Search NASA⌕ Search

SEARCH · Search NASA

Results for “POLISHING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 451 records · Page 25

Characterization of material surfaces exposed to atomic oxygen on space shuttle missions

Material samples prepared for exposure to ambient atomic oxygen encountered during space shuttle flights in low Earth orbit were characterized by the experimental techniques of ELLIPSOMETRY, ESCA, PIXE, and RBS. The first group of samples, which were exposed during the STS-8 mission, exhibited some very interesting results. The second group of samples, which are to be exposed during the upcoming STS-17 mission, have been especially prepared to yield quantitative information on the optical changes, oxygen solution, and surface layer formation on metal films of silver, gold, nickel, chromium, aluminum, platinum, and palladium evaporated onto optically polished silicon wafers.

Fromhold, A. T.↗

Antarctic Meteorite Newsletter, volume 8, number 1

Preliminary descriptions and classifications of meteorites examined since the July 1984 newsletter are presented. Each macroscopic description summarizes features that were visible to the eye (with, at most, 50X magnification). Each thin section description represents features that were found in a survey-level examination of a polished thin section that was prepared from a small (usually extrior) chip of the meteorite. Classification is based on microscopic petrography and reconnaissance-level electron-probe microanalyses.

Source record↗

Effects of High Mean Stress on High-cycle Fatigue Behavior of PWA 1480

PWA 1480 is a potential candidate material for use in the high-pressure fuel turbine blade of the space shuttle main engine. As an engine material it will be subjected to high-cycle fatigue loading superimposed on a high mean stress due to combined centrifugal and thermal loadings. The present paper describes the results obtained in an ongoing program at the Argonne National Laboratory, sponsored by NASA Lewis, to determine the effects of a high mean stress on the high-cycle fatigue behavior of this material. Straight-gauge high-cycle fatigue specimens, 0.2 inch in diameter and with the specimen axis in the 001 direction, were supplied by NASA Lewis. The nominal room temperature yield and ultimate strength of the material were 146 and 154 ksi, respectively. Each specimen was polished with 1-micron diamond paste prior to testing. However, the surface of each specimen contained many pores, some of which were as large as 50 micron. In the initial tests, specimens were subjected to axial-strain-controlled cycles. However, very little cyclic plasticity was observed.

Majumdar, S.↗

Fracture behavior in silicon

The fracture mechanics of crystalline Si are reviewed, together with known techniques for minimizing the occurences of fracture and/or their effects. The fracture toughness (Kic) of Si varies only 10 percent from cell-to-cell and standard values have been established for different types of crystalline Si cells. A critical flaw size of 10-100 microns has been identified, and also pertains to polycrystalline materials. Chemical polishing is known to double the value of Kic, while edge rounding has no effect. Internal stresses, particularly those caused during ribbon growth, do not exceed 10 percent of Kic. External stresses are imposed by the module hardware and the ambient environment. Multiple contacts reduce the effects of cell fracture and series-parallel wiring in modules in arrays ameliorates the effects of single-cell failures. During manufacturing, maintenance of quality control and removal of sheets displaying aberrations can, depending on the costs and the implementation of the array reliability features, result in arrays delivering any desired level of reliability.

Leipold, M. H.↗

Wetting layers and dispersion forces for a fluid in contact with a vertical wall

Ellipsometric measurements of the thickness of the wetting layer of sulfur hexafluoride that forms on a fused-silica surface partially immersed in the liquid are presented. The components of the experiment included a He-Ne laser (0.6328 micron), polarizer, and quarter-wave plate with 45-deg azimuth. An optical-grade fused-silica prism was polished to wavelength/20, and strain-induced birefringence was accounted for. It was found that the layer thickness decreases from 40 to 20 nm with a height increase from 0.7 to 3 mm above the liquid-vapor interface. The thickness is independent of the temperature between 10 and 0.1 K below the critical temperature (319 K). The results are compared in detail to the theory of Dzyaloshinskii et al. (1961), and are noted to coincide closely.

Kayser, R. F.↗

Design and technology considerations for the far ultraviolet spectroscopic explorer (FUSE) telescope

An initial assessment of telescope designs satisfying the basic requirements derived for the FUSE mission is presented. A review of recent optical coating technology indicates that normal incidence telescope designs are viable only for wavelengths greater than about 600 A. It is noted that glancing incidence telescope designs, such as the Wolter Type II or thg Wolter-Schwarzschild, are the only designs with acceptable throughputs for the entire FUSE spectral range. Initial design trade studies have established the fundamental framework for the selection of an optimum Type II design satisfying the FUSE science and engineering requirements. It is also found that current optical fabrication technology, e.g., computer controlled polishing, can accommodate meter class glancing incidence components with figure errors commensurate with 1-2 arcsec imaging.

Davila, P. S. M.↗

Chemical reactions involved in the initiation of hot corrosion of IN-738

Sodium-sulfate-induced hot corrosion of preoxidized IN-738 was studied at 975 C with special emphasis placed on the processes occurring during the long induction period. Thermogravimetric tests were run for predetermined periods of time, and then one set of specimens was washed with water. Chemical analysis of the wash solutions yielded information about water soluble metal salts and residual sulfate. A second set of samples was cross sectioned dry and polished in a nonaqueous medium. Element distributions within the oxide scale were obtained from electron microprobe X-ray micrographs. Evolution of SO was monitored throughout the thermogravimetric tests. Kinetic rate studies were performed for several pertinent processes; appropriate rate constants were obtained from the following chemical reactions; Cr203 + 2 Na2S04(1) + 3/2 02 yields 2 Na2Cr04(1) + 2 S03(g)n TiO2 + Na2S04(1) yields Na20(T102)n + 503(g)n T102 + Na2Cro4(1) yields Na2(T102)n + Cr03(g).

Fryburg, G. C.↗

Microscopic evaluation of a polyimide (PMR-15)-graphite composite

An effort to evaluate the high temperature performance of a polyimide (PMR-15)-graphite composite which consists of several plies of woven strands of carbon fibers was undertaken. The longterm effect of high temperature on the dry material was studied by exposing polished test specimens of 473 F in a oven for nearly 400 hours. Periodically the specimens were removed and observed microscopically. Gradually surface cracks began to appear and the number of cracks increased over time. At the conclusion of the exposure the specimens were graudually ground down and observed in order to determine the depth of the cracks into the interior of the material. This procedure was repeated at an exposure temperature of 550 F.

Fedderly, J. J.↗

Electron microscopic observations of hydrogen implantation in ilmenites

Hydrogen ion beams were found to form submicrometer, bumpy textures on the surface of ilmenite grains. From this effect, it is believed that similar bumpy textures seen on lunar ilmenite, pyroxene, and olivine grains are likely to be caused by solar wind irradiation. As a consequence, the concentration of bumpy textured grains may be a useful index of surface maturity for lunar soils. An attempt was made to search for grains with these bumpy textures in interplanetary dust and lunar and meteoritic regolith breccias in order to obtain information about the duration of their exposure to the solar wind. Solar wind irradiation was simulated on natural, terrestrial ilmenite. Hydrogen ion beams were directed at small grains and polished sections which were then examined by electron microscopy.

Blanford, G. E.↗

Growth of high-quality thin-film Ge single crystals by plasma-enhanced chemical vapor deposition

Thin-film Ge single crystals (approx. 10 microns) have been epitaxially grown on polished NaCl(100) substrates at 450C by using plasma-enhanced chemical vapor deposition. Films on approximately 1 sq cm and larger were separated from the NaCl by either melting the salt or by differential shear stress upon cooling to room temperature. The ordered growth of the Ge was found to be most sensitive to the initial plasma power and to the continuum flow dynamics within the carbon susceptor. The films were visually specular and exhibited a high degree of crysalline order when examined by X-ray diffraction. The films were found to be p-type with a carrier concentration of approximately 3 x 10 to the 16th power/cu cm, a resistivity of 0.11 ohm-cm, and a Hall hole mobility of 1820 sq cm/v/s at room temperature. Vacuum firing minimized the primary contaminant, Na, and corresponding lowered the carrier concentration to 4 x 10 to the 14th power/cu cm.

Outlaw, R. A.↗

Characterization of the tribological coating composition 77 wt % CaF2 - 23 wt % Li F fused to IN-750 alloy

A coating composed of 77 wt % CaF2 - 23 wt % LiF fused on IN-750 nickel-based alloy was studied using SEM, XRD, EDX, and optical microscopic methods. The surfaces examined were the as-fused coating with no subsequent treatment, the coating after ultrasonic cleaning in water, and the uncoated polished and etched metal. It was found that the coating reacts during fusion with Ti and Nb rich inclusions in the alloy. Numerous small rectangular crystallites of Ca(Ti,Nb) oxide are formed beneath an overlay of fused fluoride composition. These crystallines are stubby and appear to be embedded in the metal substrate surface. It is known from previous studies that this coating-alloy system has good tribological properties in extreme conditions, such as liquid fluorine. It has been concluded from the present study that the short firmly embedded crystalline protuberances contribute to the coating adherence and thereby to enhanced coating wear life.

Deadmore, D. L.↗

Excimer laser annealing for fabrication of low-cost solar cells

Pulsed excimer laser annealing was successfully performed using a 50 w laser. Both polished and texturized cells were tried, however, there are serious problems with nonuniformity on texturized cells. A number of cells were produced and compared to diffusion furnace annealed cells. There was no clear economic advantage in using an excimer laser and there was a small penalty on average efficiency. The conclusion was that the excimer laser anneal process must be able to produce superior cells to be considered as a viable process option.

Spitzer, M. B.↗

Phosphate-sulfide assemblages and Al/Ca ratios in type-3 chondrites

Electron microscopic examinations were carried out on various chondrites to re-examine previously reported anomalously high Al/Ca ratios. Polished thin sections of the three CV3, two CO3 and the Krymka LL3 chondrites were scanned to characterize the phosphate-sulfide inclusions. The formation of the assemblages was interpreted as proceeding in five steps, starting with the formation of metal grains with early nebular material and finishing with a reaction between schreibersite with Ca, O and Cl to form merrillite and chloropatite. The abundances of the observed assemblages were not high enough to imply Al/Ca ratios similar to whole-rocks. It is concluded that the specimens were originally examined with a broader electron beam than used to examine standard samples, and resulted in the anomalously high Al/Ca ratios.

Rubin, A. E.↗

APART/PADE analytical evaluation of the diffuse infrared background experiment for NASA's cosmic background explorer

The stray light performance of NASA's Diffuse Infrared Background Experiment (DIRBE) has been calculated using the APART/PADE code. That code has been upgraded to handle off-axis optical systems such as DIRBE. Under observing conditions, sunlight is attenuated by 21 to 29 orders-of-magnitude; uniform diffuse illumination, by 6 to 9 orders of magnitude. The sunlight is attenuated by multiple diffraction at an external sun shield and by a forebaffle at the entrance to the DIRBE. Stray light is nearly a linear function of the Bidirectional Reflectance Distribution Function (BRDF) of the primary mirror at all wavelengths - or it can be made to be so by reducing the size of the field defining stop from 0.866 to 0.7 degrees square. For uniform diffuse illumination, half of the stray radiation comes from within 5 degrees of the center of the field-of-view. Particulate contamination of the primary mirror is expected to be a problem and special polishing and cleaning procedures are recommended - before mirror overcoating and again before flight.

Evans, D. C.↗

Optical and interfacial electronic properties of diamond-like carbon films

Hard, semitransparent carbon films were prepared on oriented polished crystal wafers of silicon, indium phosphide and gallium arsenide, as well as on KBr and quartz. Properties of the films were determined using IR and visible absorption spectrocopy, ellipsometry, conductance-capacitance spectroscopy and alpha particle-proton recoil spectroscopy. Preparation techniques include RF plasma decomposition of methane (and other hydrocarbons), ion beam sputtering, and dual-ion-beam sputter deposition. Optical energy band gaps as large as 2.7 eV and extinction coefficients lower than 0.1 at long wavelengths are found. Electronic state densities at the interface with silicon as low as 10 to the 10th states/eV sq cm per were found.

Woollam, J. A.↗

Properties of the Guin ungrouped iron meteorite - The origin of Guin and of group-IIE irons

The composition and structure of the Guin ungrouped iron meteorite inclusions have been investigated experimentally. The structural characteristics of polished and etched slabs of the meteorite were studied microscopically in reflected light. Modal abundances of troilite nodules and silicate inclusions were determined by weighing paper traces. The bulk composition of the silicate inclusions was calculated by combining modal phase abundances and mineral compositions. It is found that the largest silicate inclusion (2 x 4 cm) consists mostly of a shock-melted plagioclase-rich matrix surrounding large, partly melted augite grains. The oxygen isotopic composition of the inclusion is near that of LL chondrites. The inclusion is found to be similar in composition to selected melt pocket glasses in ordinary chondrites produced in situ by preferential melting of plagioclase rock due to shock compression. It is suggested that the Guin assemblage was formed by impact melting on a chondritic parent body. Silicate inclusions in IIE irons share many of the compositional and petrological characteristics of the Guin inclusions, indicating that IIE irons also formed by impact-melting of chondritic materials. Black and white photomicrographs of the silicate inclusions are provided.

Rubin, A. E.↗

Evidence for successive episodes of condensation at high temperature in a part of the solar nebula

A polished thin section of a Ca-Al-rich inclusion CAI 3643 from the Allende meteorite has been studied by means of light and scanning electron microscopes, and electron and proton microprobes. The appearance and the mineral composition of the inclusion's three concentric layers: core, mantle, and crust are described. Despite differences in texture and composition, the three layers display a continuity in their modal mineralogical compositions, their extreme Al2O3 enrichments (53-69 percent, compared to 25-45 percent in other CAIs), and their trace element complementarity. This implies that all the layers of CAI 3643 have formed from the same cooling gaseous reservoir within a limited interval of time and space, consistent with an origin in a local transient heating event in the CV chondrite formation region of the nebula.

Wark, D. A.↗

Mapping of carbon concentrations in the Allende meteorite with the C-12(d,p)C-13 method

Carbon concentrations in a 4.2 x 4.2 mm area of the Allende meteorite were mapped with the C-12(d,p)C-13 nuclear method. The x,y resolution perpendicular to the deuteron beam was 65 microns; the depth resolution was 0.6 micron. The matrix of the meteorite contains about 1 wt pct carbon, which is uniformly distributed at the 65-micron level of resolution. The matrix contains most, perhaps close to all, C of this meteorite. The coarse-grained constituents, such as chondrules, show a very strong enhancement of C in the depth range 2 to about 0 micron; the matrix does not show this enhancement. The enhancement may be due to contamination of the coarse-grained areas or else to migration of C in solid solution from the interiors of comparatively large crystals to their freshly polished surfaces.

Van Der Stap, C. A. H.↗