Search NASA⌕ Search

SEARCH · Search NASA

Results for “predictive lifetime”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Stirling engine: Available tools for long-life assessment

A review is presented for the durability approaches applicable to long-time life assessment of Stirling engine hot-section components. The crucial elements are experimental techniques for generating long-time materials property data (both monotonic and cyclic flow and failure properties); analytic representations of slow strain rate material stress-strain response characteristics (monotonic and cyclic constitutive relations) at high temperatures and low stresses and strains; analytic creep-fatigue-environmental interaction life prediction methods applicable to long lifetimes at high temperatures and small stresses and strains; and experimental verification of life predictions. Long-lifetime design criteria for materials of interest are woefully lacking. Designing against failures due to creep, creep-rupture, fatigue, environmental attack, and creep-fatigue-environmental interaction will require considerable extrapolation. Viscoplastic constitutive models and time-temperature parameters will have to be calibrated for the hot-section materials of interest. Analysis combined with limited verification testing in a short-time regime will be required to build confidence in long-lifetime durability models.

Halford, Gary R.↗

Stirling engine - Available tools for long-life assessment

A review is presented for the durability approaches applicable to long-time life assessment of Stirling engine hot-section components. The crucial elements are experimental techniques for generating long-time materials property data (both monotonic and cyclic flow and failure properties); analytic representations of slow strain rate material stress-strain response characteristics (monotonic and cyclic constitutive relations) at high temperatures and low stresses and strains; analytic creep-fatigue-environmental interaction life prediction methods applicable to long lifetimes at high temperatures and small stresses and strains; and experimental verification of life predictions. Long-lifetime design criteria for materials of interest are woefully lacking. Designing against failures due to creep, creep-rupture, fatigue, environmental attack, and creep-failure-environmental interaction will require considerable extrapolation. Viscoplastic constitutive models and time-temperature parameters will have to be calibrated for the hot-section materials of interest. Analysis combined with limited verification testing in a short-time regime will be required to build confidence in long-lifetime durability models.

Halford, Gary R.↗

Advanced ceramic coating development for industrial/utility gas turbine applications

The effects of ceramic coatings on the lifetimes of metal turbine components and on the performance of a utility turbine, as well as of the turbine operational cycle on the ceramic coatings were determined. When operating the turbine under conditions of constant cooling flow, the first row blades run 55K cooler, and as a result, have 10 times the creep rupture life, 10 times the low cycle fatigue life and twice the corrosion life with only slight decreases in both specific power and efficiency. When operating the turbine at constant metal temperature and reduced cooling flow, both specific power and efficiency increases, with no change in component lifetime. The most severe thermal transient of the turbine causes the coating bond stresses to approach 60% of the bond strengths. Ceramic coating failures was studied. Analytic models based on fracture mechanics theories, combined with measured properties quantitatively assessed both single and multiple thermal cycle failures which allowed the prediction of coating lifetime. Qualitative models for corrosion failures are also presented.

Andersson, C. A.↗

Analysis of Present Day and Future OH and Methane Lifetime in the ACCMIP Simulations

Results from simulations performed for the Atmospheric Chemistry and Climate Modeling Intercomparison Project (ACCMIP) are analysed to examine how OH and methane lifetime may change from present day to the future, under different climate and emissions scenarios. Present day (2000) mean tropospheric chemical lifetime derived from the ACCMIP multi-model mean is 9.8+/-1.6 yr (9.3+/-0.9 yr when only including selected models), lower than a recent observationally-based estimate, but with a similar range to previous multi-model estimates. Future model projections are based on the four Representative Concentration Pathways (RCPs), and the results also exhibit a large range. Decreases in global methane lifetime of 4.5 +/- 9.1% are simulated for the scenario with lowest radiative forcing by 2100 (RCP 2.6), while increases of 8.5+/-10.4% are simulated for the scenario with highest radiative forcing (RCP 8.5). In this scenario, the key driver of the evolution of OH and methane lifetime is methane itself, since its concentration more than doubles by 2100 and it consumes much of the OH that exists in the troposphere. Stratospheric ozone recovery, which drives tropospheric OH decreases through photolysis modifications, also plays a partial role. In the other scenarios, where methane changes are less drastic, the interplay between various competing drivers leads to smaller and more diverse OH and methane lifetime responses, which are difficult to attribute. For all scenarios, regional OH changes are even more variable, with the most robust feature being the large decreases over the remote oceans in RCP8.5. Through a regression analysis, we suggest that differences in emissions of non-methane volatile organic compounds and in the simulation of photolysis rates may be the main factors causing the differences in simulated present day OH and methane lifetime. Diversity in predicted changes between present day and future OH was found to be associated more strongly with differences in modelled temperature and stratospheric ozone changes. Finally, through perturbation experiments we calculated an OH feedback factor (F) of 1.24 from present day conditions (1.50 from 2100 RCP8.5 conditions) and a climate feedback on methane lifetime of 0.33+-0.13 yr/K, on average. Models that did not include interactive stratospheric ozone effects on photolysis showed a stronger sensitivity to climate, as they did not account for negative effects of climate-driven stratospheric ozone recovery on tropospheric OH, which would have partly offset the overall OH/methane lifetime response to climate change.

atmospheric composition↗

Recent results from Long Duration Exposure Facility materials testing

The overall goals of the Long Duration Exposure Facility (LDEF) investigations, established by the Materials Special Investigation Group (MSIG) prior to LDEF retrieval, are to provide useful engineering data to people designing and building spacecraft, and secondarily, to obtain data of potential interest to materials researchers. The specific objectives are to support predictions of materials lifetimes under the various low earth orbit (LEO) environments to determine how long the material will physically survive; to estimate the engineering performance lifetimes of these same materials under specific LEO exposures; to identify materials and processes by which given materials degrade; and to provide insights into development of new, more inherently LEO environmentally resistant materials. To achieve the established objectives, two criteria were established to select which materials had the highest priorities for analyses. The first criteria was to examine materials which are still being used on new spacecraft. The second priority was to examine materials with multiple exposure locations on LDEF, because this provided the opportunity to develop predictions on how a material will behave as the exposure environment varies. The goals as defined led to the identification of silverized Teflon (Ag/FEP), chromic acid anodized aluminum, and certain thermal control paints used on LDEF as the material types of highest priority for examination. Ag/FEP was chosen because of an excellent a/e ratio (extremely low), and extensive flight history. Also influencing the decision was the fact that the Hubble Space Telescope uses Ag/FEP as its primary passive thermal control system (and was launched shortly after LDEF retrieval) and that a number of other spacecraft are using or considering this material for use. The various forms of Ag/FEP were used on virtually every side of the LDEF except the earth end. The potential uses of this material, and the location distribution and therefore, exposure conditions, have provided the rationale and opportunity for a comprehensive study of this material.

Pippin, H. Gary↗

Type-II seesaw dominance in nonsupersymmetric and split-supersymmetry SO(10) models and proton lifetime

Recently type-II seesaw in a supersymmetricSO(10) framework has been found useful in explaining large solar and atmospheric mixing angles as well as a larger value of {theta}{sub 13} while unifying quark and lepton masses. An important question in these models is whether there exists consistency between coupling unification and type-II seesaw dominance. Scenarios where this consistency can be demonstrated have been given in a SUSY framework. In this paper we give examples where type-II dominance occurs in SO(10) models without supersymmetry but with additional TeV-scale particles and also in models with split-supersymmetry. Grand unification is realized in a two step process via breaking of SO(10) to SU(5) and then to a TeV-scale standard model supplemented by extra fields and an SU(5) Higgs multiplet 15{sub H} at a scale of about 10{sup 12} GeV to give a type-II seesaw. The predictions for proton lifetime in these models are in the range {tau}{sub p}{sup 0}=2x10{sup 35} yrs. to 6x10{sup 35} yrs. A number of recent numerical fits to GUT-scale fermion masses can be accommodated within this model.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Modeling the Impact of the Organic Aerosol Phase State on Multiphase OH Reactive Uptake Kinetics and the Resultant Heterogeneous Oxidation Timescale of Organic Aerosol in the Amazon Rainforest

Accurate predictions of chemical lifetime, i.e., oxidation timescale and change in the mass of organic aerosols (OAs) in atmospheric models, are critical to quantify the impacts of OA on aerosol–cloud interactions, radiative forcing, and air quality. The heterogeneous oxidation of OA by hydroxyl (OH) radicals is a key process governing OA mass changes during their oxidation. Recently, laboratory observations of the OH uptake coefficient (γ OH ) and heterogeneous reaction rate (k het,OH ) for different OA systems with varying phase states have been combined to develop a new parameterization of γ OH and k het,OH as a function of the OA phase state, i.e., viscosity (η OA ). Here, in this work, we use a recently published viscosity prediction framework to analyze the new γ OH and k het,OH parameterization with a box model. Subsequently, we implement this box model to predict γ OH and k het,OH over the Amazon rainforest in the dry-to-wet transition season with both significant biomass burning and biogenic influences. Relevant parameters within our box model are specified based on detailed regional model simulations over the Amazon using the Weather Research and Forecasting model coupled with Chemistry (WRF-Chem). η OA is predicted as a function of species volatility, OA composition (including water uptake) along with ambient relative humidity (RH), and temperature. Based on ambient conditions simulated by WRF-Chem over the entire atmospheric column, we use the box model to predict the upper bounds of the heterogeneous oxidation timescale of OA. Based on previous laboratory measurements, we assume that this heterogeneous OH oxidation causes fragmentation (carbon loss) of OA, followed by the evaporation of the fragmented molecules that results in the exponential decay of OA. We predict that the oxidation timescale of OA is ~1 month near the Earth’s surface in the pristine Amazonian background because of low OH concentrations. But OA is oxidized more rapidly within urban and wildfire plumes near the Earth’s surface with an order of magnitude higher OH concentrations compared to the pristine background, causing the simulated oxidation timescale of OA to be much shorter, ~3–4 days. At 3–5 km altitudes where biomass burning OA is predicted to be semisolid, the heterogeneous oxidation timescale is estimated as ~6 days to 3 weeks and decreases with increasing OH concentrations within plumes. We show that the simulated mass loss of OA is strongly size-dependent, where smaller particles oxidize more rapidly compared to larger particles due to their greater per-particle surface area-to-volume ratio. Increasing urbanization and deforestation in the Amazon in the future might increase OH concentrations in the background Amazon, causing faster oxidation of OA. At higher altitudes above liquid clouds, especially in the upper troposphere where temperatures approach ~250 K, future measurements are needed to reduce the uncertainties related to the mass loss of OA at colder temperatures and low relative humidity conditions due to its heterogeneous OH oxidation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Significant Improvements to Si Calendar Lifetime Using Rapid Electrolyte Screening via Potentiostatic Holds

Silicon-based lithium-ion batteries exhibit severe time-based degradation resulting in poor calendar lives. This has been identified as the major impediment towards commercialization with cycle life considered a solved issue through nanosizing and protective coatings allowing over 1000 cycles of life to be achieved. In this work, rapid screening of sixteen electrolytes for calendar life extension of Si-rich systems (70 wt% Si) is performed using the voltage hold (V-hold) protocol. V-hold significantly shortens the testing duration over the traditional open circuit voltage reference performance test allowing us to screen electrolytes within a span of two months. We find a novel ethylene carbonate (EC) free electrolyte formulation containing lithium hexafluorophosphate (LiPF 6 ) salt, and binary solvent mix of fluoroethylene carbonate (FEC), ethyl methyl carbonate (EMC) that extends calendar life of Si cells as compared to conventional EC based electrolyte. Our coupled experimental-theoretical analysis framework provides a decoupling of the parasitic currents during V-hold, allowing us to extrapolate the capacity loss to predict semiquantitative calendar lifetimes. Subsequently, cycle aging and oxidative stability tests of the EC free system also show enhanced performance over baseline electrolyte.

25 ENERGY STORAGE↗

Accelerated test protocols to predict service life and durability of solid oxide fuel cells

Reliable accelerated test protocols are needed for solid oxide fuel cell research to facilitate rapid learning on key durability issues, identify potential modes of failure expeditiously, and eventually predict the calendar lifetime of an electrochemical cell. In this work, solid oxide fuel cells operated at a constant current density were compared to cells undergoing accelerated measurements, which are composed of intermittent current injection to the cell. A general accelerated test profile was developed by cycling a solid oxide fuel cell from open circuit to a predetermined operating current density that is the same as the current density during a steady-state operation, to accelerate the local redox environment. The following parameters were studied: current density, operation temperature, moist level, sintering temperature, cycling current, cycling frequency, and operation time. Up to 1,320,000 cycles were generated in this work. The cell degradation was accelerated by nearly 10 times, suggesting the feasibility of using this protocol for acceleration test to predict life performance and durability of solid oxide fuel cells.

08 HYDROGEN↗

Evidence for a dispersion in the lithium abundances of extreme halo stars

Evidence is presented to the effect that there exists a small dispersion in the lithium abundances of extreme halo dwarfs. This dispersion cannot be accounted for by standard stellar models alone, particularly toward the turnoff, and would thus require early differential Galactic Li enrichment, perhaps independent of metallicity. The magnitude of the dispersion is also consistent with the predictions of evolutionary models of halo stars with rotation, which do not require, but do not rule out either, early Galactic enrichment. These rotational models also predict a significant depletion in the lithium abundance during the stars' lifetime. The rotational models predict that stars which formed with very low initial angular momentum will have lithium abundances measurably above the plateau.

Deliyannis, Constantine P.↗

Plasma Surface Interactions: Bridging from the Surface to the Micron Frontier through Leadership Class Computing (Final Technical Progress Report)

The performance demands on plasma-facing components (PFCs) in future fusion power plants are beyond the capability of current materials. In defining the plasma-surface interaction (PSI), it is evident that three coupled spatial regions influence PFC materials evolution and performance. These regions consist of (1) the edge and scrape-off layer region of the plasma, (2) the near-surface material response to extreme thermal and particle fluxes under the influence of, and feedback to, the plasma sheath, and (3) the structural material’s response to an intense, 14 MeV peaked neutron spectrum, which produces very high concentrations of transmuted elements through (n,p) and (n,α) reactions and structural material property degradation. The objective of this project is to develop and deploy validated, high-performance simulation tools capable of predicting the performance of tungsten-based plasma-facing components (PFCs) in a burning fusion plasma environment, which includes modeling surface morphology evolution in either erosion or re-deposition regimes, and the recycling of hydrogen species. This requires the development of a leadership-scale computational code to predict PFC behavior that is well integrated to a suite of multiscale modeling techniques to bridge the scales needed to address complex physical and computational issues at the plasma surface interface and the transition region below the surface where neutron damage processes in the bulk dominate material behavior. Successful completion of this project will provide PFC simulation tools to evaluate steady-state performance of tungsten-based PFC and divertor components in burning plasma environments. This will enable the identification of critical experiments to confirm whether practical PFC solutions exist for magnetic fusion energy beyond ITER. More specifically, the research activities within this project focus on two broadly defined research thrusts: 1) Developing a new simulation code, Xolotl-PSI to predict PFC operating lifetime and performance, that is specifically designed to take advantage of leadership class computing facilities; and 2) Integrating and applying discrete particle-based, as well as continuum-based, multiscale modeling techniques to provide scientific discovery of the mechanisms controlling PFC and bulk materials evolution under fusion plasma and 14-MeV neutron exposure; in this thrust, the challenge of scale-bridging between atomistic/microstructural modeling and the continuum-scale of PFC device performance is achieved through multiscale modeling techniques. Throughout the grant period, research at UMass Amherst focused on the atomic-scale analysis of the dynamics and kinetics (transport and reactions) of small mobile helium clusters near surfaces and grain boundaries in plasma-exposed tungsten, as well as the proper parameterization and incorporation of these processes into our SciDAC team’s continuum-level cluster dynamics code (Xolotl). Our work also included characterization of large-scale molecular-dynamics (MD) simulation results of helium implantation into tungsten based on the findings of our analysis and comparisons of Xolotl simulation predictions with the large-scale MD simulation results for Xolotl validation purposes; emphasis was placed on the impact of helium cluster dynamics/kinetics on tungsten surface morphology, near-surface tungsten structure, and helium retention. Furthermore, our work included initiation of a research program on evaluating the impact of structural defects in tungsten due to plasma exposure (such as helium nanobubbles) on tungsten’s thermophysical properties, focusing on lattice thermal conductivity. Our studies contributed to a fundamental understanding of the effects of plasma-surface interactions on the dynamical response of plasma-facing materials in nuclear fusion devices and the development of predictive hierarchical multiscale computational tools for the quantitative description of the material’s dynamical response to plasma exposure.

36 MATERIALS SCIENCE↗

Effect of Specimen Thickness on Microstructural Changes During Oxidation of the NiCrW Alloy 230 at 950–1050°C

An accurate procedure for predicting oxidation-induced damage and lifetime limits is crucial for the reliable operation of high-temperature metallic components in practical applications. In order to develop a predictive oxidation lifetime model for Ni–Cr alloys, specimens of wrought NiCrW alloy 230 with different thicknesses were cyclically oxidized in air at 950–1050°C for up to 3000 h. After prolonged exposure, two types of carbides as well as a Cr-rich nitride (π-phase) precipitated in the γ-Ni matrix. In the case of oxidation-induced loss of Cr from the alloy resulted in the formation of subscale zones, which were free of the Cr-rich carbide and nitride but also of the Ni-W rich M 6 C. The width of the M 6 C-free zone was smaller than that free of the Cr-rich precipitates. Thermodynamic and diffusion calculations of the observed time- and temperature-dependent Cr depletion processes identified that back diffusion of C occurred which resulted in an increased volume fraction of M 23 C 6 in the specimen core. Moreover, with increasing time and temperature, the amount of π-phase in the specimen core increased. The subscale depletion of the initially present Cr-nitrides and the formation of Cr-nitrides in the specimen center is believed to be related to a mechanism which is qualitatively similar to that described for the Cr carbide enrichment. However, with increasing time and decreasing specimen thickness, N uptake from the atmosphere becomes apparent. As a result, the precipitates present in the specimen center eventually consisted almost exclusively of nitrides.

36 MATERIALS SCIENCE↗

Submerged Medium Voltage Cable Systems at Nuclear Power Plants: A Review of Research Efforts Relevant to Aging Mechanisms and Condition Monitoring

In a submerged environment, power cables may experience accelerated insulation degradation due to water-related aging mechanisms. Direct contact with water or moisture intrusion in the cable insulation system has been identified in the literature as a significant aging stressor that can affect performance and lifetime of electric cables. Progressive reduction of the dielectric strength is commonly a result of water treeing which involves the development of permanent hydrophilic structures in the insulation coinciding with the absorption of water into the cable. Water treeing is a phenomenon in which dendritic microvoids are formed in electric cable insulation due to electrochemical reactions, electromechanical forces, and diffusion of contaminants over time. These reactions are caused by the combined effects of water presence and high electrical stresses in the material. Water tree growth follows a tree-like branching pattern, increasing in volume and length over time. Although these cables can be “dried out,” water tree degradation, specifically the growth of hydrophilic regions, is believed to be permanent and typically worsens over time. Based on established research, water treeing or water induced damage can occur in a variety of electric cables including XLPE, TR-XLPE and other insulating materials, such as EPR and butyl rubber. Once water trees or water induced damage form, the dielectric strength of an insulation material will decrease gradually with time as the water trees grow in length, which could eventually result in failure of the insulating material. Under wet conditions or in submerged environments, several environmental and operational parameters can influence water tree initiation and affect water tree growth. These parameters include voltage cycling, field frequency, temperature, ion concentration and chemistry, type of insulation material, and the characteristics of its defects. In this effort, a review of academic and industrial literature was performed to identify: 1) findings regarding the degradation mechanisms of submerged cabling and 2) condition monitoring methods that may prove useful in predicting the remaining lifetime of submerged medium voltage power cables. The research was conducted by a multi-disciplinary team, and sources included official NRC reports, national laboratory reports, IEEE standards, conference and journal proceedings, magazine articles, PhD dissertations, and discussions with experts. The purpose of this work was to establish the current state-of-the-art in material degradation modeling and cable condition monitoring techniques and to identify research gaps. Subsequently, future areas of focus are recommended to address these research gaps and thus strengthen the efficacy of the NRC’s developing cable condition monitoring program. Results of this literature review and details of the testing recommendations are presented in this report.

24 POWER TRANSMISSION AND DISTRIBUTION↗

Platelet composite coatings for tin whisker mitigation

In this study, reliable methods for tin whisker mitigation are needed for applications that utilize tin-plated commercial components. Tin can grow whiskers that can lead to electrical shorting, possibly causing critical systems to fail catastrophically. The mechanisms of tin whisker growth are unclear and this makes prediction of the lifetimes of critical components uncertain. The development of robust methods for tin whisker mitigation is currently the best approach to eliminating the risk of shorting. Current mitigation methods are based on unfilled polymer coatings that are not impenetrable to tin whiskers. In this paper we report tin whisker mitigation results for several filled polymer coatings. The whisker-penetration resistance of the coatings was evaluated at elevated temperature and high humidity and under temperature cycling conditions. The composite coatings comprised Ni and MgF 2 -coated Al/Ni/Al platelets in epoxy resin or silicone rubber. In addition to improved whisker mitigation, these platelet composites have enhanced thermal conductivity and dielectric constant compared with unfilled polymers.

36 MATERIALS SCIENCE↗

Effects of the Electron Beam Welding Process on the Microstructure, Tensile, Fatigue and Fracture Properties of Nickel Alloy Nimonic 80A

The purpose of this study was to evaluate rotary bending high-cycle fatigue properties and crack growth of Nimonic 80A-based metal and electron beam-welded joints. All the tests were performed at room temperature. Fracture surfaces under high-cycle fatigue and fatigue crack growth were observed by scanning electron microscopy. Microstructure, hardness and tensile properties were also evaluated in order to understand the effects on the fatigue results obtained. It was found that the tensile properties, hardness and high-cycle fatigue properties of the welded joint are lower than the base metal. The fracture surface of the high-cycle fatigue shows that fatigue crack initiated from the surface under the high stress amplitude and from the subsurface under the low stress amplitude. The effect of the welding process on the statistical fatigue data was studied with a special focus on probabilistic life prediction and probabilistic lifetime limits. The fatigue crack growth rate versus stress intensity factor range data were obtained from the fatigue crack growth tests. From the results, it was evident that the fatigue crack growth rates of the welded are higher than the base metal. The mechanisms and fracture modes of fatigue crack growth of welded specimens were found to be related to the stress intensity factor range ΔK. In addition, the effective fatigue crack propagation thresholds and mismatch of welded joints were described and discussed.

36 MATERIALS SCIENCE↗

Uncovering the Role of Hole Traps in Promoting Hole Transfer from Multiexcitonic Quantum Dots to Molecular Acceptors

The understanding of electronic dynamics in multiexcitonic quantum dots (QDs) is important for designing efficient systems useful in high power scenarios, such as solar concentrators and multielectron charge transfer. The multiple charge carriers within a QD can undergo undesired Auger recombination events, which rapidly annihilate carriers on picosecond time scales and generate heat from absorbed photons instead of useful work. Compared to the transfer of multiple electrons, the transfer of multiple holes has proven to be more difficult due to slower hole transfer rates. To probe the competition between Auger recombination and hole transfer in CdSe, CdS, and CdSe/CdS QDs of varying sizes, we synthesized a phenothiazine derivative with optimized functionalities for binding to QDs as a hole accepting ligand and for spectroscopic observation of hole transfer. Transient absorption spectroscopy was used to monitor the photoinduced absorption features from both trapped holes and oxidized ligands under excitation fluences where the averaged initial number of excitons in a QD ranged from ~1 to 19. We observed fluence-dependent hole transfer kinetics that last around 100 ps longer than the predicted Auger recombination lifetimes, and the transfer of up to 3 holes per QD. Theoretical modeling of the kinetics suggests that binding of hole acceptors introduces trapping states significantly different from those in native QDs passivated with oleate ligands. Holes in these modified trap states have prolonged lifetimes, which promotes the hole transfer efficiency. These results highlight the beneficial role of hole-trapping states in devising hole transfer pathways in QD-based systems under multiexcitonic conditions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

How spin relaxes and dephases in bulk halide perovskites

Abstract Spintronics in halide perovskites has drawn significant attention in recent years, due to their highly tunable spin-orbit fields and intriguing interplay with lattice symmetry. Here, we perform first-principles calculations to determine the spin relaxation time ( T 1 ) and ensemble spin dephasing time ( $${T}_{2}^{*}$$ T 2 * ) in a prototype halide perovskite, CsPbBr 3 . To accurately capture spin dephasing in external magnetic fields we determine the Landé g -factor from first principles and take it into account in our calculations. These allow us to predict intrinsic spin lifetimes as an upper bound for experiments, identify the dominant spin relaxation pathways, and evaluate the dependence on temperature, external fields, carrier density, and impurities. We find that the Fröhlich interaction that dominates carrier relaxation contributes negligibly to spin relaxation, consistent with the spin-conserving nature of this interaction. Our theoretical approach may lead to new strategies to optimize spin and carrier transport properties.

74 ATOMIC AND MOLECULAR PHYSICS↗