Search NASA⌕ Search

SEARCH · Search NASA

Results for “recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 433 records · Page 24

Effect of intermediate annealing time on microstructure, texture and mechanical properties of Al-Mg-Si-Cu alloy

Highlights: • Long intermediate annealing time could be beneficial to the improvement of deep drawability. • Long intermediate annealing time could give rise to more particles with a larger average size. • As intermediate annealing time increases, strength will change and it has no positive correlation with annealing time, • A particle dissolution model is proposed to illustrate the variation of the strengths with intermediate annealing time. - Abstract: The effect of intermediate annealing time on the microstructure, texture and mechanical properties of Al-Mg-Si-Cu alloys was studied by mechanical properties, microstructure and texture characterization in the present study. The results show that the intermediate annealing time has some influence on the microstructure, recrystallization texture, and final mechanical properties. After the pre-aging treatment and natural aging treatment (T4P treatment), in contrast to the sheet with short intermediate annealing time, the sheet with long intermediate annealing time possesses higher plastic strain ratio r value. Strength has no positive correlation with annealing time, and when applying the annealing time of 16 h, the strength is highest. Before solution treatment, the sheet with long intermediate annealing time has more particles with a larger average size, compared with the sheet with short intermediate annealing time. After solution treatment, they possess the similar recrystallization equiaxed grain structure and recrystallization texture. The sheet with short intermediate annealing time is comprised of Cube{sub ND} {001} <310>, Goss {110}<001> and P {011}<122> orientations, while the sheet with long intermediate annealing time possesses weak texture including Cube{sub ND} {001}<310>, Goss {110}<001> and {015}<751> orientations. Finally, a particle dissolution model during solution treatment is proposed to explain the variation of strength with annealing time.

36 MATERIALS SCIENCE↗

Microstructure and texture evolution of duplex stainless steels with different molybdenum contents

Highlights: • The 3.05Mo steel has higher resistance to strain-induced transformation than the 0.28Mo steel. • The increased Mo content affects the grain growth of austenite and ferrite due to the effects of segregation and anchoring. • At high annealing temperatures, this Mo retarding effect is weakened. • The suppression of γ-fiber development in the ferrite texture is associated with the increased Mo content. • High amounts of Mo generate unfavorable conditions for the formation of CSL boundaries. - Abstract: The microstructure and texture evolution of duplex stainless steels with different molybdenum contents were studied. For this purpose, hot-rolled 2205 and 2304 samples were solution-annealed at 1100 °C for 1800 s and then cold-rolled to a 75% thickness reduction. This was followed by an isothermal annealing at 900 and 1100 °C for 180 s. The EBSD technique was used to determine the phase ratio, crystallographic texture, and microstructural characteristics. The hot-rolled steel had a work hardened microstructure and the samples submitted to intermediate annealing presented mainly deformation-free grains. Cold rolling resulted in a substantial reduction in the phase spacing with the formation of the strain-induced α′-martensite (SIM) from the metastable austenite. After annealing at 900 °C, the ferrite grains retained the elongated shape of the cold-rolled condition and the primary recrystallization progressed in the austenite phase. Increasing the Mo content increased the resistance to strain-induced martensitic transformation and inhibited the grain growth of austenite phase during annealing at 900 °C. Increasing annealing temperature to 1100 °C promoted the coarsening of both bcc and fcc structures with the formation of annealing twins in the austenitic grains. The recrystallization kinetics and subsequent grain growth occur earlier in ferrite than in austenite phase. Differences in Mo content did not significantly alter the evolution of austenite texture, whereas in the ferrite phase the increase in Mo content suppressed the γ-fiber development. Oriented nucleation was the predominant mechanism observed during the recrystallization of ferritic grains in the 2205 samples. The development of ∑19a boundaries was associated with the selected growth of {554}<225>{sub α} grains in the annealed 2304 samples. Annealing twins were associated with the formation of Σ3 boundaries after the heat treatments. Grain coarsening resulted in a larger fraction of the special boundaries in ferrite phase but inhibited the CSL formation in the austenite phase.

36 MATERIALS SCIENCE↗

Multi-scale and multi-technic microstructure analysis of a linear friction weld of the metastable-β titanium alloy Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) towards a new Post-Weld Heat Treatment

Highlights: • Soft joint showing sharp macro-zones and marked by asymmetrical process effects • Gradient of thermomechanical loads identified through progressive stages of transformation • Highly textured recrystallized β grains at the joint core with distorted β lattice • Lattices, phase fractions, microstructures and hardness homogenized after heat treatment - Abstract: Linear Friction Welding (LFW) is a solid-state joining process producing narrow joints mainly developed for the aircraft industry. The Thermo-Mechanical Processing (TMP) loads imposed on the material cause complex microstructure transformations. This study aimed at characterizing the local microstructures and crystallographic configurations to identify the mechanisms impacting the stability and the mechanical properties of a Ti17 LFW joint with the objective of establishing an innovative homogenizing Post-Weld Heat Treatment (PWHT). The process caused a narrow zone of ±2 mm from the friction interface to reach the isothermal α → β transformation temperature under a heating rate of 500 K/s followed by quenching (−100 K/s). The TMP resulted in the formation a ±3 mm wide soft Process Affected Zone (PAZ) delimited by three characteristic zones: the Welding Line (WL width ≈ 400 μm), The Thermo-Mechanically Affected Zone (TMAZ width ≈ 1 mm) and the Heat Affected Zone (HAZ). β TMP resulted in the total dissolution of the α phase in the joint core (WL + TMAZ) and formed strongly textured {110}<111> β recrystallized grains in the WL by continuous dynamic recrystallization of squeezed prior-β grains in the TMAZ. α + β TMP led to a gradual loss of hardness in the HAZ whose microstructure is similar to the one of the base material (BM) but is subject to gradual α laths dissolution due to the local temperatures experienced during LFW. A PWHT consisting in a β annealing followed by an α + β ageing resulted in a uniformly hardened weld with a homogenized Widmanstätten microstructure in the whole assembly.

36 MATERIALS SCIENCE↗

Shape memory and superelasticity of nanograined Ti-51.2 at.% Ni alloy processed by severe plastic deformation via high-ratio differential speed rolling

A novel method of producing nanograined Ni-rich superelastic NiTi alloys in sheet form was proposed using a combination of severe plastic deformation via high-ratio differential speed rolling (HRDSR) and post-deformation annealing. The HRDSR-processed microstructure was composed of heavily deformed austenite and martensite grains, and amorphous phases. After annealing at 673 K, the severely deformed microstructure with no functional properties evolved to the nanograined structure (20–70 nm) composed of austenite and martensite nanograins and sub-nanograins through static recovery or continuous static recrystallization process. The nanograined microstructure had a high resistance to martensitic transformation upon cooling and slip deformation during straining. As a result, the HRDSR-processed alloy annealed at 673K exhibited superior superelasticity compared to the alloys with coarse grains. At the higher annealing temperature of 873 K, the micron-sized recrystallized grains with low dislocations developed through discontinuous static recrystallization process. In this case, deformation during straining was governed by the detwinning of twinned martensite, and as a result, shape memory effect was more significantly pronounced than superelasticity.

36 MATERIALS SCIENCE↗

Elucidation of microstructural evolution of beta-type titanium alloy joint during friction stir welding using liquid CO2 cooling

Highlights: • Microstructural evolution during FSW was elucidated along real material flow line. • Stirring and cooling stages of FSW can be investigated separately using CO{sub 2} cooling. • In stirring stage, discontinuous dynamic recrystallization predominantly occurred. • In cooling stage, static recovery and grain growth mainly occurred. - Abstract: Normal friction stir welding (FSW) and liquid CO{sub 2} cooling FSW were conducted on the β-type Ti-15V-3Cr-3Al-3Sn (Ti-15-3, mass%) alloy plates under a processing condition. Since liquid CO{sub 2} cooling with high cooling efficiency can freeze the microstructure formed during the high-temperature stirring stage of FSW, it is possible to separately elucidate the microstructural evolution of the Ti-15-3 alloy during the high-temperature stirring stage and the post-stirring cooling stage in FSW. The deformation temperature during the normal and the CO{sub 2} cooling FSW was similar in the top and the bottom of stir zone, which is considered to be owing to that the top and bottom are located adjacent to the heat sources, i.e., the shoulder and probe surfaces. In the high-temperature stirring stage of FSW, discontinuous dynamic recrystallization predominantly occurred, and a simple shear texture generated in an early stage of the material flow around the tool, then the microstructure started to evolve steadily after a steady-state dynamic recrystallization. In the post-stirring cooling stage of FSW, static recovery and grain growth were found to mainly occur within the stir zone.

36 MATERIALS SCIENCE↗

Synthesis and electrochemical properties of NiO nanospindles

Graphical abstract: NiO nanospindles with a different electrochemical activity as compared to those previous reports were synthesized via an agglomeration–dissolution–recrystallization growth process without the addition of any surfactant. - Highlights: • NiO nanospindles were synthesized without the addition of any surfactant. • The agglomeration–dissolution–recrystallization growth process was used to explain the precursors’ formation process of the spindle-like NiO. • As-obtained spindle-like NiO showed a different electrochemical activity as compared to those previous reports. - Abstract: NiO nanospindles were successfully synthesized via a hydrothermal and post-treatment method. The as-synthesized nanospindles were about several hundred nanometers in width and about one micrometer in length. X-ray diffraction (XRD) analysis revealed that the spindle-like structure was cubic NiO phase crystalline. Scanning electron microscopy (SEM) and high-resolution transmission electron microscopy (HRTEM) analysis indicated that these NiO nanospindles were of single crystal nature. On the basis of time-dependent experiments, a possible agglomeration–dissolution–recrystallization growth process was proposed to explain the formation process of the spindle-like precursors. The cyclic voltammetry (CV) measurement showed that the as-prepared spindle-like NiO exhibited a pseudo-capacitance behavior.

36 MATERIALS SCIENCE↗

Solid-phase epitaxy of silicon amorphized by implantation of the alkali elements rubidium and cesium

The redistribution of implanted Rb and Cs profiles in amorphous silicon during solid-phase epitaxial recrystallization has been investigated by Rutherford backscattering spectroscopy and secondary ion mass spectroscopy. For the implantation dose used in these experiments, the alkali atoms segregate at the a-Si/c-Si interface during annealing resulting in concentration peaks near the interface. In this way, the alkali atoms are moved towards the surface. Rutherford backscattering spectroscopy in ion channeling configuration was performed to measure average recrystallization rates of the amorphous silicon layers. Preliminary studies on the influence of the alkali atoms on the solid-phase epitaxial regrowth rate reveal a strong retardation compared to the intrinsic recrystallization rate.

36 MATERIALS SCIENCE↗

The structure of CO{sub 2} hydrate between 0.7 and 1.0 GPa

A deuterated sample of CO{sub 2} structure I (sI) clathrate hydrate (CO{sub 2}·8.3 D{sub 2}O) has been formed and neutron diffraction experiments up to 1.0 GPa at 240 K were performed. The sI CO{sub 2} hydrate transformed at 0.7 GPa into the high pressure phase that had been observed previously by Hirai et al. [J. Phys. Chem. 133, 124511 (2010)] and Bollengier et al. [Geochim. Cosmochim. Acta 119, 322 (2013)], but which had not been structurally identified. The current neutron diffraction data were successfully fitted to a filled ice structure with CO{sub 2} molecules filling the water channels. This CO{sub 2}+water system has also been investigated using classical molecular dynamics and density functional ab initio methods to provide additional characterization of the high pressure structure. Both models indicate the water network adapts a MH-III “like” filled ice structure with considerable disorder of the orientations of the CO{sub 2} molecule. Furthermore, the disorder appears to be a direct result of the level of proton disorder in the water network. In contrast to the conclusions of Bollengier et al., our neutron diffraction data show that the filled ice phase can be recovered to ambient pressure (0.1 MPa) at 96 K, and recrystallization to sI hydrate occurs upon subsequent heating to 150 K, possibly by first forming low density amorphous ice. Unlike other clathrate hydrate systems, which transform from the sI or sII structure to the hexagonal structure (sH) then to the filled ice structure, CO{sub 2} hydrate transforms directly from the sI form to the filled ice structure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electron Backscatter Diffraction of CdTe Thin Films: Effects of CdCl2 Treatment

In this work, the authors describe procedures to prepare the surface of close-spaced sublimation CdTe thin films necessary for producing good electron backscatter diffraction (EBSD) data. They found that polishing resulted in an amorphous layer on the surface and no Kikuchi pattern; however, ion-beam milling produced a relatively flat and good-quality surface, resulting in high-quality patterns and, consequently, excellent EBSD data. The authors used a combination of polishing and ion-beam milling or etching to study the crystalline structure of the CdTe film at different depths. They also used EBSD, in conjunction with other analytical techniques, to investigate the effects of the CdCl{sub 2} treatment, performed at different temperatures and times, on the recrystallization process of physical vapor deposition CdTe thin films. The authors found that the untreated films were <111> oriented, with grain sizes smaller than 1 {micro}m. The CdCl{sub 2} at 350 C produced partially recrystallized films, whereas treatments at 400 C or 420 C produced completely recrystallized films, with no texture, and grains with grain sizes varying from about 1 {micro}m to more than 40{micro}m. These films were so flat that good EBSD data could be obtained without any surface preparation. Atomic force microscopy and scanning electron microscopy showed that large grains had different morphologies than smaller grains, and EBSD showed that these large grains had <111> texture. These results indicate that the (111) surface is the lowest energy surface in these films and, consequently, <111>-oriented grains grow at the expense of grains oriented in less-favorable directions. Regardless of the deposition method and treatment, the CdTe films have a high density of 60{sup o} <111> twin boundaries.

14 SOLAR ENERGY↗

The Nature of the Nonsingularity of Inner Interfaces in Hydroxyapatite Ceramics

The morphology of inner interfaces in hydroxyapatite (HA) based calcium phosphate ceramics has been studied by transmission electron microscopy. Grain boundaries in the ceramics have been shown to have a vicinal character, which is related to the mechanism of secondary recrystallization in the material: layer growth of grains via sequential motion of elementary steps on planes corresponding to the {11̄00} HA prism faces, which grow through transitions of atoms from adjacent grains that are in contact through their planes with large Miller indices. The recrystallization process may be accompanied by a “collision” of vicinal growth surfaces of grains with relatively large misalignment angles and the formation of grain boundaries nanofaceted by prism planes of adjacent grains. The recrystallization process in such a case should be expected to continue in the grain with a smaller nonsingularity of the growth front. Grain boundaries may allow for a match between planes differing in Miller indices, nd{sub h1k1l1} ≈ md{sub h2k2l2}, and the formation of grain-boundary Pumphrey dislocations, which compensate for the size mismatch between interplanar spacings and/or misalignment of the planes. The observed characteristic grain match configurations are typical of both ceramics produced by sintering HA powders and HA films produced by ion sputtering.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Redistribution of Erbium and Oxygen Recoil Atoms and the Structure of Silicon Thin Surface Layers Formed by High-Dose Argon Implantation through Er and SiO{sub 2} Surface Films

Using analytical high-resolution electron microscopy, the Si structure and the redistribution of Er and O recoil atoms embedded in thin (~10 nm) surface layers by Ar{sup +} implantation with an energy of 250–290 keV and a dose of 1 × 10{sup 16} cm{sup –2} through Er and SiO{sub 2} films, respectively, and subsequent annealing are studied. It is established that Si recrystallization fails at a distance of ~20 nm from the surface, where the erbium concentration of 5 × 10{sup 19} cm{sup –3} critical for failure is achieved at T = 950°C. It disproves the generally accepted model of Er-atom transfer by the recrystallization front into SiO{sub 2} on the surface. Instead, it is shown that the redistribution of O recoil atoms to the initial oxide during annealing for immobile Er atoms provides the formation of surface-inhomogeneous erbium phases in such a way that the oxygen-enriched Er–Si–O phase turns out to be concentrated in the oxide, while the depleted Er–Si phase remains in Si. It explains the partial loss of implanted Er after removal of the oxide together with the Er–Si–O phase. It was shown that the formation of a high density of microtwins (locally up to 10{sup 13} cm{sup –2}) is associated with the formation of Ar bubbles and clusters, which is atypical for (100)–Si recrystallization.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Ionization-induced effects in amorphous apatite at elevated temperatures

Electron-beam induced effects in pre-amorphized Sr2Nd8(SiO4)6O2 is investigated in situ using transmission electron microscopy with 200 keV electrons at temperatures ranging from 380 to 780 K. While epitaxial recrystallization is observed from amorphous/crystalline toward surface within the electron irradiated area with its rate increasing as temperature increases from 380 to 580 K, structural contrast features (i.e., O deficient amorphous materials) as well as recrystallization are observed even outside of the irradiation area at temperatures from 680 to 780 K. Ionization-induced processes and local non-stoichiometry induced by oxygen migration and desorption are possible mechanisms for the electron-beam induced recrystallization and for the formation of the structural contrast features, respectively.

58 GEOSCIENCES↗

Rare Earth Phosphate Glass and Glass-Ceramic Proton Conductors

The structure and conductivity of cerium and lanthanum phosphate glasses and glass-ceramics were investigated. The effects of varying the metal to phosphate ratio in the glasses, doping LaP3O9 glasses with Ce, and recrystallization of CeP3O9 glasses, on the glasses' microstructure and total conductivity were investigated using XRD, SEM, and AC impedance techniques. Strong increases in conductivity occurred when the glasses were recrystallized: the conductivity of a cerium metaphosphate glass increased conductivity after recrystallization from 10-7.5 S/cm to 10-6 S/cm at 400oC.

30 DIRECT ENERGY CONVERSION↗

Comparative Characterization of Magnetic Properties of Textured Ni–5 at.%W Alloy Substrates

The hysteresis loss of Ni–5 at.%W (Ni5W) substrate contributes considerably to the alternating current (AC) loss of coated conductors (CCs) working at low transporting current or low-frequency field. In the present work, the evolution of texture and magnetic properties in Ni5W substrates is analyzed and also the relationship between magnetic properties and the extrinsic characteristics (evolved due to the processing techniques) is determined. By making the comparison, we discovered the magnetic domain structures of Ni5W substrates for the first time, achieving a strip/branched domain structures in the recrystallized substrates. The hysteresis loss has been decreased dramatically for the recrystallized substrates. Interestingly, we also observed that this loss is also related to the annealing temperature in the fully recrystallized substrates. The reduced loss can be mainly attributed toward the decrease of grain boundary, which proves the contribution of grain size toward the reduction of hysteresis loss. This result provides a new insight to tailor the hysteresis loss of Ni5W substrates used for coated conductors.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Creep Deformation and Dynamic Grain Growth in an Interstitial-Free Steel

Dynamic grain growth is demonstrated to be much faster than static grain growth in a body-centered-cubic, interstitial-free steel sheet material at 850°C. Dynamic grain growth occurs during concurrent plastic deformation at elevated temperature, whereas static grain growth occurs during static annealing. Grain growth during steady-state plastic flow in tension at 850°C to a true strain of 0.2 at a true-strain rate of 10 -4 s -1 doubled grain size, while static annealing for the same time produced no increase in grain size. This is described as dynamic normal grain growth (DNGG) because no abnormally large grains were observed. The recrystallized microstructure of the steel demonstrated a log-normal distribution of grain sizes. DNGG produced bimodal grain size distributions that deviate from the theoretical expectation of a simple shift to larger sizes during normal growth. The bimodal distributions contained a remnant of small grains that were not consumed during grain growth. DNGG produced a crystallographic texture that is unique from both the recrystallized material and that produced by lattice rotation alone. DNGG strengthened the {111}&lang;110&rang; and {111}&lang;112&rang; components of the strong γ-fiber component in the original recrystallization texture. Lattice rotation from tensile deformation, by contrast, strengthened the α-fiber components that intersect the original γ-fiber.

36 MATERIALS SCIENCE↗

Sagging Mechanisms of Three-Layer Aluminum Clad Foils used in the Heat Exchanger in the Brazing Process

The sagging mechanisms of a three-layer aluminum clad foils (AA4343/AA3003Mod/AA4343) with final rolling reduction of 20-50% during brazing were studied. The results show that the sagging behavior of the aluminum brazed foils during the brazing cycle can be divided into four stages: Stage I is the slight sagging stage, during which sagging deformation can almost be ignored; Stage II is referred to as the accelerative sagging stage, and the sagging behavior is mainly ascribed to recovery. In stage II, the greater the reduction ratio is, the earlier the recovery ends, and the smaller the value of the sagging distance is. Stage III is the slow sagging stage, and sliding deformation along the grain boundaries is responsible for the slow sagging rate. Stage IV is the erosion stage. During stage IV, the coarsely recrystallized grains can inhibit erosion and are helpful in obtaining excellent sagging resistance, while the foils with finely recrystallized grains or non-recrystallized structure show severe erosion and limited sagging resistance.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Property Inhomogeneities of a Modified AZ80 Magnesium Alloy Wide Plate Under Horizontal Flat Die Extrusion

In the present paper, inhomogeneities in the microstructure and mechanical properties of a modified AZ80 plate under industrial production conditions were investigated. The results indicated that the microstructure of the edge and middle region shows more homogeneous and fine recrystallized grains. Additionally, more coarse recrystallized grains existed between the edge and the middle region. The ultimate tensile strength and yield strength of the edge region of the plate are maximal (287 and 162 MPa), and those near the 1/8 W region are minimal (259 and 152 MPa). The grain size increased from 19.5 to 27.2 μm along the center layer to the surface layer. The ultimate tensile stress (yield stress) increases from 258 (121 MPa) to 284 MPa (176 MPa) in the direction from the surface layer to the middle layer. The microhardness decreased from the surface layer (72HV) to the center layer (64HV). The metal strain state and temperature distribution lead to different degrees of dynamic recrystallization, which causes the microstructure and mechanical properties of the plate.

36 MATERIALS SCIENCE↗

Flow Characteristics of a Medium–High Carbon Mn-Si-Cr Alloyed Steel at High Temperatures

This study investigates the deformation behavior of a medium–high carbon Mn-Si-Cr alloyed steel using hot compression tests. The tests were performed on a Gleeble 1500D thermomechanical simulator with a temperature range of 950–1150 °C and a strain rate range of 0.005–5 s{sup −1}. The processing parameters (i.e., temperature T, strain rate ε-dot , and strain ε) influenced the flow softening behavior of the material. The dynamic recrystallization occurred during hot deformation. Correlations between the Zener–Hollomon parameter and the size and the volume fraction of new recrystallized grains were developed. These findings are described using mathematical models. The strain-compensated Arrhenius-type constitutive model and the multiple-linear model were developed based on the true stress–strain curves we obtained. A comparative study was performed in order to measure the validity of the two models in representing hot deformation behavior. Both models were shown to accurately predict flow stress across a range of conditions, reflecting the characteristics of true stress–strain curves by exhibiting work hardening, dynamic recovery, and dynamic recrystallization. The empirical multiple-linear mathematical model was shown to be more efficient and accurate when calculating the hot deformation behavior of steel at elevated temperatures.

36 MATERIALS SCIENCE↗