Ultrahigh Molecular Weight Aromatic Siloxane Polymers
Silphenylene-siloxane polymers can be prepared by a condensation reaction of a diol 1,4-bis(hydroxydimethylsilyl)benzene and a silane bis(dimethylamino)dimethylsilane. Using a stepwise condensation technique, a polymer (R=CH3) with a molecular weight in excess of 1.0 x 1 million has been produced. The polymer exhibits increased thermal stability, compared to a methyl siloxane polymer without the aromatic phenyl ring in the backbone. The use of bis(dimethylamino)methylvinylsilane should allow for ready crosslinking at the vinyl sites (R=-CH=CH2) introduced into the backbone. However, under the conditions of the reaction system a high molecular weight polymer was not obtained or the polymer underwent a crosslinking process during the synthesis.