Search NASA⌕ Search

SEARCH · Search NASA

Results for “EXAFS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 451 records · Page 25

The role of titanium-oxo clusters in the sulfate process for TiO 2 production

TiO 2 is manufactured for white pigments, solar cells, self-cleaning surfaces and devices, and other photocatalytic applications. The industrial synthesis of TiO 2 entails: (1) the dissolution of ilmenite ore (FeTiO 3 ) in aqueous sulfuric acid which precipitates the Fe while retaining the Ti in solution, followed by (2) dilution or heating the Ti sulfate solution to precipitate the pure form of TiO 2 . The underlying chemistry of these processing steps remains poorly understood. Here we show that the dissolution of a simple Ti IV -sulfate salt, representative of the industrial sulfate process for the production of TiO 2 , immediately self-assembles into a soluble Ti-octadecameric cluster, denoted as {Ti 18 }. We observed {Ti 18 } in solution by small-angle X-ray scattering and Ti extended X-ray absorption fine structure (Ti-EXAFS) analysis, and ultimately crystallized it for absolute identification. The {Ti 18 } metal-oxo cluster was previously reported as a polycation; but shown here, it can also be a polyanion, dependent on the number of sulfate ligands it carries. After immediate self-assembly, the {Ti 18 }-cluster persists until TiO 2 precipitates, with no easily identified structural intermediates in the solution or solid state, despite the fact that the atomic arrangement of {Ti 18 } differs vastly from that of titania. The evolution from solution phase {Ti 18 } to precipitated TiO 2 nanoparticles was detailed by X-ray scattering and Ti-EXAFS. Here, we offer a hypothesis for the key mechanism of complete separation of Fe from Ti in the industrial sulfate process. These findings also highlight the emerging importance of the unusual Ti(Ti) 5 pentagonal building unit, featured in {Ti 18 } as well as other early d 0 transition metal-oxo clusters including Nb, Mo and W. Finally, this study presents an example of crystal growth mechanisms in which the observed “pre-nucleation cluster” does not necessarily predicate the structure of the precipitated solid.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Operando structural and chemical evolutions of TiS 2 in Na-ion batteries

Titanium disulfide (TiS 2 ) with high electric conductivity, fast rate capability, and good cycling performance is a promising candidate for electrode material in sodium (Na)-ion batteries. Despite the well-studied electrochemical behaviors of TiS 2 in Li-ion batteries, the detailed reaction mechanism of TiS 2 in Na-ion batteries is not yet fully understood due to a more complex multi-phase conversion process. In this work, reactions of TiS 2 in Na-ion batteries are investigated via a multi-modal synchrotron approach: operando X-ray Absorption Spectroscopy (XAS) – including X-ray Absorption Near-Edge Structure (XANES) and Extended X-ray Absorption Fine Structure (EXAFS) – and ex situ X-ray Powder Diffraction (XPD), coupled with computational modeling. Operando XANES spectra indicate that the redox reactions occur in both Ti and S during the electrochemically driven phase transformation. Multivariate Curve Resolution-Alternating Least Squares (MCR-ALS) analysis of XAS suggests that different numbers of components are involved in the lithiation and sodiation of TiS 2 , with the sodiation including at least one intermediate phase in addition to the starting material and the final sodiation product. Ex situ XPD and Rietveld refinement further determined and quantified the unknown phases, showing that three phases, TiS 2 , Na 0.55 TiS 2 , and NaTiS 2 , participate in the sodiation of TiS 2 . Operando EXAFS results show the changes in the Ti–Ti coordination number and interatomic distance. This explains the coulombic efficiency decay due to the incomplete recovery of the coordination number of Ti after cycling. Overall, this work reveals the reaction mechanism occurring in Na–TiS 2 batteries with a greater quantitative understanding of the structural evolution. By combining the multi-modal synchrotron approach and computational work, this study provides a framework for studying a broader range of electrochemically driven phase-transformation systems towards advanced energy storage and conversion applications.

25 ENERGY STORAGE↗

Tungsten-dioxo single-site heterogeneous catalyst on carbon: synthesis, structure, and catalysis

This study investigates the application of a novel third-row metal, tungsten, to carbon-supported single-site metal-oxo heterogeneous catalysis. Tungsten is a green and earth-abundant metal, but an unexplored candidate in this role. The carbon (AC = activated carbon)-supported tungsten dioxo complex, AC/WO 2 was prepared via grafting of (DME)WO 2 Cl 2 (DME = 1,2-dimethoxyethane) onto high-surface-area activated carbon. AC/WO 2 was fully characterized by ICP-OES, XPS, EXAFS, XANES, SMART-EM, and DFT. W 4d 7/2 XPS and W L III -Edge XANES assign the oxidation state as W(VI), while EXAFS reveals two W=O double and two W–O single bonds at distances of 1.73 and 1.92 Å, respectively. These data align well with DFT computational results, supporting the structure as Carbon(–μ-O–) 2 M(=O) 2 . SMART-EM verifies that single W(VI) catalytic sites are bonded in an out-of-plane manner. The catalytic performance of air- and water-stable AC/WO 2 is compared to that of AC/MoO 2 . AC/WO 2 is more active and selective than the molybdenum analog in mediating alcohol dehydration of various substrates, and is recyclable. Notably, AC/WO 2 is an effective and recyclable catalyst for primary aliphatic alcohol dehydration and forms no dehydrogenation side products in contrast to AC/MoO 2 . However, AC/WO 2 is less effective in epoxidation and PET depolymerization. Overall, this work demonstrates the potential of carbon-supported third row metals for future studies.

02 PETROLEUM↗

Nearest-neighbor oxygen distances in liquid water and ice observed by x-ray Raman based extended x-ray absorption fine structure

We report the nearest-neighbor oxygen-oxygen radial distribution function (NN O-O RDF) of room temperature liquid water and polycrystalline ice Ih (-16.8 deg. C) obtained by x-ray Raman based extended x-ray absorption fine structure (EXAFS) spectroscopy. The spectra of the two systems were taken under identical experimental conditions using the same procedures to obtain the NN O-O RDFs. This protocol ensured a measurement of the relative distance distribution with very small systematic errors. The NN O-O RDF of water is found to be more asymmetric (tail extending to longer distances) with longer average distance (2.81 A ring for water and 2.76 A ring for ice) but a slightly shorter peak position (2.70 A ring for water and 2.71 A ring for ice). The refinement also showed a small but significant contribution from the linear O-H-O multiple scattering signal. The high sensitivity to short range distances of the EXAFS probe will set further restrictions to the range of possible models of liquid water.

36 MATERIALS SCIENCE↗

Local structures surrounding Zr in nanostructurally stabilized cubic zirconia: Structural origin of phase stability

Local environment surrounding Zr atoms in the thin films of nanocrystalline zirconia (ZrO{sub 2}) has been investigated by using the extended x-ray absorption fine structure (EXAFS) technique. These films prepared by the ion beam assisted deposition exhibit long-range structural order of cubic phase and high hardness at room temperature without chemical stabilizers. The local structure around Zr probed by EXAFS indicates a cubic Zr sublattice with O atoms located on the nearest tetragonal sites with respect to the Zr central atoms, as well as highly disordered locations. Similar Zr local structure was also found in a ZrO{sub 2} nanocrystal sample prepared by a sol-gel method. Variations in local structures due to thermal annealing were observed and analyzed. Most importantly, our x-ray results provide direct experimental evidence for the existence of oxygen vacancies arising from local disorder and distortion of the oxygen sublattice in nanocrystalline ZrO{sub 2}. These oxygen vacancies are regarded as the essential stabilizing factor for the nanostructurally stabilized cubic zirconia.

36 MATERIALS SCIENCE↗

Extended x-ray absorption fine structure study of arsenic in HgCdTe: p-type doping linked to nonsubstitutional As incorporation in an unknown AsHg{sub 8} structure

An extended x-ray absorption fine structure (EXAFS) investigation has been carried out on arsenic-doped Hg{sub 70}Cd{sub 30}Te samples. The incorporation of atomic arsenic has been achieved using a nonconventional radio-frequency plasma source in a molecular beam epitaxy reactor. Two samples from the same epitaxial wafer have been studied. One underwent a 400 deg. C activation annealing under Hg pressure, leading to n to p-type conversion. In the commonly admitted scenario, this conversion is associated with the annealing-induced migration of As from a Hg site to a Te site. This study shows that this is not the case. Before annealing, As is found to be involved in noncrystalline structures: 50% inside an As{sub 2}Te{sub 3} chalcogenide glass and 50% inside a new AsHg{sub 8} compact structure. After annealing, the As{sub 2}Te{sub 3} chalcogenide glass disappears, 31% of As occupies Hg sites and 69% incorporates inside this new AsHg{sub 8} compact structure that occupies Te sites. The EXAFS results are in excellent agreement with 77 K Hall-effect measurements. The new AsHg{sub 8} structure is found to have an acceptor behavior. Overall, this study provides an entirely new vision of extrinsic p-type doping of HgCdTe as well as the first experimental evidence of As site transfer induced by annealing.

36 MATERIALS SCIENCE↗

Annealing Temperature and Initial Iron Valence Ratio Effects on the Structural Characteristics of Nanoscale Nickel Zinc Ferrite

Nickel zinc ferrite (NZFO) nanoparticles were synthesized via a reverse micelle method with a nonionic surfactant. Three different initial Fe{sup 3+}/Fe{sup 2+} ratios were employed along with three different firing temperatures (200, 500, 1000 C) to investigate the effects on the NZFO system. Extended x-ray absorption fine structure (EXAFS) results reveal zinc loss at high annealing temperatures; at 1000 C, the loss is nearly total for Fe{sup 3+}/Fe{sup 2+} ratios other than 10:90. Annealing at 500 C, however, appears necessary for fully incorporating the zinc and nickel into the spinel phase. The best nanoferrite was thus obtained using an initial Fe{sup 3+}/Fe{sup 2+} ratio of 10:90 and a moderate firing temperature of 500 C. This sample exhibits a room temperature saturation magnetization of 58 emu/g as measured via vibrating sample magnetometry, comparable with bulk values and greater than that of confirmed nano-NZFOs found in the literature. EXAFS also indicates that in all cases in which the elements adopted a spinel structure, the nickel occupies only octahedral sites and the zinc primarily tetrahedral sites.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Quick extended x-ray absorption fine structure instrument with millisecond time scale, optimized for in situ applications

In order to learn about in situ structural changes in materials at subseconds time scale, we have further refined the techniques of quick extended x-ray absorption fine structure (QEXAFS) and quick x-ray absorption near edge structure (XANES) spectroscopies at beamline X18B at the National Synchrotron Light Source. The channel cut Si (111) monochromator oscillation is driven through a tangential arm at 5 Hz, using a cam, dc motor, pulley, and belt system. The rubber belt between the motor and the cam damps the mechanical noise. EXAFS scan taken in 100 ms is comparable to standard data. The angle and the angular range of the monochromator can be changed to collect a full EXAFS or XANES spectrum in the energy range 4.7-40.0 KeV. The data are recorded in ascending and descending order of energy, on the fly, without any loss of beam time. The QEXAFS mechanical system is outside the vacuum system, and therefore changing the mode of operation from conventional to QEXAFS takes only a few minutes. This instrument allows the acquisition of time resolved data in a variety of systems relevant to electrochemical, photochemical, catalytic, materials, and environmental sciences.

43 PARTICLE ACCELERATORS↗

Effects of annealing on the local structure of FE and Co in CoFeB/MgO/CoFeB tunnel junctions: An extended x-ray absorption fine structure study

Extended x-ray-absorption fine structure (EXAFS) was used to study the evolution of the local structure of Fe and Co as a function of annealing time in CoFeB/MgO/CoFeB magnetic tunnel junctions. EXAFS indicates B depletion and crystallization of the CoFeB layers within a few seconds of the post growth high temperature anneal. The decrease in first-shell Debye-Waller factor and hence the increase in structural order during annealing explains the increase in tunnel magnetoresistance observed as a result of post deposition annealing.

36 MATERIALS SCIENCE↗

The dedicated QEXAFS facility at the SLS: Performance and Scientific Opportunities

The SuperXAS beamline at the Swiss Light Source (SLS) features a permanently installed monochromator for quick scanning EXAFS (QEXAFS) spectroscopy in series with a conventional double crystal monochromator (DCM). All installed optical components like collimating and focussing mirrors can be used by both devices. The remote exchange of the monochromators is possible in less than five minutes while maintaining the beam geometry on the sample. The QEXAFS system allows fast absorption scans down to the millisecond range for the investigation of time dependent processes. Using a Si(111) channel cut crystal the energy range from 5-16 keV can be covered, with a Si(311) cut the range 9.5-30 keV. Usually a quick scanning interval of 0.1 deg. - 2 deg. in Bragg angle is selected, thus covering XANES, full EXAFS or multiple edge scans of e.g. all L-edges of a heavy element. Up to about 80 spectra per second can be collected, corresponding to a time resolution of 12.5 ms. The high intensity of the beamline even facilitates fluorescence measurements on dilute samples.

43 PARTICLE ACCELERATORS↗

Cadmium Chemical Form in Mine Waste Materials by X-ray Absorption Spectroscopy

This study examines the molecular form of cadmium (Cd) present in mine wastes by X-ray Absorption Spectroscopy (XAS; Cd>20 mg/kg) using the K-edge of Cd at the Photon Factory Advanced Ring (PF-AR), NW10A beam line at KEK-Tsukuba-Japan. Mine waste materials and zinc concentrate were analyzed for Cd by ICPMS prior to undertaking XAS (range 21-452 mg/kg). Model compounds (CdO, Cd(OH){sub 2}, CdCO{sub 3}, Cdacetate, CdS, Cdstearate, CdDEDTC) and samples were examined in solid form at 20 K. The XANES spectra showed similar E max values for both model compounds and samples. The EXAFS showed that Cd-S in CdS, gives a flatter spectrum in the extended region compared to Cd-O found with CdCO{sub 3}, CdO and Cd Stearate. Linear combination fitting with model Cd compounds did not give clear assignments of composition, indicating that more detailed EXAFS spectra is required as mineral forms containing Cd were present rather than simple Cd compounds such as CdCO{sub 3}. The Cd bond for a single shell model in mine waste sample matrices appears to be either Cd-O or Cd-S, or a combination of both. Comparison of molecular data from the XAS studies with bioaccessibility data giving a prediction of bioavailability for mine waste materials provides useful information about the significance of the cadmium form as a contaminant for health risk assessment purposes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A wavelet analysis for the X-ray absorption spectra of molecules

We present a Wavelet transform analysis for the X-ray absorption spectra of molecules. In contrast to the traditionally used Fourier transform approach, this analysis yields a 2D correlation plot in both R- and k-space. As a consequence, it is possible to distinguish between different scattering pathways at the same distance from the absorbing atom and between the contributions of single and multiple scattering events, making an unambiguous assignment of the fine structure oscillations for complex systems possible. We apply this to two previously studied transition metal complexes, namely iron hexacyanide in both its ferric and ferrous form, and a rhenium diimine complex, [ReX(CO){sub 3}(bpy)], where X = Br, Cl, or ethyl pyridine (Etpy). Our results demonstrate the potential advantages of using this approach and they highlight the importance of multiple scattering, and specifically the focusing phenomenon to the extended X-ray absorption fine structure (EXAFS) spectra of these complexes. We also shed light on the low sensitivity of the EXAFS spectrum to the Re-X scattering pathway.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Local structure of amorphous GaN{sub 1-x}As{sub x} semiconductor alloys across the composition range

Typically only dilute (up to {approx}10%) highly mismatched alloys can be grown due to the large differences in atomic size and electronegativity of the host and the alloying elements. We have overcome the miscibility gap of the GaN{sub 1-x}As{sub x} system using low temperature molecular beam epitaxy. In the intermediate composition range (0.10 < x < 0.75), the resulting alloys are amorphous. To gain a better understanding of the amorphous structure, the local environment of the As and Ga atoms was investigated using extended x-ray absorption fine structure (EXAFS). The EXAFS analysis shows a high concentration of dangling bonds compared to the crystalline binary endpoint compounds of the alloy system. The disorder parameter was larger for amorphous films compared to crystalline references, but comparable with other amorphous semiconductors. By examining the Ga local environment, the dangling bond density and disorder associated with As-related and N-related bonds could be decoupled. The N-related bonds had a lower dangling bond density and lower disorder.

36 MATERIALS SCIENCE↗

A platform for x-ray absorption fine structure study of dynamically compressed materials above 1 Mbar [A platform for XAFS study of dynamically compressed materials above 1 Mbar]

Here, a platform consisting of a multi-shock drive and an implosion backlighter has been developed for x-ray absorption fine structure (XAFS) measurements on materials compressed to multi-Mbar pressures. The experimental setup, target design, and backlighter characteristics are presented. Extended XAFS (EXAFS) measurements for various materials have been demonstrated. A quintuple-crystal design is described to enhance the efficiency of the x-ray spectrometer, enabling observation of very weak EXAFS signals in a single shot.

47 OTHER INSTRUMENTATION↗

Enhanced Jahn-Teller response induced by low-dose 10 MeV I{sup +} irradiation of La{sub 0.7}Ca{sub 0.3}MnO{sub 3−δ} films

The structural response of pulsed laser deposited La{sub 0.7}Ca{sub 0.3}Mn0{sub 3−δ} films to low-level 10 MeV I{sup +} irradiation is correlated with magnetic and electronic properties. A series of annealed pulsed laser deposited films were subjected to ion irradiation at doses of 0.5–2.0 × 10{sup 13} 10 MeV iodine ions/cm{sup 2}. X-ray diffraction measurements show no measurable increase in the full width at half maximum values of major reflections before and after irradiation. Extended x-ray absorption fine structure analyses (EXAFS), employing both a model independent fitting using expanded cumulants as well as a nonlinear least squares multiple scattering model based on FEFF generated theoretical EXAFS data, were employed to measure local properties relative to the Mn ions. Increasing irradiation doses lead to an unambiguous evolution of MnO{sub 6} octahedra from highly symmetric (i.e., undistorted) to a clear bimodal structure in which the MnO{sub 6} octahedra are measured to undergo a c-axis stretching bearing resemblance to a Jahn-Teller distortion. Concomitantly, the metal to insulator transition temperature decreases more than 270 K and the magnetoresistance increases from 10{sup 2}% to 10{sup 6}%.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Unraveling halide hydration: A high dilution approach

The hydration properties of halide aqua ions have been investigated combining classical Molecular Dynamics (MD) with Extended X-ray Absorption Fine Structure (EXAFS) spectroscopy. Three halide-water interaction potentials recently developed [M. M. Reif and P. H. Hünenberger, J. Chem. Phys. 134, 144104 (2011)], along with three plausible choices for the value of the absolute hydration free energy of the proton (ΔG{sub hyd}{sup ⊖}[H{sup +}]), have been checked for their capability to properly describe the structural properties of halide aqueous solutions, by comparing the MD structural results with EXAFS experimental data. A very good agreement between theory and experiment has been obtained with one parameter set, namely L{sub E}, thus strengthening preliminary evidences for a ΔG{sub hyd}{sup ⊖}[H{sup +}] value of −1100 kJ mol{sup −1} [M. M. Reif and P. H. Hünenberger, J. Chem. Phys. 134, 144104 (2011)]. The Cl{sup −}, Br{sup −}, and I{sup −} ions have been found to form an unstructured and disordered first hydration shell in aqueous solution, with a broad distribution of instantaneous coordination numbers. Conversely, the F{sup −} ion shows more ordered and defined first solvation shell, with only two statistically relevant coordination geometries (six and sevenfold complexes). Our thorough investigation on the effect of halide ions on the microscopic structure of water highlights that the perturbation induced by the Cl{sup −}, Br{sup −}, and I{sup −} ions does not extend beyond the ion first hydration shell, and the structure of water in the F{sup −} second shell is also substantially unaffected by the ion.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗