Search NASA⌕ Search

SEARCH · Search NASA

Results for “electrolyte engineering”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Intrinsic chemical reactivity of solid-electrolyte interphase components in silicon–lithium alloy anode batteries probed by FTIR spectroscopy

Herein we report the solid reaction products from the chemical reaction of aprotic battery electrolyte and three purported components of the Si-based anode SEI : SiO 2 nanoparticles (NPs), lithium silicate (Li x SiO y ) powders, and Si NPs. We use FTIR and classical molecular dynamics/density functional perturbation theory to assess the solid products remaining with these model materials after exposure to electrolyte. The absence of electrochemical bias provides a view of the chemical speciation resulting from early-stage chemical reactivity during battery assembly as well as under open circuit storage conditions. We believe these species represent the initial stages of SEI growth and predict they likely drive subsequent chemical and electrochemical reactions by controlling molecular interactons at the Si active material interface. We find that nominally equivalent materials react differently even before any electrochemistry is performed (e.g., acidic SiO 2 dissolves whereas alkaline SiO 2 is relatively robust), and derive new understanding of the chemical species that could and could not form stable SEI components in Si-based anodes. These results can be used to inform how to passivate Si anode surfaces and potentially generate an artificially engineered SEI that would be stable and enable next-generation battery anodes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Influence of Alkyl Spacers and Molecular Weight on the Charge Transport and Storage Properties of Oxy‐Bithiophene‐Based Conjugated Polymers

Abstract Conjugated polymers (CPs) with polar side chains can conduct electronic and ionic charges simultaneously, making them promising for bioelectronics, electrocatalysis and energy storage. Recent work showed that adding alkyl spacers between CP backbones and polar side chains improved electronic charge carrier mobility, reduced swelling and enhanced stability, without compromising ion transport. However, how alkyl spacers impact polymer backbone conformation and, subsequently, electronic properties remain unclear. In this work, we design two oxy‐bithiophene‐based CP series, each featuring progressively extended alkyl spacer lengths and two distinct molecular weight (MW) distributions. Using operando characterisations, we evaluate the (spectro)electrochemical and swelling properties of the polymer thin films, and their performance in organic field‐effect transistors and organic electrochemical transistors. Surprisingly, alkyl spacers negatively impact the hole mobility of our polymers, with higher MW amplifying this effect. Using molecular dynamics simulations, we show that it is thermodynamically favourable for adjacent non‐polar alkyl spacers to aggregate in polar electrolytes, leading to backbone twisting. Further spectroscopic measurements corroborate this prediction. Our findings demonstrate the active interactions between side chain structure, MW and electrolyte/solvent polarity in influencing polymer performance, underscoring the importance of considering solvation environment effects on polymer conformation when designing new mixed conducting CPs for electrochemical applications.

Yu, Hang [Department of Physics and Centre for Pro↗

Optimal conditions for efficient flow-electrode capacitive deionization

One of the current barriers to achieving fast and stable performance for flow-electrode capacitive deionization (FCDI) is determining optimal operating parameters. To date, however, no consensus has been reached for universal conditions for FCDI. Through experimental and modeling approaches in this study, we systematically evaluated the influence of applied potential (V = 1.2–2.4 V) and electrolyte concentration (C0 = 0.05–0.5 M) on the FCDI and electrodialysis (ED) desalination processes. Evaluation indicators include the concentration decrease in the desalinated solution, salt removal rates, pH fluctuations, charge efficiency, and energy consumption. Results demonstrated that the dynamic curves of concentration decrease at 2.0 V nearly overlapped with the response at 1.6 V at certain electrolyte concentrations, while the salt removal rates at 0.2 M salt concentration were the best among all concentrations tested at a range of applied potential. Therefore, it was thus concluded that the optimum conditions for FCDI operation are 1.6 V applied potential and 0.2 M initial salt concentration, under which faradaic reactions are not being triggered, and concentration polarization does not significantly affect ion transfer. Furthermore, a comparative study between FCDI and ED indicated that ED has a different dependence on the electrolyte concentration and applied potential, in which the desalination can be linearly enhanced with increasing potential but greatly limited at high concentrations. Due to the presence of carbon particles in FCDI, the enhanced charge/ion transfer is probably the main reason for the different desalination performance of FCDI and ED. Overall, the optimal operating parameters obtained in this work could be used as basic test conditions for further development of new carbon-based materials for FCDI.

42 ENGINEERING↗

Reactive boride infusion stabilizes Ni-rich cathodes for lithium-ion batteries

Engineered polycrystalline electrodes are critical to the cycling stability and safety of lithium-ion batteries, yet it is challenging to construct high-quality coatings at both the primary- and secondary-particle levels. Here, we present a room-temperature synthesis route to achieve full surface coverage of secondary particles and facile infusion into grain boundaries, thus offering a complete “coating-plus-infusion” strategy. Cobalt boride metallic glass is successfully applied to Ni-rich layered cathode LiNi 0.8 Co 0.1 Mn 0.1 O 2 . Here, it dramatically improves the rate capability and cycling stability, including under high-discharge-rate and elevated-temperature conditions and in pouch full cells. The superior performance originates from simultaneous suppression of microstructural degradation of intergranular cracking and side reactions with electrolyte. Atomistic simulations identified the critical role of strong selective interfacial bonding, which offers not only a large chemical driving force to ensure uniform reactive wetting and facile infusion but also lowered the surface/interface oxygen activity, contributing to the exceptional mechanical and electrochemical stabilities of the infused electrode.

25 ENERGY STORAGE↗

Long–Cycling Sulfide–Based All–Solid–State Batteries Enabled by Electrochemo–Mechanically Stable Electrodes

Anode significantly determines the energy density of all-solid-state Lithium batteries (ASLBs). Silicon (Si) and Lithium (Li) metal are two of the most attractive anodes because of their ultrahigh theoretical capacities. However, most investigations focus on Li metal; the great potential of Si is underrated. This study investigates Si anode's stability, processability, and cost in ASLBs and compares them with Li metal. Moreover, the single-crystal LiNi 0.8 Co 0.1 Mn 0.1 O 2 is stabilized with a lithium silicate (Li 2 SiO x ) through a scalable sol-gel method. ASLBs with a cell-level energy density of 285 Wh kg -1 are obtained through sandwiching Si anode, thin sulfide solid-state electrolyte membrane, and interface stabilized LiNi 0.8 Co 0.1 Mn 0.1 O 2 . The full cell delivered a high capacity of 145 mAh g -1 at C/3 and maintained stability for 1000 cycles. This work inspires commercializing the ASLBs on a large scale with exciting manufacturing lines for large-scale, safe, and economical energy storage.

25 ENERGY STORAGE↗

A Study on the Synthesis and Proton Transport Behavior of Multilayered ZSM-5 Zeolite Nanosheet Membranes Laminated on Polymer Substrates

Single crystalline ZSM-5 ZNs with thicknesses around 6 nm were obtained by secondary growth of silicalite nanoparticles using diquaternary bis-1,5(tripropyl ammonium) pentamethylene diiodide (dC5) as a structure-directing agent (SDA). The dC5 could be effectively removed from the ZN pores by either high-temperature calcination or UV irradiation in air at room temperature but not by the piranha solution treatment. Ultrathin ZN-laminated membranes (ZNLMs) were fabricated by sandwiching a UV-activated multilayered ZN film between two recast Nafion® layers (ZNLM-Nafion) and by filtration coating from a suspension of thermally activated ZNs on a nonionic porous PVDF (ZNLM-PVDF). The ZNLMs on both supports demonstrated the ability of highly proton-selective ion conduction with low resistances in aqueous electrolyte solutions. The ZNLM-PVDF with PVDF binder was structurally stable, and it achieved a comparably low ASR but much higher proton selectivity compared with a Nafion membrane of same overall thickness. However, detachment between the ZNLM and Nafion layers occurred when the ZNLM-Nafion operated in aqueous electrolyte solutions. Results of this study show the potential for developing ZNLMs as efficient proton-conducting membranes without using expensive ionic polymer matrices. However, the development of polymer-supported ZNLMs is hindered by the current inefficiency in preparing well-dispersed suspensions of open-pore ZNs. Future development of efficient methods for synthesizing open-pore ZNs in dispersed states is key to realizing high-performance ZNLMs on polymers.

36 MATERIALS SCIENCE↗

A quantitative figure of merit for battery SEI films and their use as functional solid-state electrolytes

As a key passivation film that governs battery operation, the solid electrolyte interphase (SEI) has long been credited for enabling high-performance batteries or blamed for their eventual death. However, qualitative descriptions of the SEI often found in the literature (e.g., “conductive,” “passivating”) highlight our incomplete understanding of this layer, where even the most basic properties foundational to SEI function remain difficult to measure. Here, we quantify SEI conductivities and SEI transference numbers using a separator-free Cu|SEI|Li architecture that treats the SEI as a functional solid-state electrolyte (SSE). We find that while any SEI property alone (e.g., electronic conductivity) is weakly correlated (R 2 < 0.67) with battery performance (e.g., Coulombic efficiency), a strong correlation (R 2 > 0.99) can be achieved by defining the “SEI cT number” as a product between the SEI transference number (T) and the ratio of SEI conductivities (c). Analogous to the thermoelectric figure of merit (i.e., zT ), SEI cT quantitatively benchmarks the holistic impact of SEI properties on battery performance and underscores the pitfalls of citing such properties in isolation. Perhaps most strikingly, we demonstrate that Li metal deposition and stripping at room temperature is possible in our separator-free Cu|SEI|Li cell, confirming that the SEI can function precisely as an SSE. Together, these results enrich our understanding of the SEI, not just as a passivation layer but as a functional structure that can potentially have important implications for solid-state batteries.

Science & Technology - Other Topics↗

Investigations of the stability of etched or platinized p-InP(100) photocathodes for solar-driven hydrogen evolution in acidic or alkaline aqueous electrolytes

Here, the stability of p-InP photocathodes performing the hydrogen-evolution reaction (HER) has been evaluated in contact with either 1.0 M H 2 SO 4 (aq) or 1.0 M KOH(aq), with a focus on identifying corrosion mechanisms. Stability for the solar-driven HER was evaluated using p-InP electrodes that were either etched or coated with an electrodeposited Pt catalyst (p-InP/Pt). Variables such as trace O 2 were systematically controlled during the measurements. Changes in surface characteristics after exposure to electrochemical conditions as well as electrode dissolution processes were monitored using X-ray photoelectron spectroscopy (XPS) and inductively coupled plasma mass spectrometry (ICP-MS). In either H 2 SO 4 or KOH, etched p-InP photoelectrodes corroded cathodically under illumination, forming metallic In 0 at the electrode surface. In contrast, electrodeposition of Pt kinetically stabilized illuminated p-InP photocathodes in both H 2 SO 4 and KOH by inhibiting the cathodic corrosion pathway. Notably, when held at 0 V vs. the reversible hydrogen electrode (RHE) in 1.0 M H 2 SO 4 (aq), p-InP/Pt exhibited a stable current density (J) of ~–18 mA cm –2 for >285 h under simulated 1 Sun illumination. The long-term current density vs. potential (J–E) behavior at pH 0 and pH 14 of p-InP/Pt photocathodes correlated with changes in the surface chemistry as well as the dissolution of p-InP. In acidic media, the J–E behavior of p-InP/Pt photocathodes remained nearly constant with time, but the surface of a p-InP/Pt electrodes gradually turned P-rich via a slow and continuous leaching of In ions. In alkaline electrolyte, the surface of p-InP/Pt electrodes was passivated by formation of an InO x layer that exhibited negligible dissolution but led to a substantial degradation in the J–E characteristics. Consequently, changes in the catalytic kinetics and surface stoichiometry are both important considerations for determining the corrosion chemistry and the long-term operational stability of InP photoelectrodes.

14 SOLAR ENERGY↗

Crossover Effects of Transition‐Metal Ions on Lithium‐Metal Anode in Localized High Concentration Electrolytes

Abstract The stability of the solid–electrolyte interphase (SEI) is critical to the cycle life of lithium‐metal batteries (LMBs). While the crossover effect of transition‐metal ions from cathode to anode is extensively studied in lithium‐ion batteries with graphite anodes, its impact on LMBs remains largely unexplored. Herein, this study investigates the electrochemical and chemical properties of SEI layers formed on lithium‐metal anodes in localized high‐concentration electrolytes (LHCEs) containing dissolved transition‐metal ions (Ni 2+ , Mn 2+ , and Co 2+ ). It is demonstrated that transition‐metal ions in LHCEs reduce the coulombic efficiency (CE) and significantly degrade the cycle life of LMBs. Time‐of‐flight secondary‐ion mass spectrometry (ToF‐SIMS) reveals that SEI structures differ depending on the dissolved TM ion, with Mn 2+ and Co 2+ inducing severe destabilization, and Ni 2+ exhibiting a less severe impact. These findings underscore the detrimental effects of transition‐metal crossover effects in LMB systems.

Guo, Zezhou [Materials Science and Engineering Pro↗

A free-standing lithium phosphorus oxynitride thin film electrolyte promotes uniformly dense lithium metal deposition with no external pressure

Lithium phosphorus oxynitride (LiPON) is an amorphous solid electrolyte that has been extensively studied over the last three decades. Despite the promise of pairing it with various electrode materials, LiPON’s rigidity and air sensitivity set limitations to understanding its intrinsic properties. We report a methodology to synthesize LiPON in a free-standing form that manifests remarkable flexibility and a Young’s modulus of ∼33 GPa. We use solid-state nuclear magnetic resonance and differential scanning calorimetry to quantitatively reveal the chemistry of the Li/LiPON interface and the presence of a well-defined LiPON glass-transition temperature of 207 °C. Combining interfacial stress and a gold seeding layer, our free-standing LiPON shows a uniformly dense deposition of lithium metal without the aid of external pressure. This free-standing LiPON film offers opportunities to study fundamental properties of LiPON for interface engineering for solid-state batteries.

25 ENERGY STORAGE↗

Integrated electro- and chemical characterization of sulfide-based solid-state electrolytes

Sulfide solid-state electrolytes (SSEs) represent a critical advancement towards enabling next-generation lithium metal batteries. However, a profound knowledge gap remains in understanding the structure–property relationships inherent to these sulfide SSEs. Electrochemical assessment and spectroscopic tools, such as Raman spectroscopy, offer bench-top ready, non-invasive, powerful avenues for operando and in situ analyses. Despite this potential, the integration of these methodologies, particularly for real-time interrogation, is markedly under-investigated. This review endeavors to catalog the use of diverse electrochemical techniques and spectroscopic tools in elucidating the structural and functional nuances of sulfide SSEs. Through the harmonization of these multifaceted evaluation strategies, our objective is to chart a course towards optimized sulfide SSEs, thereby aiding in the development of informed protocols for a deeper comprehension and understanding of the structure–property relationship and interfacial engineered design of solid-state batteries using sulfide-based SSEs.

36 MATERIALS SCIENCE↗

Observation of single-defect memristor in an MoS2 atomic sheet

Non-volatile resistive switching, also known as memristor effect, where an electric field switches the resistance states of a two-terminal device, has emerged as an important concept in the development of high-density information storage, computing and reconfigurable systems. The past decade has witnessed substantial advances in non-volatile resistive switching materials such as metal oxides and solid electrolytes. It was long believed that leakage currents would prevent the observation of this phenomenon for nanometre-thin insulating layers. However, the recent discovery of non-volatile resistive switching in two-dimensional monolayers of transition metal dichalcogenide and hexagonal boron nitride sandwich structures (also known as atomristors) has refuted this belief and added a new materials dimension owing to the benefits of size scaling. Here we elucidate the origin of the switching mechanism in atomic sheets using monolayer MoS 2 as a model system. Atomistic imaging and spectroscopy reveal that metal substitution into a sulfur vacancy results in a non-volatile change in the resistance, which is corroborated by computational studies of defect structures and electronic states. These findings provide an atomistic understanding of non-volatile switching and open a new direction in precision defect engineering, down to a single defect, towards achieving the smallest memristor for applications in ultra-dense memory, neuromorphic computing and radio-frequency communication systems.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

In situ , in vivo , and in operando imaging and spectroscopy of liquids using microfluidics in vacuum

This review offers a succinct overview of the development of a vacuum-compatible microfluidic reactor system for analysis at the liquid vacuum interface (SALVI), and its diverse applications in in situ, in vivo, and in operando imaging of liquid surfaces as well as the air-liquid (a-l), liquid-liquid (l-l), and solid-liquid (s-l) interfaces in the past decade. SALVI is one of the first microfluidics-based reactors that has enabled direct analysis of volatile liquids in vacuum surface tools such as scanning electron microscopy (SEM) and time-of-flight secondary ion mass spectrometry (ToF-SIMS). Its integration into ambient and vacuum spectroscopy and microscopy is illustrated. Several applications are highlighted including (1) imaging nanoparticles in liquid using in situ SEM; (2) mapping the evolving l-l interface using in situ x-ray absorption spectroscopy and ToF-SIMS; (3) following complex a-l interfacial oxidation reaction products using in situ ToF-SIMS; (4) capturing biological interfaces of cells and microbes via in vivo multimodal and correlative imaging; and (5) monitoring the dynamic solid electrode and liquid electrolyte interface using in operando molecular imaging. Finally, outlook and recommendations are presented. Besides showing the holistic information volume obtained by real-time multiplexed imaging, this review intends to convey the importance of tool development in revolutionizing surface and interface analysis using vacuum platforms previously limited to solid surfaces. Microfluidics is manifested to be not limited to ambient conditions in many examples in this review. Moreover, fundamental interfacial phenomena underpinning mass and charge transfer can now be pursued in real time via innovated chemical imaging and spectroscopy.

42 ENGINEERING↗

Regulating the Third Metal to Design and Engineer Multilayered NiFeM (M: Co, Mn, and Cu) Nanofoam Anode Catalysts for Anion-Exchange Membrane Water Electrolyzers

In this study, alkaline anion-exchange membrane water electrolyzers (AEMWEs) for green hydrogen production have received intensive attention due to their feasibility of using earth-abundant platinum group metal (PGM)-free catalysts. Herein, the third metal is incorporated into NiFe-based catalysts to regulate their electronic structures and morphologies, aiming to achieve sufficient oxygen evolution reaction (OER) activity and performance in AEMWEs. The ternary NiFeM (M: Cu, Co, or Mn) catalysts are featured with multiple layered structures and nanofoam network morphologies, consisting of highly OER-active amorphous Ni-rich oxide shells and electrically conductive metallic alloy cores. The physical and electronic perturbations to the NiFe induced by a third element lead to a fine-tuning of the redox ability of the metal sites at the reaction centers, which breaks the scaling relationship between OH* and O* intermediates at the reaction centers. Thus, the unique structural configuration and electronic regulation simultaneously benefit catalytic activity and performance improvements. These NiFeM nanofoam catalysts demonstrated promising anode performance in actual AEMWEs, comparable to the IrO 2 reference, especially at high current densities. Notably, using various electrolytes (e.g., KOH solution or pure water) for AEMWEs exhibited a different performance trend among studied NiFeM catalysts, likely due to dynamic changes of catalysts under various OER environments.

25 ENERGY STORAGE↗

A stable cathode-solid electrolyte composite for high-voltage, long-cycle-life solid-state sodium-ion batteries

Rechargeable solid-state sodium-ion batteries (SSSBs) hold great promise for safer and more energy-dense energy storage. However, the poor electrochemical stability between current sulfide-based solid electrolytes and high-voltage oxide cathodes has limited their long-term cycling performance and practicality. Here, we report the discovery of the ion conductor Na 3-x Y 1-x Zr x Cl 6 (NYZC) that is both electrochemically stable (up to 3.8 V vs. Na/Na + ) and chemically compatible with oxide cathodes. Its high ionic conductivity of 6.6 × 10 –5 S cm –1 at ambient temperature, several orders of magnitude higher than oxide coatings, is attributed to abundant Na vacancies and cooperative MCl 6 rotation, resulting in an extremely low interfacial impedance. A SSSB comprising a NaCrO 2 + NYZC composite cathode, Na 3 PS 4 electrolyte, and Na-Sn anode exhibits an exceptional first-cycle Coulombic efficiency of 97.1% at room emperature and can cycle over 1000 cycles with 89.3% capacity retention at 40 °C. These findings highlight the immense potential of halides for SSSB applications.

99 GENERAL AND MISCELLANEOUS↗

Development of electronically passivating surfaces to enhance battery performance

For many decades, lithium metal batteries (LMBs) have been studied for their high energy density, though they suffer from high reactivity, which safety concerns such as explosions and fires. These events can occur as a result of degradation due to redox reactions and lithium morphology that evolve during cycling. Mostly, the failure is caused by the electrolyte degradation leading to the creation of a solid electrolyte interphase (SEI), which tends to induce electron leakage, lithium dendrite growth, and capacity decay. SEI formation is practically inevitable. This work investigated the minimization of degradation events by modifying different battery configurations. Modifications were made by exchanging electrolytes, electrode surfaces, and even annexing innovative components. Our goal is to achieve a configuration where Li-ion transfer is facilitated, and electron transfer is limited which would enable a longer lithium metal battery life cycle. When performing these modifications and testing their electrochemical performance, a current reduction was observed when the electrodes were spontaneously coated with preformed SEI. Herein several classes of artificial SEI layers are explored for their ability to form passivating layers through use of a redox active molecule.

25 ENERGY STORAGE↗

Identifying Dense NiSe 2 /CoSe 2 Heterointerfaces Coupled with Surface High-Valence Bimetallic Sites for Synergistically Enhanced Oxygen Electrocatalysis

Constructing heterostructures with abundant interfaces is essential for integrating the multiple functionalities in single entities. Herein, the synthesis of NiSe 2 /CoSe 2 heterostructures with different interfacial densities via an innovative strategy of successive ion injection is reported. The resulting hybrid electrocatalyst with dense heterointerfaces exhibits superior electrocatalytic properties in an alkaline electrolyte, superior to other benchmarks and precious metal catalysts. Advanced synchrotron techniques, post structural characterizations, and density functional theory (DFT) simulations reveal that the introduction of atomic-level interfaces can lower the oxidation overpotential of bimetallic Ni and Co active sites (whereas Ni$^{2+}$ can be more easily activated than Co$^{2+}$) and induce the electronic interaction between the core selenides and surface in situ generated oxides/hydroxides, which play a critical role in synergistically reducing energetic barriers and accelerating reaction kinetics for catalyzing the oxygen evolution. Hence, the heterointerface structure facilitates the catalytic performance enhancement via increasing the intrinsic reactivity of metallic atoms and enhancing the synergistic effect between the inner selenides and surface oxidation species. This work not only complements the understanding on the origins of the activity of electrocatalysts based on metal selenides, but also sheds light on further surface and interfacial engineering of advanced hybrid materials.

36 MATERIALS SCIENCE↗

Interfacial Defect of Lithium Metal in Solid‐State Batteries

Abstract All‐solid‐state battery with Li metal anode is a promising rechargeable battery technology with high energy density and improved safety. Currently, the application of Li metal anode is plagued by the failure at the interfaces between lithium metal and solid electrolyte (SE). However, little is known about the defects at Li–SE interfaces and their effects on Li cycling, impeding further improvement of Li metal anodes. Herein, by performing large‐scale atomistic modeling of Li metal interfaces with common SEs, we discover that lithium metal forms an interfacial defect layer of nanometer‐thin disordered lithium at the Li–SE interfaces. This interfacial defect Li layer is highly detrimental, leading to interfacial failure such as pore formation and contact loss during Li stripping. By systematically studying and comparing incoherent, coherent, and semi‐coherent Li–SE interfaces, we find that the interface with good lattice coherence has reduced Li defects at the interface and has suppressed interfacial failure during Li cycling. Our finding discovered the critical roles of atomistic lithium defects at interfaces for the interfacial failure of Li metal anode, and motivates future atomistic‐level interfacial engineering for Li metal anode in solid‐state batteries.

Yang, Menghao↗