolyte conditions. The concept of a 3D artificial SEI will shed light on developing safe and stable Li-metal anodes.

25 ENERGY STORAGE↗

High‐Energy LiNiO 2 Li Metal Batteries Enabled by Hybrid Electrolyte Consisting of Ionic Liquid and Weakly Solvating Fluorinated Ether

Abstract In pursuit of the highest possible energy density, researchers shift their focus to the ultimate anode material, lithium metal (Li 0 ), and high‐capacity cathode materials with high nickel content (Ni > 80%). The combination of these aggressive electrodes presents unprecedented challenges to the electrolyte. Here, we report a hybrid electrolyte consisting of a highly fluorinated ionic liquid and a weakly solvating fluorinated ether, whose hybridization structure enables the reversible operation of a battery chemistry based on Li 0 and LiNiO 2 (Ni = 100%), delivering nearly theoretical capacity of the latter (up to 249 mAh g −1 ) for >300 cycles with retention of 78.6% and in absence of unwanted morphological changes in both electrodes. Extensive characterization assisted by molecular dynamic simulation and density functional theory calculations reveals the function of the fluorinated ether to be far more profound than simple dilution and viscosity reduction. Instead, it induces drastic changes in Li + ‐solvation environment, the consequence of which engenders simultaneous stabilization of electrode/electrolyte and interfacing via formation of respective interfacial chemistries. This study further unlocks fundamental knowledge underneath the prevailing “diluent strategy” that is extensively applied by the electrolyte researchers and opens more design space for the next‐generation electrolytes and interphases for these coveted battery chemistries.

25 ENERGY STORAGE↗

A Solution-Processable High-Modulus Crystalline Artificial Solid Electrolyte Interphase for Practical Lithium Metal Batteries

The solid electrolyte interphase (SEI) has been identified as a key challenge for Li metal anodes. The brittle and inhomogeneous native SEI generated by parasitic reactions between Li and liquid electrolytes can devastate battery performance; therefore, artificial SEIs (ASEIs) have been proposed as an effective strategy to replace native SEIs. Herein, as a collaboration between academia and industrial R&D teams, a multifunctional (crystalline, high modulus, and robust, Li + ion conductive, electrolyte-blocking, and solution processable) ASEI material, LiAl-FBD (where “FBD” refers to 2,2,3,3-tetra-fluoro-1,4-butanediol), for improving Li metal battery performance is designed and synthesized. The LiAl-FBD crystal structure consists of Al 3+ ions bridged by FBD 2– ligands to form anion clusters while Li + ions are loosely bound at the periphery, enabling an Li + ion conductivity of 9.4 × 10 –6 S cm –1 . Further, the fluorinated, short ligands endow LiAl-FBD with electrolyte phobicity and high modulus. The ASEI is found to prevent side reactions and extend the cycle life of Li metal electrodes. Specifically, pairing LiAl-FBD coated 50 μm thick Li with industrial 3.5 mAh cm –2 NMC811 cathode and 2.8 μL mAh –1 lean elec-trolyte, the Li metal full cells show superior cycle life compared to bare ones, achieving 250 cycles at 1 mA cm –2 .

25 ENERGY STORAGE↗

Electrochemical and Interfacial Behavior of All Solid State Batteries Using Li10SnP2S12 Solid Electrolyte

Thio-Lithium Superionic Conductor (Thio-LISICON) Li10GeP2S12 equivalent Li10SnP2S12 (LSPS) is comparable in ionic conductivity yet with a lower cost as an electrolyte for all solid-state batteries (ASSBs). ASSBs with LSPS solid electrolyte (SE), lithium-indium alloy anode, and LiCoO2 (LCO) cathode were successfully fabricated and their electrochemical performance at 60 °C was examined. Atomic layer deposition of Li3NbO4 on LCO was conducted to improve the interfacial stability. The Li3NbO4 coating significantly improves the cycle stability of the ASSB, which retains about 85% of the initial capacity after 70 cycles at a current density of 0.13 mA/cm2, while the ASSB with uncoated LCO retains ~ 60% of the initial capacity after 70 cycles. Electrochemical impedance spectroscopy tests indicate a rapid growth of charge transfer resistance upon cycling for the cell with the uncoated LCO, primarily due to the surface instability and build-up of a space charge layer between LSPS and LCO. However, the ASSBs with Li3NbO4 coated LCO show a more stable interface with a negligible impedance increase upon cycling, attributable to the buffering and passivating roles of the Li3NbO4 coating. The interfacial microstructure was analyzed to elucidate at the underlying reasons for the impedance increase and the pivotal role of the Li3NbO4 coating. Our study indicates that the surface coating significantly improves the cycle stability of the ASSBs with LSPS as the electrolyte, mostly due to an improvement of the charge transfer mechanism. The coating reduced the interphase thickness and the interfacial resistance to about a third of the uncoated one after 10 cycles.

Vinado, Carolina↗

Mechanically and Chemically Robust Sandwich-Structured C@Si@C Nanotube Array Li-Ion Battery Anodes

Stability and high energy densities are essential qualities for emerging battery electrodes. Because of its high specific capacity, silicon has been considered a promising anode candidate. However, the several-fold volume changes during lithiation and delithiation leads to fractures and continuous formation of an unstable solid-electrolyte interphase (SEI) layer, resulting in rapid capacity decay. Here, we present a carbon–silicon–carbon (C@Si@C) nanotube sandwich structure that addresses the mechanical and chemical stability issues commonly associated with Si anodes. The C@Si@C nanotube array exhibits a capacity of ~2200 mAh g –1 (~750 mAh cm –3 ), which significantly exceeds that of a commercial graphite anode, and a nearly constant Coulombic efficiency of ~98% over 60 cycles. In addition, the C@Si@C nanotube array gives much better capacity and structure stability compared to the Si nanotubes without carbon coatings, the ZnO@C@Si@C nanorods, a Si thin film on Ni foam, and C@Si and Si@C nanotubes. In situ SEM during cycling shows that the tubes expand both inward and outward upon lithiation, as well as elongate, and then revert back to their initial size and shape after delithiation, suggesting stability during volume changes. The mechanical modeling indicates the overall plastic strain in a nanotube is much less than in a nanorod, which may significantly reduce low-cycle fatigue. Furthermore, the sandwich-structured nanotube design is quite general, and may serve as a guide for many emerging anode and cathode systems.

25 ENERGY STORAGE↗

Porous and Amorphous Mn x Mo 3 S 13 Chalcogel Electrode for High-Capacity Conversion-Based Lithium-Ion Batteries

While Li-ion batteries (LIBs) are a leading energy storage technology, their energy densities are limited by the low capacity of conventional intercalation cathodes, driving interest in high energy-density Li–S batteries that make use of conversion chemistry. Achieving high capacity, reversibility, and cycle stability, and controlling volume changes in conversion batteries during the charge–discharge process, however, remains challenging. Here, in this study, we present a porous, amorphous, sulfide-based Mn x Mo 3 S 13 chalcogel, which concurrently offers high capacity and cycle stability. The solution-processable room temperature synthesized Mn x Mo 3 S 13 (x = 0.25) chalcogel exhibits a local structure that resembles the Mo 3 S 13 cluster with Mn 2+ distributed across the Mo 3 S 13 matrix, as determined by synchrotron X-ray pair distribution function (PDF) and extended X-ray absorption fine structure (EXAFS). Ab initio molecular dynamics (AIMD) simulations reveal that Mn 2+ incorporation shortens the polysulfide chain in the gel matrix compared to the Mo 3 S 13 chalcogel, while forming a coordination environment with disulfide groups, analogous to the experimental findings. A Li/Mn 0.25 Mo 3 S 13 half-cell delivers 897 mAh g –1 capacity during the first discharge and retains 571 mAh g –1 capacity after 100 cycles at a C/3 rate. Distribution of relaxation time (DRT) unveils a stable solid–electrolyte interphase (SEI) formation upon cycling that enables charge–discharge reversibility. Here, the enhanced capacity retention and cycle stability compared to those of the Li/Mo 3 S 13 cell are attributed to the reduced dissolution of active mass into the electrolyte, facilitated by the formation of shorter polysulfide chains within the Mn 0.25 Mo 3 S 13 structure and the strong affinity of Lewis-acidic Mn 2+ for polysulfide anions generated during the charge–discharge process of the Li/Mn 0.25 Mo 3 S 13 cell. Thus, this work illustrates a design principle of material for high-capacity and cycle-stable Li-metal sulfide batteries.

25 ENERGY STORAGE↗

Mechanisms of Water-Stimulated Mg 2+ Intercalation in Vanadium Oxide: Toward the Development of Hydrated Vanadium Oxide Cathodes for Mg Batteries

As lithium-ion batteries approach their theoretical limits for energy density, magnesium-ion batteries are emerging as a promising next-generation energy storage technology. However, progress in magnesium-ion battery research has been stymied by a lack of available high capacity cathode materials that can reversibly insert magnesium ions. Vanadium Oxide (V 2 O 5 ) has emerged as one of the more promising candidate cathode materials, owing to its high theoretical capacity, facile synthesis methods, and relatively high operating voltage. This review focuses on the outlook of hydrated V 2 O 5 structures as a high capacity cathode material for magnesium-ion batteries. In general, V 2 O 5 structures exhibit poor experimental capacity for magnesium-ion insertion due to sluggish magnesium-ion insertion kinetics and poor electronic conductivity. However, several decades ago, it was discovered that the addition of water to organic electrolytes significantly improves magnesium-ion insertion into V 2 O 5 . This review clarifies the various mechanisms that have been used to explain this observation, from charge shielding to proton insertion, and offers an alternative explanation that examines the possible role of structural hydroxyl groups on the V 2 O 5 surface. While the mechanism still needs to be further studied, this discovery fueled new research into V 2 O 5 electrodes that incorporate water directly as a structural element. The most promising of these hydrated V 2 O 5 materials, many of which incorporate conductive additives, nanostructured architectures, and thin film morphologies, are discussed. Ultimately, however, these hydrated V 2 O 5 structures still face a significant barrier to potential applications in magnesium-ion batteries. During full cell electrochemical cycling, these hydrated structures tend to leach water into the electrolyte and passivate the surface of the magnesium anode, leading to poor cycle life and low capacity retention. Recently, some promising strides have been made to remedy this problem, including the use of artificial solid electrolyte interphase layers as an anode protection scheme, but a call to action for more anode protection strategies that are compatible with trace water and magnesium metal is required.

25 ENERGY STORAGE↗

Pushing Lithium–Sulfur Batteries towards Practical Working Conditions through a Cathode–Electrolyte Synergy

The commercialization of lithium-sulfur (Li-S) batteries is still hindered by the unsatisfactory cell performance under practical working conditions, which is mainly caused by the sluggish cathode redox kinetics, severe polysulfide shuttling, and poor Li striping/platting reversibility. We reported an effective strategy by combining Se-doped S hosted in an ordered macroporous framework with highly fluorinated ether (HFE)-based electrolyte to simultaneously address the aforementioned issues in both cathode and anode. A reversible and stable high areal capacity of > 5.4 mAh cm -2 with high coulombic efficiency > 99.2% can be achieved under high areal Se/S loading (5.8 mg cm -2 ), while the underlying mechanism was further revealed through synchrotron X-ray probes and Time-of-Flight Secondary Ion Mass Spectrometry (ToF-SIMS). The practical application potential was further evaluated at low (0 °C) and high (55 °C) temperatures under high areal Se/S loading (> 5.0 mg cm -2 ) and thin Li metal (40 µm).

25 ENERGY STORAGE↗

Rapid charging made practical in graphite-based lithium batteries: surface-acoustic wave turbulent electrolyte mixing to overcome diffusion limited charging rates [Final Report]

One of the key limits in rapidly recharging a lithium-ion battery is the depletion of lithium ions within the electrolyte adjacent the anode during charging and long diffusion time to overcome this depletion. It also causes dendrite formation, inefficient use of the lithium, and battery degradation over many charge-discharge cycles. Because the liquid electrolyte remains quiescent and unmixed, this depletion layer’s depth rapidly grows to match the anode-cathode separation distance at even modest charge rates. The solution proposed by PI Prof. James Friend and Co-PI Prof. Ping Liu, both from the University of California, San Diego, is to mix the electrolyte and minimize the Li+ ion concentration gradient during charging. Even in the presence of the separator, the charging rate could then be significantly increased. They propose to accomplish this using surface acoustic wave (SAW)-driven acoustic streaming, a technique employing 10-mW fingernail-sized solid-state devices from the telecommunications industry to drive turbulent mixing to submicron length scales in a manner completely compatible with the typical 20700 and 18650 cells used in electric vehicles. 0.1. Turbulent acoustic streaming mixes the electrolyte during charging—even with separator Our proposed 100-MHz SAW device used to recirculate the electrolyte is compatible with lithium- ion battery electrochemistry, as it is made in our lab of single-crystal lithium niobate. Their solution is straightforward to drive from a DC power source alongside the signal provided during battery charging. The device is only needed during charging and does not consume power dur- ing battery discharge. Uniquely, SAW generates extreme accelerations of over 1 billion meters per second squared in the fluid, driving turbulent mixing from centimeter to submicron length scales, even through the porous separator materials that tend to be used in batteries, all while avoiding interfering with the anode’s solid electrolyte interphase layer that forms during use. By employing novel fluid mechanics, the investigators are proposing a new direction for battery research away from direct use of materials science and electrochemistry. The chemistry agnostic solution may be employed in any battery chemistry that makes use of liquid electrolytes, providing a broader transformative benefit to the battery research community. They are to produce a series of prismatic and 20700-cell sized 2 Ah batteries capable of being charged and discharged at least 500 times without more than 20% loss in battery capacity, and to provide analysis tools useful to the battery research and development community for adopting this approach for other battery chemistries and configurations.

25 ENERGY STORAGE↗

Structural and Interphasial Stabilities of Sulfurized Polyacrylonitrile (SPAN) Cathode

Sulfurized polyacrylonitrile (SPAN) has attracted a lot of attention because of its low cost, high capacity, and great reversibility. Due to its structural complexity and amorphous nature, reaction mechanism of SPAN is little understood. Here, for this paper, we study the structural and interphasial changes of SPAN using synchrotron-based pair distribution function (PDF) analysis and soft X-ray absorption spectroscopy (sXAS). PDF identifies key structural features, including C–S bond, sulfur dimer, and sulfur chain in SPAN. The sulfur dimer bridging the pyridine network partially converts to sulfur chain during the first charging. In the following cycles, sulfur chain goes through lithiation and delithiation with reversibility dependent on the electrolytes. SXAS reveals surface changes of SPAN. After the first cycle, a negatively charged carbon or fused benzene layer is formed, on top of which is another layer formed by the electrolyte decomposition. The layer formed by localized high concentration electrolyte is stable during cycling.

25 ENERGY STORAGE↗

Surface Engineering of Electrospun Fibers to Optimize Ion and Electron Transport in Li + Battery Cathodes

This report documents research into the fabrication of Lithium Manganese Oxide (Spinel) (LMO) cathode material in the form of fibrous mats, the degradation process of this material in a battery electrolyte, the formation of core-shell coated fibers and the electrochemical properties of the active cathode core fiber. In practice, LMO experiences several degradation mechanisms ranging from capacity fading, the Jahn-Teller distortion phenomenon leading to dissolution in the electrolyte phase, and the formation of surface films by degradation of the electrolyte, and/or phase transitions at the surface to form Mn 2 O 3 . Density Functional Theory (DFT) was applied to model from first principles the interactions between the electrolyte and the surface leading to Mn ion dissolution. Thermodynamic values of solvation energy were calculated and related to the applied potential on the material during electrochemical cycling. Direct in situ observation of the degradation process was conducted on fiber structures using AFM and coin cell measurements, showing the rapid formation of theorized surface films. This provides the first direct evidence of processes occurring at the interface, such as dissolution of the active material, facet development, decomposition of the electrolyte to form a surface electrolyte interface (SEI) layer, or the formation of Li alcoxides/carboxylates. Methods for fabricating fiber structures of LMO were researched using two techniques; electrospinning and forcespinning. Chemical precursors were evaluated and optimized to lead to polycrystalline, hollow fibers of LMO, as well as tetragonal zirconia fiber mats. Sol-gel chemistries for the synthesis of LMO and zirconia have been implemented to generate these fiber morphologies. Core-shell methods were attempted using both techniques, proving partial success and insight into the physics of coherent core-shell fibers. The knowledge developed in this program has increased understanding of the degradation mechanisms of the active energy storage material, and aided development of a protective interface which resists these processes while permitting rapid Li + transport, good e - conductivity, a stable interface, and prevention of the formation of a solid-electrolyte interphase (SEI) layer.

25 ENERGY STORAGE↗

Catalytic Electrolyte Additive for High-Loading and Lean Electrolyte Li–S Batteries

The cycle life of high-energy Li–S cells is largely constrained by the quick electrolyte depletion. LiNO 3 has been a well-established additive known for protecting the Li metal anode and stabilizing the battery from polysulfide “shuttling”. However, it can be depleted prematurely and can pose safety risks when exposed to carbon, sulfur, or Li metal under harsh conditions. Here, in this study, LiPO 2 F 2 was explored as a safe and durable alternative additive in ether-based electrolytes. LiPO 2 F 2 demonstrates superior performance in Li/S batteries, especially under high sulfur loading (∼4 mg/cm 2 ) and lean electrolyte conditions (E/S = 4), achieving a long-term cycling stability of 40%, compared to 14.7% with LiNO 3 . This additive facilitates the disproportionation of polysulfides, reducing their dissolution and mitigating the shuttle effect. Additionally, LiPO 2 F 2 promotes the formation of a stable solid-electrolyte interphase (SEI) composed of inorganic anion-derived species, improving the battery’s overall stability and functionality. These findings blaze a trail in the design of safer and more durable electrolytes for Li–S batteries.

Li-S batteries↗

Ternary Potassium‐Bismuth‐Telluride Intermetallic Support Promotes Electrochemical Stability in Potassium Metal Anodes

We employed accumulative roll bonding to fabricate self‐standing metallurgical composite of in situ formed alkaline potassium‐bismuth‐telluride intermetallic K 2 (Bi 2/6 Te 3/6 Vac 1/6 ) embedded in potassium metal. This newly discovered thermodynamically stable potassiophilic crystal, termed “KBT”, is fcc antifluorite with K 2 Te archetype. Symmetric cells achieve 880 h of cycling at 0.5 mA cm −2 and 0.5 mAh cm −2 . Potassium metal battery (KMB) with Prussian blue (PB) cathode in carbonate electrolyte retains 80% capacity after 200 cycles at 1C. In ether‐based electrolyte with organic cathode, it achieves 80% retention after 900 cycles at 2C. Combined synchrotron X‐ray nano‐tomography, cryogenic‐focused ion beam microscopy (Cryo‐FIB) and sputter‐down X‐ray photoelectron spectroscopy (XPS) demonstrate uniform electrodeposits, versus baseline of potassium filaments intermixed with pores and coarse SEI. Binary K 3 Bi‐K and K 2 Te‐K intermetallic supports also provide improved electrochemical performance, albeit to lesser extent. Multiscale simulation provides insight into role of support structure in adatom energetics, film nucleation, early‐stage SEI morphology and interfacial stability.

36 MATERIALS SCIENCE↗

Unusual Li 2 O sublimation promotes single-crystal growth and sintering

Li 2 O is rarely used for cathode material synthesis due to its high melting point (1,438 °C). Here we discover that Li 2 O can sublimate at 800-1,000 °C under ambient pressure, opening new possibilities for cathode synthesis. We propose a mechanism that enables synthesis of single crystals-such as LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) or LiNi 0.9 Mn 0.05 Co 0.05 O 2 (NMC90)-without direct contact with Li 2 O salts. We show that Li 2 O vapour successfully converts spent polycrystalline NMC811 into segregated single crystals without milling or post-treatment. The Li 2 O vapour, derived from Li 2 O solids, diffuses rapidly and reacts with precursors, mimicking a molten-salt environment, which facilitates single-crystal growth. The chemical lithiation process continuously drives Li 2 O sublimation, sintering the crystals. Single crystals derived from Li 2 O and fresh precursors or spent polycrystals exhibit outstanding cycling after 1,000 cycles in full cells. The demonstrated Li 2 O sublimation and its universal role in promoting single-crystal growth provides an effective approach for single-crystal synthesis, scale-up and recycling.

25 ENERGY STORAGE↗